1000 resultados para Complex Viscosity
Resumo:
A synergic effect of amylose on rheological characteristics of lysozyme physical gels evolved out of dimethylsulfoxide-water was verified and analyzed. The dynamics of the gels were experimentally approached by oscillatory rheology. The synergic effect was characterized by a decrease in the threshold DMSO volume fraction required for lysozyme gelation, and by a significant strengthening of the gel structure at over-critical solvent and protein concentrations. Drastic changes in the relaxation and creep curve patterns for systems in the presence of amylose were verified. Complex viscosity dependence on temperature was found to conform to an Arrhenius-like equation, allowing the determination of an activation energy term (Ea, apparent) for discrimination of gel rigidity. A dilatant effect was found to be induced by temperature on the flow behavior of lysozyme dispersions in DMSO-H(2)O in sub-critical conditions for gelation, which was greatly intensified by the presence of amylose in the samples. That transition was interpreted as reflecting a change from a predominant colloidal flow regime, where globular components are the prevailing structural elements, to a mainly fibrillar, polymeric flow behavior.
Resumo:
The dynamic theological behaviour of gamma-irradiated 12.8 wt% poly(vinyl alcohol) (PVA), 12.8 wt% poly(vinyl pyrrolidone) (PVP), and a blend of 8 wt% PVA and 4.8 wt% PVP aqueous solutions have been studied pre- and post-gelation. The non-irradiated solutions displayed theological behaviour typical of dilute to semi-dilute polymer solutions, with the complex viscosity being independent of the frequency and shear rate (i.e. Newtonian behaviour) over the range of frequencies tested and the loss modulus G(omega) and storage modulus G(omega) being nearly proportional to omega and omega(2) respectively. After a set of doses of gamma-radiation, the magnitudes of the dynamic moduli G'(omega) and G(omega) increased as the absorbed dose increased, with notable differences between the two homopolymers and the blend. The stages of gelation were effectively monitored by means of dynamic theological measurements, allowing the possible mechanisms of network formation to be elucidated. The doses required for gelation of the PVA, PVP, and blend samples, determined on the basis of the Winter and Chambon criteria for gelation, were found to be 12 kGy for the 12.8 wt% PVA, 4 kGy for the 12.8 wt% PVP, and 5 kGy for the 8 wt% PVA/4.8 wt% PVP solutions. The unexpected lower gelation dose demonstrated by the blend sample, compared with predictions based on the blend composition, and the associated gelation mechanism are also discussed.
Resumo:
This article reports the phase behavior determi- nation of a system forming reverse liquid crystals and the formation of novel disperse systems in the two-phase region. The studied system is formed by water, cyclohexane, and Pluronic L-121, an amphiphilic block copolymer considered of special interest due to its aggregation and structural proper- ties. This system forms reverse cubic (I2) and reverse hexagonal (H2) phases at high polymer concentrations. These reverse phases are of particular interest since in the two-phase region, stable high internal phase reverse emulsions can be formed. The characterization of the I2 and H2 phases and of the derived gel emulsions was performed with small-angle X-ray scattering (SAXS) and rheometry, and the influence of temperature and water content was studied. TheH2 phase experimented a thermal transition to an I2 phase when temperature was increased, which presented an Fd3m structure. All samples showed a strong shear thinning behavior from low shear rates. The elasticmodulus (G0) in the I2 phase was around 1 order of magnitude higher than in theH2 phase. G0 was predominantly higher than the viscousmodulus (G00). In the gel emulsions,G0 was nearly frequency-independent, indicating their gel type nature. Contrarily to water-in-oil (W/O) normal emulsions, in W/I2 and W/H2 gel emulsions, G0, the complex viscosity (|η*|), and the yield stress (τ0) decreased with increasing water content, since the highly viscous microstructure of the con- tinuous phase was responsible for the high viscosity and elastic behavior of the emulsions, instead of the volumefraction of dispersed phase and droplet size. A rheological analysis, in which the cooperative flow theory, the soft glass rheology model, and the slip plane model were analyzed and compared, was performed to obtain one single model that could describe the non-Maxwellian behavior of both reverse phases and highly concentrated emulsions and to characterize their microstructure with the rheological properties.
