995 resultados para Constant current


Relevância:

100.00% 100.00%

Publicador:

Resumo:

A theoretical approach has been developed to relate the voltage delay transients of the Mg-MnO2 dry cell observed during discharge by two commonly employed modes, viz., (1) at constant current, and (2) across a constant resistance. The approach has been verified by comparison of experimentally obtained transients with those generated from theory. The method may be used to predict the delay parameters of the Mg-MnO2 dry cell under the two modes of discharge and can, in principle, be extended to lithium batteries.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A high efficiency hard switching constant current LED driver is presented with high overall efficiency, high current precision, high LED efficacy, flicker-free and wide constant current dimming ratio. The high stable lighting source provides the best solution for office light, reading light and LCD backlight. © 2013 IEEE.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This article assesses the use of the constant current (CC) method for characterizing dielectric films. The method is based on charging the sample with a constant current (current stress) and measuring the corresponding voltage rise under the closed circuit condition. Our article shows that the CC method is an alternative to the constant voltage stressing method to study the electric properties of nonpolar, ferroelectric, and polar polymers. The method was tested by determining the dielectric constant of polytetrafluoroethylene, and investigating the electric conduction in poly(ethylene terephthalate). For the ferroelectric polymer poly(vinylidene fluoride), it is shown that hysteresis loops and the dependence of the ferroelectric polarization on the electric field can be obtained. (C) 2001 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This article reports systematic results of corona poling measurements obtained on biaxially stretched polyvinylidene fluoride films charged in dry air. Charging was performed using the constant current corona triode. The dependence of the poling process on the sample thickness, charging current, and successive charging processes was investigated. Phase transitions from alpha to delta and to beta phases were observed when virgin samples were corona charged. The thermal pulse technique showed that the polarization profiles during charging can be made consistently almost uniform and that the ferroelectric reorientation can be associated with the rising plateau region displayed on potential buildup curves. (C) 1995 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A simple constant-current electrocutaneous stimulator for high-impedance loads using low-cost, standard high-voltage components is presented. A voltage-regulator powers an oscillator built across the primary of a transformer whose secondary delivers, after rectification, the high-voltage supply to switched current-mirrors in the driving stage. Since the compliance high-voltage is proportional to the stimulation current, overall power consumption is minimized. By adjusting the regulated voltage, control of the pulsed-current amplitude is achieved. A prototype with readily available components features stimulation currents of amplitude and pulsewidth in the range 0≤Iskin≤20mA and 50μs ≤Tpulse≤1ms, respectively. Pulse-repetition spans from 1 Hz to 10Hz. Worst-case ripple is 3.7% @Iskin=1mA. Measured pulse fall-time is shorter than 32μs. Overall consumption is 4.4W @Iskin=20mA. Subject isolation from line is 4KV.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

OBJECTIVE: To determine the minimum alveolar concentration (MAC) of isoflurane in Shetland ponies using a sequence of three different supramaximal noxious stimulations at each tested concentration of isoflurane rather than a single stimulation. STUDY DESIGN: Prospective, experimental trial. ANIMALS: Seven 4-year-old, gelding Shetland ponies. METHODS: The MAC of isoflurane was determined for each pony. Three different modes of electrical stimulation were applied consecutively (2 minute intervals): two using constant voltage (90 V) on the gingiva via needle- (CVneedle) or surface-electrodes (CVsurface) and one using constant current (CC; 40 mA) via surface electrodes applied to the skin over the digital nerve. The ability to clearly interpret the responses as positive, the latency of the evoked responses and the inter-electrode resistance were recorded for each stimulus. RESULTS: Individual isoflurane MAC (%) values ranged from 0.60 to 1.17 with a mean (+/-SD) of 0.97 (+/-0.17). The responses were more clearly interpreted with CC, but did not reach statistical significance. The CVsurface mode produced responses with a longer delay. The CVneedle mode was accompanied by variable inter-electrode resistances resulting in uncontrolled stimulus intensity. At 0.9 MAC, the third stimulation induced more positive responses than the first stimulation, independent of the mode of stimulation used. CONCLUSIONS: The MAC of isoflurane in the Shetland ponies was lower than expected with considerable variability among individuals. Constant current surface electrode stimulations were the most repeatable. A summation over the sequence of three supramaximal stimulations was observed around 0.9 MAC. CLINICAL RELEVANCE: The possibility that Shetland ponies require less isoflurane than horses needs further investigation. Constant current surface-electrode stimulations were the most repeatable. Repetitive supramaximal stimuli may have evoked movements at isoflurane concentrations that provide immobility when single supramaximal stimulation was applied.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

In this paper the effects of constant and cyclic power loads on the evolution of interfacial reaction layers in lead-free solder interconnections are presented. Firstly, the differences in the growth behavior of intermetallic compound (IMC) layers at the cathode and anode sides of the interconnections are rationalized. This is done by considering the changes in the intrinsic fluxes of elements owing to electromigration as well as taking into account the fact that the growth of Cu3Sn and Cu6Sn5 are coupled via interfacial reactions. In this way, better understanding of the effect of electron flux on the growth of each individual layer in the Cu-Sn system can be achieved. Secondly, it is shown that there is a distinct difference between steady-state current stressing (constant current, constant temperature) and power cycling with alternating on- and off-cycle periods (accompanied by a change of temperature). The reasons behind the observed differences are subsequently discussed. Finally, special care is taken to ensure that the current densities are chosen in such a way that there is no risk for even partial melting of the solder interconnections.