848 resultados para polishing slurry
Resumo:
The present work develops and optimizes a method to determine copper in samples of feces and fish feed by graphite furnace atomic absorption spectrometry (GFAAS) through the direct introduction of slurries of the samples into the spectrometer's graphite tube coated internally with metallic rhodium and tungsten carbide that acts as chemical modifiers. The limits of detection (LOD) and quantification (LOQ) calculated for 20 readings of the blank of the standard slurries (0.50% m/v of feces or feed devoid of copper) were 0.24 and 0.79 μg L -1 for the standard feces slurries and 0.26 and 0.87 μg L -1 for the standard feed slurries. The proposed method was applied in studies of absorption of copper in different fish feeds and their results proved compatible with that obtained from samples mineralized by acid digestion using microwave oven. © Springer Science+Business Media, LLC 2008.
Resumo:
The aim of this study was to evaluate the Shore A hardness and color stability of two soft lining materials after thermocycling and when chemical polishing was used or omitted. Two acrylic-based soft lining materials were tested: Coe-Soft and Soft Confort, 14 specimens were made for each material. They were distributed in four groups according to the treatment performed. The specimens were thermocycled (1000 cycles) and half of the group submitted to chemical polishing (methyl methacrylate). Shore A hardness was determined and color stability was calculated by means of Commission International de l'Eclairage Lab uniform color scale using a spectrophotometer, the measurements were made immediately after deflasked, chemical polishing and thermocycling. Analysis of variance (ANOVA) and Tukey's tests were performed at p < 0.01. Color changes (deltaE) were observed after thermocycling in both soft lining materials: Soft Confort (10.60) showed significantly higher values than Coe-Soft (4.57). Coe-Soft (26.42) showed higher Shore A hardness values than Soft Confort (19.42). Chemical polishing did not influence in the color stability of both materials; however, influenced in the hardness values of Coe-Soft.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The aim of this study was to evaluate the influence of 2 different surface polishing procedures - glazing (GZ) and manual polishing (MP) - on the roughness of ceramics processed by computer-aided design/computer-aided manufacturing (CAD/CAM) and conventional systems (stratification technique). Eighty ceramic discs (diameter: 8 mm, thickness: 1 mm) were prepared and divided among 8 groups (n = 10) according to the type of ceramic disc and polishing method: 4 GZ and 4 MP. Specimens were glazed according to each manufacturer's recommendations. Two silicone polishing points were used on the ceramic surface for manual polishing. Roughness was measured using a surface roughness tester. The roughness measurements were made along a distance of 2 mm on the sample surface and the speed of reading was 0.1 mm/s. Three measurements were taken for each sample. The data (μm) were statistically analyzed using analysis of variance (ANOVA) and Tukey's test (α = 0.05). Qualitative analysis was performed using scanning electron microscopy (SEM). The mean (± SD) roughness values obtained for GZ were: 1.1 ± 0.40 μm; 1.0 ± 0.31 μm; 1.6 ± 0.31 μm; and 2.2 ± 0.73 μm. For MP, the mean values were: 0.66 ± 0.13 μm; 0.43 ± 0.14 μm; 1.6 ± 0.55 μm; and 2.0 ± 0.63 μm. The mean roughness values were significantly affected by the ceramic type (P = 0.0001) and polishing technique (P = 0.0047). The SEM images confirmed the roughness data. The manually polished glass CAD/CAM ceramics promoted lower surface roughness than did the glazed feldspathic dental ceramics.
Resumo:
A simple procedure for the sequential determination of Cd, Cu and Pb in tea leaves by slurry introduction to thermospray flame furnace atomic absorption spectrometry was developed. Detection limits were 0.05 mg kg-1 for Cd, 2.1 mg kg-1 for Cu and 0.68 mg kg-1 for Pb using 0.67 % (m/v) slurries (100 mg/15 mL). © 2013 Springer Science+Business Media New York.
Resumo:
Objective. To evaluate the surface roughness of IPS Empress 2 ceramic when treated with different finishing/polishing protocols. Materials and methods. Sixteen specimens of IPS Empress 2 ceramic were made from wax patterns obtained using a stainless steel split mold. The specimens were glazed (Stage 0-S0, control) and divided into two groups. The specimens in Group 1 (G1) were finished/polished with a KG Sorensen diamond point (S1), followed by KG Sorensen siliconized points (S2) and final polishing with diamond polish paste (S3). In Group 2 (G2), the specimens were finished/polished using a Shofu diamond point (S1), as well as Shofu siliconized points (S2) and final polishing was performed using Porcelize paste (S3). After glazing (S0) and following each polishing procedure (S1, S2 or S3), the surface roughness was measured using TALYSURF Series 2. The average surface roughness results were analyzed using ANOVA followed by Tukey post-hoc tests (α = 0.01) Results. All of the polishing procedures yielded higher surface roughness values when compared to the control group (S0). S3 yielded lower surface roughness values when compared to S1 and S2. Conclusions. The proposed treatments negatively affected the surface roughness of the glazed IPS Empress 2 ceramic. © 2013 Informa Healthcare.
Resumo:
Objectives: This study evaluated the gloss behaviour of experimental resin composites loaded with different filler percentages, immediately after polishing and after toothbrushing simulation. Methods: Sixteen disc-shaped specimens were fabricated for each different-charged composite (40%, 50%, 60%, 70% and 75%) and polished with SiC abrasive papers. Gloss measurements were made prior to simulated toothbrushing. The specimens were subjected to the simulation for 5, 15, 30 and 60 min using an electrical toothbrush with a standardized pressure while being immersed in a toothpaste/artificial saliva slurry. Results: Baseline composite gloss values ranged from 69.7 (40%) to 81.3 (75%) GU (gloss units) and from 18.1 (40%) to 32.3 (75%) GU after 1 h of brushing. Highest gloss values were obtained by 75%-charged resin, while the lowest values were obtained by the 40%-charged one. Conclusions: All tested materials showed a gloss decrease. However, the higher filler load a composite resin has, the higher gloss it can achieve. Clinical significance: Gloss of resin composite materials is an important factor in determining aesthetic success of anterior restorations, and this property may vary according to the filler charge of the restorative material. Higher filler load of a composite resin results in higher gloss values. © 2013 Elsevier Ltd. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Purpose: The execution of adjustments on ceramic restorations is sometimes necessary for either correction of occlusion and/or inadequate contours or esthetical improvements. Clinically, the surfaces undergo weariness through fine grinding diamond burs which remove the superficial glazing layer. Several materials for ceramic polishing have been used in an attempt to reach a satisfactory surface smoothness. The aim of this study was to perform a literature review on different polishing protocols of several dental ceramics. Study selection: This is a literature review performed through scientific articles published between 2004 and 2012, indexed in MEDLINE, PubMed and Scielo databases. The study selected and analyzed a total of 20 relevant articles that evaluated different types of ceramics, polishing treatment and surface roughness.Results: After an extensive literature review, this study observed: 1 - after the rupture of the glazing layer due to the adjustments of the restorations, the best choice for the polishing of the surface will depend on the type of ceramics used; 2 - glazing procedure provide excellent results regarding to the superficial smoothness; however, if reglazing is impossible, either abrasive rubber cups/points or sandpaper discs followed by the use of diamond polishing pastes results in a satisfactory superficial smoothness; 3 - clinical studies that take into account the behavior of the protocols polishing are scarce and should be encouraged; 4 - the large number of variables influence the final outcome of polishing should be considered. Conclusions: The necessity in standardization of methodologies to enable a comparison among researches. (c) 2014 Japan Prosthodontic Society. Published by Elsevier Ireland. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Aim: The aim of the study was evaluate the finishing and polishing effect of the color stability of the composite resin Filtek Supreme XT, according to different fluoride solutions and time. Material and Methods: Specimens were prepared (n=140) with half of the samples finished and polished. The experimental groups were divided according to the presence or absence of finishing and polishing and immersion solutions (artificial saliva, sodium fluoride solution at 0.05% - manipulated, Fluordent Reach, Oral B, Fluorgard). The specimens remained in artificial saliva for 24 hours and were subjected to an initial color analysis using a spectrophotometer CIELab system. Then, they were immersed in the experimental solutions for 1 minute a day. The readings of the color change were made after 24 and 48 hours, 7, 14, 21, 30 and 60 days after the first immersion. The three-way mixed Analysis of Variance (ANOVA) ("finishing/polishing", "immersion medium" and “time”) were performed. For multiple comparisons, the Sidak test for repeated measure was used, with a 5% level of significance. Results: The finishing and polishing factor showed significant variability, independently of the immersion media (p<0.001). Cconclusion: Finishing and polishing procedures yielded better color stability to composite resin over time, regardless of the immersion media.
Resumo:
This study evaluated the influence of finishing and polishing procedures and differ-ent fluoride solutions on superficial morphology and chemistry of the nanofilled composite resinSupreme XT (3M) through the EDX analysis and SEM evaluation. Circular specimens (n 5 30) of 10mm diameter and 2 mm thickness were prepared, with half of the sample assays finished and polishedwith Super-Snap1sandpaper. The experimental groups were divided according to the presence or ab-sence of finishing and polishing and solutions (arti ficial saliva, 0.0 5% of manipulated sodium fluoridesolution, Fluordent Re ach, Oral B, Fluorgard). Specimens were immersed in each respective solutionfor 1 min per day, during 60 days and stored in artificial saliva at 37 6 18C between immersion peri-ods. Topography and chemical analysis was qualitative. It was observed that specimens submitted tofinishing and polishing procedures had lower superficial degradation. Fluoride solutio ns promoted su-perficial alterations on specimens, being the highest degradation obtained with Fluordent Reach. Itca n be concluded that finishing and polishing procedures and the immersion media influence the su-perficial morphology of composite resin tested; the Fluordent Reach was the flu oride solution thatmo st affected the material’s surface.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Esthetics and durability of materials used to fabricate artificial eyes has been an important issue since artificial eyes are essential to restore esthetics and function, protect the remaining tissues and help with patients' psychological therapy. However, these materials are submitted to degrading effects of environmental agents on the physical properties of the acrylic resin. OBJECTIVE: This study assessed the color stability of acrylic resins used to fabricate sclera in three basic shades (N1, N2 and N3) when subjected to accelerated aging, mechanical and chemical polishing. MATERIAL AND METHODS: Specimens of each resin were fabricated and submitted to mechanical and chemical polishing. Chromatic analysis was performed before and after accelerated aging through ultraviolet reflection spectrophotometry. RESULTS: All specimens revealed color alteration following polishing and accelerated aging. The resins presented statistically significant chromatic alteration (p<0.01) between the periods of 252 and 1008 h. CONCLUSIONS: Both polishing methods presented no significant difference between the values of color derivatives of resins.
Resumo:
This study evaluated the influence of finishing and polishing procedures and different fluoride solutions on superficial morphology and chemistry of the nanofilled composite resin Supreme XT (3M) through the EDX analysis and SEM evaluation. Circular specimens (n = 30) of 10 mm diameter and 2 mm thickness were prepared, with half of the sample assays finished and polished with Super-Snap (R) sandpaper. The experimental groups were divided according to the presence or absence of finishing and polishing and solutions (artificial saliva, 0.05% of manipulated sodium fluoride solution, Fluordent Reach, Oral B, Fluorgard). Specimens were immersed in each respective solution for 1 min per day, during 60 days and stored in artificial saliva at 37 +/- 1 degrees C between immersion periods. Topography and chemical analysis was qualitative. It was observed that specimens submitted to finishing and polishing procedures had lower superficial degradation. Fluoride solutions promoted superficial alterations on specimens, being the highest degradation obtained with Fluordent Reach. It can be concluded that finishing and polishing procedures and the immersion media influence the superficial morphology of composite resin tested; the Fluordent Reach was the fluoride solution that most affected the material's surface. Microsc. Res. Tech. 2011., (c) 2011 Wiley Periodicals, Inc.