999 resultados para Cross-relaxation
Resumo:
H-1- and C-13-NMR spectroscopy and FT-Raman spectroscopy are used to investigate the properties of a polymer gel dosimeter post-irradiation. The polymer gel (PACT) is composed of acrylamide, N,N'-methylene-bisacrylamide, gelatin, and water. The formation of a polyacrylamide network within the gelatin matrix follows a dose dependence nonlinearly correlated to the disappearance of the double bonds from the dissolved monomers within the absorbed dose range of 0-50 Gy. The signal from the gelatin remains constant with irradiation. We show that the NMR spin-spin relaxation times (T-2) of PAGs irradiated to up to 50 Gy measured in a NMR spectrometer and a clinical magnetic resonance imaging scanner can be modeled using the spectroscopic intensity of the growing polymer network. More specifically, we show that the nonlinear T-2 dependence against dose can be understood in terms of the fraction of protons in three different proton pools. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Therllloelynalllics of lllodel 11lel1ll)rane systeills containing 1110nollnsaturatecl I)lloSI)holil) ids is strongly infllienced l)y the I)osition of the C==C dOlll)le })ond in tIle acyl chain. The telllI)eratllres of both chain-nlelting (TM) and La -+ HI! (TH) I)hase traIlsitions are lowered by IIp to 20°C when C==C is Inoved froln positions 6 or 11 to I)osition 9 in an 18-carl)on chain. This work is an attellll)t to ellicidate the uIlderlying Illoleclilar Illechanisllls reSI)Onsi])le for tllese draillatic tllerillodynaillic changes. Mixtllres of di-18: 1 l)hoSI)hatidylethanolanline with C==C at l)ositioIlS 6, 9, 11 were llsed, witll a sI1lall aI1lOlint of I)erdellterated tetradecanol, known to })e a gooel rel)Orter of the cllain Illoleclilar order. SI)ectral second 11I0I1lents were llsed to Illonitor tIle La -+ HII I)hase transition, which was fOllnd to ])e ])road (2-6°C), with a slight llysteresis on heatiIlg/cooling. The orientational order I)rofiles were nleasllred 1lSiIlg 2H Illiclear Illagnetic resonance and changes in these order I)rofiles between La aIld HII I)hases silow l)oth a local increase in order in the vicinity of the C==C bonds and an o\Terall decrease ill the average orientational order of the chain as a whole. These Sll])tle changes recluire })oth high-fidelity SI)ectrosCol)y and a careflll data analysis that takes into aCCOllnt the effects due to l)artiall1lagnetically-indllced orientational ordering of the l)ilayers. In tIle COIltext of SOllle recently rel)Orted cross-relaxation 11leaSlirenlents in Silllilar l)llOSI)llolil)iels, 0111' reslilts sllggest that large-anll)litllde conforlllational changes in the interior of tIle I110del 111eI11])ranes I)lay a 1110re significant role than I)reviollsly thOllght.
Resumo:
Gadolinium oxysulfide powders doped with different Tb3+ concentrations were prepared from sulfur vaporization on rare earths' basic carbonate precursors. Single-phase Gd2O2S samples were obtained, with Tb3+ doping up to 9 at%. The study of the excitation mechanisms revealed that the Tb3+ emission might occur after the direct Tb3+ excitation either by energy transfer from Gd3+ or from the phosphor host. The characteristic terbium emission lines were observed, resulting from the radiative decay from D-5(3) or D-5(4), to F-7(j) levels. The cross-relaxation phenomenon was observed and its effects on the materials emission color were discussed based on the CIE diagram. By using time-resolved spectroscopy, D-5(3) -> F-7(J) and D-5(4) -> F-7(J) transitions were separated. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
In this work, GdAlO3:Pr3+ was successfully prepared by the Pechini method at lower temperatures when compared to others methods such as solid-state synthesis and sol-gel process. In accordance to the XRD data, the fully crystalline single-phase GdAlO3 could be obtained at 900 degrees C. Luminescence measurements indicate Gd -> Pr3+ energy transfer. In the emission spectra, the P-3(0) ->(3) H-4 (blue emission) and D-1(2) ->(3) H-4 (red emission) transitions of Pr3+ ions can be observed and the ratio between their intensities depends on the Pr3+ content due to the cross-relaxation phenomenon.
