The aim of this work is to report on the luminescence properties of BaZnSiO4 activated by Eu3+ and Mn2+ ions. Doped and undoped powder samples were prepared by solid-state reaction starting from oxides and carbonates or Ba2SiO4:Eu3+ and Zn2SiO4:Mn2+ precursors. X-ray diffraction powder data, IR vibrational, and UV-vis luminescence spectroscopies were carried out. Results showed that doped and undoped samples from both types of precursors have the same structure and crystallize with a superstructure of hexagonal kalsilite. Vibrational spectroscopy has confirmed the formation of a silicate group, which outlines differences between products and silicate precursors. The observed luminescence assigned to Eu3+ and Mn2+ transitions covered most parts of the visible spectrum, an important requirement for phosphors in fluorescent low-pressure mercury vapor lamps.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

One-dimensional Mn2+-doped Zn2SiO4 rnicrobelts and microfibers were prepared by a simple and cost-effective electrospinning process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), scanning electron microscopy (SEM), energy-dispersive X-ray spectrum (EDS), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL), and cathodoluminescence (CL) spectra as well as kinetic decays were used to characterize the samples. The XRD and DTA results show that the Zn2SiO4 phase begins to crystallize at 800 degrees C and crystallizes completely around 1000 degrees C. SEM results indicate that the as-prepared microbelts/fibers are smooth, whose diameters decrease with increasing the annealing temperature. The average diameter of the Zn2SiO4:Mn2+ microfibers annealed at 1000 degrees C is 0.32 mu m, and their lengths reach up to several millimeters. The average width and thickness of the Zn2SiO4:Mn2+ microbelts fired at 1000 degrees C are around 0.48 and 0.24 mu m, respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The synthesis and luminescence properties of Zn2SiO4:Mn phosphor layers on spherical silica spheres,i.e.,a kind of core-shell complex phosphor,Zn2SiO4:Mn@SiO2 were described.Firstly,monodisperse silica spheres were obtained via the Stober method by the hydrolysis of tetraethoxysilane(TEOS)Si(OC2H5)4 under base condition (using NH4OH as the catalyst).Secondly,the silica spheres were coated with a Zn2SiO4:Mn phosphor layer by a Pechini sol-gel process.X-ray diffraction(XRD),scanning electron microscope(SEM),energy-dispersive X-ray spectrum(EDS) and photoluminescence(PL) were employed to characterize the resulting complex phosphor.The results comfirm that 1000℃ annealed sample consists of crystalline Zn2SiO4:Mn shells and amorphous SiO2 cores.The phosphor show the green emission of Mn2+ at 521nm corresponding 4T1(4G)-6A1(6S) transition,and the possible luminescence mechanism is proposed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A ~si MAS NMR study of spin-lattice relaxation behaviour in paramagnetic-doped crystalline silicates was undertaken, using synthetic magnesium orthosilicate (forsterite) and synthetic zinc orthosilicate (willemite) doped with 0.1% to 20% of Co(II), Ni(II), or CU(II), as experimental systems. All of the samples studied exhibited a longitudinal magnetization return to the Boltzmann distribution of nuclear spin states which followed a stretched-exponential function of time: Y=exp [- (tjTn) n], O

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective: To determine the effect of zinc supplementation on taste perception in a group of hemodialysis patients. Design and Setting: Double-blind randomized placebo-controlled study in a teaching hospital dialysis unit. Patients: Fifteen stable hemodialysis patients randomized to placebo (6 male, 2 female; median age, 67; range, 30 to 72 years) or treatment (5 male, 2 female; median age, 60; range, 31 to 76 years). Intervention: Treatment group received zinc sulfate 220 mg per day for 6 weeks, and the placebo group received an apparently identical dummy pill. Main Outcome Measures: Taste scores by visual analogue scales, normalized protein catabolic rate and plasma, whole blood and red cell zinc levels. Results: At baseline, sweet and salt tastes were identified correctly by both groups. Sour was often