Bacterial cellulose/polymethacrylate nanocomposites have received attention in numerous areas of study and in a variety of applications. The attractive properties of methacrylate polymers and bacterial cellulose, BC, allow the synthesis of new nanocomposites with distinct characteristics. In this study, BC/poly(glycidylmethacrylate) (BC/PGMA) and BC/poly(ethyleneglycol)methacrylate (BC/PPEGMA) nanocomposites were prepared through in situ free radical polymerization of GMA and PEGMA, respectively. Ammonium persulphate (APS) was used as an initiator and N,N’methylenebisacrilamide (MBA) was used as a crosslinker in BC/PGMA. Chemical composition, morphology, thermal stability, water absorption, mechanic and surface properties were determined through specific characterization techniques. The optimal polymerization was obtained at (1:2) for BC/PGMA, (1:2:0.2) ratio for BC/GMA/MBA and (1:20) for BC/PPEGMA, with 0.5% of initiator at 60 ºC during 6 h. A maximum of 67% and 87% of incorporation percentage was obtained, respectively, for the nanocomposites BC/PGMA/MBA and BC/PPEGMA. BC/PGMA nanocomposites exhibited an increase of roughness and compactation of the three-dimensional structure, an improvement in the thermal and mechanical properties, and a decrease in their swelling ability and crystallinity. On the other hand, BC/PPEGMA showed a decrease of stiffness of three-dimensional structure, improvement in thermal and mechanical properties, an increase in their swelling ability and a decrease the crystallinity. Both BC/polymethacrylate nanocomposites exhibited a basic surface character. The acid treatment showed to be a suitable strategy to modifiy BC/PGMA nanocomposites through epoxide ring-opening reaction mechanism. Nanocomposites became more compact, smooth and with more water retention ability. A decrease in the thermal and mechanical proprieties was observed. The new nanocomposites acquired properties useful to biomedical applications or/and removal of heavy metals due to the presence of functional groups.
Resumo:
The dieletric relaxation properties of thermosetting material nanocomposites based on spherosilicate nanoplatforms were studied from room temperature to 170 degrees C, varying the frequency from 10 to 1000 KHz. Permittivity (epsilon'), dielectric loss (epsilon ''), and activation energy (E-a) were calculated. The results of dielectric relaxation were confirmed by those of the final properties. The dielectric loss amplitude decreases with increasing ODPG content until about 70-73 wt % and slightly increases at higher ODPG content. This means that the increasing of the ODPG content in the composite samples decreases the number of pendants groups and/or increases crosslink densitv, causing decreased motion of organic tethers, and subsequently decreasing of the dipolar mobility. The results of apparent activation energy, fracture toughness and tensile modulus mechanical properties show the same profile with respect to ODPG content, in the sense that they exhibit maxima around 70 wt % ODPG. For the ODPG/MDA composites, this formulation of 70 wt % ODPG containing excess of amine is not composition where the highest crosslinked density is reached. This implies that the best mechanical properties and E-a are provided by some degree of chain flexibility. (c) 2007 Wiley Periodicals, Inc.
Resumo:
Nanocellulose is the crystalline domains obtained from renewable cellulosic sources, used to increase mechanical properties and biodegrability in polymer composites. This work has been to study how high pressure defibrillation and chemical purification affect the PALF fibre morphology from micro to nanoscale. Microscopy techniques and X-ray diffraction were used to study the structure and properties of the prepared nanofibers and composites. Microscopy studies showed that the used individualization processes lead to a unique morphology of interconnected web-like structure of PALF fibers. The produced nanofibers were bundles of cellulose fibers of widths ranging between 5 and 15 nm and estimated lengths of several micrometers. Percentage yield and aspect ratio of the nanofiber obtained by this technique is found to be very high in comparison with other conventional methods. The nanocomposites were prepared by means of compression moulding, by stacking the nanocellulose fibre mats between polyurethane films. The results showed that the nanofibrils reinforced the polyurethane efficiently. The addition of 5 wt% of cellulose nanofibrils to PU increased the strength nearly 300% and the stiffness by 2600%. The developed composites were utilized to fabricate various versatile medical implants. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
Cellulose nanocrystals have been evaluated as reinforcement material in polymeric matrices due to their potential to improve the mechanical, optical, and dielectric properties of these matrixes. This work describes how high pressure defibrillation and chemical purification affect the sludge fiber morphology from micro to nanoscale. Microscopy techniques and X-ray diffraction were used to study the structure and properties of the prepared nanofibers and composites. Microscopic studies showed that the used individualization processes lead to a unique morphology of interconnected web-like structure of sludge fibers. The nanofibers are bundles of cellulose fibers having widths (5 to 30 nm) and estimated lengths of several micrometers.
Resumo:
The present paper deals with the extraction of saponins from the pericarp of Sapindus mukorossi to use as compatibilizer in nanocomposites. The nanofibrils extracted from banana fibres are utilized as reinforcement of nanocomposite. These nanofibers were treated with Saponin, GPS (3-Glycidoxypropyltrimethoxysilane) and APS (3-Aminopropyltriethoxysilane) to compare the effectiveness of surface treatment. The effectiveness of surface modification was reflected on the increase in mechanical (tensile test, flexural modulus, impact test) properties and decrease in the RMS (Roughness Measurement System) roughness investigation by SFM (Scanning force microscopy) analysis.
Resumo:
Cellulose macro- and nanofibers have gained increasing attention due to the high strength and stiffness, biodegradability and renewability, and their production and application in development of composites. Application of cellulose nanofibers for the development of composites is a relatively new research area. Cellulose macro- and nanofibers can be used as reinforcement in composite materials because of enhanced mechanical, thermal, and biodegradation properties of composites. Cellulose fibers are hydrophilic in nature, so it becomes necessary to increase their surface roughness for the development of composites with enhanced properties. In the present paper, we have reviewed the surface modification of cellulose fibers by various methods. Processing methods, properties, and various applications of nanocellulose and cellulosic composites are also discussed in this paper.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Um hidrogel foi desenvolvido a partir de dextrano 70 kDa (DEX-70) e praziquantel incorporado (PZQ) como fármaco modelo. Propriedades biofarmacêuticas, como solubilidade e velocidade de dissolução, foram analisadas no desenvolvimento do hidrogel. Além disso, o hidrogel também foi caracterizado por espectroscopia na região do infravermelho e calorimetria diferencial exploratória (DSC). Testes da taxa de intumescimento mostraram que o hidrogel intumesce lentamente, embora tenha sido mais rápido do que a taxa do polímero livre. Nos testes de dissolução, o hidrogel liberou o fármaco lenta e continuamente. Esta liberação lenta foi semelhante a observada nos testes de intumescimento e resultou em uma liberação controlada do fármaco. Assim, o dextrano 70 kDa é um polímero adequado para o desenvolvimento de hidrogéis como veículos para a liberação controlada de fármacos.
Resumo:
Non-isothermal dielectric analysis (DEA) and differential scanning calorimetry (DSC) techniques were used to study the epoxy nanocomposites prepared by reacting 1,3,5,7,9,11,13,15-octa[dimethylsiloxypropylglycidylether] pentaciclo [9.5.1.1(3,9).1(5,15).1(7,13)] octasilsesquioxane (ODPG) with methylenedianiline (MDA). Loss factor (epsilon) and activation energy were calculated by DEA. The relationships between the loss factor, the activation energy, the structure of the network, and the mechanical properties were investigated. Activation energies determined by DEA and DSC, heat of polymerization, fracture toughness and tensile modulus show the same profile for mechanical properties with respect to ODPG content.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)