997 resultados para Dielectric strength
Resumo:
The dielectric strength of films made from poly(ethylene terephthalate) (PET) coated with a thin layer of polyaniline (PANI) was studied. The PANI layer was deposited on the PET films by the 'in situ' chemical polymerization method. The PANI layer of the PANI/PET films was undoped in NH4OH 0.1 M solution and re-doped with aqueous HCl solution under different pH values varying from 1 to 10. Electric breakdown measurements were performed by applying a voltage ramp and the results showed a dependence of the dielectric strength on the pH of the doping solution due to the changes in the electrical conductivity of the PANI layer. The dielectric strength of PET/PANI films treated under higher pH conditions showed an electric strength about 30% larger than the PET films, since it leads to a non-conductive PANI layer.
Resumo:
In recent times, there has been an ever-growing need for polymer-based multifunctional materials for electronic packaging applications. In this direction, epoxy-Al2O3 nanocomposites at low filler loadings can provide an excellent material option, especially from the point of view of their dielectric properties. This paper reports the dielectric characteristics for such a system, results of which are observed to be interesting, unique, and advantageous as compared to traditionally used microcomposite systems. Nanocomposites are found to display lower values of permittivity/tan delta over a wide frequency range as compared to that of unfilled epoxy. This surprising observation has been attributed to the interaction between the epoxy chains and the nanoparticles, and in this paper this phenomenon is analyzed using a dual layer interface model reported for polymer nanocomposites. As for the other dielectric properties associated with the nanocomposites, the nano-filler loading seems to have a significant effect. The dc resistivity and ac dielectric strength of the nanocomposites were observed to be lower than that of the unfilled epoxy system at the investigated filler loadings, whereas the electrical discharge resistant properties showed a significant enhancement. Further analysis of the results obtained in this paper shows that the morphology of the interface region and its characteristics decide the observed interesting dielectric behaviors.
Resumo:
The re-ignition characteristics (variation of re-ignition voltage with time after current zero) of short alternating current arcs between plane brass electrodes in air were studied by observing the average re-ignition voltages on the screen of a cathode-ray oscilloscope and controlling the rates of rise of voltage by varying the shunting capacitance and hence the natural period of oscillation of the reactors used to limit the current. The shape of these characteristics and the effects on them of varying the electrode separation, air pressure, and current strength were determined.
The results show that short arc spaces recover dielectric strength in two distinct stages. The first stage agrees in shape and magnitude with a previously developed theory that all voltage is concentrated across a partially deionized space charge layer which increases its breakdown voltage with diminishing density of ionization in the field-tree space. The second stage appears to follow complete deionization by the electric field due to displacement of the field-free region by the space charge layer, its magnitude and shape appearing to be due simply to increase in gas density due to cooling. Temperatures calculated from this second stage and ion densities determined from the first stage by means of the space charge equation and an extrapolation of the temperature curve are consistent with recent measurements of arc value by other methods. Analysis or the decrease with time of the apparent ion density shows that diffusion alone is adequate to explain the results and that volume recombination is not. The effects on the characteristics of variations in the parameters investigated are found to be in accord with previous results and with the theory if deionization mainly by diffusion be assumed.
Resumo:
Fine particles of barium ferrite (BaFe12O19) were synthesized by the conventional ceramic technique. These materials were then characterized by the X-ray diffraction method and incorporated in the natural rubber matrix according to a specific receipe for various loadings of ferrite. The rubber ferrite composites (RFC) thus obtained have several applications, and have the advantage of molding into complex shapes. For applications such as microwave absorbers, these composites should have an appropriate dielectric strength with the required mechanical and magnetic properties. The N330 (HAF) carbon black has been added to these RFCs for various loadings to modify the dielectric and mechanical properties. In this article we report the effect of carbon black on the mechanical and dielectric properties of these RFCs. Both the mechanical and dielectric properties can be enhanced by the addition of an appropriate amount of carbon black
Resumo:
Overhead distribution lines are often exposed to lightning overvoltages, whose waveforms vary widely and can differ substantially from the standard impulse voltage waveform (1,2 - 50). Different models have been proposed for predicting the strength of insulation subjected to impulses of non-standard waveforms. One of the most commonly used is the disruptive effect model, for which there are different methods for the estimation of the parameters required for its application. This paper aims at evaluating the dielectric behavior of medium voltage insulators subjected to impulses of non-standard waveforms, as well as at evaluating two methods for predicting their dielectric strength against such impulses. The test results relative to the critical lightning impulse flashover voltage (U50) and the volt-time characteristics obtained for the positive and negative polarities of different voltage waveforms are presented and discussed.
