Mid-infrared (MIR) and near-infrared (NIR) spectroscopy have been used to study the molecular structure of halloysite and potassium acetate intercalated halloysite and to determine the structural changes of halloysite through intercalation. The MIR spectra show all fundamental vibrations including the hydroxyl units, basic aluminosilicate framework and water molecules in the structure of halloysite and its intercalation complex. Comparison between halloysite and halloysite-potassium acetate intercalation complex shows almost all bands observed for halloysite are also observed for halloysite-potassium acetate intercalation complex apart from bands observed in the 1700-1300 cm-1 region, but with differences in band intensity. However, NIR, based on MIR spectra, provide sufficient evidence to analyze the structural changes of halloysite through intercalation. There are obvious differences between halloysite and halloysite-potassium acetate intercalation complex in the all spectral ranges. Therefore, the reproducibility of measurement and richness of qualitative information should be simultaneously considered for proper selection of a spectroscopic method for molecular structural analysis.
Resumo:
A series of kaolinite-potassium acetate intercalation composite was prepared. The thermal behavior and decomposition of these composites were investigated by simultaneous differential scanning calorimetry-thermogravimetric analysis (DSC-TGA), X-ray diffraction (XRD) and Fourier-transformation infrared (FT-IR). The XRD pattern at room temperature indicated that intercalation of potassium acetate into kaolinite causes an increase of the basal spacing from 0.718 to 1.428nm. The peak intensity of the expanded phase of the composite decreased with heating above 300°C, and the basal spacing reduced to 1.19nm at 350°C and 0.718nm at 400°C. These were supported by DSC-TGA and FT-IR measurements, where the endothermic reactions are observed between 300 and 600°C. These reactions can be divided into two stages: 1) Removal of the intercalated molecules between 300-400°C. 2) Dehydroxylation of kaolinite between 400-600°C. Significant changes were observed in the infrared bands assigned to outer surface hydroxyl, inner surface hydroxyl, inner hydroxyl and hydrogen bands.
Resumo:
We describe a scaling method for templating digital radiographs using conventional acetate templates independent of template magnification without the need for a calibration marker. The mean magnification factor for the radiology department was determined (119.8%, range117%-123.4%). This fixed magnification factor was used to scale the radiographs by the method described. 32 femoral heads on postoperative THR radiographs were then measured and compared to the actual size. The mean absolute accuracy was within 0.5% of actual head size (range 0 to 3%) with a mean absolute difference of 0.16mm (range 0-1mm, SD 0.26mm). Intraclass Correlation Coefficient (ICC) showed excellent reliability for both inter and intraobserver measurements with ICC scores of 0.993 (95% CI 0.988-0.996) for interobserver measurements and intraobserver measurements ranging between 0.990-0.993 (95% CI 0.980-0.997).
Resumo:
Core(polyvinyl neodecanoate-ethylene glycol dimethacrylate)-shell(polyvinyl alcohol) (core (P(VND-EGDMA))-shell(PVA)) microspheres were developed by seeded polymerization with the use of conventional free radical and RAFT/MADIX mediated polymerization. Poly(vinyl pivalate) PVPi was grafted onto microspheres prepared via suspension polymerization of vinylneodecanoate and ethylene glycol dimethacrylate. The amount of grafted polymer was found to be independent from the technique used with conventional free radical polymerization and MADIX polymerization resulting into similar shell thicknesses. Both systems—grafting via free radical polymerization or the MADIX process—were found to follow slightly different kinetics. While the free radical polymerization resulted in a weight gain linear with the monomer consumption in solution the growth in the MADIX controlled system experienced a delay. The core-shell microspheres were obtained by hydrolysis of the poly(vinyl pivalate) surface grafted brushes to form poly(vinyl alcohol). During hydrolysis the microspheres lost a significant amount of weight, consistent with the hydrolysis of 40–70% of all VPi units. Drug loading was found to be independent of the shell layer thickness, suggesting that the drug loading is governed by the amount of bulk material. The shell layer does not appear to represent an obstacle to the drug ingress. Cell testing using colorectal cancer cell lines HT 29 confirm the biocompatibility of the empty microspheres whereas the clofazimine loaded particles lead to 50% cell death, confirming the release of the drug.
