In this work Ba0.99Eu0.01MoO4 (BEMO) powders were prepared by the first time by the Complex Polymerization Method. The structural and optical properties of the BEMO powders were characterized by Fourier Transform Infra-Red (FTIR), X-ray Diffraction (XRD), Raman Spectra, High-Resolution Scanning Electron Microscopy (HR-SEM) and Photoluminescent Measurements. XRD show a crystalline scheelite-type phase after the heat treatment at temperatures greater than 400 degrees C. The ionic radius of Eu3+ (0.109 nm) is lower than the Ba2+ (0.149 nm) one. This difference is responsible for the decrease in the lattice parameters of the BEMO compared to the pure BaMoO4 matrix. This little difference in the lattice parameters show that Eu3+ is expected to occupy the Ba2+ site at different temperatures, stayed the tetragonal (S-4) symmetry characteristic of scheelite-type crystalline structures of BaMoO4. The emission spectra of the samples, when excited at 394 nm, presented the D-5(1)-> F-7(0, 1 and 2) and D-5(0)-> F-7(0, 1, 2, 3 and 4) Eu3+ transitions at 523, 533, 554, 578, 589, 614, 652 and 699 nm, respectively. The emission spectra of the powders heat-treated at 800 and 900 degrees C showed a marked increase in its intensities compared to the materials heat-treated from 400 to 700 C. The decay times for the sample were evaluated and all of them presented the average value of 0.61 ms. Eu3+ luminescence decay time follows one exponential curve indicating the presence of only one type of Eu3+ symmetry site.
Resumo:
The BaMoO4 nanopowders were prepared by the Complex Polymerization Method (CPM). The structure properties of the BaMoO4 powders were characterized by FTIR transmittance spectra, X-ray diffraction (XRD), Raman spectra, photoluminescence spectra (PL) and high-resolution scanning electron microscopy (HR-SEM). The XRD, FTIR and Raman data showed that BaMoO4 at 300 degrees C was disordered. At 400 degrees C and higher temperature, BaMoO4 crystalline scheelite-type phases could be identified, without the presence of additional phases, according to the XRD, FTIR and Raman data. The calculated average crystallite sizes, calculated by XRD, around 40 nm, showed the tendency to increase with the temperature. The crystallite sizes, obtained by HR-SEM, were around of 40-50 nm. The sample that presented the highest intensity of the red emission band was the one heat treated at 400 degrees C for 2 h, and the sample that displayed the 'highest intensity of the green emission band was the one heat treated at 700 degrees C for 2 h. The CPM was shown to be a low cost route for the production of BaMoO4 nanopowders, with the advantages of lower temperature, smaller time and reduced cost. The optical properties observed for BaMoO4 nanopowders suggested that this material is a highly promising candidate for photoluminescent applications. (C) 2005 Elsevier B.V. All rights reserved.
Resumo:
The study of the photoluminescent properties affected by order and disorder of the BaMoO4 powders is the principal objective in this work. BaMoO4 compounds were prepared using soft chemical process called Complex Polymerization Method. In this work, different deagglomeration types and different heating rates were used to promote different disorder degrees. Scheelite type phase (BaMoO4) was determined by X-ray Diffraction (XRD), Fourier Transformed Infra-Red (FTIR) and Raman spectroscopy after heat treating the sample at 400 degrees C. The room temperature luminescence spectra revealed an intense single-emission band in the visible region. Based on XRD and Raman data it was observed that the transition between the completely disordered structure to completely ordered structure is a good condition for photoluminescence (PL) emission. The best PL emission is obtained when the material possesses short range disorder, i.e., is periodically ordered (XRD), but some disorder as measured by Raman spectroscopy. The excellent optical properties observed for disordered BaMoO4 suggested that this material is a highly promising candidate for optical applications.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Europium(III) Concentration Effect on the Spectroscopic and Photoluminescent Properties of BaMoO4:Eu
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
PbMoO(4) micro-octahedrons were prepared by the coprecipitation method at room temperature without the presence of surfactants and processed in a conventional hydrothermal at different temperatures (from 60 to 120 degrees C) for 10 min. These micro-octahedrons were structurally characterized by X-ray diffraction (XRD) and micro-Raman (MR) spectroscopy, and its morphology was investigated by field-emission gun scanning electron microscopy (FEG-SEM). The optical properties were analyzed by ultraviolet-visible (UV-vis) absorption spectroscopy and photoluminescence (PL) measurements. XRD patterns and MR spectra confirmed that the PbMoO(4) micro-octahedrons are characterized by a scheelite-type tetragonal structure. FEG-SEM micrographs points, out that these structures present a polydisperse particle size distribution in consequence of a predominant growth mechanism via aggregation of particles. In addition, it was observed that the hydrothermal conditions favored a spontaneous formation of micro-octahedrons interconnected along a common crystallographic orientation (oriented-attachment), resulting in self-organized structures. An intense blue PL emission at room temperature was observed in these micro-octahedrons when they were excited with a 350 nm wavelength. The origin of the PL emissions as well as its intensity variations are explained by means of a model based on both distorted [MoO(4)] and [PbO(8)] clusters into the lattice.
Resumo:
Crystalline molybdate thin films were prepared by the complex polymerization method. The AMoO(4) (A = Ca, Sr, Ba) films were deposited onto Si wafers by the spinning technique. The Mo-O bond in the AMoO(4) structure was confirmed by FTIR spectra. X-ray diffraction revealed the presence of crystalline scheelite-type phase. The mass, size, and basicity of A(2+) cations was found to be dependent on the intrinsic characteristics of the materials. The grain size increased in the following order: CaMoO4 < SrMoO4 < BaMoO4. The emission band wavelength was detected at around 576 nm. Our findings suggest that the material's morphology and photoluminescence were both affected by the variations in cations (Ca, Sr, or Ba) and in the thermal treatment.
Resumo:
In this communication, we investigate the effect of different surfactants: cetyltrimethylammonium bromide (CTAB), sodium dodecyl sulfate (SDS) and polyvinylpyrrolidone (PVP-K40) on the growth process of zinc molybdate (beta-ZnMoO4) microcrystals synthesized under hydrothermal conditions at 140 degrees C for 8 h. These microcrystals were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), and photoluminescence (PL) measurements. XRD patterns proved that these crystals are monophasic and present a wolframite-type monoclinic structure. FE-SEM images revealed that the surfactants modified the crystal shapes, suggesting the occurrence of distinct crystal growth processes. The CTAB cationic surfactant promotes the hindrance of small nuclei that leads to the formation of rectangle-like crystals, SDS anionic surfactant induces a growth of irregular hexagons with several porous due to considerable size effect of counter-ions on the crystal facets, PVP-K40 non-ionic surfactant allows a reduction in size and thickness of plate-like crystals, while without surfactants have the formation of irregular plate-like crystals. Finally, the PL properties of beta-ZnMoO4 microcrystals were explained by means of different shape/size, surface defects and order-disorder into lattice. (C) 2011 Elsevier B.V. All rights reserved.