Fe(II) pyridinebisimine complexes activated with trialkylaluminium or modified methylaluminoxane (MMAO) as catalysts were employed for the polymerization of methyl methacrylate. Polymer yields, activities and polymer molecular weights as well as molecular weight distributions can be controlled over a wide range by the variation of the structures of the Fe(II) pyridinebisimine complexes and the reaction parameters such as Al/Fe molar ratio, monomer/catalyst molar ratio, monomer concentration, reaction temperature and time applied to the polymerization of methyl methacrylate. Under optimum condition, the catalytic activity of Fe(II) complex is of up to 74.5 kg(polym)/mol(Fe)h.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The synthesis and catalytic activity of lanthanide monoamido complexes supported by a beta-diketiminate ligand are described. Donor solvents, such as DME, can cleave the chloro bridges of the dinuclear beta-diketiminate ytterbium dichloride {[(DIPPh)(2)nacnac]YbCl(mu-Cl)(3)Yb[(DIPPh)(2)nacnac](THF)} (1) [(DIPPh)(2)nacnac = N,N-diisopropylphenyl-2,4-pentanediimine anion] to produce the monomeric complex [(DIPPh)(2)nacnac]YbCl2(DME) (2) in high isolated yield. Complex 2 is a useful precursor for the synthesis of beta-diketiminate-ytterbium monoamido derivatives. Reaction of complex 2 with 1 equiv of LiNPr2i in THF at room temperature, after crystallization in THF/toluene mixed solvent, gave the anionic beta-diketiminate-ytterbium amido complex [(DIPPh)(2)nacnac]Yb(NPr2i)(mu-Cl)(2)Li(THF)(2) (3), while similar reaction of complex 2 with LiNPh2 produced the neutral complex [(DIPPh)(2)nacnac]Yb(NPh2)Cl(THF) (4). Recrystallization of complex 3 from toluene solution at elevated temperature led to the neutral beta-diketiminate-lanthanide amido complex [{(DIPPh)(2)nacnac}Yb(NPr2i)(mu-Cl)](2) (5). The reaction medium has a significant effect on the outcome of the reaction.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

It was first found that Ind(2)Y(mu -Et)(2)AlEt2 and Ind(2)LnN(i-Pr)(2) (Ln = Y, Yb) exhibit extremely high catalytic activity in the polymerization of methyl methacrylate. The reactions can be carried out over a quite broad range of polymerization temperatures from -30 to 50 degreesC. PMMA with high molecular weight (7.8 x 10(-5)) and high isotacticity (94%) can be obtained by using Ind(2)Y(mu -Et)(2)AlEt2, and narrow molecular weight distribution (M-w/M-n < 1.5) can be obtained by using Ind(2)LnN(i-Pr)(2) (Ln = Y, Yb).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Methyl methacrylate (MMA) was polymerized with the rare earth coordination catalyst-system of Nd(O - i-Pr)(3) in toluene. The influences of various ligands in neodymium complexes, molar ratio of Al/Nd, catalyst concentration, catalyst aging time, solvents, the third component CCl4, temperature and time on the polymerization of MMA were studied. The results showed that the polymerization conversion reached more than 80% at a catalyst concentration of 9.2 x 10(-3) mol/L. The appropriate molar ratio of CCl4/Nd was 4. Hydrocarbon was preferred for the polymerzation to obtain a high conversion and a high <(M)over bar w> of PMMA. The H-1 NMR spectra of PMMA indicated that the lower the temperature, the higher the syndiotactic content of PMMA was obtained.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The complex of (CH3Cp)2Yb . DME (DME = dimethoxyethane) has been synthesized by the reduction with metallic sodium of the corresponding chloride (CH3CP)2YbCl. (CH3CP)2Yb . DME crystallized from DME in the monoclinic space group Cm, with cell constants a = 11.068(3), b = 12.338(4), c = 12.479(4) angstrom; beta = 100.51(2)-degrees, V = 1675(l) angstrom3, and D0 = 1.66 g/cm3 for Z = 4. Least-squares refinement of 1420 unique observed reflections led to final R of 0.0487. This complex can be used as a catalyst for the polymerization of methyl methacrylate (MMA).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This thesis work is part of a larger synthesis project about alkyd resins from natural sources, copolymerized with methyl acrylate and n-butyl acrylates, which wil be used for coatings purpose. The aim is to control the copolymerization of methyl acrylate and n-butyl acrylate in RAFT miniemulsion. The research was divided into three parts. First the homopolymerization of methyl methacrylate and n-butyl acrylate was studied by varying different parameters such as the amount of surfactant, the amount of initiator, pH, and especially the RAFT agent. Then two macro RAFT agents were synthesized, as suggested by the existing literature. Finally, the two monomers were copolymerized using both the RAFT used for the homopolymerization and those synthesized in the second stage. To verify the obtained control over the polymerization, the synthesized polymers were analyzed by gel permeation chromatography, GPC, thus finding their molecular weight and its polydispersity.