A plasma-assisted concurrent Rf sputtering technique for fabrication of biocompatible, functionally graded CaP-based interlayer on Ti-6Al-4V orthopedic alloy is reported. Each layer in the coating is designed to meet a specific functionality. The adherent to the metal layer features elevated content of Ti and supports excellent ceramic-metal interfacial stability. The middle layer features nanocrystalline structure and mimics natural bone apatites. The technique allows one to reproduce Ca/P ratios intrinsic to major natural calcium phosphates. Surface morphology of the outer, a few to few tens of nanometers thick, layer, has been tailored to fit the requirements for the bio-molecule/protein attachment factors. Various material and surface characterization techniques confirm that the optimal surface morphology of the outer layer is achieved for the process conditions yielding nanocrystalline structure of the middle layer. Preliminary cell culturing tests confirm the link between the tailored nano-scale surface morphology, parameters of the middle nanostructured layer, and overall biocompatibility of the coating.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Glutathione transferases are known to be important enzymes in the metabolism of xenobiotics. In humans genetic polymorphisms have been reported for the hGSTM1 and hGSTT1 genes leading to individual differences in susceptibility towards toxic effects, such as cancer. This study describes the distribution of the two polymorphisms of hGSTT1 and hGSTM1 in the normal Chinese population of Shanghai. Out of 219 healthy individuals having been genotyped for GSTTI and GSTMI, 108 (49%) were identified to be homozygously deficient for the GSTT1 gene and 107 (49%) for the GSTM1 gene.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have studied the mineral normandite using a combination of scanning electron microscopy with energy dispersive spectroscopy and vibrational spectroscopy. The mineral normandite NaCa(Mn2+,Fe2+)(Ti,Nb,Zr)Si2O7(O,F)2 is a crystalline sodium calcium silicate which contains rare earth elements. Chemical analysis shows the mineral contains a range of elements including Na, Mn2+, Ca, Fe2+ and the rare earth element niobium. No Raman bands are observed above 1100 cm−1. The mineral is characterised by Raman bands observed at 724, 748, 782 and 813 cm−1. Infrared bands are broad; nevertheless bands may be resolved at 723, 860, 910, 958, 933, 1057 and 1073 cm−1. Intense Raman bands at 454, 477 and 513 cm−1 are attributed to OSiO bending modes. No Raman bands are observed in the hydroxyl stretching region, but low intensity infrared bands are observed at 3191 and 3450 cm−1. This observation brings into question the true formula of the mineral.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The precipitation processes in dilute nitrogen alloys of titanium have been examined in detail by conventional transmission electron microscopy (CTEM) and high-resolution electron microscopy (HREM). The alloy Ti-2 at. pct N on quenching from its high-temperature beta phase field has been found to undergo early stages of decomposition. The supersaturated solid solution (alpha''-hcp) on decomposition gives rise to an intimately mixed, irresolvable product microstructure. The associated strong tweed contrast presents difficulties in understanding the characteristic features of the process. Therefore, HREM has been carried out with a view to getting a clear picture of the decomposition process. Studies on the quenched samples of the alloy suggest the formation of solute-rich zones of a few atom layers thick, randomly distributed throughout the matrix. On aging, these zones grow to a size beyond which the precipitate/matrix interfaces appear to become incoherent and the alpha' (tetragonal) product phase is seen distinctly. The structural details, the crystallography of the precipitation process, and the sequence of precipitation reaction in the system are illustrated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Power dissipation maps have been generated in the temperature range of 900 degrees C to 1150 degrees C and strain rate range of 10(-3) to 10 s(-1) for a cast aluminide alloy Ti-24Al-20Nb using dynamic material model. The results define two distinct regimes of temperature and strain rate in which efficiency of power dissipation is maximum. The first region, centered around 975 degrees C/0.1 s(-1), is shown to correspond to dynamic recrystallization of the alpha(2) phase and the second, centered around 1150 degrees C/0.001 s(-1), corresponds to dynamic recovery and superplastic deformation of the beta phase. Thermal activation analysis using the power law creep equation yielded apparent activation energies of 854 and 627 kJ/mol for the first and second regimes, respectively. Reanalyzing the data by alternate methods yielded activation energies in the range of 170 to 220 kJ/mol and 220 to 270 kJ/mol for the first and second regimes, respectively. Cross slip was shown to constitute the activation barrier in both cases. Two distinct regimes of processing instability-one at high strain rates and the other at the low strain rates in the lower temperature regions-have been identified, within which shear bands are formed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Four Cu bearing alloys of nominal