Resumo:
Deformation twinning has been observed in room-temperature rolled nanocrystalline Ni. The growth of the deformation twins via the emission of partial dislocations from a grain boundary has been examined in detail. Partial dislocations on neighboring slip planes may migrate for different distances and then remain in the grain interior, leading to the formation of a steplike twin boundary TB . With continued twin growth, the TBs become gradually distorted and lose their coherent character due to accumulated high stresses. Moreover, we propose that microtwins may form near such TBs due to the emission of partial dislocations from the TB.
Resumo:
Since the exchange coupling theory was proposed by Kneller and Hawig in 1991 there has been a significant effort within the magnetic materials community to enhance the performance of rare earth magnets by utilising nano-composite meta-materials. Inclusions of magnetically soft iron smaller than approximately 10 nm in diameter are exchange coupled to a surrounding magnetically hard Nd2Fe14B matrix and provide an enhanced saturisation magnetisation without reducing coercivity. For such a fine nanostructure to be produced, close control over the thermal history of the material is needed. A processing route which provides this is laser annealing from an amorphous alloy precursor. In the current work, relationships between laser parameters, thermal histories of laser processed amorphous stoichiometric NdFeB ribbons and the magnetic properties of the resulting nanocrystalline products have been determined with a view to applying the process to thick film nanocomposite magnet production.
Resumo:
Nanocrystalline ZnO films with strong (0002) texture and fine grains were deposited onto ultra-nanocrystalline diamond (UNCD) layers on silicon using high target utilization sputtering technology. The unique characteristic of this sputtering technique allows room temperature growth of smooth ZnO films with a low roughness and low stress at high growth rates. Surface acoustic wave (SAW) devices were fabricated on ZnO/UNCD structure and exhibited good transmission signals with a low insertion loss and a strong side-lobe suppression for the Rayleigh mode SAW. Based on the optimization of the layered structure of the SAW device, a good performance with a coupling coefficient of 5.2% has been realized, promising for improving the microfluidic efficiency in droplet transportation comparing with that of the ZnO/Si SAW device. An optimized temperature coefficient of frequency of -23.4 ppm°C-1 was obtained for the SAW devices with the 2.72 μm-thick ZnO and 1.1 μm-thick UNCD film. Significant thermal effect due to the acoustic heating has been redcued which is related to the temperature stability of the ZnO/UNCD SAW device. © 2013 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
In-situ energy dispersive x-ray diffraction on ZnS nanocrystalline was carried out under high pressure by using a diamond anvil cell. Phase transition of wurtzite of 10 nm ZnS to rocksalt occurred at 16.0 GPa, which was higher than that of the bulk materials. The structures of ZnS nanocrystalline at different pressures were built by using materials studio and the bulk modulus, and the pressure derivative of ZnS nanocrystalline were derived by fitting the equation of Birch-Murnaghan. The resulting modulus was higher than that of the corresponding bulk material, which indicates that the nanomaterial has higher hardness than its bulk materials.
Resumo:
In situ energy dispersive X-ray diffraction measurements on nanocrystalline zinc sulfide have been performed by using diamond anvil cell with synchrotron radiation. There is a phase transition which the ultimate structure is rocksalt when the pressure is up to 16.0GPa. Comparing the structure of body materials, the pressure of the phase transition of nano zinc sulfide is high. We fit the: Birch-Murnaghan equation of state and obtained its ambient pressure bulk modulus and its pressure derivative. The bulk modulus of nanocrystalline zinc sulfide is higher than that of body materials, it indicate that the rigidity of nanocrystalline zinc sulfide is high.
