964 resultados para STABILIZER, CERAMIC SUSPENSIONS
Resumo:
Al(2)O(3):Eu(3+)(1%) samples were prepared by combustion, ceramic, and Pechini methods annealed from 400 to 1400 degrees C. XRD patterns indicate that samples heated up to 1000 degrees C present disordered character of activated alumina (gamma-Al(2)O(3)). However, alpha-Al(2)O(3) phase showed high crystallinity and thermostability at 1200-1400 degrees C. The sample characterizations were also carried out by means of infrared spectroscopy (IR), scanning electron microscopy (SEM) and specific surface areas analysis (BET method). Excitation spectra of Al(2)O(3):Eu(3+) samples present broaden bands attributed to defects of Al(2)O(3) matrices and to LMCT state of O -> Eu(3+), however, the narrow bands are assigned to (7)F(0) -> (5)D(J),(5)H(J) and (5)L(J) transitions of Eu(3+) ion. Emission spectra of samples calcined up to 1000 degrees C show broaden bands for (5)D(0) -> (7)F(J) transitions of Eu(3+) ion suggesting that the rare earth ion is in different symmetry sites showed by inhomogeneous line broadening of bands, confirming the predominance of the gamma-alumina phase. For all samples heated from 1200 to 1400 degrees C the spectra exhibit narrow (5)D(0) -> (7)F(J) transitions of Eu(3+) ion indicating the conversion of gamma to alpha-Al(2)O(3) phases, a high intensity narrow peak around 695 nm assigned to R lines of Cr(3+) ion is shown. Al(2)O(3):Eu(3+) heated up to 1100 degrees C presents an increase in the Omega(2) intensity parameter with the increase of temperatures enhancing the covalent character of metal-donor interaction. The disordered structural systems present the highest values of emission quantum efficiencies (eta). CIE coordinates of Al(2)O(3):Eu(3+) are also discussed. (C) 2007 Elsevier Inc. All rights reserved.
Resumo:
Glass microspheres containing radionuclides are used to treat liver cancer. A promising alternative therapy is being developed based on the magnetic hyperthermia which is related to the heat supplied by a magnetic material under an alternating current magnetic field. The advantage of this option is that most of killed cells are cancer cells which are more susceptible to the temperature raise. In the present work aluminum iron silicate glasses containing minor glass modifiers and nucleating agents were synthesized as irregular shape particles which were further transformed in microspheres by using a petrol liquefied gas-oxygen torch. The optimized processing parameters which lead to microspheres that give a response to the magnetic field were determined. The dissolution rate in water at 90 degrees C was determined to be 3 x 10(-8) g cm(-2) min(-1). The microsphere size distribution was determined by laser scattering. The crystalline phase responsible for the ferromagnetic response was identified as magnetite. Since this phase has a high saturation magnetization and high Curie temperature, it is potentially useful for biomedical applications. The hysteresis magnetic loop was measured for materials produced in different conditions, and some of them showed to be appropriated for thermotherapy. The ratio Fe(3+)/Fe(total) was determined by Mossbauer spectroscopy. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
We performed measurements of electrical resistivity as a function of temperature, rho(T), in polycrystalline samples of YBa(2)Cu(3)O(7-delta) (Y-123) subjected to different uniaxial compacting pressures. We observed by using X-ray diffractometry that samples have a very similar composition. Most of the identified peaks are related to the superconducting Y-123 phase. Also, from the X-ray diffraction patterns performed, in powder and pellet samples, we estimated the Lotgering factor along the (00l) direction, F((00l)). The results indicate that F((00l)) increases from 0.13 to 0.16. From electrical resistivity measurements as a function of temperature, we were able to separate contributions arising from both the grain misalignment and microstructural defects. We found appreciable degradation in the normal-state transport properties of samples with an increase in uniaxial compacting pressure. It seems that this type of behavior is associated with an increase in the influence of microstructural defects at the intergranular level. The experimental results are analyzed in the framework of a current conduction model of granular samples.