Resumo:
Circuit-breakers (CBs) are subject to electrical stresses with restrikes during capacitor bank operation. Stresses are caused by the overvoltages across CBs, the interrupting currents and the rate of rise of recovery voltage (RRRV). Such electrical stresses also depend on the types of system grounding and the types of dielectric strength curves. The aim of this study is to demonstrate a restrike waveform predictive model for a SF6 CB that considered the types of system grounding: grounded and non-grounded and the computation accuracy comparison on the application of the cold withstand dielectric strength and the hot recovery dielectric strength curve including the POW (point-on-wave) recommendations to make an assessment of increasing the CB remaining life. The simulation of SF6 CB stresses in a typical 400 kV system was undertaken and the results in the applications are presented. The simulated restrike waveforms produced with the identified features using wavelet transform can be used for restrike diagnostic algorithm development with wavelet transform to locate a substation with breaker restrikes. This study found that the hot withstand dielectric strength curve has less magnitude than the cold withstand dielectric strength curve for restrike simulation results. Computation accuracy improved with the hot withstand dielectric strength and POW controlled switching can increase the life for a SF6 CB.
Resumo:
A breaker restrike is an abnormal arcing phenomenon, leading to a possible breaker failure. Eventually, this failure leads to interruption of the transmission and distribution of the electricity supply system until the breaker is replaced. Before 2008, there was little evidence in the literature of monitoring techniques based on restrike measurement and interpretation produced during switching of capacitor banks and shunt reactor banks in power systems. In 2008 a non-intrusive radiometric restrike measurement method and a restrike hardware detection algorithm were developed by M.S. Ramli and B. Kasztenny. However, the limitations of the radiometric measurement method are a band limited frequency response as well as limitations in amplitude determination. Current restrike detection methods and algorithms require the use of wide bandwidth current transformers and high voltage dividers. A restrike switch model using Alternative Transient Program (ATP) and Wavelet Transforms which support diagnostics are proposed. Restrike phenomena become a new diagnostic process using measurements, ATP and Wavelet Transforms for online interrupter monitoring. This research project investigates the restrike switch model Parameter „A. dielectric voltage gradient related to a normal and slowed case of the contact opening velocity and the escalation voltages, which can be used as a diagnostic tool for a vacuum circuit-breaker (CB) at service voltages between 11 kV and 63 kV. During current interruption of an inductive load at current quenching or chopping, a transient voltage is developed across the contact gap. The dielectric strength of the gap should rise to a point to withstand this transient voltage. If it does not, the gap will flash over, resulting in a restrike. A straight line is fitted through the voltage points at flashover of the contact gap. This is the point at which the gap voltage has reached a value that exceeds the dielectric strength of the gap. This research shows that a change in opening contact velocity of the vacuum CB produces a corresponding change in the slope of the gap escalation voltage envelope. To investigate the diagnostic process, an ATP restrike switch model was modified with contact opening velocity computation for restrike waveform signature analyses along with experimental investigations. This also enhanced a mathematical CB model with the empirical dielectric model for SF6 (sulphur hexa-fluoride) CBs at service voltages above 63 kV and a generalised dielectric curve model for 12 kV CBs. A CB restrike can be predicted if there is a similar type of restrike waveform signatures for measured and simulated waveforms. The restrike switch model applications are used for: computer simulations as virtual experiments, including predicting breaker restrikes; estimating the interrupter remaining life of SF6 puffer CBs; checking system stresses; assessing point-on-wave (POW) operations; and for a restrike detection algorithm development using Wavelet Transforms. A simulated high frequency nozzle current magnitude was applied to an Equation (derived from the literature) which can calculate the life extension of the interrupter of a SF6 high voltage CB. The restrike waveform signatures for a medium and high voltage CB identify its possible failure mechanism such as delayed opening, degraded dielectric strength and improper contact travel. The simulated and measured restrike waveform signatures are analysed using Matlab software for automatic detection. Experimental investigation of a 12 kV vacuum CB diagnostic was carried out for the parameter determination and a passive antenna calibration was also successfully developed with applications for field implementation. The degradation features were also evaluated with a predictive interpretation technique from the experiments, and the subsequent simulation indicates that the drop in voltage related to the slow opening velocity mechanism measurement to give a degree of contact degradation. A predictive interpretation technique is a computer modeling for assessing switching device performance, which allows one to vary a single parameter at a time; this is often difficult to do experimentally because of the variable contact opening velocity. The significance of this thesis outcome is that it is a non-intrusive method developed using measurements, ATP and Wavelet Transforms to predict and interpret a breaker restrike risk. The measurements on high voltage circuit-breakers can identify degradation that can interrupt the distribution and transmission of an electricity supply system. It is hoped that the techniques for the monitoring of restrike phenomena developed by this research will form part of a diagnostic process that will be valuable for detecting breaker stresses relating to the interrupter lifetime. Suggestions for future research, including a field implementation proposal to validate the restrike switch model for ATP system studies and the hot dielectric strength curve model for SF6 CBs, are given in Appendix A.
