951 resultados para Rubber of tire


Relevância:

40.00% 40.00%

Publicador:

Resumo:

The objective of this work was to evaluate the efficiency of EST‑SSR markers in the assessment of the genetic diversity of rubber tree genotypes (Hevea brasiliensis) and to verify the transferability of these markers for wild species of Hevea. Forty‑five rubber tree accessions from the Instituto Agronômico (Campinas, SP, Brazil) and six wild species were used. Information provided by modified Roger's genetic distance were used to analyze EST‑SSR data. UPGMA clustering divided the samples into two major groups with high genetic differentiation, while the software Structure distributed the 51 clones into eight groups. A parallel could be established between both clustering analyses. The 30 polymorphic EST‑SSRs showed from two to ten alleles and were efficient in amplifying the six wild species. Functional EST‑SSR microsatellites are efficient in evaluating the genetic diversity among rubber tree clones and can be used to translate the genetic differences among cultivars and to fingerprint closely related materials. The accessions from the Instituto Agronômico show high genetic diversity. The EST‑SSR markers, developed from Hevea brasiliensis, show transferability and are able to amplify other species of Hevea.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The objective of this work was to evaluate the influence of intercropping 'Conilon' coffee (Coffea canephora) with rubber trees on coffee tree microclimate, nutrition, growth, and yield. Rubber trees were planted in two double rows 33 m apart, with 4x2.3 m spacing between plants. Treatments consisted of the distances from the coffee plants to the rubber trees: 3, 6, 9, 12, and 15 m. Measurements of atmospheric variables (temperature, irradiance, and relative humidity), leaf nutrient concentration, internode length of plagiotropic and orthotropic branches, individual leaf area, chlorophyll content, and yield were performed. Intercropping promotes changes in the microclimatic conditions of coffee plants close to rubber trees, with reduction of temperature and irradiance level and increase in air relative humidity. The proximity of the coffee tree to the rubber trees promotes the elongation of the plagiotropic and orthotropic branches and increases the individual leaf area; however, it does not affect leaf concentrations of N, K, Mg, Fe, Zn, and B in 'Conilon' coffee and does not have a negative impact on yield.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

One aim of this study is to determine the impact of water velocity on the uptake of indicator polychlorinated biphenyls (iPCBs) by silicone rubber (SR) and low-density polyethylene (LDPE) passive samplers. A second aim is to assess the efficiency of performance reference compounds (PRCs) to correct for the impact of water velocity. SR and LDPE samplers were spiked with 11 or 12 PRCs and exposed for 6 weeks to four different velocities (in the range of 1.6 to 37.7 cm s−1) in river-like flow conditions using a channel system supplied with river water. A relationship between velocity and the uptakewas found for each iPCB and enables to determine expected changes in the uptake due to velocity variations. For both samplers, velocity increases from 2 to 10 cm s−1, 30 cm s−1 (interpolated data) and 100 cm s−1 (extrapolated data) lead to increases of the uptake which do not exceed a factor of 2, 3 and 4.5, respectively. Results also showed that the influence of velocity decreased with increasing the octanol-water coefficient partition (log Kow) of iPCBs when SR is used whereas the opposite effect was observed for LDPE. Time-weighted average (TWA) concentrations of iPCBs in water were calculated from iPCB uptake and PRC release. These calculations were performed using either a single PRC or all the PRCs. The efficiency of PRCs to correct the impact of velocity was assessed by comparing the TWA concentrations obtained at the four tested velocities. For SR, a good agreement was found among the four TWA concentrations with both methods (average RSD b 10%). Also for LDPE, PRCs offered a good correction of the impact of water velocity (average RSD of about 10 to 20%). These results contribute to the process of acceptance of passive sampling in routine regulatory monitoring programs.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The pathogenicity of Pratylenchus brachyurusto rubber (Hevea brasiliensis) rootstocks was studied in two experiments: 1) opencross seedlings of 'Tjir 1' x 'Tjir 16' were inoculated with zero, 7,700 or 23,100 nematodes per plant; 2) illegitimate seedlings of 'GT 1', 'RRIM 527' and 'RRIM 600' were inoculated with zero or 12,800 nematodes per plant. After 195 (1st experiment) or 105 days after inoculation (2nd experiment), P. brachyurusdid not affect the relative growth percentage in terms of plant height in both experiments but significantly diminished the stem diameter percentage and increased the stomatal resistance of 'GT 1' , 'RRIM 527' and 'RRIM 600'.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The objective of this work was to define the optimal conditions for invertase assay, seeking to determine the ideal parameters for the different isoenzymes of leaf and bark tissues in adult rubber trees. Assays of varying pH, sucrose concentration and temperature of the reaction medium were conducted for the two investigated isoenzymes. The results pointed out the existence of two different pH related isoforms for the two analyzed tissues, with an isoenzyme being more active at pH 5,5 and the other at neutral/alkaline pH. Leaf blade isoenzymes presented similar values for substrate concentration, whereas the bark isoenzyme presented maximum values below those previously reported. The assays at different temperatures presented similar values for leaf isoenzymes, though they have differed significantly among the obtained values.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Solar radiation is an important factor for plant growth, being its availability to understory crops strongly modified by trees in an Agroforestry System (AFS). Coffee trees (Coffea arabica - cv. Obatã IAC 1669-20) were planted at a 3.4 x 0.9 m spacing inside and aside rows of monocrops of 12 year-old rubber trees (Hevea spp.), in Piracicaba-SP, Brazil (22º42'30" S, 47º38'00" W - altitude: 546m). One-year-old coffee plants exposed to 25; 30; 35; 40; 45; 80; 90; 95 and 100% of the total solar radiation were evaluated according to its biophysical parameters of solar radiation interception and capture. The Goudriaan (1977) adapted by Bernardes et al. (1998) model for radiation attenuation fit well to the measured data. Coffee plants tolerate a decrease in solar radiation availability to 50% without undergoing a reduction on growth and LAI, which was approximately 2m².m-2 under this condition. Further reductions on the availability of solar radiation caused a reduction in LAI (1.5m².m-2), thus poor land cover and solar radiation interception, resulting in growth reduction.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