Resumo:
In this work, Ba(Zr(0.25)Ti(0.75))O(3) ceramic was prepared by solid-state reaction. This material was characterized by x-ray diffraction and Fourier transform Raman spectroscopy. The temperature dependent dielectric properties were investigated in the frequency range from 1 kHz to 1 MHz. The dielectric measurements indicated a diffuse phase transition. The broadening of the dielectric permittivity in the frequency range as well as its shifting at higher temperatures indicated a relaxor-like behaviour for this material. The diffusivity and the relaxation strength were estimated using the modified Curie-Weiss law. The optical properties were analysed by ultraviolet-visible (UV-vis) absorption spectroscopy and photoluminescence (PL) measurements at room temperature. The UV-vis spectrum indicated that the Ba(Zr(0.25)Ti(0.75))O(3) ceramic has an optical band gap of 2.98 eV. A blue PL emission was observed for this compound when excited with 350 nm wavelength. The polarity as well as the PL property of this material was attributed to the presence of polar [TiO(6)] distorted clusters into a globally cubic matrix.
Resumo:
The thermoluminescence (TL) response of Dy and Li doped 20CaB(4)O(7)-80CaB(2)O(4) (Wt%) glass-ceramic irradiated with ultraviolet (UV) radiation was studied. In order to act as TL activator ions, the Dy and Li ions were included in the matrix during the melting process to increase its TL efficiency. A single crystalline CaB2O4 phase was present in the glass-ceramic as determined by X-ray diffraction (XRD). The glass-ceramic 20CaB(4)O(7)-80CaB(2)O(4):Dy,Li wt% (named 20CBO7:Dy,Li) is a newly prepared TL material. Its thermoluminescent dosimetric characteristics have shown a linear response under UV radiation exposure and a good TL signal reproducibility, thus proving to be a promising material for using as an ultraviolet radiation dosimeter. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Perovskite-structured Ba(0.90)Ca(0.10)(Ti(1-x)Zr(x))O(3) ceramics were prepared in this work and subsequently studied in terms of composition-dependent dielectric and high-resolution long-range order structural properties from 30 to 450 K. The dielectric response of these materials was measured at several frequencies in the range from 1 kHz to 1 MHz. Combining both techniques, including Rietveld refinement of the X-ray diffraction data, allowed observing that, when increasing Zr(4+) content, the materials change from conventional to diffuse and relaxor ferroelectric compounds, the transition occurring spontaneously at the x = 0.18 composition. Interestingly, this spontaneous transition turned out to be prevented for a further increase of Zr(4+). On the basis of all the dielectric and structural results processed, a phase diagram of this system is presented. (C) 2010 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim
Resumo:
The residual stress distribution that arises in the glass matrix during cooling of a partially crystallized 17.2Na(2)O-32.1CaO-48.1SiO(2)-2.5P(2)O(5) (mol%) bioactive glass-ceramic was measured using the Vickers indentation method proposed by Zeng and Rowcliffe (ZR). The magnitude of the determined residual stress at the crystal/glass boundary was 1/4-1/3 of the values measured using X-ray diffraction (within the crystals) and calculated using Selsing`s model. A correction for the crack geometry factor, assuming a semi-elliptical shape, is proposed and then good agreement between experimental and theoretical values is found. Thus, if the actual crack geometry is taken into account, the indentation technique of ZR can be successfully used. In addition, a numerical model for the calculation of residual stresses that takes into account the hemispherical shape of the crystalline precipitates at a free surface was developed. The result is that near the sample surface, the radial component of the residual stress is increased by 70% in comparison with the residual stress calculated by Selsing`s model.
