Resumo:
A new approach to generating clean energy has been studied by several researchers, among which one can highlight the steam reforming of biogas. The Biogas is result of decomposition of organic matter and it hasn’t been availed in the global level, instead, the biogas has been burned in flare or discarded into the atmosphere providing damage to the environment. The generation of vector biogas energy can be realized through its steam reforming and this work examines briefly the types of digesters used for biogas generation, studying the process of steam reforming to generate hydrogen as energy vector, analyzing each step in detail, seeking to adapt its main features an ethanol reformer for a biogas reformer. Besides this it is estimated the yield of the reform process and the boiler efficiency for efficiency of the process
Resumo:
The purpose of this work is to study the incorporation of hydrogen production (Case A) and the process of gasification of sugarcane bagasse associated with combined cycle gas turbine and steam turbine (Case B) for Distillery Pioneers process. These technologies can be used to improve the energy supply in the sugarcane mill. Initially the processes for obtaining sugar and ethanol from sugarcane is discussed, with a theoretical introduction to hydrogen, the process of steam reforming and gasification of biomass (bagasse) by inserting a turbine associated with the recovery boiler gas. Subsequently makes up the energy and exergy analysis of the incorporation of the above technologies. In end stage makes it an ecological analysis considering or not the carbon cycle (photosynthesis), to determine the levels of emissions of pollutants, carbon dioxide equivalent, indicators of pollution and ecological efficiencies associated with technological developments proposed. It is concluded that hydrogen production by steam reforming of ethanol and gasification of bagasse are viable alternatives from the point of view of technical and environmental applications in the biofuels industry, contributing to the development of the sector in the country
Resumo:
This work studies the incorporation of new technologies in the sugarcane sector. Are considered the ethanol steam reforming and the gasification of sugarcane bagasse(by-product) processes associated with combined cycle systems (Gas Turbine + Steam Turbine), aggregating hydrogen production and increased electricity supply in the sector, respectively. To verify the technical feasibility of the incorporation processes was performed a thermodynamic analysis, considering data from a typical Brazilian Sugar Cane Industry. In another step the economic viability study of the hydrogen production process was made, with consideration on hydrated and anhydrous ethanol steam reform, comparing the cost of hydrogen production. Also considered studies of economic engineering of the gasification process and the generation of electricity associated. As conclusions, it follows that the ethanol steam reforming is a great alternative for hydrogen production, presenting production cost relatively low, especially when is considered the steam reforming of hydrated ethanol. For the gasification process associated with combined cycle, can be observed an increase of 8.56 times of the electricity production in the sugar cane industry, indicating a positive annual saving when the sales price of the supply electricity is greater than 0.070 US$/kWh. Finally it can be concluded that the incorporation of these new processes allow greater profitability and operational flexibility of Brazilian sugarcane mills
Resumo:
Pós-graduação em Química - IQ
Resumo:
Nowadays, there is a great interest in the economic success of direct ethanol fuel cells; however, our atomistic understanding of the designing of stable and low-cost catalysts for the steam reforming of ethanol is still far from satisfactory, in particular due to the large number of undesirable intermediates. In this study, we will report a first-principles investigation of the adsorption properties of ethanol and water at low coverage on close-packed transition-metal (TM) surfaces, namely, Fe(110), Co(0001), Ni(111), Cu(111), Ru(0001), Rh(111), Pd(111), Ag(111), Os(0001), Ir(111), Pt(111), and Au(111), employing density functional theory (DFT) calculations. We employed the generalized gradient approximation with the formulation proposed by Perdew, Burke, and Erzenholf (PBE) to the exchange correlation functional and the empirical correction proposed by S. Grimme (DFT+D3) for the van der Waals correction. We found that both adsorbates binds preferentially near or on the on top sites of the TM surfaces through the 0 atoms. The PBE adsorption energies of ethanol and water decreases almost linearly with the increased occupation of the 4d and 5d d-band, while there is a deviation for the 3d systems. The van der Waals correction affects the linear behavior and increases the adsorption energy for both adsorbates, which is expected as the van der Waals energy due to the correlation effects is strongly underestimated by DFT-PBE for weak interacting systems. The geometric parameters for water/TM are not affected by the van der Waals correction, i.e., both DFT and DFT+D3 yield an almost parallel orientation for water on the TM surfaces; however, DFT+D3 changes drastically the ethanol orientation. For example, DFT yields an almost perpendicular orientation of the C-C bond to the TM surface, while the C-C bond is almost parallel to the surface using DFT +D3 for all systems, except for ethanol/Fe(110). Thus, the van der Waals correction decreases the distance of the C atoms to the TM surfaces, which might contribute to break the C-C bond. The work function decreases upon the adsorption of ethanol and water, and both follow the same trends, however, with different magnitude (larger for ethanol/TM) due to the weak binding of water to the surface. The electron density increases mainly in the region between the topmost layer and the adsorbates, which explains the reduction of the substrate work function.