Resumo:
Poly-L-lactide (PLLA) is a widely used sustainable and biodegradable alternative to replace synthetic non-degradable plastic materials in the packaging industry. Conversely, its processing properties are not always optimal, e.g. insufficient melt strength at higher temperatures (necessary in extrusion coating processes). This thesis reports on research to improve properties of commercial PLLA grade (3051D from NatureWorks), to satisfy and extend end-use applications, such as food packaging by blending with modified PLLA. Adjustment of the processability by chain branching of commercial poly-L-lactide initiated by peroxide was evaluated. Several well-defined branched structures with four arms (sPLLA) were synthesized using pentaerythritol as a tetra-functional initiator. Finally, several block copolymers consisting of polyethylene glycol and PLLA (i.e. PEGLA) were produced to obtain a well extruded material with improved heat sealing properties. Reactive extrusion of poly-L-lactide was carried out in the presence of 0.1, 0.3 and 0.5 wt% of various peroxides [tert-butyl-peroxybenzoate (TBPB), 2,5-dimethyl-2,5-(tert-butylperoxy)-hexane (Lupersol 101; LOL1) and benzoyl peroxide (BPO)] at 190C. The peroxide-treated PLLAs showed increased complex viscosity and storage modulus at lower frequencies, indicating the formation of branched/cross linked architectures. The material property changes were dependent on the peroxide, and the used peroxide concentration. Gel fraction analysis showed that the peroxides, afforded different gel contents, and especially 0.5 wt% peroxide, produced both an extremely high molar mass, and a cross linked structure, not perhaps well suited for e.g. further use in a blending step. The thermal behavior was somewhat unexpected as the materials prepared with 0.5 wt% peroxide showed the highest ability for crystallization and cold crystallization, despite substantial cross linking. The peroxide-modified PLLA, i.e. PLLA melt extruded with 0.3 wt% of TBPB and LOL1 and 0.5 wt% BPO was added to linear PLLA in ratios of 5, 15 and 30 wt%. All blends showed increased zero shear viscosity, elastic nature (storage modulus) and shear sensitivity. All blends remained amorphous, though the ability of annealing was improved slightly. Extrusion coating on paperboard was conducted with PLLA, and peroxide-modified PLLA blends (90:10). All blends were processable, but only PLLA with 0.3 wt% of LOL1 afforded a smooth high quality surface with improved line speed. Adhesion levels between fiber and plastic, as well as heat seal performance were marginally reduced compared with pure 3051D. The water vapor transmission measurements (WVTR) of the blends containing LOL1 showed acceptable levels, only slightly lower than for comparable PLLA 3051D. A series of four-arm star-shaped poly-L-lactide (sPLLA) with different branch length was synthesized by ring opening polymerization (ROP) of L-lactide using pentaerythritol as initiator and stannous octoate as catalyst. The star-shaped polymers were further blended with its linear resin and studied for their melt flow and thermal properties. Blends containing 30 wt% of sPLLA with low molecular weight (30 wt%; Mwtotal: 2500 g mol-1 and 15000 g mol-1) showed lower zero shear viscosity and significantly increased shear thinning, while at the same time slightly increased crystallization of the blend. However, the amount of crystallization increased significantly with the higher molecular weight sPLLA, therefore the star-shaped structure may play a role as nucleating agent. PLLA-polyethylene glycol–PLLA triblock copolymers (PEGLA) with different PLLA block length were synthesized and their applicability as blends with linear PLLA (3051D NatureWorks) was investigated with the intention of improving heat-seal and adhesion properties of extrusion-coated paperboard. PLLA-PEG-PLLA was obtained by ring opening polymerization (ROP) of L-lactide using PEG (molecular weight 6000 g mol-1) as an initiator, and stannous octoate as catalyst. The structures of the PEGLAs were characterized by proton nuclear magnetic resonance spectroscopy (1H-NMR). The melt flow and thermal properties of all PEGLAs and their blends were evaluated using dynamic rheology, and differential scanning calorimeter (DSC). All blends containing 30 wt% of PEGLAs showed slightly higher zero shear viscosity, higher shear thinning and increased melt elasticity (based on tan delta). Nevertheless, no significant changes in thermal properties were distinguished. High molecular weight PEGLAs were used in extrusion coating line with 3051D without problems.
