The aim of this study was to investigate the influence of therapeutic dose X rays on the microhardness (MH) and degree of conversion (DC) of two different esthetic restorative dental materials. The materials were photo-activated with a LED light-curing unit using three cure-times: 5, 20 and 40 seconds. The photo-activation was carried out in two distinct periods: before and after irradiation with doses of 5, 35 and 70 Gy, from a 6 MV X rays beam. In accordance with the methodology used, it was conclude that a therapeutic dose does not have a detrimental effect on the photoinitiator molecules, because the photo-activation occurred after they were irradiated. When the irradiation was applied before photo-activation, the materials showed MH improvement, but when photo-activation was performed after irradiation, there was less improvement. However, there was no correlation between MH and DC. Thus, a therapeutic dose applied to cured material can promote linking and breaking of chain bonds in a non-linear way.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

PURPOSE The goal of this study was to investigate whether different computed tomography (CT) energy levels could supply additional information for the differentiation of dental materials for forensic investigations. METHODS Nine different commonly used restorative dental materials were investigated in this study. A total of 75 human third molars were filled with the restorative dental materials and then scanned using the forensic reference phantom in singlesource mode. The mean Hounsfield unit values and standard deviations (SDs) of each material were calculated at 120, 80 and 140 kVp. RESULTS Most of the dental materials could be differentiated at 120 kVp. We found that greater X-ray density of a material resulted in higher SDs and that the material volume could influence the measurements. CONCLUSION Differentiation of dental materials in CT was possible in many cases using single-energy CT scans at 120 kVp. Because of the number of dental restorative materials available and scanner and scan parameter dependence, as well as the CT imaging artifacts, the identification (in contrast to differentiation) was problematic.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of the present study was to evaluate the effects of low-dose therapeutic ionizing radiation on different aesthetic dental materials. Forty five specimens (n = 45) of three different aesthetic restorative materials were prepared and randomly divided into five groups: G1 (control group); G2, G3, G4, G5 experimental groups irradiated respectively with 0.25, 0.50, 0.75, and 1.00 Gy of gamma radiation by the (60)Co teletherapy machine. Chemical analyses were performed using a FT-IR Nicolet 520 spectrophotometer with reflectance diffuse technique. Even a minimal exposition at ionizing radiation in therapeutic doses can provide chemical changes on light-cured composite resins. The three studied restorative materials showed changes after exposure at gamma radiation, however the increase of the radiation dose did not contribute to an increase in this effect.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: The purpose of this study was to evaluate the cohesive strength of the composite using different resinous monomers to lubricate instruments used in the Restorative Dental Modeling Insertion Technique (RDMIT).Materials and Methods: The composite specimens were made by using a prefabricated Teflon device. Different resinous monomers were used at the interface to lubricate the instruments, for a total of 72 specimens divided into 6 groups: 1. control group, no resinous monomer was used; 2. Composite Wetting Resin; 3. C & B Liquid; 4. Scotchbond Multi-Purpose Adhesive; 4. Adper Single Bond Adhesive; 6. Prime & Bond NT. Specimens were submitted to the circular area tensile test to evaluate the cohesive strength at the composite interfaces. Data were analyzed using ANOVA and Tukey's test (alpha = 0.05).Results: ANOVA showed a value of p < 0.0001, which indicated that there were significant differences among the groups. The means (SD) for the different groups were: Adper Single Bond Adhesive: 26 (12) a; control group: 28 (3) ab; Prime & Bond NT: 32 (12) ab; Composite Wetting Resin: 36 (9) abc; C&B Liquid: 38 (7) bc; Scotchbond Multi-Purpose Adhesive: 46 (10) c. Groups denoted with the same letters were not significantly different. Only Scotchbond Multi-Purpose Adhesive, used for direct restorations, had a statistically significantly higher bond strength than the control group, Adper Single Bond Adhesive, and Prime & Bond NT. Adper Single Bond with Adhesive showed a statistically significantly lower mean value than C & B Liquid.Conclusion: The results of this study indicate that the resinous monomers used for lubricating the instruments in the RDMIT did not alter the mechanical properties of the composite, and therefore did not reduce the cohesive bond strength at the composite interfaces.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objective. The general aim of this article is to describe the state-of-the-art of biocompatibility testing for dental materials, and present new strategies for improving operative dentistry techniques and the biocompatibility of dental materials as they relate to their interaction with the dentin-pulp complex.Methods. The literature was reviewed focusing on articles related to biocompatibilty testing, the dentin-pulp complex and new strategies and materials for operative dentistry. For this purpose, the PubMed database as well as 118 articles published in English from 1939 to 2014 were searched. Data concerning types of biological tests and standardization of in vitro and in vivo protocols employed to evaluate the cytotoxicity and biocompatibility of dental materials were also searched from the US Food and Drug Administration (FDA), International Standards Organization (ISO) and American National Standards Institute (ANSI).Results. While there is an ongoing search for feasible strategies in the molecular approach to direct the repair or regeneration of structures that form the oral tissues, it is necessary for professionals to master the clinical therapies available at