997 resultados para LUMINESCENT PROPERTIES


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Two new star-burst compounds based on 1,3,5-triazine core and carbazole end-capped phenylene ethynylene arms (1a and 1b) were synthesized and characterized. Their photophysical properties were investigated systematically via spectroscopic and theoretical methods. Both compounds exhibit strong 1π–π⁎ transitions in the UV region and intense 1π–π⁎/intramolecular charge transfer (1ICT) absorption bands in the UV–vis region. Introducing the carbazole end-capped phenylene ethynylene arm on the 1,3,5-triazine core causes a slight bathochromic shift and enhanced molar extinction coefficient of the 1π–π⁎/1ICT transition band. Both compounds are emissive in solution at room temperature and 77 K, which exhibit pronounced positive solvatochromic effect. The emitting state could be ascribed to 1ICT state in more polar solvent, and 1π–π⁎ state in low-polarity solvent. The high emission quantum yields (Φem=0.90~1.0) of 1a and 1b (in hexane and toluene) make them potential candidates as efficient light-emitting materials. The spectroscopic studies and theoretical calculations indicate that the photophysical properties of these compounds can be tuned by the carbazole end-capped phenylene ethynylene arm, which would also be useful for rational design of photofunctional materials.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A comparative study of spherical and rod-like nanocrystalline GdO:Eu (GdEuO) red phosphors prepared by solution combustion and hydrothermal methods have been reported. Powder X-ray diffraction (PXRD) results confirm the as-formed product in combustion method showing mixed phase of monoclinic and cubic of GdO:Eu. Upon calcinations at 800C for 3 h, dominant cubic phase was achieved. The as-formed precursor hydrothermal product shows hexagonal Gd(OH):Eu phase and it converts to pure cubic phase of GdO:Eu on calcination at 600C for 3 h. TEM micrographs of hydrothermally prepared cubic GdO:Eu phase shows nanorods with a diameter of 15 nm and length varying from 50 to 150 nm, whereas combustion product shows the particles to be of irregular shape, with different sizes in the range 50-250 nm. Dominant red emission (612 nm) was observed in cubic GdO:Eu which has been assigned to transition. However, in hexagonal Gd(OH):Eu, emission peaks at 614 and 621 nm were observed. The strong red emission of cubic GdO:Eu nanophosphors by hydrothermal method are promising for high performance display materials. The variation in optical energy bandgap () was noticed in as-formed and heat treated systems in both the techniques. This is due to more ordered structure in heat treated samples and reduction in structural defects.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Undoped and Tb3+ (1-10 mol%) doped CeO2 nanophosphors were synthesized by low temperature solution combustion method. The combustion derived products were well studied by Powder X-ray diffraction (PXRD), Scanning electron microscopy (SEM), transmission electron microscopy (TEM), Fourier transform infrared spectroscopy (FTIR) and Ultraviolet visible (UV-Vis) characterizations. The thermoluminescence (TL) glow curves of CeO2: Tb3+ (1-10 mol%) nanophosphors exposed to c source (60Co) for various doses were discussed for the first time. Two TL glow peaks recorded at 182 and 262 degrees C respectively. The TL intensity at 262 degrees C peak increases linearly in the dose range 0.5-7 kGy. Further, this peak was well defined, intense and glow peak structure does not change with c-dose as a result, it was quite useful in TL dosimetry of ionizing radiations. The kinetic parameters associated with the glow peak were estimated using Chen's half width method. The photoluminescence emission (PLE) spectra consists of characteristic peaks at 544 and 655 nm which were attributed to D-5(4) -> F-7(5) and D-5(4) -> F-7(2) transitions of Tb3+ ions. The optimal concentration of Tb3+ ions was found to be 7 mol%. The color co-ordinates of CeO2: Tb3+ (1-10 mol%) located in green region. Hence, this phosphor was quite useful for display applications. (C) 2013 Elsevier B. V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we report the laser-induced periodic structure with different spatial characteristics on the surface of polished ZnO single-crystalline by high repetition rate femtosecond laser pulses. This study demonstrates that, using different laser parameters and irradiation conditions, ZnO nanoripples and nanorods were successfully prepared. We have investigated the surface by means of scanning electron microscope (SEM), Raman scattering and photoluminescence (PL). We propose that second-order harmonic has a strong influence on the formation of nanostructures. (c) 2007 Elsevier B.V All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