composition Zr25Ti25Cu50, Zr34Ti16Cu50, Zr25Hf25Cu50 and Ti25Hf25Cu50 have been rapidly solidified in order to produce ribbons. All the alloys become amorphous after meltspinning. In the Zr34Ti16Cu50 alloy localized precipitation of cF24 Cu5Zr phase can be observed in the amorphous matrix. The alloys show a tendency of phase separation at the initial stages of crystallization. The difference in crystallization behavior of these alloys with Ni bearing ternary alloys can be explained by atomic size, binary heat of mixing and Mendeleev number. It has been observed that both Laves and Anti-Laves phase forming compositions are suitable for glass formation. The structures of the phases, precipitated during rapid solidification and crystallization can be viewed in terms of Bernal deltahedra and Frank-Kasper polyhedra.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Texture evolution in a low cost beta titanium alloy was studied for different modes of rolling and heat treatments. The alloy was cold rolled by unidirectional and multi-step cross rolling. The cold rolled material was either aged directly or recrystallized and then aged. The evolution of texture in alpha and beta phases were studied. The rolling texture of beta phase that is characterized by the gamma fiber is stronger for MSCR than UDR; while the trend is reversed on recrystallization. The mode of rolling affects alpha transformation texture on aging with smaller alpha lath size and stronger alpha texture in UDR than in MSCR. The defect structure in beta phase influences the evolution of a texture on aging. A stronger defect structure in beta phase leads to variant selection with the rolled samples showing fewer variants than the recrystallized samples.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Small additions of B to Titanium alloys refine the as-cast microstructure significantly and hence improve their mechanical performance. In this work, tensile, fracture and fatigue properties of the as-cast and HIPed Ti-6Al-4V alloy with hypoeutectic wt.% of B additions have been examined, with particular emphasis on identifying the microstructural length scale that controls the mechanical properties of these alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The intensity of the EPR signal with g = 5.985 arising from a ferric ion â oxygen vacancy defect pair (Fe3+ â VO) in PbTiO3, varies with the extent of PbO nonstoichiometry at constant Fe3+ content due to an increased oxygen vacancy concentration. In PZT solid solutions, the signal intensity decreases with an increase in Zr. A lower intensity is also noticed for Fe3+ â VO signals in PbZrO3. This behaviour is explained on the basis of PbO nonstoichiometry arising from independent Pb- and O-vacancies as well as the randomly distributed crystallographic shear (CS) plane defects. The contribution to PbO nonstoichiometry from CS planes is larger in high zirconium compositions of PZT.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new method of modeling material behavior which accounts for the dynamic metallurgical processes occurring during hot deformation is presented. The approach in this method is to consider the workpiece as a dissipator of power in the total processing system and to evaluate the dissipated power co-contentJ = ∫o σ ε ⋅dσ from the constitutive equation relating the strain rate (ε) to the flow stress (σ). The optimum processing conditions of temperature and strain rate are those corresponding to the maximum or peak inJ. It is shown thatJ is related to the strain-rate sensitivity (m) of the material and reaches a maximum value(J max) whenm = 1. The efficiency of the power dissipation(J/J max) through metallurgical processes is shown to be an index of the dynamic behavior of the material and is useful in obtaining a unique combination of temperature and strain rate for processing and also in delineating the regions of internal fracture. In this method of modeling, noa priori knowledge or evaluation of the atomistic mechanisms is required, and the method is effective even when more than one dissipation process occurs, which is particularly advantageous in the hot processing of commercial alloys having complex microstructures. This method has been applied to modeling of the behavior of Ti-6242 during hot forging. The behavior of α+ β andβ preform microstructures has been exam-ined, and the results show that the optimum condition for hot forging of these preforms is obtained at 927 °C (1200 K) and a strain rate of 1CT•3 s•1. Variations in the efficiency of dissipation with temperature and strain rate are correlated with the dynamic microstructural changes occurring in the material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Evolution of crystallographic texture in the orthorhombic phase of a two-phase alloy Ti–22Al–25Nb (at%), consisting of orthorhombic (O) and bcc (β/B2) phases, was studied. The material was subjected to deformation in two-phase field as well as in the single β phase field. The resulting evolution of microstructure and crystallographic texture were recorded using scanning electron microscopy and X-ray diffraction. The orthorhombic phase underwent change in morphology (from platelets to equiaxed) on rolling in the two-phase field with the texture getting sharper with the amount of deformation. Rolling above β