Resumo:
This paper reports on the effect of glass ceramic silica matrix on [CrO4](4-) and Cr2O3 NIR and visible luminescence. Chromium-containing silica was obtained by precipitation from water-glass and chromium nitrate acid solution with thermal treatment at 1000 degrees C. From XRD results silica and silica-chromium samples are crystalline. The chromium emission spectrum presents two main broad bands: one in the NIR region (1.1-1.7 mu m) and other in the visible region (0.6-0.7 mu m) assigned to Cr4+ and to Cr3+, respectively. This thermal treated glass ceramic silica-chromium sample stabilizes the [CrO4](4-) where Cr4+ substitutes for Si4+ and also hexacoordinated Cr3+ group probably as segregated phase in the system. It can be pointed out that luminescence spectroscopy is a powerful toot for detecting the two chromium optical centers in the glass ceramic silica. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
We investigate magnetorheological fluids (MRFs) prepared with carbonyl iron powder and different types of hydrophobic and hydrophilic fumed silica. The rheological properties of the MRF suspensions were investigated with and without an applied magnetic field. The MRF samples prepared with hydrophobic silicas presented a more pronounced thixotropic effect and a higher recovery rate than those prepared with hydrophilic silicas. The application of a magnetic field to all the MRFs samples investigated leads to an increase in the viscosity and the thixotropic effect. MRF prepared with hydrophobic silicas presented smaller values of the viscosity than those prepared with hydrophilic silicas. At low applied magnetic fields, the type of the silica used to prepare the MRF leads to noticeable differences in the shear stress. However, these differences disappear at high magnetic fields. The results obtained showed that MRF samples prepared with the hydrophobic silica with the biggest particle diameter presented better characteristics for magnetorheological fluids, with higher values of yield stress, recovery rate, and elastic modulus. (C) 2009 The Society of Rheology. [DOI: 10.1122/1.3086870]
Resumo:
This work assesses the photocatalytic (TiO2/UV) degradation of a simulated acid dye bath (Yellow 3, Red 51, Blue 74, and auxiliary chemicals). Color and phytotoxicity removal were monitored by spectrophotometry and lettuce (Lactuca sativa) seeds as the test organism, respectively. Mineralization was determined by DOC analyses. Photocatalytic, photolytic, and adsorption experiments were performed, showing that adsorption was negligible. After 240 minutes of irradiation, it was achieved 96% and 78% of color removal with photocatalysis and photolysis, respectively. 37% of mineralization occurred with photocatalysis only. The dye bath was rendered completely non-toxic after 60 minutes of photocatalytic treatment; the same result was only achieved with photolysis after 90 minutes. A kinetic model composed of two first-order in series reactions was used. The first photocatalytic decolorization rate constant was k(1) = 0.062 min(-1) and the second k(2) = 0.0043 min(-1), approximately two times greater than the photolytic ones.
Resumo:
This work assesses the photocatalytic (TiO(2)/UV) degradation of a simulated reactive dye bath (Black 5, Red 239, Yellow 17, and auxiliary chemicals). Color removal was monitored by spectrophotometry. Mineralization was determined by DOC analyses. Photocatalytic, photolytic, and adsorption experiments were performed, showing that adsorption was negligible. After 30 min of irradiation, it was achieved 97% and 40% of color removal with photocatalysis and photolysis, respectively. No mineralization occurred within 30 min. A kinetic model composed of two, first-order in-series reactions was used. The first photocatalytic decolorization rate constant was k(1) = 2.6 min(-1) and the second k(2) = 0.011 min(-1). The fast decolorization of Reactive Black 5 dye is an indication that the number of azo and vinylsulfone groups in the dye molecule maybe a determining factor for the increased photolytic and photocatalytic color removal and degradation rates. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
This study shows a possibility of using municipal sewage sludge after thermal treatment in the production of a filtering material to water treatment. Due to the fast urbanization and implementation of high standards for effluent in many countries in recent years, the sewage sludge is being produced in an ever increasing amount. Therefore, the use of sludge is a suitable solution for the expected large quantity of sludge. Dehydration of sludge was performed by controlled heating at temperatures of 1100 degrees C, 850 degrees C, 650 degrees C, 350 degrees C for 3 hours. After thermal treatment the sludge was characterized by X-ray fluorescence, TG/DTG/DTA, residue solubilization and residue lixiviation tests. The aim of the present work was to observe, thought the characterization techniques, if the treated sewage sludge is or not adequate to be used as filter material to water treatment. It will be verified which treatment temperature of the sludge offer possibility to its use in water treatment without carrying pollutants in concentrations out of the standards.