present. In turn, these techniques must be applied based on knowledge of the morphological and physiological characteristics of the tissues involved, as well as the physical, mechanical and biologic properties of the biomaterials recommended for each specific situation. Thus, particularly within modern esthetic restorative dentistry, the use of minimally invasive operative techniques associated with the use of dental materials with excellent properties and scientifically proved by means of clinical and laboratory studies must be a routine for dentists. This professional and responsible attitude will certainly result in greater possibility of achieving clinical success, benefiting patients and dentists themselves.Signcance. This article provides a general and critical view of the relations that permeate the interaction between dental materials and the dentin-pulp complex, and establish real possibilities and strategies that favor biocompatibility of the present and new products used in Dentistry, which will certainly benefit clinicians and their patients. (C) 2014 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Background: The aim of this study was to evaluate the cardiovascular effects of maxillary infiltration using 2% lidocaine with 1: 100 000 adrenaline, 4% articaine with 1: 200 000 adrenaline, and 4% articaine with 1: 100 000 adrenaline in different stages during restorative dental procedures. Methods: Twenty healthy patients randomly received 1.8 mL of the three local anaesthetics. Systolic blood pressure, average blood pressure, diastolic blood pressure, and heart rate were evaluated by the oscillometric and photoplethysmograph methods in seven stages during the appointment. Results: Statistical analysis by ANOVA and Tukey tests of cardiovascular parameters did not show significant differences between the anaesthetic associations. There were significant differences for the parameters among different clinical stages. Conclusions: The variation of cardiovascular parameters was similar for lidocaine and articaine with both adrenaline concentrations and showed no advantage of one drug over the other. Cardiovascular parameters were influenced by the stages of the dental procedures, which showed the effect of anxiety during restorative dental treatment.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

To study luminescence, reflectance, and color stability of dental composites and ceramics. Materials and Methods: IPS e.max, IPS Classic, Gradia, and Sinfony materials were tested, both unpolished (as-cast) and polished specimens. Coffee, tea, red wine, and distilled water (control) were used as staining drinks. Disk-shaped specimens were soaked in the staining drinks for up to 5 days. Color was measured by a colorimeter. Fluorescence was recorded using a spectrofluorometer, in the front-face geometry. Time-resolved fluorescence spectra were recorded using a laser nanosecond spectrofluorometer. Results: The exposure of the examined dental materials to staining drinks caused changes in color of the composites and ceramics, with the polished specimens exhibiting significantly lower color changes as compared to unpolished specimens. Composites exhibited lower color stability as compared to ceramic materials. Water also caused perceptible color changes in most materials. The materials tested demonstrated significantly different initial luminescence intensities. Upon exposure to staining drinks, luminescence became weaker by up to 40%, dependent on the drink and the material. Time-resolved luminescence spectra exhibited some red shift of the emission band at longer times, with the lifetimes in the range of tens of nanoseconds. Conclusions: Unpolished specimens with a more developed surface have lower color stability. Specimens stored in water develop some changes in their visual appearance. The presently proposed methods are effective in evaluating the luminescence of dental materials. Luminescence needs to be tested in addition to color, as the two characteristics are uncorrelated. It is important to further improve the color and luminescence stability of dental materials.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

OBJECTIVES: (1) To evaluate the changes in surface roughness and gloss after simulated toothbrushing of 9 composite materials and 2 ceramic materials in relation to brushing time and load in vitro; (2) to assess the relationship between surface gloss and surface roughness. METHODS: Eight flat specimens of composite materials (microfilled: Adoro, Filtek Supreme, Heliomolar; microhybrid: Four Seasons, Tetric EvoCeram; hybrid: Compoglass F, Targis, Tetric Ceram; macrohybrid: Grandio), two ceramic materials (IPS d.SIGN and IPS Empress polished) were fabricated according to the manufacturer's instructions and optimally polished with up to 4000 grit SiC. The specimens were subjected to a toothbrushing (TB) simulation device (Willytec) with rotating movements, toothpaste slurry and at three different loads (100g/250g/350g). At hourly intervals from 1h to 10h TB, mean surface roughness Ra was measured with an optical sensor and the surface gloss (Gl) with a glossmeter. Statistical analysis was performed for log-transformed Ra data applying two-way ANOVA to evaluate the interaction between load and material and load and brushing time. RESULTS: There was a significant interaction between material and load as well as between load and brushing time (p<0.0001). The microhybrid and hybrid materials demonstrated more surface deterioration with higher loads, whereas with the microfilled resins Heliomolar and Adoro it was vice versa. For ceramic materials, no or little deterioration was observed over time and independent of the load. The ceramic materials and 3 of the composite materials (roughness) showed no further deterioration after 5h of toothbrushing. Mean surface gloss was the parameter which discriminated best between the materials, followed by mean surface roughness Ra. There was a strong correlation between surface gloss and surface roughness for all the materials except the ceramics. The evaluation of the deterioration curves of individual specimens revealed a more or less synchronous course suspecting hinting specific external conditions and not showing the true variability in relation to the tested material. SIGNIFICANCE: The surface roughness and gloss of dental materials changes with brushing time and load and thus results in different material rankings. Apart from Grandio, the hybrid composite resins were more prone to surface changes than microfilled composites. The deterioration potential of a composite material can be quickly assessed by measuring surface gloss. For this purpose, a brushing time of 10h (=72,000 strokes) is needed. In further comparative studies, specimens of different materials should be tested in one series to estimate the true variability.