Resumo:
The ionic liquid (IL) 1-ethyl-3-methylimidazolium acetate ([C2mim]OAc) is considered to be an inert solvent of cellulose and lignocellulosic biomass. Acetylation (1.7 % mol, or DS 0.017) of cellulose after dissolution in [C2mim]OAc (150 °C for 20 min), is demonstrated by compositional analysis, FTIR analysis and 13C NMR spectroscopy (in [C2min]OAc with 13C enriched acetate). This acetylation, in the absence of added acylating agents, has not been reported before and may limit [C2mim]OAc utility in industrial scale biomass processing, even at this low extent. For example, cellulose acetylation may contribute to IL loss in processes where the IL is recovered and reused and inhibit enzyme saccharification of cellulose in lignocellulosic biofuel production processes based on saccharification and fermentation.
Resumo:
The thermal decomposition and dehydroxylation process of coal-bearing strata kaolinite–potassium acetate intercalation complex (CSKK) has been studied using X-ray diffraction (XRD), infrared spectroscopy (IR), thermal analysis, mass spectrometric analysis and infrared emission spectroscopy. The XRD results showed that the potassium acetate (KAc) have been successfully intercalated into coal-bearing strata kaolinite with an obvious basal distance increase of the first basal peak, and the positive correlation was found between the concentration of intercalation regent KAc and the degree of intercalation. As the temperature of the system is raised, the formation of KHCO3, KCO3 and KAlSiO4, which is derived from the thermal decomposition or phase transition of CSKK, is observed in sequence. The IR results showed that new bands appeared, the position and intensities shift can also be found when the concentration of intercalation agent is raised. The thermal analysis and mass spectrometric analysis results revealed that CSKK is stable below 300 °C, and the thermal decomposition products (H2O and CO2) were further proved by the mass spectrometric analysis. A comparison of thermal analysis results of original coal-bearing strata kaolinite and its intercalation complex gives new discovery that not only a new mass loss peak is observed at 285 °C, but also the temperature of dehydroxylation and dehydration of coal bearing strata kaolinite is decreased about 100 °C. This is explained on the basis of the interlayer space of the kaolinite increased obviously after being intercalated by KAc, which led to the interlayer hydrogen bonds weakened, enables the dehydroxylation from kaolinite surface more easily. Furthermore, the possible structural model for CSKK has been proposed, with further analysis required in order to prove the most possible structures.
Resumo:
Medroxyprogesterone acetate (MPA) has widely been used in hormone replacement therapy (HRT), and is associated with an increased risk of breast cancer, possibly due to disruption of androgen receptor (AR) signaling. In contrast, the synthetic HRT Tibolone does not increase breast density, and is rapidly metabolized to estrogenic 3α-OH-tibolone and 3β-OH-tibolone, and a delta-4 isomer (Δ4-TIB) that has both androgenic and progestagenic properties. Here, we show that 5α-dihydrotestosterone (DHT) and Δ4-TIB, but not MPA, stabilize AR protein levels, initiate specific AR intramolecular interactions critical for AR transcriptional regulation, and increase proliferation of AR positive MDA-MB-453 breast cancer cells. Structural modeling and molecular dynamic simulation indicate that Δ4-TIB induces a more stable AR structure than does DHT, and MPA a less stable one. Microarray expression analyses confirms that the molecular actions of Δ4-TIB more closely resembles DHT in breast cancer cells than either ligand does to MPA.
Resumo:
We report the Heck coupling of 2-vinyl-4,5-dicyanoimidazole (vinazene) with selected di- and trihalo aromatics in an effort to prepare linear and branched electron-accepting conjugated materials for application in organic electronics. By selecting the suitable halo-aromatic moiety, it is possible to tune the HOMO - LUMO energy levels, absorption, and emission properties for a specific application. In this regard, materials with strong photoluminescence from blue → green → red are reported that may have potential application in organic light-emitting diodes (OLEDs). Furthermore, derivatives with strong absorption in the visible spectrum, coupled with favorable HOMO-LUMO levels, have been used to prepare promising organic photovoltaic devices (OPVs) when combined with commercially available semiconducting donor polymers.
