998 resultados para Sintering time
Resumo:
This paper presents results on the simulation of the solid state sintering of copper wires using Monte Carlo techniques based on elements of lattice theory and cellular automata. The initial structure is superimposed onto a triangular, two-dimensional lattice, where each lattice site corresponds to either an atom or vacancy. The number of vacancies varies with the simulation temperature, while a cluster of vacancies is a pore. To simulate sintering, lattice sites are picked at random and reoriented in terms of an atomistic model governing mass transport. The probability that an atom has sufficient energy to jump to a vacant lattice site is related to the jump frequency, and hence the diffusion coefficient, while the probability that an atomic jump will be accepted is related to the change in energy of the system as a result of the jump, as determined by the change in the number of nearest neighbours. The jump frequency is also used to relate model time, measured in Monte Carlo Steps, to the actual sintering time. The model incorporates bulk, grain boundary and surface diffusion terms and includes vacancy annihilation on the grain boundaries. The predictions of the model were found to be consistent with experimental data, both in terms of the microstructural evolution and in terms of the sintering time. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
In dentistry, yttrium partially stabilized zirconia (ZrO2) has become one of the most attractive ceramic materials for prosthetic applications. The aim of this series of studies was to evaluate whether certain treatments used in the manufacturing process, such as sintering time, color shading or heat treatment of zirconia affect the material properties. Another aim was to evaluate the load-bearing capacity and marginal fit of manually copy-milled custom-made versus prefabricated commercially available zirconia implant abutments. Mechanical properties such as flexural strength and surface microhardness were determined for green-stage milled and sintered yttrium partially stabilized zirconia after different sintering time, coloring process and heat treatments. Scanning electron microscope (SEM) was used for analyzing the possible changes in surface structure of zirconia material after reduced sintering time, coloring and heat treatments. Possible phase change from the tetragonal to the monoclinic phase was evaluated by X-ray diffraction analysis (XRD). The load-bearing capacity of different implant abutments was measured and the fit between abutment and implant replica was examined with SEM. The results of these studies showed that the shorter sintering time or the thermocycling did not affect the strength or surface microhardness of zirconia. Coloring of zirconia decreased strength compared to un-colored control zirconia, and some of the colored zirconia specimens also showed a decrease in surface microhardness. Coloring also affected the dimensions of zirconia. Significantly decreased shrinkage was found for colored zirconia specimens during sintering. Heat treatment of zirconia did not seem to affect materials’ mechanical properties but when a thin coating of wash and glaze porcelain was fired on the tensile side of the disc the flexural strength decreased significantly. Furthermore, it was found that thermocycling increased the monoclinic phase on the surface of the zirconia. Color shading or heat treatment did not seem to affect phase transformation but small monoclinic peaks were detected on the surface of the heat treated specimens with a thin coating of wash and glaze porcelain on the opposite side. Custom-made zirconia abutments showed comparable load-bearing capacity to the prefabricated commercially available zirconia abutments. However, the fit of the custom-made abutments was less satisfactory than that of the commercially available abutments. These studies suggest that zirconia is a durable material and other treatments than color shading used in the manufacturing process of zirconia bulk material does not affect the material’s strength. The decrease in strength and dimensional changes after color shading needs to be taken into account when fabricating zirconia substructures for fixed dental prostheses. Manually copy-milled custom-made abutments have acceptable load-bearing capacity but the marginal accuracy has to be evaluated carefully.
