994 resultados para Combustion synthesis
Resumo:
ZrMo2O8 was synthesized via two routes, namely, the traditional solid-state method and the solution combustion method. The compounds were characterized by powder X-ray diffraction, UV−visible spectroscopy, scanning electron microscopy, and transmission electron microscopy. The crystals belong to a trigonal crystal system, space group P 1c (No. 163) with a = 10.1391(6) Å, c = 11.7084(8) Å, and Z = 6. The band gap of the compounds was around 2.7 eV, and DFT calculations suggest the indirect nature of the band gap. The irregular MoO4 tetrahedra create a dipole and inhibit the process of electron−hole recombination, thereby making the material photoactive. The photocatalytic activity of the compounds prepared by both routes has been investigated for the degradation of various dyes under UV irradiation, and this showed the specificity of the compounds towards the degradation of non-anthraquinonic dyes.
Resumo:
Polymeric peroxides have received renewed attention in the recent past, in view of some significant explorations of their physical and chemical properties. The potential of polymeric peroxides as a class, as specialized fuel, and the need to synthesize such new materials have been reported in the literature. So far, this class of polymers is constituted only by a dozen or so polyperoxides. From the point of view of their use in propellant applications, the importance lies in making materials which are easy to handle etc., unlike the earlier reported poly(styrene peroxide) (PSP), a sticky semi-solid mass. However, judging from the better combustion characteristics, exploring aromatic monomers was thought worthwhile. In this preliminary communication, the synthesis of a new polymeric peroxide made from 1,4-divinylbenzene is reported. The polymer obtained was in powder form and had an exothermic heat of degradation approximately equal to that of PSP. 4 ref.--AA
Resumo:
CaSiO3 : Dy3+ (1-5 mol. %) nanophosphors were synthesized by a simple low-temperature solution combustion method. Powder X-ray diffraction patterns revealed that the phosphors are crystalline and can be indexed to a monoclinic phase. Scanning electron micrographs exhibited faceted plates and angular crystals of different sizes with a porous nature. Photoluminescence properties of the Dy3+-doped CaSiO3 phosphors were observed and analyzed. Emission peaks at 483, 573 and 610 nm corresponding to Dy3+ were assigned as F-4(9/2)-> H-6(15/2), F-4(9/2) -> H-6(13/2) and F-4(9/2) -> H-6(11/2) transitions, respectively, and dominated by the Dy3+ F-4(9/2) -> H-6(13/2) hyperfine transition. Experimental results revealed that the luminescence intensity was affected by both heat treatment and the concentration of Dy3+ (1-5 mol. %) in the CaSiO3 host. Optimal luminescence conditions were achieved when the concentration of Dy3+ was 2 mol. %. UV-visible absorption features an intense band at 240 nm, which corresponds to an O-Si ligand-to-metal charge transfer band in the SiO32- group. The optical energy band gap for the undoped sample was found to be 5.45 eV, whereas in Dy3+-doped phosphors it varies in the range 5.49-5.65 eV. The optical energy gap widens with increase of Dy3+ ion dopant.
Resumo:
Transition metal sulfite hydrazine hydrates, MSO3·xN2H4·yH2O whereM=Mn, Fe, Co, Ni and Zn have been prepared and characterized by chemical analysis, infrared spectra, thermoanalytical and combustion studies. The colours,x andy parameters of the complexes varied depending upon the preparation conditions. Thermal decomposition characteristics differ from metal to metal yielding metal oxides at relatively low temperatures.Mittels chemischer Analyse, IR-Spektren, thermoanalytischen und Verbrennungsstudien wurden die Hydrazinhydrate der hergestellten Übergangsmetallsulfite MSO3·xN2H4·yH2O mitM=Mn, Fe, Co, Ni und Zn beschrieben. Farbe sowie die Parameterx undy der Komplexe hängen von den Herstellungsbedingungen ab. Die thermische Zersetzung, bei der bei relativ niedrigen Temperaturen Metalloxide entstehen, ist von Metall zu Metall verschieden.
Resumo:
Spherical and rod like nanocrystalline Nd2O3 phosphors have been prepared by solution combustion and hydrothermal methods respectively The Powder X-ray diffraction (PXRD) results confirm that hexagonal A-type Nd2O3 has been obtained with calcination at 900 C for 3 h and the lattice parameters have been evaluated by Rietveld refinement Surface morphology of Nd2O3 phosphors show the formation of nanorods in hydrothermal synthesis whereas spherical particles in combustion method TEM results also confirm the same Raman studies show major peaks which are assigned to F-g and combination of A(g) + E-g modes The PL spectrum shows a series of emission bands at similar to 326-373 nm (UV) 421-485 nm (blue) 529-542 nm (green) and 622 nm (red) The UV blue green and red emission in the PL spectrum indicates that Nd2O3 nanocrystals are promising for high performance materials and white light emitting diodes (LEDs) (C) 2010 Elsevier B V All rights reserved
Resumo:
Diamond crystallites were synthesized using various oxygen‐hydrocarbon flames. The flames have been profiled in real time using a nonintrusive diagnostic technique. Optical emission spectra for different zones have been recorded and the active species identified. Diamond growth was observed only in the thermodynamically unequilibriated primary combustion zone of the flames. Carbon‐bearing species, atomic hydrogen, and atomic oxygen, noted to be critical for diamond growth, were observed in the flames. The diamond growth was confirmed by x‐ray diffraction, laser‐Raman analysis, and scanning electron microscopy. The study offers the first insight into the flame spectra in the context of diamond synthesis at atmospheric pressures.