Resumo:
The functional effects of lipase (0.003 and 0.006 g/100 g of flour) and emulsifier (0.5 and 1 g/100 g of flour) on fat-replaced (0%, 50% and 70%) batters and cakes with inulin (0, 7.5 and 10 g/100 g/of flour, respectively) were studied. Emulsifier addition significantly lowered the relative density of the batter. Emulsifier incorporation increased the viscoelastic properties of the batter. In contrast, lipase incorporation decreased the degree of system structuring. The evolution of the dynamic moduli and complex viscosity with rising temperatures were studied. Batters with 1 g/100 g emulsifier displayed a significantly lower complex viscosity during heating, resulting in collapsed cakes. Differential scanning calorimetry results revealed that the thermal setting in the control cakes occurred at higher temperatures, and accordingly, greater cake expansion was observed. Cakes with 0.003 g/100 g lipase or 0.5 g/100 g emulsifier displayed volume and crumb cell structure that were similar to those of control cakes. Higher concentrations of both improvers gave rise to cakes with lower volume, higher hardness and lower springiness. During storage time, cakes with lipase displayed lower hardness. Both improvers, at low concentrations, could improve certain physical characteristics, such as crumb structure, of fat-replaced cakes with inulin.
Resumo:
Hybrid siloxane-polymethylmethacrylate (PMMA) nanocomposites with covalent bonds between the inorganic (siloxane) and organic (polymer) phases were prepared by the sot gel process through hydrolysis and polycondensation of 3-(trimethoxysilyl)propylmethacrylate (TMSM) and polymerization of methylmethacrylate (MMA) using benzoyl peroxide (BPO) as initiator. The effect of MMA, BPO and water contents on the viscoelastic behaviour of these materials was analysed during gelation by dynamic rheological measurements. The changes in storage (G') and loss moduli (G), complex viscosity (eta*) and phase angle (6) were measured as a function of the reaction time showing the viscous character of the sot in the initial step of gelation and its progressive transformation to an elastic gel. This study was complemented by Si-29 and C-13 solid-state nuclear magnetic resonance (NMR/MAS) measurements of dried gel. The analysis of the experimental results shows that linear chains are formed in the initial step of the gelation followed by a growth of branched structures and formation of a three-dimensional network. Near the gel point this hybrid material demonstrates the typical scaling behaviour expected from percolation theory.
Resumo:
The viscoelastic properties of siloxane-poly(oxypropylene) (PPO) nanocomposites prepared by the sol-gel process has been analyzed during gelation by dynamic rheological measurements. The changes of storage and loss moduli, complex viscosity and phase angle has been measured as a function of time showing the newtonian viscosity of the sol in the initial step of gelation, and its progressive transformation to a viscoelastic gel. The rheologic properties have been correlated to mass fractal, nearly linear growth models and percolation theory. This study, completed by quasi-elastic light scattering and Si-29 solid state nuclear magnetic resonance measurements, shows that the mechanisms of gelation of siloxane-PPO hybrids depend on the molecular weight of the polymer and on the pH of the hybrid sol. For hybrids prepared in acid medium, a polymerization involving silicon reactive species located at the extremity of the polymer chains and presenting a functionality f = 2 occurs, forming a fractal structure during the first stage of sol-gel transition. For samples prepared under neutral pH, the fractal growth is only observed for hybrids containing short polymer chains (M-w similar to 130 gmol(-1)). The fractal dimensionality determined from the change in the rheological properties, indicates that the fractal growth mechanism changes from reaction-limited to diffusion-limited aggregation when the molecular weight of the PPO increases from 130 to 4000 gmol(-1) and as catalyst conditions change from acidic to neutral. Near the gel point, these hybrid gels have the typical scaling behavior expected from percolation theory. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
This paper describes particle aggregation process during gelation of SnO2 hydrosols. The effect of the concentration of SnO2 colloidal particles on the kinetics of gelation of hydrosols containing PVA (poly(vinyl alcohol)) was analysed by dynamic rheological measurements. The complex viscosity and the storage and loss moduli have been measured during the sol-gel transition and the results correlated to mass fractal growth, nearly linear growth models, and scalar percolation theory. The analysis of the experimental results shows that a linear aggregation occurs in the initial step of the gelation followed by a fractal growth to form a three-dimensional network. Near the gel point this physical gel exhibits the typical scaling expected from an electrical percolation analogy. (C) 1999 Elsevier B.V. B.V. All rights reserved.