Resumo:
It seeks to find an alternative to the current tantalum electrolytic capacitors in the market due to its high cost. Niobium is a potential substitute, since both belong to the same group of the periodic table and because of this have many similar physical and chemical properties. Niobium has several technologically important applications, and Brazil has the largest reserves, around 96%. There are including niobium in reserves of tantalite and columbite in Rio Grande do Norte. These electrolytic capacitors have high capacitance specifies, ie they can store high energy in small volumes compared to other types of capacitors. This is the main attraction of this type of capacitor because is growing demand in the production of capacitors with capacitance specifies increasingly high, this because of the miniaturization of various devices such as GPS devices, televisions, computers, phones and many others. The production route of the capacitor was made by powder metallurgy. The initial niobium powder supplied by EEL-USP was first characterized by XRD, SEM, XRF and laser particle size, to then be sieved into three particle size, 200, 400 e 635mesh. The powders were then compacted and sintered at 1350, 1450 and 1550°C using two sintering time 30 and 60min. Sintering is one of the most important parts of the process as it affects properties as porosity and surface cleaning of the samples, which greatly affected the quality of the capacitor. The sintered samples then underwent a process of anodic oxidation, which created a thin film of niobium pentóxido over the whole porous surface of the sample, this film is the dielectric capacitor. The oxidation process variables influence the performance of the film and therefore the capacitor. The samples were characterized by electrical measurements of capacitance, loss factor, ESR, relative density, porosity and surface area. After the characterizations was made an annealing in air ate 260ºC for 60min. After this treatment were made again the electrical measurements. The particle size of powders and sintering affected the porosity and in turn the specific area of the samples. The larger de area of the capacitor, greater is the capacitance. The powder showed the highest capacitance was with the smallest particle size. Higher temperatures and times of sintering caused samples with smaller surface area, but on the other hand the cleaning surface impurities was higher for this cases. So a balance must be made between the gain that is achieved with the cleaning of impurities and the loss with the decreased in specific area. The best results were obtained for the temperature of 1450ºC/60min. The influence of annealing on the loss factor and ESR did not follow a well-defined pattern, because their values increased in some cases and decreased in others. The most interesting results due to heat treatment were with respect to capacitance, which showed an increase for all samples after treatment
Resumo:
An experimental and theoretical study on the piezoelectric behaviour of PZT doped with a range of calcium ion concentrations is presented. A systematic study of the effect on the piezoelectric properties of PZT doped with various concentrations of CaO at constant sintering temperature and sintering time was carried out. The remanent polarization, planar coupling factor and frequency-thickness constant increase with calcium concentration. Ab initio perturbed ion calculations show that the lattice energy decreases with calcium addition for both tetragonal and rhombohedral phases of PZT.
Resumo:
Two series of lead zirconate titanate (PZT) ceramics with composition Zr/Ti approximate to 53/47 have been prepared by the organic solution route. The effects on the electrical properties of calcination temperature in one series and of sintering time period in the other were examined. Dielectric constant, electrical conductivity and impedance spectroscopy results differed from one series to the other, probably due to differences in structure of the precursor powders, as seen by X-ray diffraction. Tetragonal and rhombohedral phases predominate in the powders used, respectively, in the calcined and sintered series. Physical and electrical behavior of ceramics prepared from predominantly rhombohedral powder suggests the evaporation of PbO. The presence of two semi-circles in impedance plots leads to the association of the low frequency semi-circle to the presence of PbO, which, apparently, was not eliminated from ceramics prepared from predominantly tetragonal powder. (C) 2001 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.
Resumo:
Theoretical data using ab initio perturbed ion calculation were compared with ferroelectric and piezoelectric experimental data of strontium doped PZT. Various concentrations of SrO in PZT at constant temperature and sintering time were carried out. Experimental results, such as the remanent polarization, P-R of 6.9-8.9 muC/Cm-2, the coercive field, E-C of 6.6-7.8 kVcm, and the planar coupling factor, Kp of 0.45-0.53, were compared with the energy of Zr4+ and Ti4+ ion dislocation and the lattice interaction energy which show that strontium increment in PZT alter the energies and increase the values of piezoelectric and ferroelectric variables. Calculations of lattice energy of the rhombohedral phase show that a phase non-stability is coincident with increasing experimental values of the P-R, E-C and Kp. (C) 2001 Elsevier B.V. Ltd. All rights reserved.