confused with salt. Sour solutions of different concentrations were not distinguishable. Taste scores were not different after 6 weeks for either group. There was no significant increment in zinc levels or normalized protein catabolic rate for either group. Conclusion: We found a disturbance of taste perception in hemodialysis patients, particularly for the sour modality, which was not corrected by this regimen of zinc supplementation. These results cast doubts on the conclusions of earlier studies that indicated an improvement in taste after zinc supplementation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The NIR spectra of reichenbachite, scholzite and parascholzite have been studied at 298 K. The spectra of the minerals are different, in line with composition and crystal structural variations. Cation substitution effects are significant in their electronic spectra and three distinctly different electronic transition bands are observed in the near-infrared spectra at high wavenumbers in the 12000-7600 cm-1 spectral region. Reichenbachite electronic spectrum is characterised by Cu(II) transition bands at 9755 and 7520 cm-1. A broad spectral feature observed for ferrous ion in the 12000-9000 cm-1 region both in scholzite and parascholzite. Some what similarities in the vibrational spectra of the three phosphate minerals are observed particularly in the OH stretching region. The observation of strong band at 5090 cm-1 indicates strong hydrogen bonding in the structure of the dimorphs, scholzite and parascholzite. The three phosphates exhibit overlapping bands in the 4800-4000 cm-1 region resulting from the combinations of vibrational modes of (PO4)3- units.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the structure of title compound [ZnI2(C12H10N2O2)2] from the reaction of 4-(4-nitrobenzyl)pyridine with zinc(II) iodide, the asymmetric unit contains two independent discrete distorted tetrahedral complex units [Zn-I range, 2.5472(8)-2.5666(7)A; Zn-N range, 2.044(4)-2.052(4)A], which are essentially identical conformationally and exist in the crystal structure as a racemic twin.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Raman spectra of two well-defined types of koritnigite crystals from the Jáchymov ore district, Czech Republic, were recorded and interpreted. No substantial differences were observed between both crystal types. Observed Raman bands were attributed to the (AsO3OH)2- stretching and bending vibrations, stretching and bending vibrations of water molecules and hydroxyl ions. Non-interpreted Raman spectra of koritnigite from the RRUFF database, and published infrared spectra of cobaltkoritnigite were used for comparison. The O-H...O hydrogen bond lengths in the crystal structure of koritnigite were inferred from the Raman spectra and compared with those derived from the X-ray single crystal refinement. The presence of (AsO3OH)2- units in the crystal structure of koritnigite was proved from the Raman spectra which supports the conclusions of the X-ray structure analysis.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Insight into the unique structure of hydrotalcites (HTs) has been obtained using Raman spectroscopy. Gallium-contg. HTs of formula Zn4 Ga2(CO3)(OH)12 · xH2O (2:1 ZnGa-HT), Zn6 Ga2(CO3)(OH)16 · xH2O (3:1 ZnGa-HT) and Zn8 Ga2(CO3)(OH)18 · xH2O (4:1 ZnGa-HT) have been successfully synthesized and characterised by X-ray diffraction (XRD) and Raman spectroscopy. The d(003) spacing varies from 7.62 Å for the 2:1 ZnGa-HT to 7.64 Å for the 3:1 ZnGa-HT. The 4:1 ZnGa-HT showed a decrease in the d(003) spacing, compared to the 2:1 and 3:1 compds. Raman spectroscopy complemented with selected IR data has been used to characterize the synthesized gallium-contg. HTs. Raman bands obsd. at around 1050, 1060 and 1067 cm-1 are attributed to the sym. stretching modes of the (CO32-) units. Multiple ν3 (CO32-) antisym. stretching modes are found between 1350 and 1520 cm-1, confirming multiple carbonate species in the HT structure. The splitting of this mode indicates that the carbonate anion is in a perturbed state. Raman bands obsd. at 710 and 717 cm-1 and assigned to the ν4 (CO32-) modes support the concept of multiple carbonate species in the interlayer.