Resumo:
The catalytic performance of Ni/ZrO2 catalysts loaded with different lanthanum content for steam reforming of ethanol was investigated. Catalysts were characterized by BET surface area, X-ray diffraction, UV-vis spectroscopy, temperature programmed reduction, and X-ray absorption fine structure techniques. Results showed that lanthanum addition led to an increase in the degree of reduction of both NiO and nickel surface species interacting with the support, due to the higher dispersion effect. The best catalytic performance at 450 ºC was found for the Ni/12LZ catalyst, which exhibited an effluent gaseous mixture with the highest H2 yield.
Resumo:
The research of new catalysts for the hydrogen production described in this thesis was inserted within a collaboration of Department of Industrial Chemistry and Materials of University of Bologna and Air Liquide (Centre de Recherche Claude-Delorme, Paris). The aim of the work was focused on the study of new materials, active and stable in the hydrogen production from methane, using either a new process, the catalytic partial oxidation (CPO), or a enhanced well-established process, the steam methane reforming (SMR). Two types of catalytic materials were examined: 1) Bulk catalysts, i.e. non-supported materials, in which the active metals (Ni and/or Rh) are stabilized inside oxidic matrix, obtained from perovskite type compounds (PVK) and from hydrotalcite type precursors (HT); 2) Structured catalysts, i.e. catalysts supported on materials having high thermal conductivity (SiC and metallic foams). As regards the catalytic partial oxidation, the effect of the metal (Ni and/or Rh), the role of the metal/matrix ratio and the matrix formulation of innovative catalysts obtained from hydrotalcite type precursors and from perovskites were examined. In addition, about steam reforming process, the study was carried out first on commercial type catalysts, examining the deactivation in industrial conditions, the role of the operating conditions and the activity of different type of catalysts. Then, innovative materials bulk (PVK and HT) and structured catalysts (SiC and metallic foam) were studied and a new preparation method was developed.
Resumo:
The work of this thesis has been focused on the characterization of metallic membranes for the hydrogen purification from steam reforming process and also of perfluorosulphonic acid ionomeric (PFSI) membranes suitable as electrolytes in fuel cell applications. The experimental study of metallic membranes was divided in three sections: synthesis of palladium and silver palladium coatings on porous ceramic support via electroless deposition (ELD), solubility and diffusivity analysis of hydrogen in palladium based alloys (temperature range between 200 and 400 °C up to 12 bar of pressure) and permeation experiments of pure hydrogen and mixtures containing, besides hydrogen, also nitrogen and methane at high temperatures (up to 600 °C) and pressures (up to 10 bar). Sequential deposition of palladium and silver on to porous alumina tubes by ELD technique was carried out using two different procedures: a stirred batch and a continuous flux method. Pure palladium as well as Pd-Ag membranes were produced: the Pd-Ag membranes’ composition is calculated to be close to 77% Pd and 23% Ag by weight which was the target value that correspond to the best performance of the palladium-based alloys. One of the membranes produced showed an infinite selectivity through hydrogen and relatively high permeability value and is suitable for the potential use as a hydrogen separator. The hydrogen sorption in silver palladium alloys was carried out in a gravimetric system on films produced by ELD technique. In the temperature range inspected, up to 400°C, there is still a lack in literature. The experimental data were analyzed with rigorous equations allowing to calculate the enthalpy and entropy values of the Sieverts’ constant; the results were in very good agreement with the extrapolation made with literature data obtained a lower temperature (up to 150 °C). The information obtained in this study would be directly usable in the modeling of hydrogen permeation in Pd-based systems. Pure and mixed gas permeation tests were performed on Pd-based hydrogen selective membranes at operative conditions close to steam-reforming