957 resultados para Fracture-Toughness


Relevância:

70.00% 70.00%

Publicador:

Resumo:

The mode I fracture toughness of concrete can be experimentally determined using three point bend beam in conjunction with digital image correlation (DIC). Three different geometrically similar sizes of beams are cast for this study. To study the influence of fly ash and silica fume on fracture toughness of SCC, three SCC mixes are prepared with and without mineral additions. The scanning electron microscope (SEM) images are taken on the fractured surface to add information on fracture process in SCC. From this study, it is concluded that the fracture toughness of SCC with mineral addition is higher when compared to those without mineral addition.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Inspired by the Brazilian disk geometry we examine the utility of an edge cracked semicircular disk (ECSD) specimen for rapid assessment of fracture toughness of brittle materials using compressive loading. It is desirable to optimize the geometry towards a constant form factor F for evaluating K-I. In this investigation photoelastic and finite element results for K-I evaluation highlight the effect of loading modeled using a Hertzian. A Hertzian loading subtending 4 degrees at the center leads to a surprisingly constant form factor of 1.36. This special case is further analyzed by applying uniform pressure over a chord for facilitating testing.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Among various biologically compatible materials, hydroxyapatite (HA) has excellent bioactivity/osteointegration properties and therefore has been extensively investigated for biomedical applications. However, its inferior fracture toughness limits the wider applications of monolithic HA as a load-bearing implant. To this end, HA-based biocomposites have been developed to improve their mechanical properties (toughness and strength) without compromising biocompatibility. Despite significant efforts over last few decades, the toughness of HA-based composites could not be enhanced beyond 1.5-2 MPa m(1/2), even when measured using indentation techniques. In this perspective, the present work demonstrates how spark plasma sintering can be effectively utilized to develop hydroxyapatite titanium (HA-Ti) composites with varying amounts of Ti (5, 10 and 20 wt.%) with extremely high single edge V-notch beam fracture toughness (4-5 MPa m(1/2)) along with a good combination of elastic modulus and flexural strength. Despite predominant retention of HA and Ti, the combination of critical analysis of X-ray diffraction and transmission electron microscopy investigation confirmed the formation of the CaTi4(PO4)(6) phase with nanoscale morphology at the HA/Ti interface and the formation of such a phase has been discussed in reference to possible sintering reactions. The variations in the measured fracture toughness and work of fracture with Ti addition to the HA matrix were further rationalized using the analytical models of crack bridging as well as on the basis of the additional contribution from crack deflection. The present work opens up the opportunity to further enhance the toughness beyond 5 MPa m(1/2) by microstructural designing with the desired combination of toughening phases. (C) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

This article presents the details of estimation of fracture parameters for high strength concrete (HSC, HSC1) and ultra high strength concrete (UHSC). Brief details about characterization of ingredients of HSC, HSC1 and UHSC have been provided. Experiments have been carried out on beams made up of HSC, HSC1 and UHSC considering various sizes and notch depths. Fracture characteristics such as size independent fracture energy (G(f)), size of fracture process zone (C-f), fracture toughness (K-IC) and crack tip opening displacement (CTODc) have been estimated based on the experimental observations. From the studies, it is observed that (i) UHSC has high fracture energy and ductility inspite of having a very low value of C-f; (ii) relatively much more homogeneous than other concretes, because of absence of coarse aggregates and well-graded smaller size particles; (iii) the critical SIF (K-IC) values are increasing with increase of beam depth and decreasing with increase of notch depth. Generally, it can be noted that there is significant increase in fracture toughness and CTODc. They are about 7 times in HSC1 and about 10 times in UHSC compared to those in HSC; (iv) for notch-to-depth ratio 0.1, Bazant's size effect model slightly overestimates the maximum failure loads compared to experimental observations and Karihaloo's model slightly underestimates the maximum failure loads. For the notch-to-depth ratio ranging from 0.2 to 0.4 for the case of UHSC, it can be observed that, both the size effect models predict more or less similar maximum failure loads compared to corresponding experimental values.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