Resumo:
Glass foams using float glass waste and sodium hydroxide were produced. The influence of the sodium hydroxide amount in the foam formulation was studied. Titanium dioxide was used as a strengthening agent. The variations of temperature, heating rate and sintering time were investigated during the synthesis process. Open porosity was estimated using mercury porosimetry. The morphology of the glass foams was evaluated using scanning electron microscopy, phase formation was studied using X-ray diffraction, and chemical composition was estimated using X-ray fluorescence. As a result, glass foams with macroporosity were obtained. Since the glass foams used glass waste as reactant, the results suggest the development of an alternative route for glass recycling. © 2012 Elsevier Ltd and Techna Group S.r.l.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
The nickel-titanium alloys are very attractive and so it is widely used in industry, engineering applications in general and also in biomedical and dental applications. Besides showing the shape of memory effect, biocompatibility and superelastic, the alloy commercially known as Nitinol, has excellent mechanical properties. Most devices used in Brazil have been produced nationally, but using imported material is also necessary, which shows the need of produce the alloy nationally. In this study we have investigated the influence of sintering temperatures and times to obtain nickel-titanium alloys by powder metallurgy alloys and the characterization of the precipitated intermetallic phases by using the post-mix of elemental nickel and titanium in proportion of 49.5% Ti - 50.5% Ni. The samples were sintered at 930ºC for periods of 30, 40 and 50 hours and were characterized by optical microscopy using metallography and x-ray diffraction. The results of the study show that the 50 hours sintering time was the most suitable time for obtaining the alloy, observing a low volume of precipitated intermetallic phases and absence of Ni and Ti residuals
Resumo:
This paper presents a study of the influence of particle size on the structural and dielectric properties of Pb0.85La0.15TiO3 (PLT15) ferroelectric ceramic samples. The samples were prepared with average grain size of 1.69 +/- 0.08 mu m and 146 +/- 8 nm using, respectively, conventional and spark plasma sintering techniques. A decrease in the tetragonality degree as the crystallite size decreased was explained by an internal stress caused by the existence of a large amount of grain boundaries. The local structure exhibited no significant modification and the dielectric measurements showed a diffuse phase transition and a reduction in the permittivity magnitude at T-m as the average grain size decreased. The nanostructured ceramic sample prepared at a relatively lower temperature and sintering time presented a dielectric constant value of approximately 2000 at room temperature. (c) 2012 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
A specific manufacturing process to obtain continuous glass fiber-reinforced RIFE laminates was studied and some of their mechanical properties were evaluated. Young's modulus and maximum strength were measured by three-point bending test and tensile test using the Digital Image Correlation (DIC) technique. Adhesion tests, thermal analysis and microscopy were used to evaluate the fiber-matrix adhesion, which is very dependent on the sintering time. The composite material obtained had a Young's modulus of 14.2 GPa and ultimate strength of 165 MPa, which corresponds to approximately 24 times the modulus and six times the ultimate strength of pure RIFE. These results show that the RIFE composite, manufactured under specific conditions, has great potential to provide structural parts with a performance suitable for application in structural components. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
The present research concentrates on the fabrication of bulk aluminum matrix nanocomposite structures with carbon nanotube reinforcement. The objective of the work was to fabricate and characterize multi-walled carbon nanotube (MWCNT) reinforced hypereutectic Al-Si (23 wt% Si, 2 wt% Ni, 1 wt% Cu, rest Al) nanocomposite bulk structure with nanocrystalline matrix through thermal spray forming techniques viz. plasma spray forming (PSF) and high velocity oxy-fuel (HVOF) spray forming. This is the first research study, which has shown that thermal spray forming can be successfully used to synthesize carbon nanotube reinforced nanocomposites. Microstructural characterization based on quantitative microscopy, scanning and transmission electron microscopy (SEM and TEM), energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), Raman spectroscopy and X ray photoelectron spectroscopy (XPS) confirms (i) retention and macro/sub-macro level homogenous distribution of multiwalled carbon nanotubes in the Al-Si matrix and (ii) evolution of nanostructured grains in the matrix. Formation of ultrathin β-SiC layer on MWCNT surface, due to chemical reaction of Si atoms diffusing from Al-Si alloy and C atoms from the outer walls of MWCNTs has been confirmed theoretically and experimentally. The presence of SiC layer at the interface improves the wettability and the interfacial adhesion between the MWCNT reinforcement and the Al-Si matrix. Sintering of the as-sprayed nanocomposites was carried out in an inert environment for further densification. As-sprayed PSF nanocomposite showed lower microhardness compared to HVOF, due to the higher porosity content and lower residual stress. The hardness of the nanocomposites increased with sintering time due to effective pore removal. Uniaxial tensile test on CNT-bulk nanocomposite was carried out, which is the first ever study of such nature. The tensile test results showed inconsistency in the data attributed to inhomogeneous microstructure and limitation of the test samples geometry. The elastic moduli of nanocomposites were computed using different micromechanics models and compared with experimentally measured values. The elastic moduli of nanocomposites measured by nanoindentation technique, increased gradually with sintering attributed to porosity removal. The experimentally measured values conformed better with theoretically predicted values, particularly in the case of Hashin-Shtrikman bound method.