Resumo:
Nowadays, with increase amounts of sludge derived from the treatment of domestic sewage put pressure into research on systems for the adequate use of these materials. The aim of the present work is to study the use of sludge ash, from sintering and calcinated process, as a raw material for the ceramic industry. Using the sewage sludge ashes as ceramic raw material there will be no contamination of soil and underground water. Metals and toxic compounds like Al, Fe, Ba, Cr, Cu, Mn and Zn oxides were analyzed and characterized by X-ray fluorescence (XRF), scanning electron microscopy (SEM) and plasma emission spectroscopy (ICP-OES). The leached material was chemically analyzed where the integration of oxides into the ceramic matrix of sludge ash was observed. Residual decomposition was analyzed by TG, DTG and DTA curves.
Resumo:
An archeological artifact can be seen as a chronological element, which helps to determine the age of certain society and to understand the thinking, values and the way of life of this society. Thus, the classification of archeological artifacts is one of the approaches used to study the cultural system of antique societies trying to reconstruct their history. The "Centro de Museologia, Antropologia e Argueologia (CEMAARQ)" of the "Unesp Univ Estadual Paulista" in Presidente Prudente, São Paulo state, Brazil, develops projects within this context (identification and preservation). This is the case of the archeological site named "Lagoa São Paulo-02" discovered in 1993 at the margins of the Parana river in the region of Presidente Epitacio city, São Paulo state, Brazil. This site has ceramic fragments of different shapes and sizes that have a strong influence of traces of the Guarani culture, which is one of the Brazilian native populations. These samples were basically characterized via micro-Raman scattering and Fourier transform infrared absorption (FTIR) spectroscopies. The main objective was to identify the pigments used in the manufacture of the ceramic artifacts and to analyze the composition of the ceramic body to understand how the artifacts were made. Three pigments were found: red, black and white. For the red pigment were identified characteristic bands of hematite, an iron oxide found in the red rocks of the river banks that were eroded by water. The black pigment, probably, is due to the use of vegetal charcoal, which is found in nature as the product of burning organic material such as wood. For the white pigment, the FTIR spectra suggested the use of kaolin, either in the ceramic body or in the proper white pigment, due to the presence of the characteristic bands of the kaolinite. Complementary, the additives applied as anti-plastics were identified as charcoal and quartz, being the latter found in the rocks present in the archeological site. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Sugarcane bagasse ash (SCBA) is an industrial waste that contains silicon and aluminum oxides as the major components and iron, calcium, magnesium, and potassium oxides as the main minor components. In this paper, SCBA from one Brazilian factory was characterized and tested for its influence on the ceramic properties of clay/ash ceramic probes. Prismatic probes were pressed (18 MPa) using a ceramic mass mixed with 0%, 5%, 8%, and 10% ash. The probes were fired at temperatures between 800 degrees and 1200 degrees C. X-ray diffraction, X-ray fluorescence, thermal analysis (differential thermal analysis, thermo-gravimetric analysis/differential thermogravimetric analysis), and tests for texture (particle-size analysis), flexural strength, and linear shrinkage were carried out to characterize the samples. The results showed that the amount of ash to be incorporated will depend on mainly the composition of clay but also ash, and indicated that the clay used in this work can incorporate up to 10% weight of ash to produce solid bricks. The results also showed an improvement in ceramic/ash properties up to sintering temperatures higher than 1000 degrees C.