In this work, the fracture behavior of magnesium single crystals is studied by conducting experiments with notched three point bend specimens of three crystallographic orientations. In the first and second orientations, the c-axis is along the normal to the flat surface of the notch, while in the third it is aligned with the notch front. For all the orientations, in situ electron back scattered diffraction observations made around the notch root show profuse tensile twinning of {10 (1) over bar2} type. Further, in the first two orientations basal and prismatic slip traces are identified from optical metallography. The width of the most prominent twin saturates at around 120-150 mu m, while twins continue to nucleate farther away to accommodate plastic deformation. In all the orientations, crack initiation occurs before the attainment of peak load and the crack grows stably along twin-matrix interface before deflecting at twin-twin intersections. Results show that profuse tensile twinning is an important energy dissipating mechanism that enhances the fracture toughness. (C) 2013 Elsevier B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Free-standing Pt-aluminide (PtAl) bond coats exhibit a linear stress strain response under tensile loading and undergo brittle cleavage fracture at temperatures below the brittle-to-ductile transition temperature (BDTT). Above the BDTT, these coatings show yielding and fail in a ductile manner. In this paper, the various micromechanisms affecting the tensile fracture stress (FS) below the BDTT and yield strength (YS) above the BDTT in a PtAl bond coat have been ascertained and quantified at various temperatures. The micromechanisms have been identified by carrying out microtensile testing of stand-alone PtAl coating specimens containing different levels of Pt at temperatures between room temperature and 1100 degrees C and correlation of the corresponding fracture mechanisms with the deformation substructure in the coating. An important aspect of the influence of Pt on the tensile behavior, slip characteristics, FS/YS and BDTT in the PtAl coating has also been examined. The addition of Pt enhances the FS of the coating by Pt solid solution strengthening and imparts a concomitant increase in fracture toughness and yet causes a significant increase in the BDTT of the coating. Published by Elsevier Ltd. on behalf of Acta Materialia Inc.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

When dropped, electronic packages often undergo failure by propagation of an interfacial crack in solder joints under a combination of tensile and shear loading. Hence, it is crucial to understand and predict the fracture behavior of solder joints under mixed-mode high-rate loading conditions. In this work, the effects of the loading conditions (strain rate and loading angle) and microstructure interfacial intermetallic compound (IMC) morphology and solder yield strength] on the mixed-mode fracture toughness of Sn-3.8 wt.%Ag-0.7 wt.%Cu solder joints sandwiched between two Cu substrates with electroless nickel immersion gold (ENIG) metallization have been studied, and compared with the fracture behavior of joints attached to bare Cu. Irrespective of the surface finish, the fracture toughness of the solder joints decreased monotonically with strain rate and mode-mixity, both resulting in increased fracture proportion through the interfacial IMC layer. Furthermore, the proportion of crack propagation through the interfacial IMC layer increased with increase in the thickness and the roughness of the interfacial IMC layer and the yield strength of the solder, resulting in a decrease in the fracture toughness of the joint. However, under most conditions, solder joints with ENIG finish showed higher resistance to fracture than joints attached directly to Cu substrates without ENIG metallization. Based on the experimental observations, a fracture mechanism map is constructed correlating the yield strength of the solder, the morphology and thickness of the interfacial IMC, and the fracture mechanisms as well as the fracture toughness values for different solder joints under mode I loading.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

In this work, Mode-I fracture experiments are conducted using notched compact tension specimens machined from a rolled AZ31 Mg alloy plate having near-basal texture with load applied along rolling direction (RD) and transverse direction (TD). Moderately high notched fracture toughness of J(C) similar to 46 N/mm is obtained in both RD and TD specimens. Fracture surface shows crack tunneling at specimen mid-thickness and extensive shear lips near the free surface. Dimples are observed from SEM fractographs suggesting ductile fracture. EBSD analysis shows profuse tensile twinning in the ligament ahead of the notch. It is shown that tensile twinning plays a dual role in enhancing the toughness in the notched fracture specimens with reduced triaxiality. It provides significant dissipation in the background plastic zone and imparts hardening to the material surrounding the fracture process zone via operation of several mechanisms which retards micro-void growth and coalescence. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The influence of Pt layer thickness on the fracture behavior of PtNiAl bond coats was studied in situ using clamped micro-beam bend tests inside a scanning electron microscope (SEM). Clamped beam bending is a fairly well established micro-scale fracture test geometry that has been previously used in determination of fracture toughness of Si and PtNiAl bond coats. The increasing amount of Pt in the bond coat matrix was accompanied by several other microstructural changes such as an increase in the volume fraction of alpha-Cr precipitate particles in the coating as well as a marginal decrease in the grain size of the matrix. In addition, Pt alters the defect chemistry of the B2-NiAl structure, directly affecting its elastic properties. A strong correlation was found between the fracture toughness and the initial Pt layer thickness associated with the bond coat. As the Pt layer thickness was increased from 0 to 5 mu m, resulting in increasing Pt concentration from 0 to 14.2 at.% in the B2-NiAl matrix and changing alpha-Cr precipitate fraction, the initiation fracture toughness (K-IC) was seen to rise from 6.4 to 8.5 MPa.m(1/2). R-curve behavior was observed in these coatings, with K-IC doubling for a crack propagation length of 2.5 mu m. The reasons for the toughening are analyzed to be a combination of material's microstructure (crack kinking and bridging due to the precipitates) as well as size effects, as the crack approaches closer to the free surface in a micro-scale sample.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Essential work of fracture (EWF) analysis is used to study the effect of the silica doping level on fracture toughness of polyimide/silica (PI/SiO2) hybrid films. By using double-edge-notched-tension (DENT) specimens with different ligament lengths, it seems that the introduction of silica additive can improve the specific essential work of fracture (w (e) ) of PI thin films, but the specific non-essential work of fracture (beta w (p) ) will decease significantly as the silica doping level increasing from 1 to 5 wt.%, and even lower than that of neat PI. The failure process of the fracture is investigated with online scanning electron microscope (SEM) observation and the parameters of non-essential work of fracture, beta and w (p) , are calculated based on finite element (FE) method.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Mode I steady-state crack growth is analyzed under plane strain conditions in small scale yielding. The elastic-plastic solid is characterized by the mechanism-based strain gradient (MSG) plasticity theory [J. Mech. Phys. Solids 47 (1999) 1239, J. Mech. Phys. Solids 48 (2000) 99]. The distributions of the normal separation stress and the effective stress along the plane ahead of the crack tip are computed using a special finite element method based on the steady-state fundamental relations and the MSG flow theory. The results show that during the steady-state crack growth, the normal separation stress on the plane ahead of the crack tip can achieve considerably high value within the MSG strain gradient sensitive zone. The results also show that the crack tip fields are insensitive to the cell size parameter in the MSG theory. Moreover, in the present research, the steady-state fracture toughness is computed by adopting the embedded process zone (EPZ) model. The results display that the steady-state fracture toughness strongly depends on the separation strength parameter of the EPZ model and the length scale parameter in the MSG theory. Furthermore, in order for the results of steady crack growth to be comparable, an approximate relation between the length scale parameters in the MSG theory and in the Fleck-Hutchinson strain gradient plasticity theory is obtained.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Crack propagation and strain field evolution in two metallic glassy ribbons are studied using in situ scanning electron microscopy and the white digital speckle correlation method. Strain state at the crack tip, which depends heavily on the fracture toughness, plays a key role in fracture. A high degree of shear strain concentration in tough glassy ribbon can satisfy the critical shear strain, resulting in shear fracture, whereas a high degree of linear strain concentration in brittle glassy ribbon can initiate normal tensile fracture. (C) 2008 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

