The transitions and reactions involved in the thermal treatment of several commercial azodicarbonamides (ADC) in an inert atmosphere have been studied by dynamic thermogravimetry analysis (TGA), mass spectrometry and Fourier transform infrared (FTIR) spectroscopy. A pseudo-mechanistic model, involving several competitive and non-competitive reactions, has been suggested and applied to the correlation of the weight loss data. The model applied is capable of accurately representing the different processes involved, and can be of great interest in the understanding and quantification of such phenomena, including the simulation of the instantaneous amount of gases evolved in a foaming process. In addition, a brief discussion on the methodology related to the mathematical modeling of TGA data is presented, taking into account the complex thermal behaviour of the ADC.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The transitions and reactions involved in the thermal processing of binary mixtures of polyethylene and poly(ethylene-co-vinyl acetate) copolymers with different concentrations of a foaming agent (azodicarbonamide) were studied using differential scanning calorimetry (DSC). The effect of ZnO as a kicker also was discussed. The temperature at the maximum rate and the heat evolved were measured for all the processes—melting, transitions, and reactions—all the mixtures prepared were measured and compared. Azodicarbonamide decomposed differently depending on the polymeric matrix. These data can be very useful for the plastic processing industry.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Semicarbazide (SEM), the marker residue for the banned nitrofuran veterinary antibiotic nitrofurazone (NFZ), has been detected regularly in foods (47% of recent nitrofuran EU Rapid Alerts involve SEM). However, the validity of SEM as a definitive marker for NFZ has been undermined by SEM arising from other sources including azodicarbonamide, a plastics blowing agent and flour treatment additive. An inexpensive screening test for SEM in food matrices is needed-all SEM testing currently uses expensive LC-MS/MS instrumentation. We now report the first production of antibodies against derivatised SEM. A novel carboxyphenyl SEM derivative was used to raise a polyclonal antibody that has been incorporated into a semi-quantitative microtitre plate ELISA, validated according to the criteria set out in Commission Decision 2002/657/EC, for use with chicken muscle. The antibody is highly specific for derivatised SEM, cross-reactivity being 1.7% with NFZ and negligible with a wide range of other nitrofurans and poultry drugs. Samples are derivatised with o-nitrobenzaldehyde and simultaneously protease digested before extraction by cation exchange SPE. The ELISA has a SEM detection capability (CC beta) of 0.25 mu g kg(-1) when a threshold of 0.21 mu g kg(-1) is applied to the selection of samples for confirmation (lowest observed 0.25 mu g kg(-1) fortified sample, n = 20), thus satisfying the EU nitrofurans' minimum required performance limit of 1 mu g kg(-1). N-FZ-incurred muscles (12) containing SEM at 0.5-5.0 mu g kg(-1) by LC-MS/MS, all screened positive by this ELISA protocol which is also applicable to egg and chicken liver. (C) 2007 Elsevier BN. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

En el presente trabajo se han estudiado mediante DSC, las reacciones involucradas en el tratamiento térmico de los principales componentes en las formulaciones de materiales espumados como son EVA, PE, azodicarbonamida y α- α’-bis(tertbutil-peroxi)-m/p-diisopropilbenceno. Los ensayos se han realizado a una velocidad de calefacción constante de 10 ºC/min en atmósfera inerte de N2. Por otro lado, también se proponen una serie de modelos cinéticos mecanísticos que contemplan la existencia de una o más fracciones reactivas y/o reacciones. Además se ha introducido la variación de las capacidades caloríficas con la temperatura, consiguiendo de esta forma una mejora considerable del ajuste de los datos experimentales. Los modelos presentados son capaces de representar los diferentes procesos observados (con varios picos) y pueden ser de gran interés para la compresión de este tipo de fenómenos, así como para el modelado de la transferencia de calor que se produce durante los procesos industriales de espumado. (Nota: se incluye al final un lisado actualizado con bibliografía específica sobre modelado cinético).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Presentation submitted to PSE Seminar, Chemical Engineering Department, Center for Advanced Process Design-making (CAPD), Carnegie Mellon University, Pittsburgh (USA), October 2012.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The decomposition of azodicarbonamide, used as foaming agent in PVC—plasticizer (1/1) plastisols was studied by DSC. Nineteen different plasticizers, all belonging to the ester family, two being polymeric (polyadipates), were compared. The temperature of maximum decomposition rate (in anisothermal regime at 5 K min−1 scanning rate), ranges between 434 and 452 K. The heat of decomposition ranges between 8.7 and 12.5 J g−1. Some trends of variation of these parameters appear significant and are discussed in terms of solvent (matrix) and viscosity effects on the decomposition reactions. The shear modulus at 1 Hz frequency was determined at the temperature of maximum rate of foaming agent decomposition, and differs significantly from a sample to another. The foam density was determined at ambient temperature and the volume fraction of bubbles was used as criterion to judge the efficiency of the foaming process. The results reveal the existence of an optimal shear modulus of the order of 2 kPa that corresponds roughly to plasticizer molar masses of the order of 450 ± 50 g mol−1. Heavier plasticizers, especially polymeric ones are too difficult to deform. Lighter plasticizers such as diethyl phthalate (DEP) deform too easily and presumably facilitate bubble collapse.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Cette étude est destinée à la production et à la caractérisation des composites d’acide polylactique (PLA) et des fibres naturelles (lin, poudre de bois). Le moussage du PLA et ses composites ont également été étudiés afin d’évaluer les effets des conditions de moulage par injection et du renfort sur les propriétés finales de ces matériaux. Dans la première partie, les composites constitués de PLA et des fibres de lin ont été produits par extrusion suivit par un moulage en injection. L’effet de la variation du taux de charge (15, 25 et 40% en poids) sur les caractéristiques morphologique, mécanique, thermique et rhéologique des composites a été évalué. Dans la deuxième étape, la poudre de bois (WF) a été choisie pour renforcer le PLA. La préparation des composites de PLA et WF a été effectuée comme dans la première partie et une série complète de caractérisations morphologique, mécanique, thermique et l’analyse mécanique dynamique ont été effectués afin d’obtenir une évaluation complète de l’effet du taux de charge (15, 25 et 40% en poids) sur les propriétés du PLA. Finalement, la troisième partie de cette étude porte sur les composites de PLA et de renfort naturel afin de produire des composites moussés. Ces mousses ont été réalisées à l’aide d’un agent moussant exothermique (azodicarbonamide) via le moulage par injection, suite à un mélange du PLA et de fibres naturelles. Dans ce cas, la charge d’injection (quantité de matière injectée dans le moule: 31, 33, 36, 38 et 43% de la capacité de la presse à injection) et la concentration en poudre de bois (15, 25 et 40% en poids) ont été variées. La caractérisation des propriétés mécanique et thermique a été effectuée et les résultats ont démontré que les renforts naturels étudiés (lin et poudre de bois) permettaient d’améliorer les propriétés mécaniques des composites, notamment le module de flexion et la résistance au choc du polymère (PLA). En outre, la formation de la mousse était également efficace pour le PLA vierge et ses composites car les masses volumiques ont été significativement réduites.