transus temperature led to hot deformation of single β phase microstructure and its subsequent cooling produced transformed coarse platelets of orthorhombic phase with texture in orientation relation with the high temperature deformed β phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pro gradu -tutkielmani käsittelee levytettyä lastenmusiikkia Suomessa, lastenmusiikintekijöitä ja lastenmusiikin asemaa levy-yhtiöissä. Lastenmusiikin kentällä on viime vuosina ilmennyt uusi aalto, joka on lisännyt kiinnostusta lastenmusiikin laatuun. Työssäni tarkoitan lastenmusiikilla nimenomaan levytettyä kaupallista lastenmusiikkia, joka on tuotettu varta vasten lapsille. Lastenmusiikkikulttuuri ei asetu jäännöksettömästi mihinkään musiikinkategoriaan. Lastenmusiikki voi sisältää elementtejä yhtä hyvin populaari-, kansan-, maailman- ja taidemusiikista. Lastenmusiikkiäänitteitä on julkaistu lähes tulkoon läpi koko suomalaisen äänilevyteollisuuden historian. Pro graduni yhtenä tarkoituksena on selventää, miten eri toimijat lastenmusiikin kentällä ovat sijoittuneet ja mikä rooli lastenmusiikilla on osana isompaa kokonaisuutta, suomalaista levyteollisuutta. Suomessa lastenkulttuurin asemaa, sisältöjä ja tekijöitä on tutkittu erittäin vähän. Lastenmusiikin historiaa ei myöskään ole tutkittu laajasti, ja lastenmusiikin kentän nykytilan tutkimus on ollut vähäistä. Pro graduni esimerkkiyhtyeet ovat pitkänlinjan lastenmusiikkiyhtyeitä ja kasvatustieteen ammattilaisia. Musiikkikasvatuksella on iso rooli suuressa osassa kotimaista lastenmusiikkia. Lapsille suunnattujen musiikkituotteiden määrä on kasvanut viime vuosina, ja lastenmusiikin kentälle tulee jatkuvasti uusia tekijöitä. Lastenkulttuurin tuotteistaminen on tänä päivänä tehokasta. Työssäni pyrin löytämään syitä siihen, miksi lastenmusiikki ei kuitenkaan aina löydä kuulijoitaan. On oleellista tietää, minkä kanssa lastenmusiikkiprojektit kilpailevat esimerkiksi rahoituksesta ja mediahuomiosta. Pro graduni tarkoitus on vastata lastenmusiikin tutkimustarpeeseen ja esitellä lastenmusiikin nykykentän toimijoita ja lastenmusiikin monimuotoisuutta. Päähuomioni kiinnittyy lastenmusiikin asemaan sekä mahdollisuuksiin, joiden avulla lastenmusiikin asemaa voitaisiin kohentaa.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A microstructural and X-ray investigation of Ti-AI-Mo alloys Ti-31 Al-15 Mo, Ti-31 Al-13 Mo, Ti-31Al-9Mo and Ti-35Al-9Mo (containing the Ti3Al, TiAl and β phases) indicates that the existing phase diagram of the ternary system for this composition range published by Ge Dhzhi-Min and Pylaeva is in error above 1473 K. An analysis of phase relations reveals that the error has arisen from their use of the Ti-AI diagram due to Bumps, Kessler and Hansen as a basis for generating the ternary. It is shown that a phase diagram of the ternary, consistent with the experimental results, can be generated using a version of the Ti-AI system due to Margolin. Simple geometric arguments are used to build up a new semi-quantitative description of the Ti-AI-Mo system which can be used as a basis for a detailed investigation of phase equilibria in this system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fine powders consisting of aggregated submicron crystallites of Ba(Ti,Zr)O3 in the complete range of Ti/Zr ratios are prepared at 85–130°C by hydrothermal method, starting from TiO2 + ZrO2 · xH2O mixed gel and Ba(OH)2 solution. The products obtained below 110°C incorporate considerable amounts of H2O and OH− within the lattice. As-prepared BaTiO3 is cubic and converts to tetragonal phase after the heat treatment at 1200°C, accompanied by the loss of residual hydroxyl ions. TEM investgations of the growth features show a transformation of the gel to the crystallite. Ba2+ ions entering the gel produce chemical changes within the gel, followed by dehydration, resulting in a cubic perovskite phase irrespective of Ti/Zr. The sintering properties of these powders to fine-grained, high density ceramics and their dielectric properties are presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fine powders of submicron-sized crystallites of BaTiO3 were prepared at 85–130°C by the hydrothermal method, starting from TiO2.ξH2O gel and Ba(OH)2 solution. The products obtained below 110°C incorporated considerable amounts of H2O and OH− in the lattice. As-prepared BaTiO3 is cubic and converts to the tetragonal phase after heat treatment at 1200°C, accompanied by the loss of residual OH− ions. Hydrothermal reaction of SnO2.ξH2O gel with Ba(OH)2 at 150–260°C gives rise to the hydrated phase, BaSn(OH)6.3H2O, due to the amphoteric nature of SnO2.ξH2O which stabilises Sn(OH)62− anions in basic media. On heating in air or releasing the pressure in situ at 260°C, BaSn(OH)6.3H2O converts to BaSnO3 through an intermediate, BaSnO(OH)4. Solid solutions of Ba(Ti,Sn)O3 are directly formed from (TiO2 + SnO2)..ξH2O gel up to 35 mol% SnO2. At higher Sn contents, the hydrothermal products are mixtures of BaSn(OH)6.3H2O and BaTiO3, which on annealing at 1000°C result in monophasic Ba(Ti,Sn)O3. The sintering characteristics and the dielectric properties of the ceramics prepared out of these fine powders are presented. The dielectric properties of fine-grained Ba(Ti,Sn)O3 ceramics are explained on the basis of the prevailing diffuse phase transition behaviour.