6 resultados para Deagglomeration
Resumo:
Different types of aerosolization and deagglomeration testing systems exist for studying the properties of nanomaterial powders and their aerosols. However, results are dependent on the specific methods used. In order to have well-characterized aerosols, we require a better understanding of how system parameters and testing conditions influence the properties of the aerosols generated. In the present study, four experimental setups delivering different aerosolization energies were used to test the resultant aerosols of two distinct nanomaterials (hydrophobic and hydrophilic TiO2). The reproducibility of results within each system was good. However, the number concentrations and size distributions of the aerosols created varied across the four systems; for number concentrations, e.g., from 10(3) to 10(6) #/cm(3). Moreover, distinct differences were also observed between the two materials with different surface coatings. The article discusses how system characteristics and other pertinent conditions modify the test results. We propose using air velocity as a suitable proxy for estimating energy input levels in aerosolization systems. The information derived from this work will be especially useful for establishing standard operating procedures for testing nanopowders, as well as for estimating their release rates under different energy input conditions, which is relevant for occupational exposure.
Resumo:
Ba0.77Ca0.23TiO3 ceramics were produced in this work starting from nanopowders synthesized via a polymeric precursor method. By adjusting the pH values of the precursor solutions above 7, it was possible to prepare powders weakly aggregated and with a smaller particle size, both facts which traduced into an enhanced nanopowders' sintering process at comparatively lower temperatures. Irrespective of the initial pH value, highly-dense and second phase-free ceramics were obtained following optimal sintering parameters (temperature and time) extracted from dilatometric and density measurements. By considering these and other sintering conditions, moreover, polycrystalline materials with an average grain size varying from 0.35 to 8 mm were produced, the grain growth process involving liquid phase-assisted sintering for heat treatments achieved at 1320 °C. The study of grain size effects on the ferroelectric properties of these materials was conducted, the results being discussed in the light of previous debates, including grain size-dependent degree of tetragonal distortion in such materials, as verified in this work.
Resumo:
Stability of airborne nanoparticle agglomerates is important for occupational exposure and risk assessment in determining particle size distribution of nanomaterials. In this study, we developed an integrated method to test the stability of aerosols created using different types of nanomaterials. An aerosolization method, that resembles an industrial fluidized bed process, was used to aerosolize dry nanopowders. We produced aerosols with stable particle number concentrations and size distributions, which was important for the characterization of the aerosols' properties. Next, in order to test their potential for deagglomeration, a critical orifice was used to apply a range of shear forces to them. The mean particle size of tested aerosols became smaller, whereas the total number of particles generated grew. The fraction of particles in the lower size range increased, and the fraction in the upper size range decreased. The reproducibility and repeatability of the results were good. Transmission electron microscopy imaging showed that most of the nanoparticles were still agglomerated after passing through the orifice. However, primary particle geometry was very different. These results are encouraging for the use of our system for routine tests of the deagglomeration potential of nanomaterials. Furthermore, the particle concentrations and small quantities of raw materials used suggested that our system might also be able to serve as an alternative method to test dustiness in existing processes.
Resumo:
The study of the photoluminescent properties affected by order and disorder of the BaMoO4 powders is the principal objective in this work. BaMoO4 compounds were prepared using soft chemical process called Complex Polymerization Method. In this work, different deagglomeration types and different heating rates were used to promote different disorder degrees. Scheelite type phase (BaMoO4) was determined by X-ray Diffraction (XRD), Fourier Transformed Infra-Red (FTIR) and Raman spectroscopy after heat treating the sample at 400 degrees C. The room temperature luminescence spectra revealed an intense single-emission band in the visible region. Based on XRD and Raman data it was observed that the transition between the completely disordered structure to completely ordered structure is a good condition for photoluminescence (PL) emission. The best PL emission is obtained when the material possesses short range disorder, i.e., is periodically ordered (XRD), but some disorder as measured by Raman spectroscopy. The excellent optical properties observed for disordered BaMoO4 suggested that this material is a highly promising candidate for optical applications.
