A unique strategy was adopted here to improve the compatibility between the components of an immiscible polymer blend and strengthen the interface. PMMA, a mutually miscible polymer to both PVDF and ABS, improved the compatibility between the phases by localizing at the blends interface. This was supported by the core-shell formation with PMMA as the shell and ABS as the core as observed from the SEM micrographs. This phenomenon was strongly contingent on the concentration of PMMA in the blends. This strategy was further extended to localize graphene oxide (GO) sheets at the blends interface by chemically coupling it to PMMA (PMMA-g-GO). A dramatic increment of ca. 84% in the Young's modulus and ca. 124% in the yield strength was observed in the presence of PMMA-g-GO with respect to the neat blends. A simultaneous increment in both the strength and the modulus was observed in the presence of PMMA-g-GO whereas, only addition of GO resulted in a moderate improvement in the yield strength. This study reveals that a mutually miscible polymer can render compatibility between the immiscible pair and can improve the stress transfer at the interface.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new method is presented for the extraction of single-chain form factors and interchain interference functions from a range of small-angle neutron scattering (SANS) experiments on bimodal homopolymer blends. The method requires a minimum of three blends, made up of hydrogenated and deuterated components with matched degree of polymerization at two different chain lengths, but with carefully varying deuteration levels. The method is validated through an experimental study on polystyrene homopolymer bimodal blends with M A≈1/2MB. By fitting Debye functions to the structure factors, it is shown that there is good agreement between the molar mass of the components obtained from SANS and from chromatography. The extraction method also enables, for the first time, interchain scattering functions to be produced for scattering between chains of different lengths. © 2014 The Authors. Published by WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The phase behaviors of comblike block copolymer A(m+1)B(m)/homopolymer A mixtures are studied by using the random phase approximation method and real-space self-consistent field theory. From the spinodals of macrophase separation and microphase separation, we can find that the number of graft and the length of the homopolymer A have great effects on the phase behavior of the blend. For a given composition of comblike block copolymer, increasing the number of graft does not change the macrophase separation spinodal curve but decreases the microphase separation region. The addition of a small quantity of long-chain homopolymer A increases the microphase separation of comblike block copolymer/homopolymer A mixture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

BACKGROUND: How to promote the formation of the gamma-form in a certain propylene-ethylene copolymer (PPR) under atmospheric conditions is significant for theoretical considerations and practical applications. Taking the epitaxial relationship between the alpha-form and gamma-form into account, it is expected that incorporation of some extrinsic alpha-crystals, developed by propylene homopolymer (PPH), can enhance the crystallization of the gamma-form of the PPR component in PPR/PPH blends.RESULTS: The PPH component in the blends first crystallizes from the melt, and its melting point and crystal growth rate decrease with increasing PPR fraction. On the other hand, first-formed alpha-crystals of the PPH component can induce the lateral growth of PPR chains on themselves, indicated by sheaf-like crystal morphology and positive birefringence, which is in turn responsible for enhanced crystallization of the gamma-form of the PPR component.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Compatibility of graft copolymer compatibilized two incompatible homopolymer A and B blends was simulated by using Monte Carlo method in a two-dimensional lattice model. The copolymers with various graft structures were introduced in order to study the effect of graft structure on the compatibility. Simulation results showed that incorporation of both A-g-B (A was backbone) and B-g-A (B was backbone) copolymers could much improve the compatibility of the blends. However, A-g-B copolymer was more effective to compatibilize the blend if homopolymer A formed dispersed phase. Furthermore, simulation results indicated that A-g-B copolymers tended to locate at the interface and anchor two immiscible components when the side chain is relatively long. However, most of A-g-B copolymers were likely to be dispersed into the dispersed homopolymer A phase domains if the side chains were relatively short. On the other hand, B-g-A copolymers tended to be dispersed into the matrix formed by homopolymer B. Moreover, it was found that more and more B-g-A copolymers were likely to form thin layers at the phase interface with decreasing the length of side chain.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cloud-point temperatures (T-cl's) of poly(ethylene oxide) (PEO) and poly(ethylene oxide)-block-polydimethylsiloxane (P(EO-b-DMS)) homopolymer and block-oligomer mixtures were determined by turbidity measurements over a range of temperatures (105 to 130degrees), pressures (1 to 800 bar), and compositions (10-40 wt.-% PEO). The system phase separates upon cooling and T-cl was found to decrease with an increase in pressure for a constant composition. In the absence of special effects, this finding indicates negative excess volumes. Special attention was paid to the demixing temperatures as a function of the pressure for the different polymer mixtures and the plots in the T-phi plane (where phi signifies volume fractions). The cloud-point curves of the polymer mixture under pressures were observed for different compositions. The Sanchez-Lacombe (SL) lattice fluid theory was used to calculate the spinodals, the binodals, the Flory-Huggins (FH) interaction parameter, the enthalphy of mixing, and the volume changes of mixing. The calculated results show that modified P(EO-b-DMS) scaling parameters with the new combining rules can describe the thermodynamics of the PEO/P(EO-b-DMS) system well with the SL theory.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The nonisothermal crystallization behavior of polyethylene oxide (PEO) in poly(ethylene terephthalate)poly(ethylene oxide) (PETPEO) segmented copolymer and PEO homopolymer has been studied by means of differential scanning calorimetry, as well as transmission electron microscope. The kinetics of PEO in copolymer and PEO homopolymer under nonisothermal crystallization condition has been analyzed by Ozawa equation. The results show that Ozawa equation only describes the crystallization behavior of PEO-6000 homopolymer successfully, but fails to describe the whole crystallization process of PEO in copolymer because the secondary crystallization in the later stage could not be neglected. Due to the constraint of PET segments imposed on the PEO segments, a distinct two stage of crystallization of PEO in copolymer has been investigated by using Avrami equation modified by Jeziorny to deal with the nonisothermal crystallization data. In the case of PEO-6000 homopolymer, good linear relation for the whole crystallization process is obtained owing to the secondary crystallization does not occur under our experimental condition. (C) 2001 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The crystallization, morphology, and crystalline structure of dilute solid solutions of tetrahydrofuran-methyl methacrylate diblock copolymer (PTHF-b-PMMA) in poly(ethylene oxide) (PEO) and PTHF have been studied with differential scanning calorimetry (DSC), X-ray, and optical microscopy. This study provides a new insight into the crystallization behavior of block copolymers. For the dilute PTHF-b-PMMA/PEO system containing only 2 to 7 wt % of PTHF content, crystallization of the PTHF micellar core was detected both on cooling and on heating. Compared the crystallization of the PTHF in the dilute solutions with that in the pure copolymer, it was found that the crystallizability of the PTHF micellar core in the solution is much greater than that of the dispersed PTHF microdomain in the pure copolymer. The stronger crystallizability in the solution was presumably due to a softened PMMA corona formed in the solution of the copolymer with PEG. However, the "soft" micelles formed in the solution (meaning that the glass transition temperatures (T-g) of the micelle is lower than the T-m of the matrix phase) showed almost no effects on the spherulitic morphology of the PEO component, compared with that of the pure PEO sample. In contrast, significant effects of the micelles with a "hard" PMMA core (meaning that the T-g of the core is higher than the T-m of the PTHF homopolymer) on the nucleation, crystalline structure, and spherulitic morphology were observed for the dilute PTHF-b-PMMA/PTHF system. (C) 1998 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility of blends of poly(styrene-co-allyl alcohol) (SAA) with poly(methyl methacrylate) (PMMA), poly(ethyl methacrylate) (PEMA), poly(n-butyl methacrylate) (PnBMA), poly-epsilon-caprolactone (PCL) or polycarbonate (PC) has been studied by means of NMR, FT-IR and DSC techniques. It was found that SAA and PMMA, PEMA or PCL form miscible blends and