Resumo:
Polycrystalline SrTiO3 films were prepared by pulsed excimer laser ablation on Si and Pt coated Si substrates. Several growth parameters were varied including ablation fluence, pressure, and substrate temperature. The structural studies indicated the presence of [100] and [110] oriented growth after annealing by rapid thermal annealing at 600-degrees-C for 60 s. Deposition at either lower pressures or at higher energy densities encouraged film growth with slightly preferred orientation. The scanning electron microscopy studies showed the absence of any significant particulates on the film surface. Dielectric studies indicated a dielectric constant of 225, a capacitance density of 3.2 fF/mum2, and a charge density of 40 fC/mum for films of 1000 nm thick. The dc conductivity studies on these films suggested a bulk limited space charge conduction in the high field regime, while the low electric fields induced an ohmic conduction. Brief time dependent dielectric breakdown studies on these films, under a field of 250 kV/cm for 2 h, did not exhibit any breakdown, indicating good dielectric strength.
Resumo:
In recent years, the time dependant maintenance of expensive high voltage power equipments is getting replaced by condition based maintenance so as to detect apriori an impending failure of the equipment. For condition based maintenance, most monitoring systems concentrate on the electrical quantities such as measurement and evaluation of partial discharges, tan delta, tip-up test, dielectric strength, insulation resistance, polarization and depolarization current. However, in the case of equipments being developed with novel nanodielectric insulating materials, the variation in these parameters before an impending failure is not available. Hence in this work, accelerated electrothermal aging studies have been conducted on unfilled epoxy as well as epoxy nanocomposite samples of 5 wt% filler loading, and the tan d values were continuously monitored to obtain the condition of the samples under study. It was observed that those samples whose tan d increased at a rapid rate failed first.
Resumo:
Composites made of Calcium-modified lead titanate (PTCa) and poly (ether-etherketone) (PEEK) high performance polymer matrix were prepared in the film form using a hot press. The ceramic volume fraction reaches up to 60 percent providing a composite with 0-3 and 1-3 mixed connectivities due to the high ceramic content and the resulting materials could be considered PEEK-bonded PTCa particulate composite. The composites were characterized using piezoelectric spectroscopy and ultrasonic immersion techniques. Values up to 38.5 pC/N were obtained for the longitudinal d33 piezoelectric coefficient. The composite was surface-mounted on a carbon fiber plate-like specimen and the ability of the PTCa/PEEK composite to detect acoustic emission (AE) is reported. © 2006 IEEE.
Resumo:
Die FT-Rheologie wird zur Unterscheidung verschiedener Kamm-Topologien in Polystyrollösungen und –schmelzen angewendet. Die Polystyrole werden in Abhängigkeit der Deborahzahl De unter LAOS-Bedingungen vermessen. Die Meßergebnisse zeigen, daß der Schritt von wohldefinierten Systemen (lineare Ketten, Sterne) zu solchen mit statistischer Verteilung wie in Kämmen zu großen Veränderungen sowohl im linearen als auch im nichtlinearen Bereich der rheologischen Messungen führt. Sowohl die Masterkurven als auch die Intenstiäten I3/1 und Phasen Phi3 der Nichtlinearitäten der einzelnen Proben weisen jeweils deutliche Unterschiede untereinander auf. Diese sind durch die bisherigen Ergebnisse noch nicht vollständig mit topologischen Merkmalen in Verbindung zu bringen. Die Messungen wurden mit dem von McLeish eingeführten Pom-pom Modell und daraus weiterentwickelten double convected-Pom-pom Modell (DCPP) simuliert und lieferten gute Übereinstimmung sowie auch Vorhersagen über den experimentell nicht mehr zugänglichen Bereich. Zur Untersuchung des Einflusses von mechanischer Scherung auf die lokale, molekulare Dynamik wird das LAOS-Experiment in situ mit dielektrischer Spektroskopie kombiniert. Dazu wurde eine Apparatur entwickelt, die das hochsensitive ARES-Rheometer mit dem hochauflösenden dielektrischen ALPHA-Analyzer verbindet. Mit dieser Apparatur wurde das Typ-A Polymer 1,4-cis-Polyisopren, mit einem Dipolmoment entlang des Rückgrats, bei oszillatorischer Scherung unter gleichzeitiger Aufnahme eines dielektrischen Spektrums vermessen. Es konnte gezeigt werden, daß die oszillatorische Verscherung weder die charakteristische Relaxationszeit noch die Form des Normal Mode Peaks beeinflußt, wohl aber die dielektrische Stärke Delta epsilon. Diese entspricht der Fläche unter dem e“-Peak und kann mit einer Debye- und einer Cole/Davidson-Funktion angepasst werden. Die Abnahme der dielektrischen Stärke mit zunehmender Scheramplitude kann mit der Orientierungsverteilung der End-zu-End-Vektoren in der Probe erklärt werden.
