This paper reports the application of linearly increasing stress testing (LIST) to the study of stress corrosion cracking (SCC) of carbon steel in 4 N NaNO3 and in Bayer liquor. LIST is similar to the constant extension-rate testing (CERT) methodology with the essential difference that the LIST is load controlled whereas the CERT is displacement controlled. The main conclusion is that LIST is suitable for the study of the SCC of carbon steels in 4 N NaNO3 and in Bayer liquor. The low crack velocity in Bayer liquor and a measured maximum stress close to that of the reference specimen in air both indicate that a low applied stress rate is required to study SCC in this system. (C) 1998 Chapman & Hall.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Analytical electron microscopy was used to measure the composition of grain boundaries (GBs) and interconstituent boundaries (IBs) of X52 pipeline steel using specimens about 40-60 nm in thickness. All elements of interest were examined with the exception of carbon. With this caveat; there was no segregation at proeutectoid ferrite GBs. This indicated that the commonly expected species S and P are not responsible for preferential corrosion of GBs during intergranular stress corrosion cracking of pipeline steels. Manganese was the only species measured to segregate at the IBs. Manganese segregated to the IBs between proeutectoid ferrite and pearlitic cementite, and desegregated from IBs between proeutectoid ferrite and pearlitic ferrite. The pearlitic cementite was Mn rich. There was no Mn segregation at the IBs between pearlitic ferrite and pearlitic cementite. The pattern of Mn segregation could be explained in terms of diffusion in the process zone ahead of the pearlite during the austenite to pearlite transformation and diffusion in the IBs between the proeutectoid ferrite and pearlite. (C) 1998 Acta Metallurgica Inc. Published by Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The intercalated discs of working myocardium and Purkinje fibers of the monkey heart were examined by scanning and transmission electron microscopy. The NaOH/ultrasonication technique resulted in the digestion of connective tissue and a separation of the intercellular junctions of intercalated discs, such that these could be visualized three-dimensionally. The intercalated discs of ventricular myocytes, atrial myocytes and Purkinje fibers vary considerably in number and configuration, as do the intercalated discs of the three different layers of the ventricular myocardium. Myocytes in the subepicardial, middle and subendocardial layers of the ventricle have 1-3, 4-5 and 5-6 intercalated discs at the end of these cells, respectively, Those in the endocardial layer are characterized by the presence of small laterally-placed intercalated discs. Atrial myocytes and Purkinje fibers usually only have 1-2 intercalated discs, Individual intercalated discs in ventricular myocytes have complicated stairs with 10-30 steps and corresponding risers, while those of atrial myocytes and Purkinje fibers have simple stairs with 1-3 steps and risers, Steps equivalent to the plicate segments are characterized by densely-packed microplicae and finger-like microprojections which greatly increase surface area in vertricular myocytes, Microprojections in atrial myocytes and Purkinje fibers are sparse by comparison, Risers equivalent to the interplicate segments containing large gap junctional areas are most numerous in left ventricular myocytes, followed by right ventricular myocytes, Purkinje fibers and atrial myocytes in decreasing order. The geometric arrangement of the various types of myocytes may be related with impulse propagation. Large intercalated discs of cell trunks and series branches may participate in longitudinal propagation, while small laterally-placed ones may be the site of transverse propagation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To evaluate the remodeling of collagen fibers in the articular cartilage of rat ankles, with and without immobilization, after application of muscle stretching protocol. Twenty three Wistar rats were divided into four groups: immobilized (I), n = 6; immobilized and stretched (IS), n = 6; stretched (S), n = 6 and control (C), n = 5. The animals in groups I and IS were submitted to immobilization. After the period of immobilization, the animals in groups IS and S were submitted to a muscle stretching protocol. At the end of the experiment, the animals were euthanized and the joints removed, processed and stained with Picrosirius red. The analysis was carried out using a polarized light microscope. The density of collagen fibers were quantified according to the intensity of birefringence displayed. By way of statistical analyses, the right and left hind limbs of the different groups were compared based on the total density of collagen fibers, the density of thick collagen fibers and the density of thin collagen fibers. Immobilization promoted a reduction in density of the thin fibers and of total collagen. The muscle stretching protocol after immobilization promoted a reduction in density of the total collagen and of the thick fibers, but the density of the thin fibers showed the same values as control. The collagen fibers were remodeled by the different stimuli. Immobilization was harmful to the collagen fibers and the muscle stretching protocol only recovered the thin collagen fibers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An examination has been carried out of the secondary passive film on Type 304 stainless steel in 0.5 M H2SO4. The characterization techniques used were electrochemical (potentiodynamic; potentiostatic, and film reduction experiments) and surface analytical. A bilayer model for the secondary passive film is proposed. It appears that next to the metal, there is a modified passive film which controls the electrochemical response; i.e., governs the current for any applied potential. On top of this modified passive film, the experimental data are consistent with a ''porous'' corrosion-product film which adds to the total film thickness but has little influence on the electrochemical response. The composition of the secondary passive film corresponds most probably to a mixed Fe/Cr oxide/hydroxide enriched in Cr3+, With a composition similar to a primary passive film.