When using appropriate inflation pressures and load capacity (ballast), it may obtain a higher yield and prolongation of the life of the tire, besides it may minimize the problems of loss of traction, increased slippage and fuel consumption. This study aimed to evaluate the fuel consumption of a tractor operating with new and worn tires in three conditions of ballasting and three inflation pressures, when driving on compacted soil with vegetation cover. The experiment was conducted at the experimental unit from the Department of Animal Science, Federal University of Lavras, state of Minas Gerais, Brazil, in an agricultural soil compacted by cattle trampling and with vegetation cover. It was used a tractor 4x2 with front wheel assist, of a 65.62 kW engine power. The tires were of R1 type, diagonal (front: 12.4 to 24; and rear: 18.4 to 30), the average height of the clutches of the new tires were 0.3 and 0.35 m for front and rear tires, respectively, and for the worn tires were 0.018 and 0.0045 m, for the front and the rear tires, respectively. The results showed advantages for the tractor equipped with new tires.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

OBJECTIVE: to verify the effectiveness of the rubber elastic band in the treatment of large wounds of the body wall of rabbits by means of traction of its edges. METHODS: we studied 30 New Zealand rabbits, divided into three groups (n=10): Group 1- healing by secondary intention; Group 2- removal and eutopic repositioning of skin as full thickness skin graft; Group 3- Approximation of wound edges with elastic rubber band. In all animals, we removed a segment of the back skin and subcutaneous tissue down to the fascia, in accordance with an acrylic mold of 8cm long by 12cm wide. All animals were observed for 21 days. RESULTS: two animals of groups 1 and 2 had wound abscess. In Group 2, there was partial or total graft loss in 90% of animals. The complete closure of the wounds was observed in four animals of Group 1, six of Group 2 and eight of Group 3. There was no difference between the scar resistance values of groups 2 and 3, which were higher than those in Group 1. The scars of the three groups were characterized by the presence of mature connective tissue mixed with blood vessels and inflammatory infiltration, predominantly polymorphonuclear. CONCLUSION: the tensile strength of the wound edges with rubber elastic band is as efficient as the skin graft to treat rabbits' large body wounds.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Mémoire numérisé par la Division de la gestion de documents et des archives de l'Université de Montréal

Relevância:

40.00% 40.00%

Publicador:

Resumo:

In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Prevulcanized natural rubber latex was prepared by the heating of the latex compound at 55°C for different periods of time (2, 4, 6, 8, and 10 h). The changes in the colloidal stability and physical properties were evaluated during the course of prevulcanization. The prevulcanized latex compounds were stored for 300 days, and the properties were monitored at different storage intervals (0, 20, 40, 60, 120, 180, 240, and 300 days). During prevulcanization, the mechanical stability time increased, and the viscosity remained almost constant. The tensile strength increased during storage for a period of 20 days. The degree of crosslinking, modulus, elongation at break, and chloroform number were varied with the time of storage.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A novel method of blending natural rubber with polyvinylchloride in the latex stage was developed, Dioctyl phthalate (DOP) and Amine terminated natural rubber (ATNR) were used as plasticisers, for improving the mechanical properties of these blends. Properties of the latex stage blends were compared with those of dry blends. Latex stage blends showed superior mechanical properties compared to the blends prepared in the dry state. The ageing resistance, oil resistance and processability were found to be improved by latex stage blending.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Natural rubber/isora fibre composites were cured at various temperatures. The solvent swelling characteristics of natural rubber composites containing both untreated and alkali treated fibres were investigated in aromatic and aliphatic solvents like toluene, and n-hexane. The diffusion experiments were conducted by the sorption gravimetric method. The restrictions on elastomer swelling exerted by isora fibre as well as the anisotropy of swelling of the composite have been confirmed by this study. Composite cured at 100°C shows the lowest percentage swelling. The uptake of aromatic solvent is higher than that of aliphatic solvent for the composites cured at all temperatures. The effect of fibre loading on the swelling behaviour of the composite was also investigated in oils like petrol, diesel, lubricating oil etc. The % swelling index and swelling coefficient of the composite were found to decrease with increase in fibre loading. This is due to the increased hindrance exerted by the fibres at higher fibre loadings and also due to the good fibre-rubber interactions. Maximum uptake of solvent was observed with petrol followed by diesel and then lubricating oil. The presence of bonding agent in the composites restrict the swelling considerably due to the strong interfacial adhesion. At a fixed fibre loading, the alkali treated fibre composite showed lower percentage swelling compared to the untreated one.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent.