999 resultados para Pith
Resumo:
Coir pith black liquor obtained as a dark brown filtrate from oxidative delignification needs to be decolourised before releasing to open environment. From this liquor industrially valuable lignin was recovered using acid precipitation method. ‘Biochar’ was produced by slow pyrolysis of coir pith at 500oC and 600oC. Water holding capacity and pH of the biochar were estimated. CHNS analysis was carried out to identify the nutrient profile. Structural characterization was done using FTIR and SEM Studies. Biochar produced at 600oC was found to be more suitable for decolourisation of the coir pith black liquor. FTIR analysis indicated peak changes while SEM analysis indicated surface area and porosity changes. Biochar decolourisation experiments were carried out on crude coir pith black liquor and also on lignin recovered coir pith black liquor.
Resumo:
In this study, a novel improved technology could be developed to convert the recalcitrant coir pith into environmental friendly organic manure. The standard method of composting involves the substitution of urea with nitrogen fixing bacteria viz. Azotobacter vinelandii and Azospirillum brasilense leading to the development of an improved method of coir pith. The combined action of the microorganisms could enhance the biodegradation of coir pith. In the present study, Pleurotus sajor caju, an edible mushroom which has the ability to degrade coir pith, and the addition of nitrogen fixing bacteria like Azotobacter vinelandii and Azospirillum brasilense could accelerate the action of the fungi on coir pith. The use of these microorganisms brings about definite changes in the NPK, Ammonia, Organic Carbon and Lignin contents in coir pith. This study will encourage the use of biodegraded coir pith as organic manure for agri/horti purpose to get better yields and can serve as a better technology to solve the problem of accumulated coir pith in coir based industries
Resumo:
The aim of this work was to determine PAs levels in pith tissues and callus cultures from haploid and diploid tobacco plants, explanted from the apical and basal regions of the stem. These explants were cultured in an RM-64 medium supplied with IAA and kinetin, under light or in the dark, during successive subcultures. PAs levels followed a basipetal decrease in diploid and an increase in haploid, pith tissues. A similar pattern of total PAs (free + conjugated) was observed for the callus of diploid and haploid plants maintained in the light, and for the haploid callus in the dark, whereas the diploid callus in the dark showed a constant increase in total PAs levels until the end of culture. The PA increase in the diploid callus in the dark was related to free Put levels increase. The ploidy status of the plants could express different PA gradients together with the plant pith and in vitro callus cultures.
Resumo:
Background: Lignin and hemicelluloses are the major components limiting enzyme infiltration into cell walls. Determination of the topochemical distribution of lignin and aromatics in sugar cane might provide important data on the recalcitrance of specific cells. We used cellular ultraviolet (UV) microspectrophotometry (UMSP) to topochemically detect lignin and hydroxycinnamic acids in individual fiber, vessel and parenchyma cell walls of untreated and chlorite-treated sugar cane. Internodes, presenting typical vascular bundles and sucrose-storing parenchyma cells, were divided into rind and pith fractions. Results: Vascular bundles were more abundant in the rind, whereas parenchyma cells predominated in the pith region. UV measurements of untreated fiber cell walls gave absorbance spectra typical of grass lignin, with a band at 278 nm and a pronounced shoulder at 315 nm, assigned to the presence of hydroxycinnamic acids linked to lignin and/or to arabino-methylglucurono-xylans. The cell walls of vessels had the highest level of lignification, followed by those of fibers and parenchyma. Pith parenchyma cell walls were characterized by very low absorbance values at 278 nm; however, a distinct peak at 315 nm indicated that pith parenchyma cells are not extensively lignified, but contain significant amounts of hydroxycinnamic acids. Cellular UV image profiles scanned with an absorbance intensity maximum of 278 nm identified the pattern of lignin distribution in the individual cell walls, with the highest concentration occurring in the middle lamella and cell corners. Chlorite treatment caused a rapid removal of hydroxycinnamic acids from parenchyma cell walls, whereas the thicker fiber cell walls were delignified only after a long treatment duration (4 hours). Untreated pith samples were promptly hydrolyzed by cellulases, reaching 63% of cellulose conversion after 72 hours of hydrolysis, whereas untreated rind samples achieved only 20% hydrolyzation. Conclusion: The low recalcitrance of pith cells correlated with the low UV-absorbance values seen in parenchyma cells. Chlorite treatment of pith cells did not enhance cellulose conversion. By contrast, application of the same treatment to rind cells led to significant removal of hydroxycinnamic acids and lignin, resulting in marked enhancement of cellulose conversion by cellulases.
