551 resultados para ionospheric scintillation


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Commercially available LaBr3:5% Ce3+ scintillators show with photomultiplier tube readout about 2.7% energy resolution for the detection of 662 keV γ-rays. Here we will show that by co-doping LaBr3:Ce3+ with Sr2+ or Ca2+ the resolution is improved to 2.0%. Such an improvement is attributed to a strong reduction of the scintillation light losses that are due to radiationless recombination of free electrons and holes during the earliest stages (1–10 ps) inside the high free charge carrier density parts of the ionization track.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reports on the effects of Li+, Na+, Mg2+, Ca2+, Sr2+, and Ba2+ co-doping on the scintillation properties of LaBr3:5%Ce3+. Pulse-height spectra of various gamma and X-ray sources with energies from 8 keV to 1.33 MeV were measured from which the values of light yield and energy resolution were derived. Sr2+ and Ca2+ co-doped crystals showed excellent energy resolution as compared to standard LaBr3:Ce. The proportionality of the scintillation response to gamma and X-rays of Ca2+, Sr2+, and Ba2+ co-doped samples also considerably improves. The effects of the co-dopants on emission spectra, decay time, and temperature stability of the light yield were studied. Multiple thermoluminescence glow peaks, decrease of the light yield at temperatures below 295 K, and additional long scintillation decay components were observed and related to charge carrier traps appearing in LaBr3:Ce3+ with Ca2+, Sr2+, and Ba2+ co-doping.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sr2+ co-doped LaBr3:5%Ce scintillators show a record low energy resolution of 2% at 662 keV and a considerably better proportional response compared to standard LaBr3:5%Ce. This paper reports on the optical properties and time response of Sr co-doped LaBr3:5%Ce. Multiple excitation and emission bands were observed in X-ray and optically excited luminescence measurements. Those bands are ascribed to three different Ce3+ sites. The first is the unperturbed site with the same luminescence properties as those of standard LaBr3:Ce. The other two are perturbed sites with red-shifted 4f-5d1 Ce3+ excitation and emission bands, longer Ce3+ decay times, and smaller Stokes shifts. The lowering of the lowest 5d level of Ce3+ was ascribed to larger crystal field interactions at the perturbed sites. Two types of point defects in the LaBr3 matrix were proposed to explain the observed results. No Ce4+ ions were detected in Sr co-doped LaBr3:5%Ce by diffuse reflectance measurements.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The scintillation and luminescence properties of pure CsBa2I5 and CsBa2I5 doped with 0.5% Eu and 5% Eu were studied between 78 K and 600 K. Single crystals were grown by the vertical Bridgman method from the melt. CsBa2I5:5% Eu showed a light yield of 80,000 photons/MeV, an energy resolution of 2.3% for the 662 key full absorption peak, and an excellent proportional response. Two broad emission bands centered at 400 nm and 600 nm were observed in the radioluminescence spectrum of pure CsBa2I5. The Eu2+ 5d-4f emission band was observed at 430 nm. The radiative lifetime of the Eu2+ excited state was determined as 350 ns. With increasing temperature and Eu concentration the Eu2+ emission shifts to longer wavelengths and its decay time lengthens as a result of self-absorption of the Eu2+ emission. Multiple thermoluminescence glow peaks and a sharp decrease of the light yield at temperatures below 200 K were observed and related to the presence of the charge carrier traps in CsBa2I5:Eu.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A scintillation crystal can include Ln(1-y)REyX3, wherein Ln represents a rare earth element, RE represents a different rare earth element, y has a value at 0-1, and X represents a halogen. In an embodiment, the scintillation crystal is doped with a Group 1 element, a Group 2 element, or a mixt. thereof, and the scintillation crystal is formed from a melt having a concn. of such elements or mixt. thereof of at least ∼0.02%. In another embodiment, the scintillation crystal can have unexpectedly improved proportionality and unexpectedly improved energy resoln. properties. In a further embodiment, a radiation detection app. can include the scintillation crystal, a photosensor, and an electronics device. Such a radiation detection app. can be useful in a variety of applications.