ones. Two membranes (one produced in this work and another produced by NGK Insulators Japan) showed a virtually infinite selectivity and good permeability. Mixture data revealed the existence of non negligible resistances to hydrogen transport in the gas phase. Even if the decrease of the driving force due to polarization concentration phenomena occurs, in principle, in all membrane-based separation systems endowed with high perm-selectivity, an extensive experimental analysis lack, at the moment, in the palladium-based membrane process in literature. Moreover a new procedure has been introduced for the proper comparison of the mass transport resistance in the gas phase and in the membrane. Another object of study was the water vapor sorption and permeation in PFSI membranes with short and long side chains was also studied; moreover the permeation of gases (i.e. He, N2 and O2) in dry and humid conditions was considered. The water vapor sorption showed strong interactions between the hydrophilic groups and the water as revealed from the hysteresis in the sorption-desorption isotherms and thermo gravimetric analysis. The data obtained were used in the modeling of water vapor permeation, that was described as diffusion-reaction of water molecules, and in the humid gases permeation experiments. In the dry gas experiments the permeability and diffusivity was found to increase with temperature and with the equivalent weight (EW) of the membrane. A linear correlation was drawn between the dry gas permeability and the opposite of the equivalent weight of PFSI membranes, based on which the permeability of pure PTFE is retrieved in the limit of high EW. In the other hand O2 ,N2 and He permeability values was found to increase significantly, and in a similar fashion, with water activity. A model that considers the PFSI membrane as a composite matrix with a hydrophilic and a hydrophobic phase was considered allowing to estimate the variation of gas permeability with relative humidity on the basis of the permeability in the dry PFSI membrane and in pure liquid water.
Resumo:
H2 demand is continuously increasing since its many relevant applications, for example, in the ammonia production, refinery processes or fuel cells. The Water Gas Shift (WGS) reaction (CO + H2O = CO2 + H2 DeltaH = -41.1 kJ.mol-1) is a step in the H2 production, reducing significantly the CO content and increasing the H2 one in the gas mixtures obtained from steam reforming. Industrially, the reaction is carried out in two stages with different temperature: the first stage operates at high temperature (350-450 °C) using Fe-based catalysts, while the second one is performed at lower temperature (190-250 °C) over Cu-based catalysts. However, recently, an increasing interest emerges to develop new catalytic formulations, operating in a single-stage at middle temperature (MTS), while maintaining optimum characteristics of activity and stability. These formulations may be obtained by improving activity and selectivity of Fe-based catalysts or increasing thermal stability of Cu-based catalysts. In the present work, Cu-based catalysts (Cu/ZnO/Al2O3) prepared starting from hydrotalcite-type precursors show good homogeneity and very interesting physical properties, which worsen by increasing the Cu content. Among the catalysts with different Cu contents, the catalyst with 20 wt.% of Cu represents the best compromise to obtain high catalytic activity and stability. On these bases, the catalytic performances seem to depend on both metallic Cu surface area and synergetic interactions between Cu and ZnO. The increase of the Al content enhances the homogeneity of the precursors, leading to a higher Cu dispersion and consequent better catalytic performances. The catalyst with 20 wt.% of Cu and a molar ratio M(II)/M(III) of 2 shows a high activity also at 250 °C and a good stability at middle temperature. Thus, it may be considered an optimum catalyst for the WGS reaction at middle temperature (about 300 °C). Finally, by replacing 50 % (as at. ratio) of Zn by Mg (which is not active in the WGS reaction), better physical properties were observed, although associate with poor catalytic performances. This result confirms the important role of ZnO on the catalytic performances, favoring synergetic interactions with metallic Cu.