A complete development for the higher-order asymptotic solutions of the crack tip fields and finite element calculations for mode I loading of hardening materials in plane strain are performed. The results show that in the higher-order asymptotic solution (to the twentieth order), only three coefficients are independent. These coefficients are determined by matching with the finite element solutions carried out in the present paper (our attention is focused on the first five terms of the higher-order asymptotic solution). We obtain an analytic characterization of crack tip fields, which conform very well to the finite element solutions over wide range. A modified two parameter criterion based on the asymptotic solution of five terms is presented. The upper bound and lower bound fracture toughness curves predicted by modified two parameter criterion are given. These two curves agree with most of the experimental data and fully capture the proper trend.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The fracture toughness and fatigue fracture behaviour of carbon-fiber-reinforced modified bismaleimide (BMI) composites have been studied. These composites were found to have higher fracture toughnes, better damage tolerance and longer fatigue life than carbon-fiber composites with epoxy matrices. Delamination is the major mode of failure in fatigue and it is controlled by the properties of the matrix and interface. The improved performance is dire to the presence of thermoplastic particles in the modified BMI matrix which gives rise to enhanced fiber/matrix adhesion and more extensive plastic deformation. The fatigue behaviour also depends on the stacking sequence, with the multidirectional [45/90/-45/0] fiber-reinforced modified BMI composite having a lower crack propagation rate and longer fatigue life than the unidirectional laminate. This arises because of the constraint on the damage processes due to the different fiber orientation in the plies.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Amorphous metals that form fully glassy parts over a few millimeters in thickness are still relatively new materials. Their glassy structure gives them particularly high strengths, high yield strains, high hardness values, high resilience, and low damping losses, but this can also result in an extremely low tolerance to the presence of flaws in the material. Since this glassy structure lacks the ordered crystal structure, it also lacks the crystalline defect (dislocations) that provides the micromechanism of toughening and flaw insensitivity in conventional metals. Without a sufficient and reliable toughness that results in a large tolerance of damage in the material, metallic glasses will struggle to be adopted commercially. Here, we identify the origin of toughness in metallic glass as the competition between the intrinsic toughening mechanism of shear banding ahead of a crack and crack propagation by the cavitation of the liquid inside the shear bands. We present a detailed study over the first three chapters mainly focusing on the process of shear banding; its crucial role in giving rise to one of the most damage-tolerant materials known, its extreme sensitivity to the configurational state of a glass with moderate toughness, and how the configurational state can be changed with the addition of minor elements. The last chapter is a novel investigation into the cavitation barrier in glass-forming liquids, the competing process to shear banding. The combination of our results represents an increased understanding of the major influences on the fracture toughness of metallic glasses and thus provides a path for the improvement and development of tougher metallic glasses.