Resumo:
Nanocrystalline silicon (nc-Si) embedded SiO2 matrix has been formed by annealing the SiOx films fabricated by plasma-enhanced chemical vapor deposition (PECVD) technique. Absorption coefficient and photoluminescence of the films have been measured at room temperature. The experimental results show that there is an "aUrbach-like" b exponential absorption in the spectral range of 2.0-3.0 eV. The relationship of (alpha hv)(1/2) proportional to(hv - E-g) demonstrates that the luminescent nc-Si have an indirect band structure. The existence of Stokes shift between photoluminescence and absorption edge indicates that radiative combination can take place not only between electron states and hole states but also between shallow trap states of electrons and holes. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
The improved mechanical properties of surface nano-crystallized graded materials produced by surface severe plastic deformation ((SPD)-P-2) are generally owing to the effects of the refined structure, work-hardened region and compressive residual stress. However, during the (SPD)-P-2 process, residual stress is produced simultaneously with work-hardened region, the individual contribution of these two factors to the improved mechanical properties remains unclear. Numerical simulations are carried out in order to answer this question. It is found that work hardening predominates in improving the yield strength and the ultimate tensile strength of the surface nano-crystallized graded materials, while the influence of the residual stress mainly emerges at the initial stage of deformation and decreases the apparent elastic modulus of the surface nano-crystallized graded materials, which agrees well with the experimental results. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
In the present work, nanocrystalline Ni (nc-Ni) with a broad grain size distribution (BGSD) of 5-120 nm and an average grain size of 27.2 nm was prepared. The BGSD nc-Ni sample shows a similar strength and good ductility in comparison with electrodeposited nc-Ni with a narrow grain size distribution. The intracrystalline dislocation network was observed in the post-deformed microstructure confirming the conventional intracrystalline dislocation sliding mechanism in BGSD nc-Ni. The uniaxial tensile loading-unloading-loading deformation shows BGSD nc-Ni has the capability to store dislocations in the grain interior, which is very limited compared with that of coarse grained metals. For BGSD nc-Ni, the strain rate sensitivity of flow stress m enhances with decreasing strain rate. At the strain rate of 5 x 10(-6) s(-1), m was estimated to be 0.055. At the corresponding strain rate, the enhanced ductility along with the decreased strength was achievable, indicating activation of other deformation mechanisms, e. g. grain boundary sliding or diffusion.
Resumo:
Nanocrystalline Gd1.77Yb0.2 Er0.03O3 samples were prepared by combustion and precipitation methods. Structures and upconversion luminescence properties of samples were studied. The results of XRD show that all samples are cubic structure, the average crystallite size could be calculated as 23 nm and 39 nm, respectively. The lattice constants were obtained. The FT-IR spectra were measured to investigate the vibrational feature of the samples.
Combustion synthesis and luminescent properties of the Eu3+-doped yttrium oxysulfide nanocrystalline
Resumo:
Nanocrystallinc Y2O2S:Eu3+ was successfully prepared with a combustion synthesis method, the corresponding bulk Y2O2S:Eu3+ was synthesized by conventional sulfur flux method. The results of XRD indicated that both bulk and nanocrystalline Y2O2S:Eu3+ have Pure hexagonal phases. The crystallite size was calculated to be about 20 nm according to Scherrer formula, which was consistent with the size as indicated by transmission electron microscopy (TEM).
Resumo:
A novel nano-scaled bulk hard material (W0.5Al0.5)C-Co with "rounded" grains was prepared by nanocrystalline "rounded" (W0.5Al0.5)C powders with "rounded" particle shape in this study. The nano-scaled "rounded" particles do not contain sharp edges, which form local tensile stress concentrations on loading of the composite, thus leading to improved toughness and reduced sensitivity to crack. Nanocrystalline (W0.5Al0.5)C powders with "rounded" particle shape were used as starting materials. X-ray diffraction, scanning electron microscopy, and transmission electron microscopy were used to characterize the samples.
Resumo:
In this paper, nanocrystalline YVO4:Eu3+ powders have been successfully synthesized via high-temperature solution-phase synthesis process. The nanocrystalline YVO4:Eu3+ particles were characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), UVNis absorption spectra and luminescence spectra, luminescence decay curve and Fourier transform infrared (FT-IR), X-ray photoelectron spectra (XPS) respectively. The as-prepared nanocrystalline YVO4:Eu3+ particles are well crystallized with ellipsoidal morphology.
Resumo:
Blue, yellow and white light emissive LaOCl:Tm3+, LaOCl:Dy3+ and LaOCl: Tm3+, Dy3+ nanocrystalline phosphors were synthesized through the Pechini-type sol-gel process. X-Ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), photoluminescence (PL) and cathodoluminescence (CL) spectra were used to characterize the samples. Under UV radiation (229 nm) and low-voltage electron beam (0.5-5 kV) excitation, the Tm3+-doped LaOCl phosphor shows a very strong blue emission corresponding to the characteristic transitions of Tm3+ (D-1(2), (1)G(4) -> F-3(4), H-3(6)) with the strongest emission at 458 nm. The cathodoluminescent color of LaOCl:Tm3+ is blue to the naked eye with CIE coordinates of x = 0.1492, y = 0.0684. This phosphor has better CIE coordinates and higher emission intensity than the commercial product Y2SiO5:Ce3+.