Resumo:
The research of new advanced processes for syngas production is a part of a European project for the production of a new Gas to Liquid Process (NextGTL). The crucial points in the production of GTL process are the energy required for the air separation used in autothermal reforming or the heat required for steam reforming and the efficiency in carbon utilization. Therefore a new multistep oxy-reforming process scheme was developed at lower temperature with intermediate H2 membrane separation to improve the crucial parameter. The process is characterized by a S/C of 0.7 and O2/C of 0.21 having a smoothed temperature profile in which kinetic regime is easily obtained. Active catalysts for low temperature oxy-reforming process have been studied working at low pressure to discriminate among the catalyst and at high pressure to prove it on industrial condition. It allows the selection of the Rh as active phase among single and bimetallic VIII group metal. The study of the matrix composition and thermal treatment has been carried out on Rh-Mg/Al hydrotalcite selected as reference catalyst. The research to optimize the catalyst lead to enhanced performances through the identification of a limitation of the Rh reduction from the oxides matrix as key point to increase the Rh performances. The Rh loading have been studied to allow the catalyst scale up for pilot process in Chieti in a shape of Rh-HT on honeycomb ceramic material. The developed catalyst has enhanced methane conversion in a inch diameter monolith reactor if compared with the semi-industrial catalyst chosen in the project as the best reference.
Resumo:
The present study is focused on the development of new VIII group metal on CeO2 – ZrO2 (CZO) catalyst to be used in reforming reaction for syngas production. The catalyst are tested in the oxyreforming process, extensively studied by Barbera [44] in a new multistep process configuration, with intermediate H2 membrane separation, that can be carried out at lower temperature (750°C) with respect the reforming processes (900 – 1000°C). In spite of the milder temperatures, the oxy-reforming conditions (S/C = 0.7; O2/C = 0.21) remain critical regarding the deactivation problems mainly deriving from thermal sintering and carbon formation phenomena. The combination of the high thermal stability characterizing the ZrO2, with the CeO2 redox properties, allows the formation of stable mixed oxide system with high oxygen mobility. This feature can be exploited in order to contrast the carbon deposition on the active metal surface through the oxidation of the carbon by means of the mobile oxygen atoms available at the surface of the CZO support. Ce0.5Zr0.5O2 is the phase claimed to have the highest oxygen mobility but its formation is difficult through classical synthesis (co-precipitation), hence a water-in-oil microemulsion method is, widely studied and characterized. Two methods (IWI and bulk) for the insertion of the active metal (Rh, Ru, Ni) are followed and their effects, mainly related to the metal stability and dispersion on the support, are discussed, correlating the characterization with the catalytic activity. Different parameters (calcination and reduction temperatures) are tuned to obtain the best catalytic system both in terms of activity and stability. Interesting results are obtained with impregnated and bulk catalysts, the latter representing a new class of catalysts. The best catalysts are also tested in a low temperature (350 – 500°C) steam reforming process and preliminary tests with H2 membrane separation have been also carried out.
Resumo:
L’accoppiamento di diverse operazioni unitarie può in certi casi portare ad una cosiddetta “intensificazione di processo”, cioè ad un aumento sostanziale delle rese, dell’efficienza e della sostenibilità. Nel presente lavoro sono state pertanto analizzate le potenzialità di accoppiamento della fotocatalisi, il più studiato tra i “processi di ossidazione avanzata”, sia con alcuni processi a membrana per la sintesi verde di aromi sia con l’ozonizzazione per la depurazione di acque. È stato dimostrato che in entrambi i casi l’ottenimento di una significativa intensificazione di processo dipende in gran parte dai parametri operativi, in particolare dal rapporto, delta, tra la velocità caratteristica di fotocatalisi e quella del processo accoppiato. Nel caso della sintesi di aromi, in cui la fotocatalisi viene accoppiata con la pervaporazione o con la dialisi ricircolando al reattore il retentato dalla cella con la membrana. Il parametro delta dipende dalla velocità di reazione, dalle proprietà di trasporto delle membrane e naturalmente dal volume del rettore e dall’area della membrana. La reazione fotocatalitica produce l’aroma, ad esempio vanillina da acido ferulico, per ossidazione parziale e grazie al recupero del prodotto se ne evita l’ulteriore ossidazione aumentandone pertanto la resa. L’operare in apparati separati offre diversi vantaggi come la possibilità di variare senza vincoli il rapporto tra area della membrana e volume del reattore, ma impone di considerare anche il grado effettivo di accoppiamento dei processi. In questo caso, come evidenziato dal modello matematico, un sufficientemente elevato rapporto di ricircolo consente comunque di integrare efficacemente i processi. Nell’ozonizzazione fotocatalitica si hanno due importanti vantaggi: l’aumento della velocità di degradazione grazie alla sinergia tra i processi e la capacità di controllare la formazione di prodotti pericolosi. La sinergia viene massimizzata ad un valore ottimale di delta, mentre la formazione dei prodotti indesiderati viene controllata operando secondo le procedure che sono state individuate.