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reports on measurements of crack growth by environmental assisted fracture (EAF) for 4340 steel in water and in air at various relative humidities. Of most interest is the observation of slow crack propagation in dry air. Fractographic analysis leads to the strong suggestion that this slow crack propagation is due to hydrogen cracking caused by internal hydrogen in solid solution inside the sample material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective/Hypothesis: To describe the arrangement of collagen fibers in the superficial layer of the lamina propria of the vocal folds with Reinke` edema. Study Design: Cross sectional analysis of the lamina propria of the vocal folds with Reinke`s edema (RE). Method: The picrosirius polarization method was used to study the arrangement of collagen fiber. Findings of collagen disarrangement were categorized semiquantitatively and correlated with RE severity, age, cigarette smoking and duration of dysphonia. Results: Analysis of 20 specimens of vocal folds with RE showed that the intertwined network of collagen fibers resembling a wicker-basket normally observed in vocal folds was disarranged in RE. The collagen fibers were loosely arranged, fragmented and intermixed with varying amounts of myxoid stroma. Moderate and large areas of disarrangement (90% of cases) predominated. Collagen fiber arrangement in the region underneath the epithelium was better preserved when compared with fibers in the deeper region of the superficial layer of the lamina propria. There was a statistical difference in collagen disarrangement between grade II and grade III severity (P = .007) that appeared to be due to the large areas of disarrangement observed in 73% of patients with grade III severity and in 44% of grade II severity. Age was the only variable correlated with collagen fiber disarrangement (r = 0.47, P = .037). Conclusion: Our findings suggest that the flexible framework which maintains the uniformity of the lamina propria was lost in RE caused by the disarrangement of the collagen fibers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: We describe the distribution of elastic system fibers in the superficial layer of the lamina propria of Reinke`s edema, as compared with normal vocal folds. Methods: Weigert`s resorcin-fuchsin stain after oxidation with 10% oxone was used to study the arrangement of elastic fibers. The findings were categorized and afterward compared with the severity of Reinke`s edema. Results: Analysis of 20 specimens of vocal folds with Reinke`s edema showed that the network of thin elastic fibers in Reinke`s space lost their undulated appearance and had a tangled aspect. In addition, these fibers were no longer parallel to the epithelial basement membrane, but had a random distribution scattered throughout Reinke`s space. The elastic fiber network immediately below the epithelial basement membrane also appeared more fragmented in Reinke`s edema because of some alteration in organization combined with the 5-mu m-thick histologic sectioning plane. No significant difference in the degree of elastic system fiber disarrangement was observed between severity grades II and III (p = 0.382). Large areas of disarrangement were predominant (80% of cases). Conclusions: The disarrangement of elastic fibers in Reinke`s edema may cause insufficient tissue resistance and resilience, contributing to the hypermobility observed in Reinke`s edema.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have demonstrated that phrenic nerves` large myelinated fibers in streptozotocin (STZ)-induced diabetic rats show axonal atrophy, which is reversed by insulin treatment. However, studies on structural abnormalities of the small myelinated and the unmyelinated fibers in the STZ-model of neuropathy are limited. Also, structural changes in the endoneural vasculature are not clearly described in this model and require detailed study. We have undertaken morphometric studies of the phrenic nerve in insulin-treated and untreated STZ-diabetic rats and non-diabetic control animals over a 12-week period. The presence of neuropathy was assessed by means of transmission electron microscopy, and morphometry of the unmyelinated fibers was performed. The most striking finding was the morphological evidence of small myelinated fiber neuropathy due to the STZ injection, which was not protected or reversed by conventional insulin treatment. This neuropathy was clearly associated with severe damage of the endoneural vessels present on both STZ groups, besides the insulin treatment. The STZ-diabetes model is widely used to investigate experimental diabetic neuropathies, but few studies have performed a detailed assessment of either unmyelinated fibers or capillary morphology in this animal model. The present study adds useful information for further investigations on the ultrastructural basis of nerve function in diabetes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

