991 resultados para THERMAL DECOMPOSITION OF POLYMERIC PRECURSORS


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lead zir conyl oxalate hexahydrate (LZO) and lead titanyl zirconyl oxalate hydrate (LTZO) are prepared and characterized. Their thermal decompositions have been investigated by thermoanalytical and gas analysis techniques. The decomposition in air or oxygen has three steps — dehydration, decomposition of the oxalate to a carbonate and the decomposition of carbonate to PbZrO3. In non oxidising atmosphere, partial reduction of Pb(II) to Pb(0) takes place at the oxalate decomposition step. The formation of free metallic lead affects the stoichiometry of the intermediate carbonate and yields a mixture of Pb(Ti,Zr)O3 and ZrO2 as the final products. By maintaining oxidising atmosphere and low heating rate, direct preparation of stoichiometric, crystalline Pb(Ti,Zr)O3 at 550°C is possible from the corresponding oxalate precursor.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The present work investigates the influence of milling and calcination atmosphere on the thermal decomposition of SrTiO3 powder precursors. Both pure and neodymium-modified SrTiO3 samples were studied. Milling did not significantly influence numerical mass loss value, but reduced the number of decomposition steps, modifying the profiles of the TG and DTA curves. on the other hand, milling increases the amount of energy liberated by the system upon combustion of organic matter. It was also observed that the milling process, associated to the calcination in an oxygen atmosphere, considerably decreases the amount of organic matter and increases the final mass loss temperature.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This work aimed to develop plurimetallic electrocatalysts composed of Pt, Ru, Ni, and Sn supported on C by decomposition of polymeric precursors (DPP), at a constant metal: carbon ratio of 40:60 wt.%, for application in direct ethanol fuel cell (DEFC). The obtained nanoparticles were physico-chemically characterized by X-ray diffraction (XRD) and energy dispersive X-ray spectroscopy (EDX). XRD results revealed a face-centered cubic crystalline Pt with evidence that Ni, Ru, and Sn atoms were incorporated into the Pt structure. Electrochemical characterization of the nanoparticles was accomplished by cyclic voltammetry (CV) and chronoamperometry (CA) in slightly acidic medium (0.05 mol L-1 H2SO4), in the absence and presence of ethanol. Addition of Sn to PtRuNi/C catalysts significantly shifted the ethanol and CO onset potentials toward lower values, thus increasing the catalytic activity, especially for the quaternary composition Pt64Sn15Ru13Ni8/C. Electrolysis of ethanol solutions at 0.4 V vs. RHE allowed determination of acetaldehyde and acetic acid as the main reaction products. The presence of Ru in alloys promoted formation of acetic acid as the main product of ethanol oxidation. The Pt64Sn15Ru13Ni8/C catalyst displayed the best performance for DEFC.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This work aimed to develop plurimetallic electrocatalysts composed of Pt, Ru, Ni, and Sn supported on C by decomposition of polymeric precursors (DPP), at a constant metal:carbon ratio of 40:60 wt.%, for application in direct ethanol fuel cell (DEFC). The obtained nanoparticles were physico-chemically characterized by X-ray diffraction (XRD) and energy dispersive X-ray spectroscopy (EDX). XRD results revealed a face-centered cubic crystalline Pt with evidence that Ni, Ru, and Sn atoms were incorporated into the Pt structure. Electrochemical characterization of the nanoparticles was accomplished by cyclic voltammetry (CV) and chronoamperometry (CA) in slightly acidic medium (0.05 mol L-1 H2SO4), in the absence and presence of ethanol. Addition of Sn to PtRuNi/C catalysts significantly shifted the ethanol and CO onset potentials toward lower values, thus increasing the catalytic activity, especially for the quaternary composition Pt64Sn15Ru13Ni8/C. Electrolysis of ethanol solutions at 0.4 V vs. RHE allowed determination of acetaldehyde and acetic acid as the main reaction products. The presence of Ru in alloys promoted formation of acetic acid as the main product of ethanol oxidation. The Pt64Sn15Ru13Ni8/C catalyst displayed the best performance for DEFC.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influence of polymerization on the thermal decomposition of polymeric precursors and phase formation was investigated during synthesis of SrTiO3. The precipitation of polymeric precursor in acetone produced a more thermal stable precursor with lower weight loss during decomposition. This more stable precursor retarded the formation of the SrTiO3 phase. From thermal analysis, XRD and FT-IR the presence of an intermediate phase during decomposition of the precursors was observed. This is a mixed (Sr,Ti) carbonate phase with the proposed composition of Sr2Ti2O5.CO3. © 1995.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Crystalline PbTiO3 was obtained through the thermal decomposition of 8-hydroxyquinolinate of lead(II) and that of titanium(IV), which was monitored by TG/DTG/DTA under different atmospheric conditions and with varying heating rates. The compound was prepared from adding 8-hydroxyquinoline solution in the solution of metallic ions Pb(II):Ti(IV) (1:1) Linder constant stirring at 3degreesC, having the pH adjusted to 10. The results of these investigations show that different thermal behavior related to the precursor occurred and also the consequent formation of residues which have different crystallinities. No carbonate residues from the thermal decomposition could be determined by XRD and IR. Only PbTiO3 was observed and confirmed by DSC at 470degreesC, temperature lower than the tetragonal-cubic transition.