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A study has been made of the anionic polymerization of methyl methacrylate using butyllithium and polystyryl lithium as initiators and using aluminium triisobutyl as a cocatalyst. The aspects of the polymerization that were examined were the effect of changing the order of addition of reagents, the temperature at which polymerization takes place and the polarity of the solvent. Trends were assessed in terms of molecular weight, molecular weight distribution and tacticity. In addition, a second monomer addition test was carried out to verify that the polymerization was truly a living one, and a kinetic study was attempted. Studies to investigate the effect of changing the order of addition of reagents showed that polymer with similar polydispersities and tacticities are produced whether the pre-mixing (mixing initiator and cocatalyst before addition of monomer) or the post-mixing (mixing monomer and cocatalyst before addition of initiator) method were used. However, polymerizations using the post-mixing mixing method demonstrated lower initiator efficiencies, possibly indicating a different initiating species. Investigations into the effect of changing the polymerization temperature show the molecular weight distribution to narrow as the temperature decreases, although a small amount of low molecular weight tailing was also observed at low temperature. A clear relationship between tacticity and temperature was observed with syndiotacticity increasing with decreasing temperature. Changes in solvent polarity were achieved by using mixtures of the standard solvent, toluene, with varying amounts of cyclohexane, tetrahydrofuran or dichloromethane. Experiments at low solvent polarity (using toluene/cyclohexane mixtures) showed problems with initiator solubility but produced polymer with lower polydispersity and higher syndiotacticity than in toluene alone. Experiments using toluene/THF mixtures yielded no polymer, thought to be owing to a side reaction between THF and aluminium triisobutyl. Increased solvent polarity, achieved using toluene/dichloromethane mixtures produced polymer with higher polydispersity and at lower yields than the conventional system, but also with higher syndiotacticity. Second monomer addition reactions demonstrated that the polymerization was 'living' since an increase in molecular weight was observed with no increase in polydispersity. Kinetic studies demonstrated the high speed of the polymerization but yielded no useful data.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The reverse atom transfer radical polymerization(RATRP) of (-)-menthyl methacrylate ((-)-MnMA) with AIBN(AIBN/CuCl2/bipyridine(bipy) or (-)sparteine((-)Sp) =1/2/4) initiating system in THF has been studied. The dependence of the specific rotation on molecular weight was investigated.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The RAFT-CLD-T methodology is demonstrated to be not only applicable to 1-substituted monomers such as styrene and acrylates, but also to 1,1-disubstituted monomers such as MMA. The chain length of the terminating macromolecules is controlled by CPDB in MMA bulk free radical polymerization at 80 degrees C. The evolution of the chain length dependent termination rate coefficient, k(t)(i,i), was constructed in a step-wise fashion, since the MMA/CPDB system displays hybrid behavior (between conventional and living free radical polymerization) resulting in initial high molecular weight polymers formed at low RAFT agent concentrations. The obtained CLD of k(t) in MMA polymerizations is compatible with the composite model for chain length dependent termination. For the initial chain-length regime, up to a degree of polymerization of 100, k(t) decreases with alpha (in the expression k(t)(i,i) = k(t)(0) . i(-alpha)) being close to 0.65 at 80 degrees C. At chain lengths exceeding 100, the decrease is less pronounced (affording an alpha of 0.15 at 80 degrees C). However, the data are best represented by a continuously decreasing nonlinear functionality implying a chain length dependent alpha.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Values of Ko, Flory constant related to unperturbed dimensions, are evaluated for methyl methacrylate-acrylonitrile random copolymers using Flory-Fox, Kurata-Stockmayer and Inagaki-Ptitsyn methods and compared with the Ko values obtained by Stockmayer-Fixman method. Ko values are seen to be less in solvents which have large a (Mark-Houwink exponent) values. A correlation between Ko and a is developed to arrive at a more reliable estimate of Ko for this copolymer system.