951 resultados para Diamond bur
Resumo:
Ultrafine diamond (UFD) was synthesized under high pressure and high temperatures generated by explosive detonation. The structure, composition, surface and thermal stability of UFD were studied by use of XRD, TEM, Raman Spectroscopy, FTIR, etc. The influences of the synthesis conditions and purification conditions on the properties of UFD were analyzed. The UFD had an average size of 4-6 nm, commonly exhibiting a spherical shape. The highest yield was of up to 10 mass% of the explosive. Attempts were made to use UFD as an additive to metal-diamond sintering and as crystallite seeds of CVD diamond films. The results show that UFD can decrease the coefficient of friction of the composite by 30%, and raise the nucleation density in CVD diamond films by 2-3 times.
Resumo:
The diamond-like carbon (DLC) films with different thicknesses on 9Crl8 bearing steels were prepared using vacuum magnetic-filtering arc plasma deposition. Vickers indentation. nanoin-dentation and nanoscratch tests were used to characterize the DLC films with a wide range of applied loads. Mechanical and tribological behaviors of these submicron films were investigated and interpreted. The hardnesses of 9Crl8 and DLC, determined by nanoindentation, are approximately 8GPa and 60GPa respectively; their elastic moduli are approximately 25OGPa and 600GPa respectively. The friction coefficients of 9Crl8, DLC. organic coating, determined by nanoscratch, are approximately 0. 35, 0. 20 and 0. 13 respectively. It is demonstrated that nanoindentation and nanoscratch tests can provide more information about the near-surface elastic-plastic deformation, friction and wear properties. The correlation of mechanical properties and scratch resistance of DLC films on 9Crl8 steels can provide an assessment for the load-carrying capacity and wear resistance
Resumo:
A new DC plasma torch in which are jet states and deposition parameters can be regulated over a wide range has been built. It showed advantages in producing stable plasma conditions at a small gas flow rate. Plasma jets with and without magnetically rotated arcs could be generated. With straight are jet deposition, diamond films could be formed at a rate of 39 mu m/h on Mo substrates of Phi 25 mm, and the conversion rate of carbon in CH4 to diamond was less than 3%. Under magnetically rotated conditions, diamond films could be deposited uniformly in a range of Phi 40 mm at 30 mu m/h, with a quite low total gas flow rate and high carbon conversion rate of over 11%. Mechanisms of rapid and uniform deposition of diamond films with low gas consumption and high carbon transition efficiency are discussed.
Resumo:
A novel normally closed microcage has been fabricated and characterized. This device was made from a highly compressively stressed diamond like carbon (DLC) and electroplated Ni bimorph structure. The large stress in the DLC causes the bimorph layer to curve once it is released from the substrate. The radius of curvature is in the range of 18 - 50μm, and can be controlled by varying the DLC and the Ni thicknesses. The devices can be operated in a pulsed mode current with low operation temperature, and can be opened by ∼60μm laterally with a power consumption of only ∼16mW. © 2004 IEEE.
Resumo:
Multi-finger, normally-closed microgrippers made from a bilayer of a metal and diamond-like carbon (DLC) or a trilayer of a polymer, metal and DLC have been analysed, simulated and fabricated. Temperatures of ∼700 K are necessary to open Ni/DLC bimorph structures. Microgrippers made from an SU8/DLC bilayer or SU8/Al/DLC trilayer have also been fabricated, and fully closed microcages with diameters of ∑40 μm have been obtained. Using SU8 reduces the opening temperature of these devices to only ∼400 K.
Resumo:
By means of Tersoff and Morse potentials, a three-dimensional molecular dynamics simulation is performed to study atomic force microscopy cutting on silicon monocrystal surface. The interatomic forces between the workpiece and the pin tool and the atoms of workpiece themselves are simulated. Two partial edge dislocations are introduced into workpiece Si, it is found that the motion of dislocations does not occur during the atomic force microscopy cutting processing. Simulation results show that the shear stress acting on dislocations is far below the yield strength of Si. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
By means of Tersoff and Morse potentials, a three-dimensional molecular dynamics simulation is performed to study atomic force microscopy cutting on silicon monocrystal surface. The interatomic forces between the workpiece and the pin tool and the atoms of workpiece themselves are calculated. A screw dislocation is introduced into workpiece Si. It is found that motion of dislocations does not occur during the atomic force microscopy cutting processing. Simulation results show that the shear stress acting on dislocation is far below the yield strength of Si.