Resumo:
The use of fertilization in forest stands results in yield gains, yet little attention has been directed to its potential effects on the quality of wood produced. Information is scarce about the effect of fertilization on anatomical structures of older Eucalyptus wood. This work aims to study the effect of fertilization on tissue cell size of wood from an Eucalyptus grandis stand at age 21 years, the management system of which is based on selective thinning and fertilizer application at the start of the thinning season. Factors to consider include: presence or absence of fertilizers, two log positions and five radial (pith to bark) positions. Results led to the conclusion that fertilization significantly influenced only vessel frequency. Vessel element length was influenced by tree height. Fiber length, fiber diameter, fiber wall thickness, vessel element length, vessel diameter and vessel frequency were influenced by the radial position of the sample in relation to the log. A positive correlation was observed between fiber length, fiber diameter, fiber wall thickness, vessel element length, vessel diameter, ray width and radial position, while a negative correlation was observed between ray frequency and radial position.
Resumo:
The objective of this study was to show the radial variation of some anatomic characteristics, wood density and natural durability of teak (Tectona grandis L.F.) growing in Costa Rica. Samples of trees 13 years old were obtained from two growing sites (high and low growing) of plantations established in a humid tropical climate (CHT) and dry tropical climate (CST). The variables measured of the fibers as well as for the rays were not affected by the climate or the type of growing site, except for the length of the fibers. The fibers of teak wood from the best growing site were significantly larger. Vessels were found with a greater frequency for the CST but mostly solitary in comparison with the CBT. Average density, maximum density and the variation within the ring presented a light higher magnitude for the CST. The quality of the growing site did not affect these variables. The resistance of fungus attack was similar in the area of heartwood near the pith compared to the heartwood near the sapwood for all the conditions evaluated. Nevertheless, it was observed in some trees a similar resistance of fungus attack for areas of sapwood compared to similar areas of heartwood.
Resumo:
The synthetic hydrous niobium oxide has been used for phosphate removal from the aqueous solutions. The kinetic data correspond very well to the pseudo second-order equation The phosphate removal tended. to increase with a decrease of pH. The equilibrium data describe very well the Langmuir isotherm. The peak appearing at 1050 cm(-1) in IR spectra after adsorption was attributed to the bending vibration of adsorbed phosphate. The adsorption capacities are high, and increased with increasing temperature. The evaluated Delta G degrees and Delta H degrees indicate the spontaneous and endothermic nature of the reactions. The adsorptions occur with increase in entropy (Delta S positive) value suggest increase in randomness at the solid-liquid interface during the adsorption. A phosphate desorbability of approximately 60% was observed with water at pH 12, which indicated a relatively strong bonding between the adsorbed phosphate and the sorptive sites on the surface of the adsorbent. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The adsorption kinetics of phosphate onto Nb(2)O(5)center dot nH(2)O was investigated at initial phosphate concentrations 10 and 50 mg L(-1). The kinetic process was described by a pseudo second-order rate model very well. The adsorption thermodynamics was carried out at 298, 308, 318, 328 and 338 K. The positive values of both Delta H and Delta S suggest an endothermic reaction and increase in randomness at the solid-liquid interface during the adsorption. Delta G values obtained were negative indicating a spontaneous adsorption process. The Langmuir model described the data better than the Freundlich isotherm model. The peak appearing at 1050 cm(-1) in IR spectra after adsorption was attributed to the bending vibration of adsorbed phosphate. The effective desorption could be achieved using water at pH 12. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
A type of Nb(2)O(5)center dot 3H(2)O was synthesized and its phosphate removal potential was investigated in this study. The kinetic study, adsorption isotherm, pH effect, thermodynamic study and desorption were examined in batch experiments. The kinetic process was described by a pseudo-second-order rate model very well. The phosphate adsorption tended to increase with a decrease of pH. The adsorption data fitted well to the Langmuir model with which the maximum P adsorption capacity was estimated to be 18.36 mg-Pg(-1). The peak appearing at 1050 cm(-1) in IR spectra after adsorption was attributed to the bending vibration of adsorbed phosphate. The positive values of both Delta H degrees and Delta S degrees suggest an endothermic reaction and increase in randomness at the solid-liquid interface during the adsorption. Delta G degrees values obtained were negative indicating a spontaneous adsorption process. A phosphate desorbability of approximately 68% was observed with water at pH 12, which indicated a relatively strong bonding between the adsorbed phosphate and the sorptive sites on the surface of the adsorbent. The immobilization of phosphate probably occurs by the mechanisms of ion exchange and physicochemical attraction. Due to its high adsorption capacity, this type of hydrous niobium oxide has the potential for application to control phosphorus pollution.