Resumo:
SnO2 supported membranes have been prepared by sol-casting on alumina tubular substrate, using aqueous colloidal suspensions prepared by sol-gel route. The viscoelastic behaviour during sol ageing was analyzed by dinamic rheologial measurements. The complex viscosity and the storage and loss moduli have been followed during the sol-gel transition and the results have been correlated with the linear aggregates growth and the scalar percolation models. The scanning electron microscopy has evidenced that the homogeneity and thickness of the membrane depend on the sol ageing time. Crack-free and homogeneous membranes have been obtained for coated layers of 0.5μm thickness. © 1997 Trans Tech Publications.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
A simple and scalable procedure was used to obtain thin, stable, homogeneous, and easy-to-handle films composed of silicone derived from dimethicones containing dispersed hydrotalcite-type materials previously organo-modified with amino acids. The absence of the typical X-ray pattern of the bioinorganic LDH filler suggested an exfoliation process that was further indirectly evidenced by a drastic change in the rheological behavior, which turned from a quasi-Newtonian behavior for the silicone free of LDH filler to an extensive developed gel-like structure for the nanocomposite derivatives. Visualized by the shear-thinning exponent of the complex viscosity in the low-frequency range, the percolation threshold was evident for filler loading as low as <5 w/W%, suggesting the presence of a largely developed interface between the filler and the polymer. The increase of more than one order of magnitude in viscosity was explained by the rather strong attrition phenomenon between the tethered amino acid anions and the silicone chains. UVB radiation absorption profiles make such bioinorganic polymer nanocomposites potentially applicable in skin protection. Thermo-gravimetric analysis revealed significant improvement in the thermal stability, especially in the final step of the polymer combustion, thus underlining the role of the hybrid material as a thermal retardant agent. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The effect of different propionaldehyde ratios on the properties of bis-GMA-based comonomers and copolymers diluted with propoxylated bis-GMA (CH3bis-GMA) was evaluated. Five experimental comonomers were prepared combining bis-GMA with CH3bis-GMA and propionaldehyde at 0, 2, 8, 16, 24 mol%. Light polymerization was effected with the use of 0.2 wt. (%) each of camphorquinone and N,N-dimethyl-p-toluidine. Resin degrees of conversion (%DC) were evaluated by FT-IR spectrophotometry and Tg by Differential Scanning Calorimeter. Complex viscosity (η*), the effect of temperature on η*, and Microhardness (H) for dry and wet samples were also determined. Data were analyzed by Student's t-test, one-way ANOVA and Tukey-Kramer test (α = 0.05). The group with 24 mol% additive had a significant increase in %DC and H, and the lowest comonomer Tg and η*. No remarkable variation was noted in copolymers Tg s. All resins presented Newtonian behavior of viscosity, which linearly decreased with increased temperature. The η* decreased sigmoidally as the additive ratio increased.
