The thermal and hydrothermal stabilities of HZSM-5 zeolites with crystal sizes less than 100 nm have been studied by multinuclear solid-state NMR, combined with BET and XRD. As evidenced by Al-27 and Si-29 MAS as well as their corresponding cross-polarization/MAS NMR investigations, the thermal stability of nanosized HZSM-5 is not so good as that of microsized HZSM-5. This is due to two processes concerning dealumination and desilicification involved in the calcination of nanosized HZSM-5, while only the dealumination process is conducted in microsized HZSM-5 under the similar calcination process. The hydrothermal stability of nanosized HZSM-5 is, contrary to what was expected, not so bad as that of the microsized HZSM-5 in the course of steam treatment. The actual resistance of the hydrothermal stability to the crystal size of HZSM-5 can be ascribed to an active reconstruction of zeolitic framework through an effective filling of amorphous Si species into nanosized HZSM-5 during hydrothermal treatment. (C) 2001 Published by Elsevier Science B.V.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Carbonaceous deposits formed during the temperature-programmed surface reaction (TPSR) of methane dehydro-aromatization (MDA) over Mo/HZSM-5 catalysts have been investigated by TPH, TPCO2 and TPO, in combination with thermal gravimetric analysis (TG). The TPO profiles of the coked catalyst after TPSR of MDA show two temperature peaks: one is at about 776 K and the other at about 865 K. The succeeding TPH experiments only resulted in the diminishing of the area of the high-temperature peak, and had no effect on the area of the low-temperature peak. On the other hand, the TPO profiles of the coked catalyst after succeeding TPCO2 experiments exhibited obvious reduction in the areas of both the high-and low-temperature peaks, particularly in the area of the low-temperature peak. On the basis of TPSR, TPR and TPCO2 experiments and the corresponding TG analysis, quantitative analysis of the coke and the kinetics of its burning-off process have been studied. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The secondary pores in the nanosized HZSM-5 zeolite have been observed for the first time via Xe-129 NMR spectroscopy using xenon as a probe; the location of non-framework Al can also be identified.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

High-throughput screening of HZSM-5 supported metal-oxides catalysts were carried out for the coupling reaction of methane with CO to aromatics in a multi-stream reactor system. Zn/HZSM-5 and Mo/HZSM-5 were observed to be rather effective for the catalytic formation of aromatics from the coupling reaction of methane with CO. Temperature-programmed reaction has further proven the efficiency of the coupling of methane and CO over Zn/HZSM-5 catalyst. The results were also validated in a conventional fixed-bed reactor coupled with GC. The results propose that the coupling methane with CO toward benzene and naphthalene can be catalyzed by Zn/HZSM-5 at 500 ° C. Both methane and CO are needed for the formation of reactive coke on the catalyst, and the reactive coke may be the initial product in the producing of hydrocarbons. © 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In order to investigate the effect of acid properties on the coke behavior and stability of butene aromatization, we prepared the AHZSM-5 samples with various acid properties by the methods of hydrothernial treatment and K addition. The reaction of butene aromatization was carried out at 350 degrees C and 0.5 MPa in a continuous flow fixed bed. The characterization of the fresh/coked catalysts with NH3-TPD, N-2 adsorption-desorption measurement, and TG techniques has shown that a large amount of acid sites (high acid density) of the AHZMS-5 catalyst can cause a large quantity of coke deposit and serious channel blockage, and so result in a rapid loss of aromatization activity. On the contrary, after a great reduction in strong acid sites of AHZSM-5 catalyst resulting from some K-modification, the presence of only many weak acid sites also could not lessen the formation of coke nor improve the reaction stability of butene aromatization. Interestingly, the simultaneous reduction in the strong and weak acid sites to a desirable level by hydrothermal treating the AHZSM-5 catalyst at a proper temperature can effectively suppress the coke formation and channel blockage, and thus improve its olefin aromatization stability. (c) 2005 Elsevier B.V. All rights reserved.