Resumo:
It seeks to find an alternative to the current tantalum electrolytic capacitors in the market due to its high cost. Niobium is a potential replacement for be lighter and cheaper than tantalum. They belong to the same table group periodically and thus exhibit several physical and chemical properties similar. Niobium is used in many technologically important applications, and Brazil has the largest reserves, around 96%. These electrolytic capacitors have high specific capacitance, so they can store high energy in small volumes compared to other types of capacitors. This is the main attraction of this type of capacitor because is growing demand in the production of capacitors with capacitance specifies increasingly high, this because of the miniaturization of various devices such as GPS devices, televisions, computers, phones and many others. The production route of the capacitor was made by powder metallurgy. The initial niobium poder was first characterized by XRD, SEM and laser particle size to then be sieved into particle size 400mesh. The powder was then compacted at pressure of 150MPa and sintered at 1400, 1450 and 1500°C using two sintering time 30 and 60min. Sintering is an important part of the process as it affects properties as porosity and surface cleaning of the samples, which greatly affected the quality of the capacitor. After sintering the samples were underwent a process of anodic oxidation (anodizing), which created a thin film of niobium pentoxide over the whole surface of the sample, this film is the dielectric capacitor. The anodizing process variables influenced a lot in film formation and consequently the capacitor. The samples were characterized by electrical measurements of capacitance, loss factor and ESR (equivalent series resistance). The sintering has affected the porosity and in turn the specific area of the samples. The capacitor area is directly related to the capacitance, that is, the higher the specific area is the capacitance. Higher sintering temperatures decrease the surface area but eliminate as many impurities. The best results were obtained at a temperature of 1400°C with 60 minutes. The most interesting results were compared with the specific capacitance and ESR for all samples.
Resumo:
It seeks to find an alternative to the current tantalum electrolytic capacitors in the market due to its high cost. Niobium is a potential replacement for be lighter and cheaper than tantalum. They belong to the same table group periodically and thus exhibit several physical and chemical properties similar. Niobium is used in many technologically important applications, and Brazil has the largest reserves, around 96%. These electrolytic capacitors have high specific capacitance, so they can store high energy in small volumes compared to other types of capacitors. This is the main attraction of this type of capacitor because is growing demand in the production of capacitors with capacitance specifies increasingly high, this because of the miniaturization of various devices such as GPS devices, televisions, computers, phones and many others. The production route of the capacitor was made by powder metallurgy. The initial niobium poder was first characterized by XRD, SEM and laser particle size to then be sieved into particle size 400mesh. The powder was then compacted at pressure of 150MPa and sintered at 1400, 1450 and 1500°C using two sintering time 30 and 60min. Sintering is an important part of the process as it affects properties as porosity and surface cleaning of the samples, which greatly affected the quality of the capacitor. After sintering the samples were underwent a process of anodic oxidation (anodizing), which created a thin film of niobium pentoxide over the whole surface of the sample, this film is the dielectric capacitor. The anodizing process variables influenced a lot in film formation and consequently the capacitor. The samples were characterized by electrical measurements of capacitance, loss factor and ESR (equivalent series resistance). The sintering has affected the porosity and in turn the specific area of the samples. The capacitor area is directly related to the capacitance, that is, the higher the specific area is the capacitance. Higher sintering temperatures decrease the surface area but eliminate as many impurities. The best results were obtained at a temperature of 1400°C with 60 minutes. The most interesting results were compared with the specific capacitance and ESR for all samples.