Resumo:
A produção de energia é um dos grandes desafios deste século, principalmente com a necessidade no desenvolvimento de processos que utilizem preferencialmente fontes renováveis. Nesse contexto, é claro o interesse por pesquisas baseada no hidrogênio. Porém, os ganhos ambientais efetivos estão associados também à matéria-prima usada no processo de geração do hidrogênio, senso assim mais significativo quando do uso de fontes renováveis. No presente trabalho foi estudado o efeito da adição de diferentes teores de CeO2 em catalisadores de NiZnO, preparados pelo método da co-precipitação. Os catalisadores foram estudados frente à reação de reforma a vapor do etanol (RVE) para produção de H2, e no decorrer do trabalho foi pertinente incluir o estudo da reforma a vapor da acetona (RVA), como complemento dos estudos da RVE. Além disso, esta é uma molécula modelo para reforma a vapor do bio-óleo. Nos sistemas catalíticos sintetizados houve a formação da liga NiZn3, o que aparenta proporcionar um efeito sinérgico entre esses elementos. Observou-se um efeito altamente promotor do CeO2 com relação a diminuição do coque formado, devido a uma menor da formação da acetona, durante as etapas de reforma do etanol. O que consequentemente interferiu na produção de H2. O catalisador contendo 20% de CeO2 denominado NiZn20Ce apresentou um desempenho altamente promissor, pois de acordo com as análises de DRIFT, a presença do CeO2 levou a formação de espécies de formiato, o que consequentemente interferiu em uma menor formação de coque e maior produção de H2. Foi comprovado também que a natureza dos depósitos carbonáceos depende tanto do substrato utilizado quanto das etapas precursoras inicias que levarão a formação desse coque, sendo o ponto chave para um melhor desempenho do catalisador.
Resumo:
Catalisadores de Ni (10% em massa) suportado em matrizes mistas MgO-SiO2 foram aplicados na reação de reforma a vapor de glicerol. Os efeitos do teor de MgO como aditivo e do método de preparação foram avaliados frente às propriedades físico-químicas e texturais dos materiais; assim como à atividade, seletividade, estabilidade e formação de carbono na reforma a vapor do glicerol. Os catalisadores foram preparados com diferentes teores mássicos de MgO (10%, 30% e 50%) sobre SiO2 comercial, utilizando processo via seca (mistura física) e via úmida (impregnação sequencial com diferentes solventes: água, etanol e acetona). Foram utilizadas as técnicas de caracterização de espectroscopia de energia dispersiva de raios X, fisissorção de nitrogênio, difratometria de raios X, termogravimetria, difratometria de raios X in situ com O2, redução a temperatura programada com H2, difratometria de raios X in situ com H2, dessorção a temperatura programada com H2 e microscopia eletrônica de varredura. Foi observado que o Ni(II) interage de forma variada com os suportes com diferentes teores de MgO, e que a polaridade do solvente de impregnação utilizado no processo de preparação influencia as propriedades dos catalisadores. A fim de verificar a atividade, seletividade e deposição de carbono; os catalisadores foram testados na reação de reforma a vapor de glicerol a 600oC, por um período de 5h e razão molar água:glicerol de 12:1. Após as reações, os catalisadores foram novamente submetidos às análises de termogravimetria, difratometria de raios X e microscopia eletrônica de varredura, visando a caracterização dos depósitos de carbono obtidos durante o processo catalítico. Os catalisadores de matrizes mistas se mostraram ativos e apresentaram seletividades similares para os produtos gasosos CH4, CO e CO2, além de um alto rendimento em H2. Observou-se que a adição de MgO no suporte, aumentou a dispersão do Ni(II) no material, que por sua vez, influenciou na quantidade de carbono depositado ao longo da reação. A polaridade do solvente de impregnação também teve influência na dispersão metálica, sendo que, quanto menor a polaridade do solvente, maior foi a dispersão obtida no catalisador, e menor a deposição de carbono na reação. O material que apresentou o melhor desempenho catalítico frente ao rendimento de H2 e à deposição de carbono, foi o catalisador preparado com 30% de MgO com etanol como solvente de impregnação.