Resumo:
As variações na retratibilidade no lenho das árvores são as principais causas dos defeitos de secagem, como o empenamento e fendilhamento das peças de madeira. Os tipos de madeira presentes em um tronco estão relacionados com as variações dessa importante propriedade física. Este trabalho teve como objetivo estudar a retratibilidade da madeira de sete espécies de eucaliptos. Os parâmetros de retratibilidade, bem como a sua variação na direção radial da medula em direção à periferia do tronco de sete espécies de eucaliptos, foram avaliados de acordo com a Norma brasileira. De modo geral, os resultados indicaram que as espécies de eucaliptos estudados possuíam madeira com elevada retratibilidade. À exceção das madeiras de Eucalyptus tereticornis e E. pilularis, as demais espécies estudadas apresentaram valores menores de retratibilidade na região próxima da medula.
Resumo:
Objetivou-se neste trabalho avaliar a variação das dimensões das fibras e dos vasos da madeira de Eucalyptus grandis com quatro diferentes idades (10, 14, 20 e 25 anos), proveniente de talhões comerciais. A amostragem do material na árvore foi feita através da coleta de três discos, retirados da base e das extremidades das duas primeiras toras, ambas com o comprimento comercial de 3 m. De cada disco, retiraram-se cinco amostras, de dimensões 1,0 x 1,0 x 1,0 cm, tomadas de pontos eqüidistantes, correspondentes a 0; 25; 50; 75; e 100% da seção, no sentido radial medula-casca, fazendo-se a medição das fibras e dos vasos. Verificou-se, em todos os parâmetros, o efeito da idade e da variação radial, no sentido medula-casca, à exceção da largura e do diâmetro do lume das fibras; todos os demais parâmetros apresentaram correlação positiva.
Resumo:
Este trabalho objetivou testar a variação da flexão estática da madeira de Eucalyptus grandis, ao longo da seção radial e sob quatro diferentes idades (10, 14, 20 e 25 anos), provenientes de talhões comerciais. As amostras foram retiradas da prancha diametral, de cada uma das 16 árvores (quatro para cada idade), tomadas de quatro posições eqüidistantes (0, 33, 66 e 100%), no sentido medula-casca, com oito repetições por posição. Verificou-se que os módulos de elasticidade (MOE) e de ruptura (MOR) apresentaram valores médios de 129.230 kgf/cm2 e 854 kgf/cm2, respectivamente, e ambos se mostraram positivamente correlacionados com a idade e com a posição radial, no sentido medula-casca. Os maiores valores foram conseguidos nas madeiras de 20 anos de idade e localizadas na região mais próxima da casca.
Resumo:
As variações de umidade e da densidade do lenho das árvores são as principais causas dos defeitos de secagem, como o empenamento e fendilhamento das peças de madeira. Os tipos de madeira presentes em um tronco estão relacionados com as variações dessas duas importantes propriedades físicas. Os gradientes de umidade e da densidade da madeira de sete espécies de eucalipto foram avaliados nas direções radial e longitudinal do tronco de árvores recém-abatidas. Os resultados apontaram uma maior homogeneidade de distribuição de umidade dentro das árvores de E. paniculata e E. citriodora, indicada pelos coeficientes de variação e desvio-padrão. O diferencial de umidade da madeira nas regiões internas do tronco de E. paniculata e E. citriodora foi de 20% e de E. urophylla e E. grandis, de 80%. A densidade básica da madeira aumentou na direção radial do tronco, e cada espécie de eucalipto apresentou um modelo de variação.
Resumo:
A ultra-estrutura e a composição química da madeira, bem como suas propriedades físicas e mecânicas, variam significativamente entre espécies, entre árvores de uma mesma espécie e, mesmo, entre diferentes partes de uma mesma árvore. Com este trabalho objetivou-se o estudo dos parâmetros de retratibilidade e de densidade básica da madeira Eucalyptus saligna, com idade de 16 anos, proveniente de talhões experimentais da EMBRAPA Florestas, de Colombo, Paraná. As amostras foram retiradas à altura do DAP de quatro posições eqüidistantes a partir da medula em direção à periferia, correspondendo a 0, 33, 66 e 100%, com dimensões nominais de 1,0 x 2,0 x 3,0 cm, sendo a última dimensão no sentido longitudinal. Elas foram mantidas em câmara fechada com ventilação, próximo de soluções salinas supersaturadas, com o objetivo de proporcionar diferentes condições de umidade relativa. Uma vez atingidas as distintas condições de umidade de equilíbrio, as amostras foram secas em estufa a 105 ºC e obtidos os dados de retratibilidade e densidade básica da madeira nas posições mencionadas. Constataram-se valores de contração volumétrica mais baixos na região medular, apresentando um acréscimo para as demais posições. Comportamento semelhante foi observado para os coeficientes das contrações lineares nas direções tangencial e radial. O fator anisotrópico foi consideravelmente mais elevado na região medular, decrescendo substancialmente em direção ao alburno. A densidade básica não mostrou sinais efetivos de estabilidade, apesar de mostrar tendência de aumento em direção à periferia do tronco.