SAA is only partially miscible with PC or PnBMA. Both phenyl groups and hydroxyl groups in SAA are involved in the intermolecular interactions between SAA and PMMA, PEMA or PCL. Also the hydroxyl-carbonyl hydrogen bonds existing in all the miscible blends studied are formed partially at the expense of the disruption of self-association of hydroxyl groups in pure SAA. (C) 1997 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility of blends of poly(styrene-co-acrylonitrile) (SAN) with poly(methyl methacrylate) (PMMA) or poly(ethyl methacrylate) (PEMA) has been investigated by means of NMR and DSC techniques. It is found that there are intermolecular interactions between the phenyl groups in SAN and carbonyl groups in PMMA or PEMA, and the strength of this intermolecular interaction strongly depends on the properties of ester side groups in PEMA or PMMA, composition of the blends and a certain composition of the copolymer. It is this specific interaction instead of the intramolecular repulsion force within the copolymer that plays a key role for the miscibility of SAN/PMMA and SAN/PEMA blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility of blends of poly(vinylidene chloride-co-acrylonitrile) (VDC-AN) and poly(methyl methacrylate) (PMMA) has been studied with DSC, FT-IR, and NMR methods. The results indicate that the VDC-AN/PMMA blends are miscibile on a molecular level, and the dipole-dipole interactions between C=O and C-Cl-2 and/or interpolymer hydrogen bondings between COOCH3 and CN and CCl groups play the role on the miscibility of the blends. It is found that the -CCl2- groups have two different chemical environments in the pure VDC-AN copolymer, which may result from the different configurations of the copolymer, such as -CCl2- groups in the ''alternating'' segments and -CCl2- groups in the ''blocky'' segments as proposed. It is the -CCl2- group in the ''alternating'' segment that takes part in the dipole-dipole interaction with C=O group in PMMA.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Phase behavior of blends of poly(vinyl methyl ether) (PVME) with four styrene-butadienestyrene (SBS) triblock copolymers, being of various molecular weights, architecture, and compositions, was investigated by small-angle light scattering. Small-angle X-ray scattering investigation was accomplished for one blend. Low critical solution temperature (LCST) and a unique phase behavior, resembling upper critical solution temperature (UCST), were observed. It was found that the architecture of the copolymer greatly influenced the phase behavior of the blends. Random phase approximation theory was used to calculate the spinodal phase transition curves of the ABA/C and BAB/C systems; LCST and resembling UCST phase behavior were observed as the parameters of the system changed. Qualitatively, the experimental and the theoretical results are consistent with each other. (C) 1996 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibility of blends of PMMA with SMA (50 wt% MA) has been investigated by means of NMR, FTIR and DSC techniques. The results indicate that the SMA/PMMA blends are miscible on a molecular level, and there are strong intermolecular interactions between the phenyl groups in SMA and carbonyl groups in PMMA. It is the intermolecular interactions instead of the intramolecular repulsion forces within the SMA copolymer that make the SMA/PMMA blends miscible. It is also found that the strength of the intermolecular interactions to some degree depends on the compositions of the blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Miscibility in blends of three styrene-butadiene-styrene and one styrene-isoprene-styrene triblock copolymers containing 28%, 30%, 48%, and 14% by weight of polystyrene, respectively, with poly(vinyl methyl ether) (PVME) were investigated by FTIR spectroscopy and differential scanning calorimetry (DSC). It was found from the optical clarity and the glass transition temperature behavior that the blends show miscibility for each kind of triblock copolymers below a certain concentration of PVME. The concentration range to show miscibility becomes wider as the polystyrene content and molecular weight of PS segment in the triblock copolymers increase. From the FTIR results, the relative peak intensity of the 1100 cm-1 region due to COCH3 band of PVME and peak position of 698 cm-1 region due to phenyl ring are sensitive to the miscibility of SBS(SIS)/PVME blends. The results show that the miscibility in SBS(SIS)/PVME blends is greatly affected by the composition of the copolymers and the polystyrene content in the triblock copolymers. Molecular weights of polystyrene segments have also affected the miscibility of the blends. (C) 1995 John Wiley & Sons, Inc.