Resumo:
In this paper we present results on measurements of the dielectric strength of liquid argon near its boiling point and cathode-anode distances in the range of 0.1 mm to 40 mm with spherical cathode and plane anode. We show that at such distances the applied electric field at which breakdowns occur is as low as 40 kV/cm. Flash-overs across the ribbed dielectric of the high voltage feed-through are observed for a length of 300 mm starting from a voltage of 55 kV. These results contribute to set reference for the breakdown-free design of ionization detectors, such as Liquid Argon Time Projection Chambers (LAr TPC).
Resumo:
O trabalho aborda o estudo e o desenvolvimento de um interferômetro sensor de alta tensão, baseado em célula Pockels (modulador eletro-óptico) na topologia reflexiva (\"double pass\") e que é parte integrante de um Transformador de Potencial Óptico (TPO), que utiliza sistema interferométrico de luz branca (WLI-White Light Interferometry), que está sendo desenvolvido pelo grupo do Laboratório de Sensores Ópticos (LSO) do PEA-EPUSP, e é capaz de medir diretamente tensões presentes em sistema elétrico de potência (SEP) classe 69kVRMS. Para desenvolver o tema proposto foi feita uma revisão da literatura baseada em livros, artigos e teses para identificar topologias em moduladores eletro-ópticos transmissiva (\"single pass\") e reflexiva (\"double pass\") para definir o tipo de modulador mais adequado para a aplicação em questão. A partir dos estudos e implementações realizadas, verificou-se um enorme potencial para o desenvolvimento e aplicação da topologia \"double pass\" no sensor interferométrico da célula de alta tensão do TPO. A topologia mostrou-se vantajosa em relação aos protótipos dos TPOs desenvolvidos anteriormente, a partir de características tais como: a facilidade de recurso de alinhamento do feixe de luz, construção e reprodução relacionados ao cristal eletro-óptico, diminuição do número de componentes ópticos volumétricos e aumento da rigidez dielétrica da célula sensora. Simulações computacionais foram realizadas mediante a aplicação do método dos elementos finitos (MEF) que contribuíram para o auxílio do projeto da célula sensora, particularmente, para estimativa do valor da voltagem de meia onda, V?, parâmetro importante para o projeto do TPO. Um protótipo do TPO com célula sensora de alta tensão reflexiva foi implementado e testado no laboratório de alta tensão do IEEUSP a partir de ensaios com tensões nominais de 69kVrms a 60Hz e máxima de 140kVrms a 60 Hz. Como resultado deste trabalho, amplia-se o conhecimento e domínio das técnicas de construção de interferômetros sensores de alta tensão na topologia reflexiva aplicadas a TPOs.
Resumo:
The electrical ceramic insulators industry, uses noble raw materials such as siliceous and aluminous clays of white burning, in order to provide plasticity of the mass and contribute to electrical and mechanical properties required of the product, and feldspar with the flux function In literature references the composition of the masses indicates that the clay participates in percentage between 20 and 32, and feldspar 8 to 35, these materials have significant cost. In this research was performed the total replacement of commercial clay, for white burning clay from Santa Luzia region in southern Bahia and partial replacement of feldspar by ash residue of husk conilon coffee burning, from extreme south of Bahia. The objective of replacement these raw materials is to aver its technical feasibility and call attention for the embryo pole of ceramic industry for the existing in the south and extreme south of Bahia, which has significant reserves of noble raw materials such as clay white burning, kaolin, quartz and feldspar, and generates significant volume of gray husk conilon coffee as alternate flux. Clay Santa Luzia is prima noble material whose current commercial application is the production of white roofing. The residue of coffee husk ash is discarded near of production sites and is harmful to the environment. Phase diagrams and statistic design of experiments, were used for optimization and cost savings in research. The results confirmed the expectations of obtaining electrical ceramic insulators, with white burning clay of Santa Luzia and partial replacement up to 35.4% of feldspar, by treaty residue of conilon ash coffee husk burning. The statistic design that showed best results was for formulation with percentages of: clay 26.4 to 30.4%; kaolin 14.85 to 17.1%; feldspar 12.92 to 16.96%; R2 residue 7.08 to 9.2% and Quartz 32.5 to 38.75%, relative to the total mass of the mixture. The best results indicated; 0.2 to 1.4% apparent porosity , water absorption 0.1 to 0.7%, flexural strength 35 to 45MPa , dielectric strength 35-41 kV/cm , the transverse resistivity 8x109 2.5x1010 Ω.cm and for the dielectric constant ε/ε0 7 to 10.4, specification parameters for manufacturing ceramic electrical insulators of low and medium voltage.