Resumo:
Four nickel carbonate-bearing minerals from Australia have been investigated to study the effect of Ni for Mg substitution. The spectra of nullaginite, zaratite, widgiemoolthalite and takovite show three main features in the range of 26,720–25,855 cm−1 (ν1-band), 15,230–14,740 cm−1 (ν2-band) and 9,200–9,145 cm−1 (ν3-band) which are characteristic of divalent nickel in six-fold coordination. The Crystal Field Stabilization Energy (CFSE) of Ni2+ in the four carbonates is calculated from the observed 3A2g(3F) → 3T2g(3F) transition. CFSE is dependent on mineralogy, crystallinity and chemical composition (Al/Mg-content). The splitting of the ν1- and ν3-bands and non-Gaussian shape of ν3-band in the minerals are the effects of Ni-site distortion from regular octahedral. The effect of structural cation substitutions (Mg2+, Ni2+, Fe2+ and trivalent cations, Al3+, Fe3+) in the carbonate minerals is noticed on band shifts. Thus, electronic bands in the UV–Vis–NIR spectra and the overtones and combination bands of OH and carbonate ion in NIR show shifts to higher wavenumbers, particularly for widgiemoolthalite and takovite.
Resumo:
The reactions of pyrrole and thiophene monomers in copper-exchanged mordenite have been investigated using EPR and UV–VIS absorption spectroscopy. The EPR spectra show a decrease in the intensity of the Cu2+ signal and the appearance of a radical signal due to the formation of oxidatively coupled oligomeric and/or polymeric species in the zeolite host. The reaction ceases when ca. 50% of the copper has reacted and differences in the form of the residual Cu2+ signal between the thiophene and pyrrole reactions suggest a greater degree of penetration of the reaction into the zeolite host for pyrrole, in agreement with previous XPS measurements. The EPR signal intensities show that the average length of the polymer chain that is associated with each radical centre is 15–20 and 5–7 monomer units for polypyrrole and polythiophene, respectively. The widths of the EPR signals suggest that these are at least partly due to small oligomers. The UV–VIS absorption spectra of the thiophene system show bands in three main regions: 2.8–3.0 eV (A), 2.3 eV (B) and 1.6–1.9 eV (D, E, F). Bands A and D–F occur in regions which have previously been observed for small oligomers, 4–6 monomer units in length. Band B is assigned to longer chain polythiophene molecules. We therefore conclude that the reaction between thiophene and copper-loaded mordenite produces a mixture of short oligomers together with some long chain polythiophene. The UV–VIS spectra of the pyrrole system show bands in the regions 3.6 eV (A), 2.7–3.0 eV (B, C) and 1.5–1.9 eV (D, F). Assignments of these bands are less certain than for the thiophene case because of the lack of literature data on the spectra of pyrrole oligomers.
Resumo:
The present investigation explores the adaptability of a microwave assisted route to obtain silver nanoparticles by the reduction of AgNO3 with vanillin, an environmentally benign material. Anionic surfactants such as AOT and SDS were used separately for encapsulating AgNPs and their role was compared. The UV-Visible absorption spectra present a broad SPR band consisting of two peaks suggesting the formation of silver nanoparticle with bimodal size distribution. The TEM image shows particles with spherical and hexagonal morphologies which confirms the results of UV-Vis studies. The anisotropy in the particle morphology can be attributed to the surface oxidation which in turn produces Ag@Ag2O core-shell nanostructures. Thus an intriguing feature of this system is that the obtained colloid is a mixture of AgNPs with and without Ag2O layers. Studies on the influence of pH on the stability of the synthesized nanoparticles revealed that the presence of excess Ag2O layers has a profound influence on it. Ag2O layers can be removed from AgNPs' surface by changing the solution pH to the acidic regime. The present study attests the enhanced ability of AOT in stabilizing the AgNPs in aqueous media. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Recently, a lot of interest has been centred on the optical properties of hexagonal boron nitride (h-BN), which has a similar lattice structure to graphene. Interestingly, h-BN has a wide bandgap and is biocompatible, so it has potential applications in multiphoton bioimaging, if it can exhibit large nonlinear optical (NLO) properties. However, extensive investigation into the NLO properties of h-BN have not been done so far. Here, NLO properties of 2D h-BN nanosheets (BNNS) are reported for the first time, using 1064-nm NIR laser radiation with a pulse duration of 10 ns using the Z-scan technique. The reverse saturable absorption occurs in aqueous colloidal solutions of BNNS with a very large two-photon absorption cross section (sigma(2PA)) of approximate to 57 x 10(-46) cm(4) s(-1) photon(-1). Also, by using UV-Vis absorption spectroscopy, the temperature coefficient of the bandgap (dE(g)/dT) of BNNS is determined to be 5.9 meV K-1. Further defect-induced photoluminescence emission in the UV region is obtained in the 283-303 K temperature range, under excitations of different wavelengths. The present report of large sigma(2PA) combined with stability and biocompatibility could open up new possibilities for the application of BNNS as a potential optical material for multiphoton bioimaging and advanced photonic devices.
Resumo:
Sequentially spectrophotometric titrations by sodium hydroxide of meso-tetraphenylporphyrin derivatives bearing one, two, three, or four p-hydroxyl groups result in new types of spectra. The strong new bands appear in the visible region with splitting or broadening of the Soret band and its significant loss of oscillator strength. To understand the molecular origin of these phenomena, the Resonance Raman (RR) and Fourier Transform Infrared (FTIR) experiments are carried out. The results demonstrate that the charges of the deprotonated para-hydroxy substituted meso-tetraphenylporphyrins are localized on the substituents, not delocalized into the pi system of the porphyrin macrocycles and that the ground states of the macrocycles remain essentially unperturbed. Both the related behavior of diprotonated tetrakis(p-(dimethylamino)phenyl) porphyrin and protonated Schiff base porphyrins show that the new bands considered as hyperporphyrin spectra are due to pi(phenoxide anion) --> pi*(porphyrin) transitions, where pi is an orbital on the phenoxide anion substitutent and pi* is a LUMO on the porphyrin.