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Different thermal treatments for the synthesis of BaTiO3 powder obtained through the Pechini method were studied. The synthesis of BaTiO3 starts at 150 °C by the thermal dehydration of organic precursors. The usual inevitable formation of barium carbonate during the thermal decomposition of the precursor could be retarded at lower calcination temperatures and optimized heating rates. The organic precursors were treated at temperatures between 200 and 400 °C. Then, the samples were calcined at 700 and 800 °C for 4 and 2 h, respectively. The resulting ceramic powders were characterized by gravimetric and differential thermal analyses, X-ray powder diffraction and infrared spectroscopy. It was found that depending on the heating rate and final temperature of the thermal treatment, high amounts of BaCO3 and TiO2 could be present due to the high concentration of organics in the final calcination step. © 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The Polymeric Precursor Method has proved suitable for synthesizing reactive powders using low temperatures of calcination, especially when compared with conventional methods. However, during the thermal decomposition of the polymeric precursor the combustion event can be releases an additional heat that raises the temperature of the sample in several tens of degrees Celsius above the set temperature of the oven. This event may be detrimental to some material types, such as the titanium dioxide semiconductor. This ceramic material has a phase transition at around 600 ° C, which involves the irreversible structural rearrangement, characterized by the phase transition from anatase to rutile TiO2 phase. The control of the calcination step then becomes very important because the efficiency of the photocatalyst is dependent on the amount of anatase phase in the material. Furthermore, use of dopant in the material aims to improve various properties, such as increasing the absorption of radiation and in the time of the excited state, shifting of the absorption edge to the visible region, and increasing of the thermal stability of anatase. In this work, samples of titanium dioxide were synthesized by the Polymeric Precursor Method in order to investigate the effect of Fe (III) doping on the calcination stages. Thermal analysis has demonstrated that the Fe (III) insertion at 1 mol% anticipates the organic decomposition, reducing the combustion event in the final calcination. Furthermore, FTIR-PAS, XRD and SEM results showed that organic matter amount was reduced in the Fe (III)-doped TiO2 sample, which reduced the rutile phase amount and increased the reactivity and crystallinity of the powder samples.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Porous SnO2 and SnO2-Eu3+ nanorods have been facilely prepared using triphenyltin hydroxide microrods as precursors. The porous structure of SnO2 nanorods, which was aggregated by small SnO2 nanocrystallites, has been confirmed by TEM images and nitrogen adsorption-desorption isotherms. The optical property of the porous SnO2-Eu3+ nanorods was investigated by UV-vis absorption and photoluminescence spectra.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lead titanate powders were synthesized through the use of polymeric precursors according to the Pechini Process. The polymeric precursor was calcined at temperatures ranging from 300 to 600°C for 1 or 2 h. X-ray diffraction (XRD) showed that lead titanate crystallizes from the precursor at temperatures as low as 400°C. No intermediate carbonate phase was detected by Fourier transform infrared spectroscopy (FTIR) or by XRD. A powder with mean particle size of 150 nm was obtained after calcination of the precursor at 600°C for 1 h. © 1998 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Paper submitted to the 7th International Symposium on Feedstock Recycling of Polymeric Materials (7th ISFR 2013), New Delhi, India, 23-26 October 2013.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The morphological and chemical changes occurring during the thermal decomposition of weddelite, CaC2O4·2H2O, have been followed in real time in a heating stage attached to an Environmental Scanning Electron Microscope operating at a pressure of 2 Torr, with a heating rate of 10 °C/min and an equilibration time of approximately 10 min. The dehydration step around 120 °C and the loss of CO around 425 °C do not involve changes in morphology, but changes in the composition were observed. The final reaction of CaCO3 to CaO while evolving CO2 around 600 °C involved the formation of chains of very small oxide particles pseudomorphic to the original oxalate crystals. The change in chemical composition could only be observed after cooling the sample to 350 °C because of the effects of thermal radiation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The thermal stability and thermal decomposition pathways for synthetic iowaite have been determined using thermogravimetry in conjunction with evolved gas mass spectrometry. Chemical analysis showed the formula of the synthesised iowaite to be Mg6.27Fe1.73(Cl)1.07(OH)16(CO3)0.336.1H2O and X-ray diffraction confirms the layered structure. Dehydration of the iowaite occurred at 35 and 79°C. Dehydroxylation occurred at 254 and 291°C. Both steps were associated with the loss of CO2. Hydrogen chloride gas was evolved in two steps at 368 and 434°C. The products of the thermal decomposition were MgO and a spinel MgFe2O4. Experimentally it was found to be difficult to eliminate CO2 from inclusion in the interlayer during the synthesis of the iowaite compound and in this way the synthesised iowaite resembled the natural mineral.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bayer hydrotalcites prepared using the seawater neutralisation (SWN) process of Bayer liquors are characterised using X-ray diffraction and thermal analysis techniques. The Bayer hydrotalcites are synthesised at four different temperatures (0, 25, 55, 75 °C) to determine the effect on the thermal stability of the hydrotalcite structure, and to identify other precipitates that form at these temperatures. The interlayer distance increased with increasing synthesis temperature, up to 55 °C, and then decreased by 0.14 Å for Bayer hydrotalcites prepared at 75 °C. The three mineralogical phases identified in this investigation are; 1) Bayer hydrotalcite, 2), calcium carbonate species, and 3) hydromagnesite. The DTG curve can be separated into four decomposition steps; 1) the removal of adsorbed water and free interlayer water in hydrotalcite (30 – 230 °C), 2) the dehydroxylation of hydrotalcite and the decarbonation of hydrotalcite (250 – 400 °C), 3) the decarbonation of hydromagnesite (400 – 550 °C), and 4) the decarbonation of aragonite (550 – 650 °C).