Resumo:
In this work, GdAlO3:RE3+ (RE = Eu or Tb) was successfully prepared by the Pechini method at lower temperatures when compared to others methods as solid-state synthesis and sol-gel process. In accordance to the XRD data, the fully crystalline single-phase GdAlO3 could be obtained at 900 degrees C. The differential thermal analysis (DTA) shows a crystallization peak at 850 degrees C. The samples are composed by monocrystalline particles (50-120 nm) exhibiting the formation of aggregates among them, which indicates the beginning of the sinterization process. This feature indicates a strong tendency to the formation of aggregates, which is a suitable ability for the close-packing of particles, and hence a potential application in X-ray intensifying screens. Luminescence measurements indicate Gd3+ -> RE3+ energy transfer. The Eu3+ emission spectra exhibit all the characteristics D-5(0) -> F-7(j) transitions and the observed profile suggests that RE3+ ions occupy at least one site without center of symmetry. For terbium-doped samples, the D-5(3) -> F-7(j) (blue emission) and D-5(4) -> F-7(j) (green emission) transitions were observed and the ratio between them may depend on the Tb3+ content due to cross-relaxation processes. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Red, green, and blue emission through frequency upconversion and energy-transfer processes in tellurite glasses doped with Tm3+ and Er3+ excited at 1.064 mum is investigated. The Tm3+/Er3+-codoped samples produced intense upconversion emission signals at around 480, 530, 550 and 660 nm. The 480 nm blue emission was originated from the (1)G(4)-->H-3(6) transition of the Tm3+ ions excited by a multiphoton stepwise phonon-assisted excited-state absorption process. The 5 30, 5 50 nm green and 660 mn red upconversion luminescences were identified as originating from the H-2(11/2), S-4(3/2) --> I-4(15/2) and F-4(9/2) --> I-4(15/2) transitions of the Er3+ ions, respectively, populated via efficient cross-relaxation processes and excited-state absorption. White light generation employing a single infrared excitation source is also examined. (C) 2003 Elsevier B.V. (USA). All rights reserved.
Resumo:
Intense red upconversion emission around 650 nm in PbGeO3-PbF2-CdF2 transparent glass ceramic containing beta-PbF2:Ho3+ nanocrystals, is presented. The holmium-doped vitroceramic samples were excited by a 980 nm diode laser source. The 650 nm upconversion signal was assigned to the F-5(5) --> I-5(8) transition of holmium ions. Very low intensity signals around 490 and 540 nm corresponding to the F-5(2,3) --> I-5(8) and S-4(2), F-5(4) --> I-5(8) transitions, respectively, were also detected. The upconversion excitation mechanism was achieved through a combination of stepwise phonon-assisted multiphoton absorption, cross-relaxation processes involving pairs of holmium ions, and excited-state absorption. Using a diode laser pump source around 850 nm green upconversion emission around 540 nm was the observed predominant signal. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Frequency upconversion luminescence in erbium-doped PbGeO3-PbF2-CdF2-based transparent glass ceramics (TGC) under 980 nm infrared excitation is investigated. Upconversion emission signals around 410, 525, 550, 660, and 850 nm were generated and identified as due to the H-2(9/2) H-2(11/2), S-4(3/2), and F-4(9/2) transitions to the I-4(15/2) ground-state, and S-4(3/2)-I-4(13/2), respectively. The erbium ions excited-state emitting levels were populated via a combination of stepwise ground-state absorption (GSA), excited-state absorption (ESA), and cross-relaxation processes. The results also disclosed that both blue (410 nm) and red (660 nm) upconversion emission signals in the transparent glass ceramic sample presented twice as much intensity as compared to its vitreous counterpart. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The deactivation of the two lowest excited states of Ho3+ was investigated in Ho3+ singly doped and Ho3+, Pr3+-codoped fluoride (ZBLAN) glasses. We establish that 0.1-0.3 mol % Pr3+ can efficiently deactivate the first excited (I-5(7)) state of Ho3+ while causing a small reduction of similar to 40% of the initial population of the second excited (I-5(6)) state. The net effect introduced by the Pr3+ ion deactivation of the Ho3+ ion is the fast recovery of the ground state of Ho3+. The Burshstein model parameters relevant to the Ho3+-> Pr3+ energy transfer processes were determined using a least squares fit to the measured luminescence decay. The energy transfer upconversion and cross relaxation parameters for 1948, 1151, and 532 nm excitations of singly Ho3+-doped ZBLAN were determined. Using the energy transfer rate parameters we determine from the measured luminescence, a rate equation model for 650 nm excitation of Ho3+-doped and Ho3+, Pr3+-doped ZBLAN glasses was developed. The rate equations were solved numerically and the population inversion between the I-5(6) and the I-5(7) excited states of Ho3+ was calculated to examine the beneficial effects on the gain associated with Pr3+ codoping. (c) 2007 American Institute of Physics.
