997 resultados para Mg alloy


Relevância:

60.00% 60.00%

Publicador:

Resumo:

Advances in biomaterials have enabled medical practitioners to replace diseased body parts or to assist in the healing process. In situations where a permanent biomaterial implant is used for a temporary application, additional surgeries are required to remove these implants once the healing process is complete, which increases medical costs and patient morbidity. Bio-absorbable materials dissolve and are metabolized by the body after the healing process is complete thereby negating additional surgeries for removal of implants. Magnesium alloys as novel bio-absorbable biomaterials, have attracted great attention recently because of their good mechanical properties, biocompatibility and corrosion rate in physiological environments. However, usage of Mg as biodegradable implant has been limited by its poor corrosion resistance in the physiological solutions. An optimal biodegradable implant must initially have slow degradation to ensure total mechanical integrity then degrade over time as the tissue heals. The current research focuses on surface modification of Mg alloy (MZC) by surface treatment and polymer coating in an effort to enhance the corrosion rate and biocompatibility. It is envisaged that the results obtained from this investigation would provide the academic community with insights for the utilization of bio-absorbable implants particularly for patients suffering from atherosclerosis. The alloying elements used in this study are zinc and calcium both of which are essential minerals in the human metabolic and healing processes. A hydrophobic biodegradable co-polymer, polyglycolic-co-caprolactone (PGCL), was used to coat the surface treated MZC to retard the initial degradation rate. Two surface treatments were selected: (a) acid etching and (b) anodization to produce different surface morphologies, roughness, surface energy, chemistry and hydrophobicity that are pivotal for PGCL adhesion onto the MZC. Additionally, analyses of biodegradation, biocompatibility, and mechanical integrity were performed in order to investigate the optimum surface modification process, suitable for biomaterial implants. The study concluded that anodization created better adhesion between the MZC and PGCL coating. Furthermore, PGCL coated anodized MZC exhibited lower corrosion rate, good mechanical integrity, and better biocompatibility as compared with acid etched.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Vapour species effusing from a magnesia Knudsen cell containing Mg-Zn alloy at 923 K were condensed on a water cooled copper plate. The equilibrium composition of the vapour phase over the alloy was determined from chemical analysis of the condensate. The activity coefficients of both components in the alloy have been derived from the data using a modified Gibbs-Duhem relation. The ratio of saturation vapour pressures of pure Zn and Mg obtained from the analysis of alloy data agree well with values from the literature, providing an internal check on the accuracy of data obtained in this study. Both components of the alloy exhibit negative deviations from Raoult's law. The concentration-concentration structure factor of Bhatia and Thomton at zero wave vector, evaluated from the measurements, indicate the presence of MgZn2 type complex in the liquid state. The associated regular solution model has been used for the thermodynamic description of liquid Mg-Zn alloys.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Early studies on grain boundary sliding (GBS) in Mg alloys have suggested frequently that the contribution of GBS to creep is high even under conditions corresponding to dislocation creep. The role of creep strain and grain size in influencing the experimental measurements has not been clearly identified. Grain boundary sliding measurements were conducted in detail over experimental conditions corresponding to diffusion creep as well as dislocation creep in a single-phase Mg-0.7 wt pet Al alloy. The results indicated clearly that the GBS contribution to creep was Very high during,, diffusion creep at low stresses (similar to 75 pct) and substantially reduced during dislocation creep at high stresses (similar to 15 pct). These measurements were consistent with the observation of significant intragranular slip band activity observed in most grains at high stresses and very little slip band activity at low stresses. The experimental measurements and analysis indicated also that the GBS contribution to creep was high during the initial stages of creep and decreased to a steady-state value at large strains.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Strain rate sensitivity measurements are used to identify twinning and changes in deformation mechanisms in a Mg AZ31 alloy over a wide range of temperatures and grain sizes. At low temperatures, there is significant twinning at low strains with strain-rate insensitivity; at large strains, strain rate sensitivity is noted, corresponding to deformation by multiple slip. At high temperatures, there is very little twinning and this leads to a significant strain rate sensitivity from the early stages of deformation. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The present work describes the evolution of a strong, single-component rotated-Brass ((1 1 0) < 5 5 6 >) texture in an Al-Zn-Mg-Cu-Zr alloy by an uneven hot cross-rolling with frequent interpass annealing. This texture development is unique because hot rolling of aluminum alloys results in orientation distribution along the ``beta-fibre''. It has been demonstrated that the deformation by cross-rolling of a partially recrystallized grain structure having rotated-Cube and Goss orientations, and the recrystallization resistance of near-Brass-oriented elongated grains play a critical role in development of this texture. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Tensile experiments at 673 K and grain sizes from similar to 8 to 17 mu m revealed large ductility at a low strain rate and a reduced ductility at a high strain rate, corresponding to a change from a high to a low value for the strain rate sensitivity. High strain rate deformation led to fracture by flow localization, whereas low strain rate deformation involved fracture by cavity nucleation and growth. Analysis revealed that grain boundary migration can assist significantly in reducing the stress concentrations caused by grain boundary sliding, thereby retarding cavity nucleation. Calculations demonstrate that the interlinkage of voids parallel and perpendicular to the tensile axis occurs significantly, so that it is not always possible to use the cavity shapes to distinguish between diffusion and plasticity controlled growth. Cavitation damage evolves slowly in materials with a coarser grain size because of reduced nucleation related to a reduction in the strain rate sensitivity and associated grain boundary sliding. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The hot workability of an Al-Mg-Si alloy has been studied by conducting constant strain-rate compression tests. The temperature range and strain-rate regime selected for the present study were 300-550 degrees C and 0.001-1 s(-1), respectively. On the basis of true stress data, the strain-rate sensitivity values were calculated and used for establishing processing maps following the dynamic materials model. These maps delineate characteristic domains of different dissipative mechanisms. Two domains of dynamic recrystallization (DRX) have been identified which are associated with the peak efficiency of power dissipation (34%) and complete reconstitution of as-cast microstructure. As a result, optimum hot ductility is achieved in the DRX domains. The strain rates at which DRX domains occur are determined by the second-phase particles such as Mg2Si precipitates and intermetallic compounds. The alloy also exhibits microstructural instability in the form of localized plastic deformation in the temperature range 300-350 degrees C and at strain rate 1 s(-1).