EU3+ -doped Y3Al5O12 (YAG:Eu3+) phosphors were synthesized by a facile sol-gel combustion method. In this process, citric acid traps the constituent cations and reduces the diffusion length of the precursors. YAG phase is obtained through sintering at 900 degrees C for 2h. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed. The charge transfer band of nanocrystalline phosphors shows a shift toward the high-energy side, compared with that of amorphous ones due to lower covalency of Eu-O bond for nanocrystalline phosphors. The higher concentration quenching in YAG:EU3+ nanophosphors may be caused by the confinement effect on resonant energy transfer of nanocrystalline. It also indicates that the sol-gel combustion synthesis method provides a good distribution of Eu3+ activators in YAG host. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Silicon nanowires (SiNWs) were grown directly from n-(111) single-crystal silicon (c-Si) substrate based on a solid-liquid-solid mechanism, and Au film was used as a metallic catalyst. The room temperature photoluminescence properties of SiNWs were observed by an Xe lamp with an exciting wavelength of 350 nm. The results show that the SiNWs exhibit a strongly blue luminescent band in the wavelength range 400-480 nm at an emission peak position of 420 nm. The luminescent mechanism of SiNWs indicates that the blue luminescence is attributed to the oxygen-related defects, which are in SiOx amorphous oxide shells around the crystalline core of SiNWs.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of seven ruthenium complexes with different ligands were synthesized and their optical, electrochemical and photoluminescent properties were characterized. Electroluminescent properties of these complexes were further evaluated using a light-emitting electrochemical cell with a configuration of indium tin oxide (ITO)/complex (100 nm)/Au (100 nm).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Nanocrystallinc Y2O2S:Eu3+ was successfully prepared with a combustion synthesis method, the corresponding bulk Y2O2S:Eu3+ was synthesized by conventional sulfur flux method. The results of XRD indicated that both bulk and nanocrystalline Y2O2S:Eu3+ have Pure hexagonal phases. The crystallite size was calculated to be about 20 nm according to Scherrer formula, which was consistent with the size as indicated by transmission electron microscopy (TEM).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The ligands 4,4,4-trifluoro-1-phenyl-1.3-butanedione (Hbfa) and 1,10-phenanthroline (phen) were used to prepare ternary lanthanide (Ln) complexes [Dy(bfa)(3)phen and Tm(bfa)(3)phen]. Crystal data: Dy(bfa)(3)phen C(42)H(26)FqN(2)O(6)Dy, triclinic, P (1) over bar, a= 9.9450(6) angstrom, b = 14.0944(9) angstrom, c = 14.6043(9) angstrom, alpha = 82.104(1)degrees, beta = 87.006(1)degrees, gamma = 76.490(1)degrees, V = 1971.1(2)angstrom(3), Z = 2; Tm(bfa)(3)phen C42H26F9N2O6Tm, triclinic, P (1) over bar, a = 9.898(5)angstrom, b = 13.918(5)angstrom, c = 14.753(5)angstrom, a = 83.517(5)degrees, alpha = 86.899(5)degrees, gamma = 76.818(5)degrees, V = 1965.3(14)angstrom(3), Z = 2. The coordination number of the central Ln(3+) (Ln = Dy, Tm) ion is eight, with six oxygen atoms from three Hbfa ligands and two nitrogen atoms from the phen ligand.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of near-infrared (NIR) luminescent complexes Ho(dbm)(3)L and Pr(dbm)(3)L [where dbm = dibenzoylmethane; L = 1,10-phenanthroline (phen), 2,2'-bipyridine (bipy), or triphenyl phosphate oxide (TPPO)] were synthesized. Their elemental analyses, crystal structures, fluorescence spectra and luminescent lifetimes were successfully investigated.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Rhombohedral-calcite and hexagonal-vaterite types of LuBO:Eu3+ microparticles with various complex self-assembled 3D architectures have been prepared selectively by an efficient surfactant- and template-free hydrothermal process for the first time. X-ray diffraction, scanning electron microscopy, energy-dispersive X-ray spectrometry, transmission electron microscopy, high-resolution transmission electron microscopy, selected area electron diffraction, photoluminescence, and cathodoluminescence spectra as well as kinetic decays were used to characterize the samples.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lu3Ga5O12:Eu3+, Lu3Ga5O12:Tb3+, and Lu3Ga5O12:Pr3+ phosphors were prepared through a Pechini-type sol-gel process. X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), photoluminescence, and cathodoluminescence spectra were utilized to characterize the synthesized phosphors. The XRD results reveal that the sample begins to crystallize at 800 degrees C and fully crystallined pure Lu3Ga5O12 phase can be obtained at 1000 degrees C. The FESEM image indicates that the phosphor sample is composed of aggregated rice grainlike particles with sizes around 80-120 nm.