Resumo:
Ultrathin multilayer films have been prepared by means of alternate adsorption of iron(Ill)-substituted heteropolytungstate anions and a cationic redox polymer on the 4-aminobenzoic acid modified glassy carbon electrode surface based on electrostatic layer-by-layer assembly. Cyclic voltammetry, electrochemical impedance spectroscopy and UV-Vis absorption spectrometry have been used to easily monitor the uniformity of thus-formed multilayer films. Especially, the electrochemical impedance spectroscopy is successfully used to monitor the multilayer deposition processes and is a very useful technique in the characterization of multilayer films because it provides valuable information about the interfacial impedance features. All these results reveal regular film growth with each layer adsorption. The resulting multilayer films can effectively catalyze the reduction of H2O2,NO2- and BrO3-.
Resumo:
After meso-tetra (alpha, alpha, alpha, alpha-O-phenylacetyl benzene)porphyrin combined with McAb 1F2, there was a significant hyperchromic effect, indicating that the combination of porphyrin and antibody is rigid and compact, aromatic amino acids exist at the combining sites of antigen in antibody. These aromatic amino acids are Trys and Trps, but the numbers of Trp are more than that found for Trys. The stochiometric ratio of porphyrin to 1F2 is 1:1, the disassociation constant was determined as(2.084+/-0.216) x 10(-10) mol/L by a method of fluorescence quenching, showing that both have a high affinity.
Resumo:
We have employed several techniques, including cyclic voltammetry, UV-Vis spectrometry, small-angle X-ray diffraction, X-ray photoelectron spectroscopy and electrochemical impedance spectroscopy, to characterize the formation processes and interfacial features of ultrathin multilayer films of silicotungstate and a cationic redox polymer on cysteamine-coated Au electrodes self-assembled monolayers. All of these techniques confirm that the multilayer films are built up stepwise as well as uniformly in a layer-by-layer fashion. In particular, the electrochemical impedance spectroscopy is successfully used to monitor the multilayer deposition processes. It has been proved that the electrochemical impedance spectroscopy is a very useful technique in characterization of multilayer films because it provides valuable information about the interfacial impedance features.
Resumo:
Fe2O3 sol with the particle diameter of 3-5 nm was flocculated by the addition of SDS, and the flocculate formed was redispersed by the further addition of that surfactant. Thus the surfactant bilayer was formed on the surface of Fe2O3. The emulsion polymerization of styrene (St) adsolubilized oil the surfactant adsorbed bilayer was carried out by initiator potassium persulfate (KPS). The UV-Vis and surface photovoltage spectra (SPS) indicate that the Fe2O3 particles were encapsulated in polystyrene(PSt) successfully.
Resumo:
Phenyl-capped trianiline and tetraaniline in the leucoemeraldine oxidation state were synthesized through a modified-pseudo-high-dilution technique. The chemical oxidation process of these compounds were studied by UV-Vis spectra. It was found that phenyl-capped trianiline in the leucoemeraldine oxidation state was oxidized to its EB form and then decomposed, Phenyl-capped tetraaniline was oxidized to its EB form and then to the pernigraniline oxidation state.
Resumo:
Phenyl-capped oligoanilines in the oxidized state and their salts (by camphor sulfonic acid, CSA) were comparatively studied by UV-Vis and NMR spectroscopy. The UV-Vis spectra revealed a similar electron transfer behaviour and similar structure in the tetraaniline to those in polyaniline. Upon formation of the salt, H-1 NMR CH peaks of the oligomers showed large shifts to lower fields. The longer the molecule of a oligomer is, the more the shift, indicating that the charge brought into the N atoms by the proton was redistributed over the whole molecule. The CH and quaternary carbon peak-shifts support the electron cloud motion route H -->C -->C -->N -->H. This is in agreement with the four ring BQ derivatives model.
Resumo:
Electrochemical redox behavior of noradrenaline in alkaline solution on a glassy carbon electrode has been investigated by in situ UV-vis and CD spectroelectrochemistry by using a long optical path thin-layer cell. The experimental data were processed by using a double logarithmic method of analysis together with nonlinear regression which confirmed that the first step in both the oxidation of noradrenaline and reduction of noradrenochrome is a two-electron irreversible process governed by an EE mechanism. The kinetic parameters of the electrode reactions, i.e., charge transfer coefficient and the number of electrons transferred, alpha(1)n(1) = 0.11 and alpha(2)n(2) = 0.23, formal potentials modified with kinetics, E-1(0') = 0.65 (+/- 0.01) V and E-2(0') = 0.72V and standard rate cnstants, k(1)(0) = 7.0(+/-0.5)x10(-5) cm s(-1), for the first and second steps in the oxidation process of noradrenaline, and similarly, alpha(1)n(1) = 0.33, alpha(2)n(2) = 0.58, E-1(0') = 0.37(+/-0.01) V, E-0' = -0.25 (+/-0.01) V and k(1)(0) approximate to k(2)(0) = 1.06 (+/-0.05)x10(-4) cm s(-1) for the first and second steps in the reduction process of noradrenochrome were also determined.