Resumo:
Payload and high-tech are important characteristics when the goals are aerospace applications. The development of the technologies associated to these applications has interests that transcend national boundaries and are of strategic importance to the nations. Ultra lightweight mirrors, supports and structures for optical systems are important part of this subject. This paper reports the development of SiC substrates, obtained by pressing, to be applied on embedded precision reflective optics. Different SiC granulometries, having YAG as sintering additive, were processed by: ball milling, drying and deagglomeration, sift, uniaxial and isostatic pressing, and, finally, argon atmosphere sintering at 1900°C. Different porosities were obtained according to the amount of organic material added. Into one side of the samples pellets of organic material were introduced to generate voids to reduce the weight of samples as a whole. The substrates were grinding and polished, looking for a SiC surface having low porosity, as porosity is directly related to light scattering that should be avoided on optical surfaces. Laser surface treatments were applied (using or not SiC barbotine) as a method to improve the surface quality. The samples were characterized by optical and laser confocal microscopy, roughness measurements and mechanical tests. The results are very promissory for future applications. © 2012 Materials Research Society.
Resumo:
Das Ziel dieser Arbeit besteht darin, die Möglichkeiten der Sprühtrocknung für die Generierung von Inhalationspulvern zur Therapie von Lungenkrankheiten zu nutzen. Die Erzeugung von physikalisch stabilen und leicht dispergierbaren Partikeln steht hierbei im Vordergrund. Aufgrund von physiko-chemischen Untersuchungen (Glasübergangstemperatur, Fragilität, Relaxationsverhalten, Hygroskopizität) unterschiedlicher amorpher Hilfsstoffe (Lactose, Raffinose, Dextrane, Cyclodextrine) ist für Hydroxypropyl-β-Cyclodextrin das größte Potential für die Stabilisierung eines Wirkstoffes innerhalb einer amorphen Matrix erkennbar. Sprühgetrocknete Partikel weisen im Vergleich zu strahlgemahlenen Partikeln günstigere Dispergier- und Depositionseigenschaften auf. Dies ist vorrangig auf größere Berührungsflächen zwischen strahlgemahlenen Partikeln zurückzuführen. Kugelförmige sprühgetrocknete Partikel besitzen dagegen aufgrund einer punktförmigen Berührung geringere Haftkräfte. Versuche mit unterschiedlich stark gefalteten Partikeloberflächen weisen auf geringere Haftkräfte hin, wenn sich die Partikel an Stellen geringerer Krümmungsradien berühren. Dispergierversuche in einer definierten Rohrströmung (Deagglomerator) lassen auf einen kaskadenartigen Agglomeratzerfall schließen. Durch Sprüheinbettung unterschiedlicher Modellwirkstoffe (Salbutamolsulfat, Ipratropiumbromid, Budesonid) in Hydroxypropyl-β-Cyclodextrin konnten sowohl Einzelformulierungen als auch eine Kombinationsformulierung mit allen drei Wirkstoffen erzeugt werden. Diese weisen bei einem Wirkstoffgehalt bis max. 14% selbst nach vierwöchiger Offenlagerung bei 40°C und 75% r.F. keine bzw. nur geringfügige Veränderungen in der „Fine Particle Dose“ (FPD) auf. Die „Fine Particle Fraction“ (FPF) liegt bei diesen Formulierungen im Bereich von 40% bis 75%. In Verbindung mit einem geeigneten Pack- bzw. Trockenmittel, ist hierbei mit einer physikalischen Stabilität zu rechnen, die eine sinnvolle Produktlaufzeit eines Inhalationspulvers ermöglicht. Formulierungen mit höheren Wirkstoffkonzentrationen zeigen dagegen stärkere Veränderungen nach Stresslagerung. Als Beispiel einer kristallinen Sprühtrocknungsformulierung konnte ein Pulver bestehend aus Mannitol und Budesonid erzeugt werden.