Resumo:
CaSiO3:Eu3+ (1-5 mol%) red emitting phosphors have been synthesized by a low-temperature solution combustion method. The phosphors have been well characterized by powder X-ray diffraction (PXRD), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM) and optical spectroscopy. PXRD patterns reveal monoclinic CaSiO3 phase can be obtained at 900 degrees C. The SEM micrographs show the crystallites with irregular shape, mostly angular. Upon 254 nm excitation, the phosphor show characteristic fluorescence D-5(0) -> F-7(J) (J = 0, 1, 2, 3, 4) of the Eu3+ ions. The electronic transition located at 614 nm corresponding to D-5(0) -> F-7(2) of Eu3+ ions, which is stronger than the magnetic dipole transition located at 593 nm corresponding to D-5(0) -> F-7(1) of Eu3+ ions. Different pathways involved in emission process have been studied. Concentration quenching has been observed for Eu3+ concentration >4 mol%. UV-visible absorption shows an intense band at 240 nm in undoped and 270 nm in Eu3+ doped CaSiO3 which is attributed to oxygen to silicon (O-Si) ligand-to-metal charge-transfer (LMCT) band in the SiO32- group. The optical energy band gap is widened with increase of Eu3+ ion dopant. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Tialite, beta-Al2TiO5, a low expansion material, has been synthesised by the combustion of corresponding metal nitrates and carbohydrazide (CH) or urea redox mixtures at 500-degrees-C. As prepared powders contained tialite, rutile, and corundum in the mole ratios of 50:25:25 (CH) and 20:40:40 (urea). The combustion derived powders, when calcined 30 min at 1300-degrees-C, gave single phase beta-tialite having a surface area of 20-25 m2 g-1 and a particle size of 0.79-1.03 mum.
Resumo:
Red, blue and green emitting lamp phosphors such as EU(3+) doped Y2O3 (red phosphor), EU(2+) doped Ba0.64Al12O18.64, BaMgAl10O17 and BaMg2Al16O27 (blue phosphors) and Ce0.67Tb0.33MgAl11O19 and Eu2+, Mn2+ doped BaMgAl10O17 (green phosphors) have been prepared by the combustion of the corresponding metal nitrates (oxidizer) and oxalyl dihydrazide/urea/carbohydrazide (fuel) mixtures at 400 degrees-500 degrees C within 5 min. The formation of these phosphors has been confirmed by their characteristic powder X-ray diffraction patterns and fluorescence spectra. The phosphors showed characteristic emission bands at 611 nm (red emission), 430-450 nm (blue emission) and 515-540 nm (green emission). The fine-particle nature of the combustion derived phosphors has been investigated using powder density, particle size and BET surface area measurements.
Resumo:
A new class of epoxy resins having N-N bonds in their structure has been synthesized by reacting N,N'-aliphatic dicarboxyl bis(hydrazones) (the aldehyde/ketone derivatives of malonic, adipic, and sebacic dihydrazides) with epichlorohydrin. The reactivity of the[GRAPHICS] protons as a function of the substituent group and the number of methylene spacer groups present in the hydrazone has been examined. The resins obtained have been characterized by elemental and epoxy equivalent analyses and IR and NMR spectra. All these resins are found to have adequate viscosity and cure easily with amine curatives at elevated temperatures. Relevant properties for their use as binders in propellant formulations, such as thermal stability, heat of combustion, density, temperature dependence of viscosity, and mechanical strength of the composites, have been evaluated. (C) 1997 John Wiley & Sons, Inc.
Resumo:
Fine particle strontium substituted lanthanum ferrites La1-xSrxFeO3, where x = 0.0-1.0, have been synthesized by the solution combustion method using corresponding metal nitrates, oxalyl dihydrazide (ODH) or tetra formal tris azine (TFTA). Formation of La1-xSrxFeO3 was confirmed by the XRD and the fine particle nature of the ferrites investigated using SEM, particle size analysis and BET surface area measurements. La1-xSrxFeO3 (up to x = 0-0.4) exhibited low resistivity near the Neel temperatures. La1-xSrxFeO3 with x greater than or equal to 0.8 when used as bifunctional electrodes, showed oxygen evolution and reduction activity comparable with the orthoferrites prepared by the conventional solid state method. (C) 1999 Elsevier Science B.V. All rights reserved.