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Background: Since only a few data have been published concerning the effects of resinous dental materials on the pulp-dentin complex, the aim of this study was to evaluate the biocompatibility of resin-based materials applied as liners in deep cavities prepared in duman teeth. Methods: After preparing class V cavities, the following dental materials were applied on the axial walls: group 1, Vitrebond™ (VIT; 3M ESPE); group 2, Ultra-Blend® Plus™ (UBP; Untradent); and group 3, Clearfil™ SE Bond (CSEB; Kuraray). In group 4 (control), the hard-setting calcium hydroxide cement Dycal (CH; Caulk/Dentsply) was used. The teeth extracted at 7 days or between 30 and 85 days after the clinical procedures were processed for histological evaluation. Results: For all the experimental and control groups, most of specimens exhibited no pulpal response or slight inflammatory reaction associated with slight tissue disorganization at 7-day period. Moderate inflammatory pulpal response occurred only in one tooth (RDT = 262 μm) of group 3 in which transdentinal diffusion of resin components was observed. Conclusion: The resin-based dental cements VIT and UBP as well as the bonding agent CSEB presented acceptable biocompatibility when applied in deep cavities prepared in sound human teeth. © 2006 Wiley Periodicals, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bacterial cellulose (BC) has become established as a remarkably versatile biomaterial and can be used in a wide variety of scientific applications, especially for medical devices. In this work, the bacterial cellulose fermentation process is modified by the addition of chondroitin sulfate (1% w/w) to the culture medium before the bacteria are inoculated. Besides, biomimetic precipitation of calcium phosphate of biological interest from simulated body fluid on bacterial cellulose was studied. Chondroitin sulfate influences in bacterial cellulose were analyzed using transmission infrared spectroscopy (FTIR), XRD (X-ray diffraction) and scanning electron microscopy (SEM). FTIR analysis showed interaction between chondroitin sulfate, bacterial cellulose and calcium phosphate and XRD demonstrated amorphous calcium phosphate and carbonated apatite on bacterial cellulose nanocomposites. SEM images confirmed incorporation of calcium phosphate in bacterial celluloe nanocomposite surface and uniform spherical calcium phosphate particles. Future experiments with cells adhesion and viability are in course.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bacterial cellulose (BC) has become established as a remarkably versatile biomaterial and can be used in a wide variety of scientific applications, especially for medical devices. In this work, the bacterial cellulose fermentation process is modified by the addition of chondroitin sulfate and hyaluronic acid (1% w/w) to the culture medium before the bacteria is inoculated. Besides, biomimetic precipitation of calcium phosphate of biological interest from simulated body fluid on bacterial cellulose was studied. Chondroitin sulfate and hyaluronic acid effects in bacterial cellulose were analyzed using transmission infrared spectroscopy (FTIR), XRD (X-ray diffraction) and scanning electron microscopy (SEM). FTIR analysis showed interaction between bacterial cellulose nanobiocomposites and calcium phosphate. XRD demonstrated amorphous calcium phosphate, carbonated apatite and calcium chloride on bacterial cellulose nanobiocomposites. Monocalcium phosphate monohydrate phase formation [Ca(H2PO4)(2)center dot H2O] are here attested by FTIR, XRD and Ca/P relation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of this study was to determine the influence of thickness and aging on the intrinsic fluorescence of sealing materials and their ability to block fluorescence from the underlying surface as assessed using a laser fluorescence device. Cavities of 0.5 mm and 1 mm depth were drilled into acrylic boards which were placed over two surfaces with different fluorescence properties: a low-fluorescence surface, to assess the intrinsic fluorescence of the sealing materials, and a high-fluorescence surface, to assess the fluorescence-blocking ability of the sealing materials. Ten cavities of each depth were filled with different sealing materials: Adper Scotchbond Multi-Purpose, Adper Single Bond 2, FluroShield, Conseal f and UltraSeal XT Plus. Fluorescence was measured with a DIAGNOdent pen at five different time points: empty cavity, after polymerization, and 1 day, 1 week and 1 month after filling. The individual values after polymerization, as well as the area under the curve for the different periods were submitted to ANOVA and the Tukey test (p < 0.05). At 0.5 mm, Scotchbond, FluroShield and UltraSeal showed insignificant changes in intrinsic fluorescence with aging and lower fluorescence after polymerization than Single Bond and Conseal. At 1 mm, Scotchbond and FluroShield showed the lowest intrinsic fluorescence, but only Scotchbond showed no chagnes in fluorescence with aging. At both depths, Scotchbond blocked significantly less fluorescence. All sealing materials blocked more fluorescence when applied to a depth of 1 mm. At 0.5 mm, fissure sealants blocked more fluorescence than adhesives, and did not show significant changes with aging. Scotchbond had the least affect on the fluorescence from the underlying surface and would probably have the least affect on the monitoring of sealed dental caries by laser fluorescence.