522 resultados para Abrasion fastness
Resumo:
The ‘particle size effect’ and its manifestation in abrasion still attracts considerable debate as to its origins and the ranking of its likely causes. Experiments have been conducted to study the important contribution that the formation of wear debris can have on the progression of wear. The experiments consist of unlubricated (dry) pin-on-disk tests with silicon carbide coated paper of varying particle size, with different pin material, diameter and loads. It has been observed that the influence of debris formation on wear rate is more pronounced for fine abrasives and soft-wearing materials. Consequently, it is proposed that the particle size effect can be explained in terms of geometrical scaling and the evolution of third-body effects with diminishing particle diameter.
Resumo:
Abrasion and slurry erosion behaviour of chromium-manganese iron samples with chromium (Cr) in the range similar to 16-19% and manganese (Mn) at 5 and 10% levels have been characterized for hardness followed by microstructural examination using optical and scanning electron microscopy. Positron lifetime studies have been conducted to understand the defects/microporosity influence on the microstructure. The samples were heat treated and characterized to understand the structural transformations in the matrix. The data reveals that hardness decreased with increase in Mn content from 5 to 10% in the first instance and then increase in the section size in the other case, irrespective of the sample conditions. The abrasion and slurry erosion losses show increase with increase in the section size as well as with increase in Mn content. The positron results show that as hardness increases from as-cast to heat treated sample, the positron trapping rate and hence defect concentration showed opposite trend as expected. So a good correlation between defects concentration and the hardness has been observed. These findings also corroborate well with the microstructural features obtained from optical and scanning electron microscopy. (C) 2009 Elsevier B. V. All rights reserved.
Resumo:
Commercially available 3Y-TZP and Mg-PSZ flats mere abraded by a 150 degrees diamond cone at -196 degrees, 25 degrees, 200 degrees, and 400 degrees C. The coefficient of friction, the track width, and the morphological features of the track were recorded. Raman spectroscopy mas used to record the tetragonal-to-monoclinic phase transformation (t --> m) as a function of distance away from the track. The study was undertaken to establish the influence of tangential traction on phase transformation and surface damage.
Resumo:
Titanium flats were scribed by silicon carbide wedges over ranges of temperatures and applied strains and with lubrication. The response of the material to scribing was noted by recording the coefficient of friction, the surface morphology of track and the subsurface deformation. Additional data were obtained from (1) uniaxial compression of titanium, (2) scribing of oxygen-free high conductivity copper and (3) scribing of aluminium under dry and lubricated conditions to analyse and explain the observed variation in response of titanium to scribing with strain, temperature and lubrication.
Resumo:
A pin on cylinder wear rig has been built with precision stepping motor drives to both rotary and axial motions which enable accurate positional control to be achieved. Initial experiments using sapphire indenters running against copper substrates have investigated the build up of a single wear groove by repeated sliding along the same track. An approximate three dimensional ploughing analysis is also presented and the results of theory and experiment compared.
Resumo:
Micro-scale abrasion (ball cratering) tests were performed with different combinations of ball and bulk specimen materials, under different test conditions, such as load and abrasive slurry concentration. Wear modes were classified into two types: with rolling particle motion and with grooving particle motion. Wear rates observed with rolling particle motion were relatively insensitive to test conditions, whereas with grooving motion they varied much more. It is suggested that rolling abrasion is therefore a more appropriate mode if reproducible test results are desired. The motion of the abrasive particles can be reliably predicted from the knowledge of hardnesses and elastic properties of the ball and the specimen, and from the normal load and the abrasive slurry concentration. General trends in wear resistance measured in the micro-scale abrasion test with rolling particle motion are similar to those reported in tests with fixed abrasives with sliding particle motion, although the variation in wear resistance with hardness is significantly smaller. © 2004 Published by Elsevier B.V.
Resumo:
In the 'free-ball' version of the micro-scale abrasion or ball-cratering test the rotating ball rests against a tilted sample and a grooved drive shaft. Tests under nominally identical conditions with different apparatus commonly show small but significant differences in measured wear rate. An indirect method has been developed and demonstrated for continuous on-line measurement of the coefficient of friction in the free-ball test. Experimental investigation of the effects of sample tilt angle and drive shaft groove width shows that both these factors influence the stability of the rotation of the ball, and the shape of the abrasive slurry pool, which in turn affect the coefficient of friction in the wear scar area and the measured wear rate. It is suggested that in order to improve the reproducibility of this method the geometry of the apparatus should be specified. For the apparatus used in this work with a steel ball of 25 mm diameter, a sample tilt angle of 60-75° and a shaft groove width of about 10mm provided the most stable ball motion and a wear rate which showed least variability. © 2004 Elsevier B.V. All rights reserved.