AB Study Design. A cross-sectional study was conducted. Objective. To determine the activity of the deep and superficial fibers of the lumbar multifidus during voluntary movement of the arm. Summary of Background Data. The multifidus contributes to stability of the lumbar spine. Because the deep and superficial parts of the multifidus are near the center of lumbar joint rotation, the superficial fibers are well suited to control spine orientation, and the deep fibers to control intervertebral movement. However, there currently are limited in vivo data to support this distinction. Methods. Electromyographic activity was recorded in both the deep and superficial multifidus, transversus abdominis, erector spinae, and deltoid using selective intramuscular electrodes and surface electrodes during single and repetitive arm movements. The latency of electromyographic onset in each muscle during single movements and the pattern of electromyographic activity during repetitive movements were compared between muscles. Results. With single arm movements, the onset of electromyography in the erector spinae and superficial multifidus relative to the deltoid was dependent on the direction of movement, but the onset in the deep multifidus and transversus abdominis was not. With repetitive arm movements, peaks in superficial multifidus and erector spinae electromyography occurred only during flexion for most subjects, whereas peaks in deep multifidus electromyography occurred during movement in both directions. Conclusions. The deep and superficial fibers of the multifidus are differentially active during single and repetitive movements of the arm. The data from this study support the hypothesis that the superficial multifidus contributes to the control of spine orientation, and that the deep multifidus has a role in controlling intersegmental motion. (C) 2002 Lippincott Williams & Wilkins, Inc.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study explores several important aspects of the management of new product development (NPD) in the Chinese steel industry. Specifically it explores NPD success factors, the importance of management functions to new product success and measures of new product success from the perspective of the industry's practitioners. Based on a sample of 190 industrial practitioners from 18 Chinese steel companies, the study provides a mixed picture as China makes the transition from a centrally-controlled to market-based economy. On one hand, respondents ranked understanding users' needs as the most important factor influencing the performance of the new products. Further, formulating new product strategy and strengthening market research are perceived as the most important managerial functions in NPD. However, technical performance measures are regarded as more important and are more widely used in industry than market-based or financial measures of success.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Water wetting is a crucial issue in carbon dioxide (CO.) corrosion of multiphase flow pipelines made from mild steel. This study demonstrates the use of a novel benchtop apparatus, a horizontal rotating cylinder, to study the effect of water wetting on CO2 corrosion of mild steel in two-phase flow. The setup is similar to a standard rotating cylinder except for its horizontal orientation and the presence of two phases-typically water and oil. The apparatus has been tested by using mass-transfer measurements and CO2 corrosion measurements in single-phase water flow. CO2 corrosion measurements were subsequently performed using a water/hexane mixture with water cuts varying between 5% and 50%. While the metal surface was primarily hydrophilic under stagnant. conditions, a variety of dynamic water wetting situations was encountered as the water cut and fluid velocity were altered. Threshold velocities were identified at various water cuts when the surface became oil-wet and corrosion stopped.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A model of iron carbonate (FeCO3) film growth is proposed, which is an extension of the recent mechanistic model of carbon dioxide (CO2) corrosion by Nesic, et al. In the present model, the film growth occurs by precipitation of iron carbonate once saturation is exceeded. The kinetics of precipitation is dependent on temperature and local species concentrations that are calculated by solving the coupled species transport equations. Precipitation tends to build up a layer of FeCO3 on the surface of the steel and reduce the corrosion rate. On the other hand, the corrosion process induces voids under the precipitated film, thus increasing the porosity and leading to a higher corrosion rate. Depending on the environmental parameters such as temperature, pH, CO2 partial pressure, velocity, etc., the balance of the two processes can lead to a variety of outcomes. Very protective films and low corrosion rates are predicted at high pH, temperature, CO2 partial pressure, and Fe2+ ion concentration due to formation of dense protective films as expected. The model has been successfully calibrated against limited experimental data. Parametric testing of the model has been done to gain insight into the effect of various environmental parameters on iron carbonate film formation. The trends shown in the predictions agreed well with the general understanding of the CO2 corrosion process in the presence of iron carbonate films. The present model confirms that the concept of scaling tendency is a good tool for predicting the likelihood of protective iron carbonate film formation.