Resumo:
Fine particles of willemite, alpha -Zn2SiO4, were prepared by both solution combustion and sol-gel methods. Both processes yield single-phase, large-surface area (26- and 78-m(2)/g), sinteractive willemite powders. Thermal evolution of crystalline phases was studied using X-ray powder diffraction patterns. The combustion method favors low-temperature formation of willemite compared to the sol-gel method. The powders, when uniaxially pressed and sintered at 1300 degreesC, achieved 78-80% theoretical density. The microstructures of the sintered body show the presence of equiaxed 0.5- to 4-mum grains. Blue pigments of willemite doped with Co2+ and Ni2+ were also prepared by the combustion process.
Synthesis, Structure, Negative Thermal Expansion, and Photocatalytic Property of Mo Doped ZrV(2)O(7)
Resumo:
A new series of compounds identified in the phase diagram of ZrO(2)-V(2)O(8)-MoO(3) have been synthesized via the solution combustion method. Single crystals of one of the compounds in the series, ZrV(1.50)Mo(0.50)O(7.25), were grown by the melt-cool technique from the starting materials with double the MoO(3) quantity. The room temperature average crystal structure of the grown crystals was solved using the single crystal X-ray diffraction technique. The crystals belong to the cubic crystal system, space group Pa (3) over bar (No. 205) with a = 8.8969 (4) angstrom, V = 704.24 (6) angstrom(3), and Z = 4. The final R(1) value of 0.0213 was achieved for 288 independent reflections during the structure refinement. The Zr(4+) occupies the special position (4a) whereas V(5+) and Mo(6+) occupy two unique (8c) Wyckoff positions. Two fully occupied O atoms, (24d) and (4b), one partially occupied 0 atom (8c) have been identified for this molybdovanadate, which is a unique feature for these crystals. The structure is related to both ZrV(2)O(7) and cubic ZrMo(2)O(8). The temperature dependent single crystal studies show negative thermal expansion above 370 K. The compounds have been characterized by powder X-ray diffraction, solid-state UV-vis diffuse reflectance spectra, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The photocatalytic activity of these compounds has been investigated for the degradation of various dyes, and these compounds show specificity toward the degradation of non-azoic dyes.
Resumo:
Microwave-based methods are widely employed to synthesize metal nanoparticles on various substrates. However, the detailed mechanism of formation of such hybrids has not been addressed. In this paper, we describe the thermodynamic and kinetic aspects of reduction of metal salts by ethylene glycol under microwave heating conditions. On the basis of this analysis, we identify the temperatures above which the reduction of the metal salt is thermodynamically favorable and temperatures above which the rates of homogeneous nucleation of the metal and the heterogeneous nucleation of the metal on supports are favored. We delineate different conditions which favor the heterogeneous nucleation of the metal on the supports over homogeneous nucleation in the solvent medium based on the dielectric loss parameters of the solvent and the support and the metal/solvent and metal/support interfacial energies. Contrary to current understanding, we show that metal particles can be selectively formed on the substrate even under situations where the temperature of the substrate Is lower than that of the surrounding medium. The catalytic activity of the Pt/CeO(2) and Pt/TiO(2) hybrids synthesized by this method for H(2) combustion reaction shows that complete conversion is achieved at temperatures as low as 100 degrees C with Pt-CeO(2) catalyst and at 50 degrees C with Pt-TiO(2) catalyst. Our method thus opens up possibilities for rational synthesis of high-activity supported catalysts using a fast microwave-based reduction method.
Resumo:
Gd2O3:Eu3+ (4 mol%) co-doped with Bi3+ (Bi = 0, 1, 3, 5, 7, 9 and 11 mol%) ions were synthesized by a low-temperature solution combustion method. The powders were calcined at 800A degrees C and were characterized by powder X-ray diffraction (PXRD), transmission electron microscopy (TEM), Fourier transform infrared and UV-Vis spectroscopy. The PXRD profiles confirm that the calcined products were in monoclinic with little cubic phases. The particle sizes were estimated using Scherrer's method and Williamson-Hall plots and are found to be in the ranges 40-60 nm and 30-80 nm, respectively. The results are in good agreement with TEM results. The photoluminescence spectra of the synthesized phosphors excited with 230 nm show emission peaks at similar to 590, 612 and 625 nm, which are due to the transitions D-5(0)-> F-7(0), D-5(0)-> F-7(2) and D-5(0)-> F-7(3) of Eu3+, respectively. It is observed that a significant quenching of Eu3+ emission was observed under 230 nm excitation when Bi3+ was co-doped. On the other hand, upon 350 nm excitation, the luminescent intensity of Eu3+ ions was enhanced by incorporation of Bi3+ (5 mol%) ions. The introduction of Bi3+ ions broadened the excitation band of Eu3+ of which a new strong band occurred ranging from 320 to 380 nm. This has been attributed to the 6s(2)-> 6s6p transition of Bi3+ ions, implying a very efficient energy transfer from Bi3+ ions to Eu3+ ions. The gamma radiation response of Gd2O3:Eu3+ exhibited a dosimetrically useful glow peak at 380A degrees C. Using thermoluminescence glow peaks, the trap parameters have been evaluated and discussed. The observed emission characteristics and energy transfer indicate that Gd2O3:Eu3+, Bi3+ phosphors have promising applications in solid-state lighting.