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Different compositions of poly(methyl methacrylate-co-methyl acrylate) (PMMAMA), poly(methyl methacrylate-co-ethyl acrylate) (PMMAEA) and poly(methyl methacrylate-co-butyl acrylate) (PMMABA) copolymers were synthesized and characterized. The photocatalytic oxidative degradation of all these copolymers were studied in presence of two different catalysts namely Degussa P-25 and combustion synthesized titania using azobis-iso-butyronitrile and benzoyl peroxide as oxidizers. Gel permeation hromatography (GPC) was used to determine the molecular weight distribution of the samples as a function of time. The GPC chromatogram indicated that the photocatalytic oxidative degradation of all these copolymers proceeds by both random and chain end scission.Continuous distribution kinetics was used to develop a model for photocatalytic oxidative degradation considering both random and specific end scission. The degradation rate coefficients were determined by fitting the experimental data with the model. The degradation rate coefficients of the copolymers decreased with increase in the percentage of alkyl acrylate in the copolymer. This indicates that the photocatalytic oxidative stability of the copolymers increased with increasing percentage of alkyl acrylate. From the degradation rate coefficients, it was observed that the photocatalytic oxidative stability follows the order PMMABA > PMMAEA > PMMAMA. The thermal degradation of the copolymers was studied by using thermogravimetric analysis (TGA). The normalized weight loss and differential fractional weight loss profiles indicated that the thermal stability of the copolymer increases with an increase in the percentage of alkyl acrylate and the thermal stability of poly(methyl methacrylate-co-alkyl acrylate)s follows the order PMMAMA > PMMAEA > PMMABA. The observed contrast in the order of photostability and thermal stability of the copolymers was attributed to different mechanisms involved for the scission of polymer chain and formation of different products in both the processes.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The Stockmayer-Fixman relation was used to evaluate the short range and long range interaction parameters for methyl methacrylate/acrylonitrile copolymers of 0,566 and 0,657 mole fraction of monomeric units of acrylonitrile in the solvents acetonitrile, 2-butanone, dimethyl formamide, and y-butyrolactone, at different temperatures (30, 45, and 60 “C). The values of KO were found to be lower than those of the parent homopolymers, and their values depend on both solvent and temperature. Even negative Ko-values were obtained, in cases in which the Mark Houwink exponent a is nearly unity. The values of the polymer-solvent interaction parameter, x, , are high and close to 0,5, indicating that these solvents are not good. The values of the excess interaction parameter, xAB, are negative and are not affected by temperature. The large extension of these copolymer chains, as exhibited by a and a;-values, can be understood in terms of unusual short range interactions only. Similar results were obtained for some cellulose derivatives.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper deals with studies on the dilute solution properties of methyl methacrylate�acrylonitrile copolymer of 0.289 mole fraction (mf) of acrylonitrile composition. Mark�Houwink parameters for this copolymer have been evaluated in acetonitrile (MeCN), 2-butanone (MEK), dimethylformamide (DMF) and γ-butyrolactone (γ-BL). The solvent power is found to be in the order of MEK < MeCN < DMF < γ-BL at 30°C. Herein, probably for the first time, the steric factor for the copolymer is found to be lower than that for the parent homopolymers and the excess interaction parameter, �AB is found to be negative. This probably suggests that the units are compatible to each other.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The photolytic and photocatalytic degradation of the copolymers poly(methyl methacrylate-co-butyl methacrylate) (MMA–BMA), poly(methyl methacrylate-co-ethyl acrylate) (MMA–EA) and poly(methyl methacrylate-co-methacrylic acid) (MMA–MAA) have been carried out in solution in the presence of solution combustion synthesized TiO2 (CS TiO2) and commercial Degussa P-25 TiO2 (DP 25). The degradation rates of the copolymers were compared with the respective homopolymers. The copolymers and the homopolymers degraded randomly along the chain. The degradation rate was determined using continuous distribution kinetics. For all the polymers, CS TiO2 exhibited superior photo-activity compared to the uncatalysed and DP 25 systems, owing to its high surface hydroxyl content and high specific surface area. The time evolution of the hydroxyl and hydroperoxide stretching vibration in the Fourier transform-infrared (FT-IR) spectra of the copolymers indicated that the degradation rate follows the order MMA–MAA > MMA–EA > MMA–BMA. The same order is observed for the rate coefficients of photocatalytic degradation. The photodegradation rate coefficients were compared with the activation energy of pyrolytic degradation. In degradation by pyrolysis, it was observed that MMA–BMA was the least stable followed by MMA–EA and MMA–MAA. The observed contrast in the order of thermal stability compared to the photo-stability of these copolymers was attributed to the two different mechanisms governing the scission of the polymer and the evolution of the products.