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Processing maps have been developed for hot deformation of Mg-2Zn-1Mn alloy in as-cast condition and after homogenization with a view to evaluate the influence of homogenization. Hot compression data in the temperature range 300-500degreesC and strain rate range 0.001-100 s(-1) were used for generating the processing map. In the map for the as-cast alloy the domain of dynamic recrystallization occurring, at 450degreesC and 0.1 s(-1) has merged with another domain occurring at 500degreesC and 0.001 s(-1) representing grain boundary cracking. The latter domain is eliminated by homogenization and the dynamic recrystallization domain expanded with a higher peak efficiency occurring at 500 degreesC and 0.05 s(-1). The flow localization occurring at strain rates higher than 5 s(-1) is unaffected by homogenization.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

There is considerable interest currently in developing magnesium based alloys as replacements for aluminum alloys in automobile applications, due to their high specific strength as compared to aluminum alloys. However, the poor formability of magnesium alloys has restricted their applications; superplasticity can be utilized to form components with complex shapes. In the present study, the compressive deformation characteristics of a Mg-0.8 wt% Al alloy with an initial grain size of 19 +/- 1.0 mum have been studied in the temperature range of 623-673 K and at strain rates ranging from 10(-7) to 10(-3) s(-1). The stress exponent was observed to decrease with a decrease in stress. The results are analyzed in terms of the existing theoretical models for high temperature deformation. Furthermore, the potential for superplasticity in this alloy is explored, based on the mechanical and microstructural characteristics of the alloy.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This is the first successful attempt to produce simultaneously ultrafine grain size and weak texture in a single-phase magnesium alloy Mg-3Al-0.4Mn through an optimal choice of processing parameters in a modified multi-axial forging (MAF) process. An average grain size of similar to 0.4 mu m and a weak texture could be achieved. This has led to an increase in the strength as well as room-temperature ductility (55%). The plot of the yield loci shows a decrease in anisotropy after MAF. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Friction stir processing was carried out on the Al-Mg-Mn alloy to achieve ultrafine grained microstructure. The evolution of microstructure and micro-texture was studied in different regions of the deformed sample, namely nugget zone, thermo-mechanically affected zone (TMAZ) and base metal. The average grain sizes of the nugget zone, TMAZ and base metal are 1.5 mu m +/- 0.5 mu m, 15 mu m +/- 8 mu m, and 80 mu m +/- 10 mu m, respectively. The TMAZ exhibits excessive deformation banding structure and sub-grain formation. The orientation gradient within the sub-grain is dependent on grain size, orientation, and distance from nugget zone. The microstructure was partitioned based on the grain orientation spread and grain size values to separate the recrystallized fraction from the deformed region in order to understand the micromechanism of grain refinement. The texture of both deformed and recrystallized regions are similar in nature. Microstructure and texture analysis suggest that the restoration processes are different in different regions of the processed sample. The transition region between nugget zone and TMAZ exhibits large elongated grains surrounded by fine equiaxed grains of different orientation which indicate the process of discontinuous dynamic recrystallization. Within the nugget zone, similar texture between deformed and recrystallized grain fraction suggests that the restoration mechanism is a continuous process.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Microstructure and mechanical properties of as-cast and heat-treated Mg-12.3Zn-5.8Y-1.4Al (ZYA1261) alloy were investigated. The phase compositions of the as-cast alloy are alpha-Mg, Mg3YZn6 (I-phase), Mg(3)y(2)Zn(3) (W-phase), Mg12YZn (Z-phase), Mg24Y5, MgZn and a small quantity of Al-containing phase.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The Mg-8.31Gd-1.12Dy-0.38Zr (mass%) alloy was prepared by casting technology, and the microstructure, age hardening behavior and mechanical property have been investigated. It is noted that the alpha-Mg and the different Mg-RE (RE = Gd/Dy) compounds are subsistent in the as-cast and annealed state samples. The age hardening behavior is observed during the investigated temperature range, and the alloy exhibits high Vickers hardness, excellent ultimate tensile strength and yield strength at peak hardness.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Microstructure and mechanical properties of peak-aged Mg-4.5Zn-xGd (x=0, 0.5, 1.0 and 1.5 wt.%) alloys have been investigated. The results showed that the grain size of the alloys was refined gradually with increasing Gd. Mg5Gd and Mg3Gd2Zn3 phases were found in the Gd-containing alloys. The strengths were greatly improved with Gd additions, and the highest strength level was obtained in the Mg-4.5Zn-1.5Gd alloy, in which the ultimate tensile strength and yield strength were 231 MPa and 113 MPa, respectively.