980 resultados para Sm : YAP


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spherical SiO2 particles have been coated with rare earth oxide layers by a Pechini sol-gel process, leading to the formation of core-shell structured SiO2@RE2O3 (RE = rare earth elements) and SiO2@Gd2O3:Ln(3+) (Ln = Eu, Tb, Dy, Sm, Er, Ho) particles. X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM), photoluminescence (PL), and cathodoluminescence spectra as well as lifetimes were used to characterize the resulting SiO2@RE2O3 (RE = rare earth elements) and SiO2@Gd2O3:Ln(3+) (Eu3+, Tb3+, Dy3+, Sm3+, Er3+, Ho3+) samples. The obtained core-shell phosphors have perfect spherical shape with narrow size distribution (average size ca. 380 nm), smooth surface and non-agglomeration. The thickness of shells could be easily controlled by changing the number of deposition cycles (40 nm for two deposition cycles).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LaInO3: Sm3+, LaInO3: Pr3+ and LaInO3: Tb3+ phosphors were prepared through a Pechini-type sol-gel process. X-ray diffraction, field emission scanning electron microscopy, photoluminescence, and cathodoluminescence (CL) spectra were utilized to characterize the synthesized phosphors. XRD results reveal that the pure LaInO3 phase can also be obtained at 700 degrees C. FE-SEM images indicate that the LaInO3: Sm3+, LaInO3: Pr3+ and LaInO3: Tb3+ phosphors are composed of aggregated spherical particles with sizes around 80-120 nm. Under the excitation of ultraviolet light and low voltage electron beams (1-5 kV), the LaInO3: Sm3+, LaInO3: Pr3+ and LaInO3: Tb3+ phosphors show the characteristic emissions of Sm3+ ((4)G(5/2)-H-6(5/2,7/2,9/2) transitions, yellow), Pr3+ (P-3(0)-H-3(4), P-3(1)-H-3(5), D-1(2)-H-3(4) and P-3(0)-F-3(2) transitions, blue-green) and Tb3+ (D-5(4)-F-7(6.5,4.3) transitions, green) respectively. The corresponding luminescence mechanisms are discussed. These phosphors have potential applications in field emission displays.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three-dimensional flowerlike Lu2O3 and Lu2O3:Ln(3+) (Ln = Eu, Th, Dy, Pr, Sm, Er, Ho, Tm) microarchitectures have been successfully synthesized via ethylene glycol (EG)-mediated hydrothermal method followed by a subsequent heat treatment process. X-ray diffraction, Fourier transform infrared spectroscopy, energy-dispersive X-ray spectra, thermogravimetric and differential thermal analysis, elemental analysis, inductively coupled plasma atomic absorption spectrometric analysis, ion chromatogram analysis, X-ray photoelectron spectra, scanning electron microscopy, transmission electron microscopy, photoluminescence spectra as well kinetic decays, and cathodoluminescence spectra were used to characterize the samples. Hydrothermal temperature, EG, and CH3COONa play critical roles in the formation of the lutetium oxide precursor microflowers. The reaction mechanism and the self-assembly evolution process have been proposed. The as-formed lutetium oxide precursor could transform to Lu2O3 With their original flowerlike morphology and slight shrinkage in the size after postannealing process.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A variety of uniform lanthanide orthoborates LnBO(3) (Ln = Gd, Nd, Sm, Eu, Tb, and Dy) microplates have been successfully prepared by a general and facile conversion method. One-dimensional (ID) lanthanide hydroxides were first prepared through a simple hydrothermal process. Subsequently, uniform LnBO(3) microplates were synthesized at the expense of the ID precursors during a hydrothermal conversion process. The whole process in this method was carried out in aqueous condition without the use of any organic solvents, surfactant, or catalyst. The as-obtained rare earth ions doped GdBO3 and TbBO3 microplates show strong light emissions with different colors coming from different activator ions under ultraviolet excitation or low-voltage electron beam excitation, which might find potential applications in fields such as light phosphor powders and advanced flat panel display devices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Uniform MF/YVO4:Ln(3+) (Ln = Eu, Dy, and Sm) composite microspheres have been prepared via a simple and economical wet-chemical route at ambient pressure and low temperature. Monodisperse micrometer-sized melamine formaldehyde (MF) colloidal particles were first fabricated by a condensation process of melamine with formaldehyde. Subsequently, well-dispersed YVO4 nanoparticles were successfully grown onto the MF microspheres to form core-shell structured composite particles in aqueous Solution. The as-obtained composite microspheres with perfect spherical shape are uniform in size and distribution, and the thickness and roughness of the YVO4 shells on MF cores could be tuned by varying the reaction temperature. The MF/YVO4:Ln(3+) composite phosphors show strong light emissions with different colors coming from different activator ions under ultraviolet excitation, which might find potential applications in fields such as light phosphor powders and advanced flat panel displays.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Five new complexes based on rare-earth-radical [Ln(hfac)(3)(NIT-5-Br-3py)](2) (Ln=Pr (1), Sm (2), Eu (3), Tb (4), Tm (5); hfac = hexafluoroacetylacetonate; NIT-5-Br-3py = 2-(4,4,5,5-tetramethyl-3-oxylimidazoline-1-oxide)-5-bromo-3-pyridine) have been synthesized and characterized by X-ray crystal diffraction. The single-crystal structures show that these complexes have similar structures, in which a NIT-5-Br-3py molecule acts as a bridging ligand linking two Ln(III) ions through the oxygen atom of the N-O group and nitrogen atom from the pyridine ring to form a four-spin system. Both static and dynamic magnetic properties were measured for complex 4, which exhibits single-molecule magnetism behavior.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The photoluminescence (PL) and electroluminescence (EL) properties of a samarium complex Sm(TTA)(3)phen (TTA = 2-thenoyltri-fluoroacetonate, phen = 1, 10-phenanthroline) were investigated. The results show that Sm(TTA)3phen could be used as promising luminescent and electron transporting material in the electroluminescent devices. The difference between PL and EL spectra was noticed and discussed. Besides, it is noteworthy that the choice of the hole transporting layer (HTL) showed significant effect on the device performance, which was explained by the low-lying highest occupied molecular orbit (HOMO) level of Sm(TTA)3phen and the different hole injection barrier at the HTL/EML (emitting material layer) interface.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

New near-infrared-luminescent mesoporous materials were prepared by linking ternary lanthanide (Er3+, Nd3+, Yb3+, Sm3+, Pr3+) complexes to the ordered mesoporous MCM-41 through a functionalized 1,10-phenanthroline (phen) group 5-(N,N-bis-3-(triethoxysilyl)propyl)ureyl-1,10-phenanthroline. The resulting materials (denoted as Ln(hfth)(3)phen-M41 and Pr(tfnb)(3)phen-M41; Ln=Er, Yb, Nd, Sm; hfth = 4,4,5,5,6,6,6-heptafluoro-1-(2-thienyl)hexane-1,3-dionate; tfnb = 4,4,4-trifluoro-1-(2-naphthyl)- 1, 3-butanedionate) were characterized by powder X-ray diffraction, N-2 adsorption/desorption, and elemental analysis. Luminescence spectra of these lanthanide-complex functionalized materials were recorded, and the luminescence decay times were measured. Upon excitation at the absorption of the organic ligands, all these materials show the characteristic NIR luminescence of the corresponding lanthanide (Er3+, Nd3+, Yb3+, Sm3+, Pr3+) ions by sensitization from the organic ligands moiety. The good luminescent performances enable these NIR-luminescent mesoporous materials to have possible applications in optical amplification (operating at 1300 or 1500 nm), laser systems, or medical diagnostics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

研究了Pr3+,Sm3+掺杂对YAG∶Ce发射光谱及其荧光寿命的影响。观察到当掺杂Pr3+时,在609nm处出现Pr3+的发射峰,而掺杂Sm3+时,在616nm处呈现Sm3+的发射峰。掺杂Pr3+或Sm3+增加红光区的发射峰将有利于提高YAG∶Ce荧光粉的显色性。实验中测定了(Y0.95Sm0.01Ce0.04)3Al5O12、(Y0.95Pr0.01Ce0.04)3Al5O12、(Y0.96Ce0.04)3Al5O12的荧光寿命(τ),观察到在YAG∶Ce中掺入Pr3+或Sm3+使Ce3+的荧光寿命减小。实验结果表明,少量掺杂Pr3+或Sm3+并未引起基质的结构的变化。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sin and Pr doped CeO2 and Ce6MoO15 based materials were synthesized by sol-gel method. The structure of the powders were characterized by X-ray diffraction (XRD), Raman spectra, field emission scanning electron microscopy(FE-SEM) and the electrical conductivity of the samples was investigated by AC impedance spectroscopy. By comparing the structure and electrical properties of different systems, it could be concluded that the electrical property of Ce6MoO15 based system is better than that of CeO2 system. The added Mo element resulted in the increase of gain size and improved the grain boundary conductivity notably below 600 degrees C, while the Pr dopant induced the smaller grain size and improved the grain boundary conductivity of the materials.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

分别以相同面积的光滑 Pt电极和吸附了 Sm3+ 的铂电极作为工作电极 ,在酸性介质中采用循环伏安法对甲醇氧化进行测定 .结果表明 ,吸附了 Sm3+ 的 Pt电极上产生了更大的氧化电流 ,表明 Sm3+ 的加入对甲醇的电催化氧化起到了促进作用 .这一研究结果在直接甲醇燃料电池 ( DMFC)阳极催化剂研制方面具有较大的应用潜力

Relevância:

20.00% 20.00%

Publicador:

Resumo:

研究了在不同激发波长下三价钐离子掺杂硫氧化钇的发光强度对浓度的依赖关系。研究发现磷光体的发光强度不仅跟激活离子的浓度有关,而且跟激发时所采用的不同激发波长有关。磷光体发光强度与激活剂掺杂量的变化曲线表明,在不同激发路径下磷光体具有不同的发光性质。采用Sm3+离子直接跃迁的413nm对样品进行激发时,发生猝灭的浓度低至约02mol%;当采用263nm高能紫外线激发时,浓度猝灭发生在较高浓度处(~2mol%),后者是前者的10倍。对Sm3+离子发射强度与浓度关系曲线进行了拟合计算,结果表明Sm3+在Y2O2S中浓度猝灭的原因主要是相邻中心的偶极四极相互作用引起的交叉弛豫。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

采用固相反应法合成了一种新型的橙红色长余辉磷光粉 Gd2 O2 S:Sm3 + ,并用全自动 X射线粉末衍射仪表征了其结构 ,用荧光光谱仪测试了其激发、发射光谱、余辉光谱和余辉衰减曲线。 XRD证实其为单相的硫氧化钆。该磷光体呈现 Sm3 +的三个特征发射 (4G5/2 → 6HJ,J=5 /2 ,7/2 ,9/2 )。经紫外或可见光激发后能观察到长时间明亮的余辉发光。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Y2O3:Sm and Gd2O3:Sm powder phosphors were prepared by carbonate coprecipitation method. The purified crystalline phases of Y2O3:Sm and Gd2O3:SM were obtained at 600degreesC, and the crystallinity increases with increase in annealing temperature. Both samples contain aggregated phosphor particles. An energy transfer (ET) from Y2O3 and Gd2O3 hosts to sm(3+) has been observed, and the ET efficiency in the latter is higher than that in the former because an energy migration process like Gd3+-(Gd3+)(n)-Sm3+ has occurred in the latter. Furthermore, an upconversion luminescence from the (4)G(5/2) level of Sm3+ has been observed in both Y2O3 and Gd2O3 under the excitation of 936 nm infrared, whose mechanisms are proposed. Both the up and downconversion emission intensities of Sm3+ in Gd2O3 are stronger than those in Y2O3.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

铜激活的硫化锌 (Zn S∶ Cu)和铕激活的硫化钙 (Ca S∶ Eu)是最早获得应用的蓝色和红色长余辉材料 .随后 ,相继发现了铝酸盐体系和硅酸盐体系两大类长余辉荧光材料 [1~ 3 ] .这两类长余辉荧光材料在发光亮度、余辉时间、稳定性方面都较前述硫化物系列长余辉荧光材料有很大提高 ,从而具有非常广阔的应用前景和应用范围 [4~ 6] .但这两类长余辉荧光材料的发光颜色一般为蓝紫、蓝或黄绿 ,没有红色发光现象 .随着研究的深入 ,人们发现了稀土元素激活的碱土钛酸盐红色长余辉荧光材料 ,这种荧光材料在发光亮度及余辉上都有明显的提高 [7,8] ,而且解决了硫化物不稳定的缺点 .近年来才发展起来的以碱土金属氧化物为发光基质 ,以 Eu3 + 为激活剂的红色长余辉荧光材料进一步提高了余辉亮度及时间 [9] .传统碱土硫化物类磷光体有较宽的激发谱带 ,可在不同的光源下激发 .但它的稳定性较差 ,必须进行工艺后处理才能得到应用 .其它几类磷光体的激发光源谱带较窄 ,仅限于紫外光源 ,因此使其应用范围受到限制 .目前已报道的各种长余辉红色荧光材料在余辉时间方面有较大的差异 ,从十几分钟到几百分钟不等 ,各类红色磷光...