939 resultados para Nanopartículas de TiO2
Resumo:
Nebulized spray pyrolysis of metal-organic precursors in methanol solution has been employed to prepare powders of TiO2, ZrO2 and PbZr0.5Ti0.5O3 (PZT). This process ensures complete decomposition of the precursors at relatively low temperatures. The particles have been examined by scanning and transmission electron microscopy as well as X-ray diffraction. As prepared, the particles are hollow agglomerates of diameter 0.1-1.6 mu m, but after heating to higher temperatures the ultimate size of the particles comprising the agglomerates are considerably smaller (0.1 mu m or less in diameter) and crystalline.
Resumo:
Glass samples with compositions (100-2x)SrB4O7-xBaO-xTiO(2) (10 less than or equal to x less than or equal to 40) were prepared by conventional melt quenching and the influence of the addition of BaO-TiO2 on the structural, dielectric and optical properties of SBO glasses was studied The molar volume, glass transition temperature and the optical polarisability of the glass samples were found to decrease with increase in BaO-TiO2 content while the refractive index and optical band gap increase with increase in BaO-TiO2 content.
Resumo:
Titanium dioxide films have been deposited using DC magnetron sputtering technique onto well-cleaned p-silicon substrates at an oxygen partial pressure of 7 x 10(-5) mbar and at a sputtering pressure (Ar + O-2) Of I X 10(-3) mbar. The deposited films were calcinated at 673 and 773 K. The composition of the films as analyzed using Auger electron spectroscopy reveals the stoichiometry with an 0 and Ti ratio 2.08. The influence of post-deposition annealing at 673 and 773 K on the structural properties of the titanium dioxide thin films have been studied using XRD and Raman scattering. The structure of the films deposited at the ambient was found to be amorphous and the films annealed at temperature 673 K and above were crystalline with anatase structure. The lattice constants, grain size, microstrain and the dislocation density of the film are calculated and correlated with annealing temperature. The Raman scattering study was performed on the as-deposited and annealed samples and the existence of Raman active modes A(1g), B-1g and E-g corresponding to the Raman shifts are studied and reported. The improvement of crystallinity of the TiO2 films was also studied using Raman scattering studies. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
TiO2 thin films were prepared by sol gel method. The structural investigations performed by means of X- ray diffraction (XRD) technique, Scanning electronic microscopy (SEM) showed the shape structure at T=600°C. The optical constants of the deposited film were obtained from the analysis of the experimental recorded transmittance spectral data over the wavelengths range 200-3000 nm. The values of some important parameters (refractive index n, dielectric constant ε ∞ and thickness d), and the third order optical nonlinear susceptibility χ(3) of TiO2 film are determined from these spectra. It has been found that the dispersion data obey the single oscillator relation of the Wemple-DiDomenico model, from which the dispersion parameters and high – frequency dielectric constant were determined. The estimation of the corresponding band gap Eg , χ (3) and ε ∞ are 2.57 eV, 0.021 × 10-10 esu and 5.20,respectively.
Resumo:
The activity of Ti02 in single and two··phase regions of ihe system ZrOrTi02 has heen measured lIsing solid state cells based on yttria··doped tho ria (YDT) as the solid electrolyte at 1373 K. The cells used can be represented as: Pt, Tio.07PtO.Y3 + Zrj.,Tix0 2 / YDT / Ti02 + Tio.07Pto.93, Pt Pt, Tio.07Pto.93 + ZrJ.xTix02 + ZrTi04 / YDT / Ti02+ Tio.07PtO.93, Pt In each cell the composition of Pt-Ti alloy was identical at hoth electrodes. The emf of the cell is therefore directly related to the activity of Ti02 in oxide phase or oxide phase mixture: aTiO~ :;: cxp (-4FE/RT). The activity coefficient of Ti02 in th~ zirconia-rich solid solution with monoclinic structure (CUl2 2" XTi02 2" 0) can be expressed as:In the zirconia-rich solid solution with tetragonal structure (0.085 2" X ri02 2" 0.03), the activity coefficient is given by:In YTi02 (± 0.012) = 2.354 (1-XTiO? )2 +0.064 The standard Gibbs energy of formation of ZrTi04 is -5650 (± 200) J/mol at 1373 K .
Resumo:
he standard Gibbs energy of formation of CaCu3Ti4O12 (CCTO) from CaTiO3, CuO and TiO2 has been determined as a function of temperature from 925 to 1350 K using a solid-state electrochemical cell with yttria-stabilized zirconia as the solid electrolyte. Combining this result with information in the literature on CaTiO3, the standard Gibbs energy of formation of CCTO from its component binary oxides, CaO, CuO and TiO2, has been obtained: View the MathML source (CaCu3Ti4O12)/J mol−1 (±600) = −125231 + 6.57 (T/K). The oxygen chemical potential corresponding to the reduction of CCTO to CaTiO3, TiO2 and Cu2O has been calculated from the electrochemical measurements as a function of temperature and compared on an Ellingham diagram with those for the reduction of CuO to Cu2O and Cu2O to Cu. The oxygen partial pressures corresponding to the reduction reactions at any chosen temperature can be read using the nomograms provided on either side of the diagram. The effect of the oxygen partial pressure on phase relations in the pseudo-ternary system CaO–CuO/Cu2O–TiO2 at 1273 K has been evaluated. The phase diagrams allow identification of secondary phases that may form during the synthesis of the CCTO under equilibrium conditions. The secondary phases may have a significant effect on the extrinsic component of the colossal dielectric response of CCTO.
Resumo:
We have synthesized 5-7 nm size, highly crystalline TiO2 which absorbs radiation in the visible region of solar spectrum. The material shows higher photocatalytic activity both in UV and visible region of the solar radiation compared to commercial Degussa P25 TiO2. Transition metal ion substitution for Ti4+ creates mid-gap, states which act as recombination centers for electron-hole induced by photons thus reducing photocatalytic activity. However, Pt, Pd and Cu ion substituted TiO2 are excellent CO oxidation and NO reduction catalysts at temperatures less than 100 degrees C.
Resumo:
Degradation of dimethoate under UV irradiation using TiO2/polymer films prepared by the layer-by-layer (LbL) method was investigated. The thin films were fabricated on glass slides and the surface morphology and roughness of the thin films were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM) and atomic force microscopy (AFM). The effect of lamp intensity, catalyst loading in the layers, number of bilayers, pH and initial dimethoate concentration on the degradation of dimethoate was systematically studied. The degradation was monitored using high performance liquid chromatography (HPLC) analysis and total organic carbon (TOC) measurements as a function of irradiation time, to see the change in concentration of dimethoate and mineralization, respectively. Complete degradation of dimethoate was achieved under TiO2 optimum loading of 4 g/L at an UV irradiation time of 180 min. Increase in the lamp intensity, catalyst loading and number of bilayers increased the rate of degradation. At a pH of 4.62, complete degradation of dimethoate was observed. The degradation efficiency decreased with increase in initial dimethoate concentration. The degradation byproducts were analyzed and confirmed by gas chromatography-mass spectra (GC-MS). Toxicity of the irradiated samples was measured using the luminescence of bacteria Vibrio fischeri after 30 min of incubation and the results showed more toxicity than the parent compound. Catalyst reusability studies revealed that the fabricated thin films could be repeatedly used for up to ten times without affecting the photocatalytic activity of the films. The findings of the present study are very useful for the treatment of wastewaters contaminated with pesticides. (C) 2011 Elsevier B.V. All rights reserved.