Resumo:
The mechanism involved in the Tm3+ (F-3(4))-->Ho3+ (I-5(7)) energy transfer and Tm3+ (H-3(4), H-3(6))-->Tm3+ (F-3(4), F-3(4)) cross relaxation as a function of the donor and acceptor concentrations was investigated in Tm-Ho-codoped fluorozirconate glasses. The experimental transfer rates were determined for the Tm-->Ho energy transfer from the best fit of the acceptor luminescence decay using an expression which takes into account the Inokuti-Hirayama model and localized donor-to-acceptor interaction solution. The original acceptor solution derived from the Inokuti-Hirayama model fits well the acceptor luminescence transient only for low-concentrated systems. The results showed that a fast excitation diffusion that occurs in a very short time (t<
Resumo:
Fluorindate glasses containing 1,2,3,4 ErF3 mol % were prepared in a dry box under argon atmosphere. Absorption, Stokes luminescence (under visible and infrared excitation), the dependence of 4S3/2, 4I11/2, and 4I13/2 lifetimes with Er concentration, and upconversion under Ti-saphire laser excitation at λ=790 nm were measured, mostly at T=77 and 300 K. The upconversion results in a strong green emission and weaker blue and red emissions whose intensity obeys a power-law behavior I∼Pn, where P is the infrared excitation power and n=1.6, 2.1, and 2.9 for the red, green, and blue emissions, respectively. The red emission exponent n=1.5 can be explained by a cross relaxation process. The green and blue emissions are due to excited state absorption (ESA) and energy transfer (ET) processes that predict a factor n=2 and n=3 for the green and blue emissions, respectively. From transient measurements we concluded that for lightly doped samples the green upconverted emission is originated due to both processes ESA and ET. However, for heavily doped samples ET is the dominant process.
Resumo:
Energy transfer processes between Er3+ and Tm3+ were investigated examining the frequency upconversion emissions in a fluoroindate glass pumped at 790 nm. A 60-fold enhancement in the emission at ≈670 nm originating from Er3+ was observed when Tm3+ at concentration of 2% was introduced in a sample containing 2% of Er3+. The results are explained considering the influence of cross-relaxation processes between the active ions. © 2002 Elsevier Science B.V. All rights reserved.
Resumo:
The population inversion of the Tm3+ in GLKZ glass involved in the 1470 nm emission (3H4 → 3F 4) as a function of Tb (or Eu) concentration was calculated by computational simulation for a CW laser pumping at 792 nm. These calculations were performed using the experimental Tm→Tb an Tm→Eu transfer rates and the spectroscopic parameters of the Tm (0.1 mol %) system. The result shows that 0.2 mol % (Tb3+) and 0.4 mol % of Eu3+ ions propitiate best population inversion of Tm3+ (0.1 mol %) maximizing the amplification coefficient of germanate (GLKZ) glass when operating as laser intensity amplification at 1470 nm. Besides the effective deactivation of the 3F4 level, the presence of Tb3+ or Eu 3+ ions introduce a depopulation of the 3H4 emitting level by means of a cross relaxation process with Tm3+ ions. In spite of this, the whole effect is verified to be benefic for using Tm-doped GLKZ glass codoped with Tb3+ or Eu3+ as a suitable material for confectioning optical amplifiers that operates in the S-band for telecommunication.
Resumo:
The infrared-to-visible frequency upconversion was investigated in Er 3+-doped Ga10Ge25S65 glass and in the transparent glass-ceramic obtained by heat-treatment of the glass above its glass-transition temperature. Continuous-wave and pulsed lasers operating at 980 nm and 1480 nm were used as excitation sources. The green (2H 11/2 → 4I15/2; 4S3/2 → 4I15/2) and red (4F9/2 → 4I15/2) photoluminescence (PL) signals due to the Er3+ ions were characterized. The PL decay times were influenced by energy transfer among Er3+ ions, by cross-relaxation processes and by energy transfer from the Er3+ ions to the host material. The PL from the Er3+ ions hosted in the crystalline phase was distinguished only when the glass-ceramic was excited by the 1480 nm pulsed laser. The excitation pathways responsible for the green and red PL bands are discussed to explain the differences between the spectra observed under continuous-wave and pulsed excitation. © 2013 American Institute of Physics.
Resumo:
Processes involving visible to infrared energy conversion are presented for Pr3+-Yb3+ co-doped fluoroindate glasses. The emission in the visible and infrared regions, the luminescence decay time of the Pr 3+:3P0 → 3H4 (482 nm), Pr3+:1D2 → 3H6 (800 nm), Yb3+:2F5/2 → 2F 7/2 (1044 nm) transitions and the photoluminescence excitation spectra were measured in Pr3+ samples and in Pr3+-Yb 3+ samples as a function of the Yb3+ concentration. In addition, energy transfer efficiencies were estimated from Pr3+: 3P0 and Pr3+:1D2 levels to Yb3+:2F7/2 level. Down-Conversion (DC) emission is observed due to a combination of two different processes: 1-a one-step cross relaxation (Pr3+:3P0 → 1G4; Yb3+:2F7/2 → 2F5/2) resulting in one photon emitted by Pr3+ (1G4 → 3H5) and one photon emitted by Yb3+ (2F7/2 → 2F5/2); 2-a resonant two-step first order energy transfer, where the first part of energy is transferred to Yb3+ neighbor through cross relaxation (Pr3+:3P0 → 1G4; Yb3+:2F7/2 → 2F5/2) followed by a second energy transfer step (Pr 3+:1G4 → 3H4; Yb3+:2F7/2 → 2F5/2). A third process leading to one IR photon emission to each visible photon absorbed involves cross relaxation energy transfer (Pr3+: 1D2 → 3F4; Yb 3+:2F7/2 → 2F5/2). © 2013 Elsevier B.V. All rights reserved.