Resumo:
The thermal decomposition process of kaolinite–potassium acetate intercalation complex has been studied using simultaneous thermogravimetry coupled with Fourier-transform infrared spectroscopy and mass spectrometry (TG-FTIR-MS). The results showed that the thermal decomposition of the complex took place in four temperature ranges, namely 50–100, 260–320, 320–550, and 650–780 °C. The maximal mass losses rate for the thermal decomposition of the kaolinite–potassium acetate intercalation complex was observed at 81, 296, 378, 411, 486, and 733 °C, which was attributed to (a) loss of the adsorbed water, (b) thermal decomposition of surface-adsorbed potassium acetate (KAc), (c) the loss of the water coordinated to potassium acetate in the intercalated kaolinite, (d) the thermal decomposition of intercalated KAc in the interlayer of kaolinite and the removal of inner surface hydroxyls, (e) the loss of the inner hydroxyls, and (f) the thermal decomposition of carbonate derived from the decomposition of KAc. The thermal decomposition of intercalated potassium acetate started in the range 320–550 °C accompanied by the release of water, acetone, carbon dioxide, and acetic acid. The identification of pyrolysis fragment ions provided insight into the thermal decomposition mechanism. The results showed that the main decomposition fragment ions of the kaolinite–KAc intercalation complex were water, acetone, carbon dioxide, and acetic acid. TG-FTIR-MS was demonstrated to be a powerful tool for the investigation of kaolinite intercalation complexes. It delivers a detailed insight into the thermal decomposition processes of the kaolinite intercalation complexes characterized by mass loss and the evolved gases.
Resumo:
In the structure of the title magnesium complex with the phenoxy herbicide (2,4-dichlorophenoxy)acetic acid (2,4-D), [Mg(H2O)5(C8H5Cl2O3)]+ C8H5Cl2O3)- . 0.5H2O, the discrete cationic MgO6 complex units comprise a carboxyl O-donor from a monodentate 2,4-D cationic ligand and five water molecules in a slightly distorted octahedral coordination. The 2,4-D anions are linked to the complex units through duplex water O-H...O(carboxyl) hydrogen bonds through the coordinated water molecules. In the crystal inter-unit O-H...O hydrogen-bonding interactions involving coordinated water molecules as well as the hemi-hydrate solvate molecule with carboxyl O-atom acceptors, give a two-dimensional layered structure lying parallel (001), in which pi-pi ligand-cation interactions [minimum ring centroid separation, 3.6405(17)A] and a short O-H...Cl interaction [3.345(2)A] are also found.
Resumo:
The kaolinite (Kaol) intercalated with potassium acetate (Ac) was prepared and characterized by X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), and thermogravimetry. Molecular dynamic simulation was performed to investigate the structure of Kaol–Ac intercalation complex and the hydrogen bonds between Kaol and intercalated Ac andwater using INTERFACE forcefield. The acetate anions andwater arranged in a bilayer structure in the interlayer space of Kaol. The potassium cations distributed in the interlayer space and strongly coordinated with acetate anions aswell aswater rather than keyed into the ditrigonal holes of tetrahedral surface of Kaol. Strong hydrogen bonds formed between the hydrogen atoms of hydroxyl on the octahedral surface and oxygen atoms of both acetate anions and water. The acetate anions andwater also weakly bonded hydrogen to the silica tetrahedral surface through their hydrogen atoms with the oxygen atoms of silica tetrahedral surface.
Resumo:
In the structure of the title hydrated salt, NH4+·C8H5Cl2O3-·0.5H2O, where the anion derives from (3,5-dichlorophenoxy)acetic acid, the ammonium cation is involved in extensive N-H...O hydrogen bonding with both carboxylate and ether O-atom acceptors giving sheet structures lying parallel to (100). The water molecule of solvation lies on a crystallographic twofold rotation axis and is involved in intra-sheet O-H...Ocarboxylate hydrogen-bonding interactions. In the anion, the oxoacetate side chain assumes an antiperiplanar conformation with the defining C-O-C-C torsion angle = -171.33 (15)°.
Resumo:
This is the first report on studies carried out in detail on high-pressure oxygen copolymerization (> 50 psi) of the vinyl monomers styrene and alpha-methylstyrene (AMS). The saturation pressure of oxygen for AMS oxidation, hitherto obscure, is found to be 300 psi. Whereas the ease of oxidation is more favorable for styrene, the rate and yield of polyperoxide formation are higher for AMS. This is explained on the basis of the reactivity of the corresponding alkyl and peroxy radicals. Below 50 degrees C, degradation of the poly(styrene peroxide) formed is about 2.5 times less than that observed above 50 degrees C, so much so that it gives a break in the rate curve, and thereafter the rate is lowered. Normal free radical kinetics is followed before the break point, after which the monomer and initiator exponents become unusually high. This is interpreted on the basis of chain transfer to the degradation products. The low molecular weight of polyperoxides has been attributed to the (i) low reactivity of RO(2)(.) toward the monomer, (ii) chain transfer to degradation products, (iii) facile cleavage of O-O bond, followed by unzipping to nonradical products, and (iv) higher stability of the reinitiating radicals. At lower temperatures, (i) predominates, whereas at higher temperatures, chiefly (ii)-(iv) are the case.