Resumo:
Zusammenfassung In der vorliegenden Arbeit wurden Polymerisationseigenschaften hydrophober Monomere untersucht, die mittels methyliertem b-Cyclodextrin (me-b-CD) als Wirt/Gast-Komplexe homogen in die wäßrige Phase überführt wurden. Mit diesem Verfahren steht eine neue Variante der Polymerisation hydrophober Monomere in Wasser zur Verfügung.Die Charakterisierung der Monomer/CD-Komplexe erfolgte mittels Röntgenstrukturanalyse und 1H-NMR-Spektroskopie: steigende Größe der Gast-Komponente erhöht die Wechselwirkungen zum CD. Zur Untersuchung der Polymerisationsreaktion wurden Copolymerisationsparameter von Komplexen und Übertragungskonstanten von Mercaptoverbindungen bei Polymerisationen von Komplexen ermittelt. In Abhängigkeit der Größe der Gastkomponente und ihrer Wasserlöslichkeit resultieren unterschiedliche Reaktivitäten relativ zu Polymerisationen unkomplexierter Reaktanden in organisch-wäßriger Lösung. Außerdem wurden Copolymerisationen zwischen hydrophoben, me-b-CD-komplexierten Monomeren und wasserlöslichen Monomeren untersucht wie z.B. N-Isopropylacrylamid oder Natrium-4-(acrylamido)phenyldiazosulfonat, dessen Copolymerisation mit Styrol bislang nicht möglich war. Eine weitere Aufgabe war die Herstellung wasserstoffbrückenbindender Polymere. Hierzu wurden assoziationsfähige Monomere hergestellt und mit Methylmethacrylat copolymerisiert. Lösungen der Copolymere wurden rheologisch untersucht. Die Lösungen besitzen hohe Nullscherviskositäten bei 20°C und sind strukturviskos. Die Untersuchung der Temperaturabhängigkeit der Nullscherviskositäten ergab insbesondere bei der Lösung von Poly(N-(methacryl-2-ethyl)-N'-(3-amino-(1,2,4-triazol-2-yl))harnstoff-co-methylmethacrylat) bei niedrigen Temperaturen eine hohe Fließaktivierungsenergie, die zu höheren Temperaturen sank. Die komplexe Viskosität dieser Lösung fiel mit zunehmender Temperatur zunächst ab, stieg dann wieder an und sank erneut. Mittels DSC-Messungen konnten Phasenübergänge für dieses Fließverhalten verantwortlich gemacht werden. Außerdem kann Poly(N-(methacryl-2-ethyl)-N'-(3-amino-(1,2,4-triazol-2-yl))harnstoff-co-methylmethacrylat) thermisch vernetzen.
Resumo:
The rheological and tribological properties of single-walled carbon nanotube (SWCNT)-reinforced poly(phenylene sulphide) (PPS) and poly(ether ether ketone) (PEEK) nanocomposites prepared via melt-extrusion were investigated. The effectiveness of employing a dual-nanofiller strategy combining polyetherimide (PEI)-wrapped SWCNTs with inorganic fullerene-like tungsten disulfide (IF-WS2) nanoparticles for property enhancement of the resulting hybrid composites was evaluated. Viscoelastic measurements revealed that the complex viscosity ?, storage modulus G?, and loss modulus G? increased with SWCNT content. In the low-frequency region, G? and G? became almost independent of frequency at higher SWCNT loadings, suggesting a transition from liquid-like to solid-like behavior. The incorporation of increasing IF-WS2 contents led to a progressive drop in ? and G? due to a lubricant effect. PEEK nanocomposites showed lower percolation threshold than those based on PPS, ascribed to an improved SWCNT dispersion due to the higher affinity between PEI and PEEK. The SWCNTs significantly lowered the wear rate but only slightly reduced the coefficient of friction. Composites with both nanofillers exhibited improved wear behavior, attributed to the outstanding tribological properties of these nanoparticles and a synergistic reinforcement effect. The combination of SWCNTs with IF-WS2 is a promising route for improving the tribological and rheological performance of thermoplastic nanocomposites.