974 resultados para Carbon Black
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Ciência dos Materiais - FEIS
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
High-density polyethylene (HDPE) water-proof membranes are used as coatings in vinasse (leachate from sugar cane) storage tanks. The leachate is pumped into the tanks at temperatures of 80-90 °C. Due to these high temperatures and acidity of the waste, these membranes can be degraded, cracked and then loose the function for which they have been designed. This may cause contamination of the soil and groundwater. This study evaluated the effect of vinasse in HDPE membranes after 4 months of exposure in a controlled environment. An aggressive, alkaline pH liquid (sodium hydroxide) was also used. The objective was to evaluate the membrane resistance in contact with acidic and alkaline residues. Physical and mechanical tests, measurement of the carbon black content and thermo gravimetric analysis (TGA) were used to determine degradation of polymer membranes after chemical immersion. While sodium hydroxide resulted caused only minor changes in the physical properties, vinasse induced a thickness change of 7.8%. With immersion in vinasse, an average decrease in strength and deformability (yield) of 34% and 23.5% were measured, respectively. The stiffness increased by 7.8% (average) and the tear strength decreased by 2.7% (average).
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Three nanostructured platinum-niobium supported on Vulcan XC-72R carbon black materials were prepared as catalysts for the ethanol electroxidation: (i) deposition of platinum and niobium on Vulcan XC-72R carbon black, (ii) platinum decorated on a mixture of commercial amorphous Nb2O5/carbon black, and (iii) the same than ii but using crystalline Nb2O5, by reduction of the precursors with sodium borohydride in ethanol. All the catalysts showed platinum crystal sizes in the range of 3-4 nm, with no or little modification of the lattice parameter. The analyses of the electronic structure from the XANES region of the XAS spectra displayed some interactions between platinum and niobium, despite the niobium was primarily in the form of pentoxide in all the catalysts. CO stripping exhibited a promising low onset potential and a large current density, especially in the case of the deposited catalyst. Ethanol electroxidation experiments revealed that the Pt-Nb(2)O(5)crystalline/C generated the largest current. However it was not effective to completely oxidize ethanol, leading to acetic acid as the main product. In this sense, the highest efficiency for the complete oxidation of ethanol was obtained for the deposited catalyst. These results were interpreted in terms of the physico-chemical characteristic displayed by the different catalysts. (C) 2012 The Electrochemical Society. [DOI: 10.1149/2.040210jes] All rights reserved.
Resumo:
DEVELOPMENT AND EVALUATION OF GAS DIFFUSION ELECTRODES (GDE) FOR GENERATION OF H2O2 IN SITU AND THEIR APPLICATION IN THE DEGRADATION OF REACTIVE BLUE 19 DYE. This work reports the development of GDE for electrogeneration of H2O2 and their application in the degradation process of Reactive Blue 19 dye. GDE produced by carbon black with 20% polytetrafluoroethylene generated up to 500 mg L-1 of H2O2 through the electrolysis of acidic medium at -0.8 V vs Ag/AgCl. Reactive Blue 19 dye was degraded most efficiently with H2O2 electrogenerated in the presence of Fe(II) ions, leading to removal of 95% of the original color and 39% of TOC at -0.8 V vs Ag/AgCl.
Resumo:
Microwave devulcanization has been studied as a method for elastomer recycling, which is based on the conversion of the reticulated and infusible structure of thermosetting rubbers in free polymeric chains able to be remolded by thermomechanical processing in recycling operations for the manufacture of other products. Elastomeric wastes are often irregularly discarded in nature, producing serious environmental damage, and their mechanical recycling is still considered a challenge. Thus, the development of alternatives for elastomer recycling is directly related to the actions of sustainable development and economic benefits to companies that pay to discard their wastes. The aim of this work is to evaluate the chemical modifications occurring in styrene butadiene rubber (SBR) after microwave devulcanization. Compounds of SBR were vulcanized in the presence of vulcanization agents and variable amounts of carbon black, and then the rubbers were milled and submitted to microwave treatment. Only the SBR with high carbon black content shows some portion of devulcanized material. However, the rubber with lower content of carbon black which was devulcanized by microwave radiation shows an increase in cross-link density. The microwave treatment also causes cross-link breaks mainly in polysulfidic bonds as well as decomposition of chemical groups containing sulfur attached to the chemical structure of SBR, while. the chemical bonds of higher energy such as monosulfidic bonds remain preserved. The improvement of the microwave method for rubber devulcanization represents a way for viable recycling of thermosetting rubbers.
Resumo:
Background: Exposure to fine fractions of particulate matter (PM2.5) is associated with increased hospital admissions and mortality for respiratory and cardiovascular disease in children and the elderly. This study aims to estimate the toxicological risk of PM2.5 from biomass burning in children and adolescents between the age of 6 and 14 in Tangara da Serra, a municipality of Subequatorial Brazilian Amazon. Methods: Risk assessment methodology was applied to estimate the risk quotient in two scenarios of exposure according to local seasonality. The potential dose of PM2.5 was estimated using the Monte Carlo simulation, stratifying the population by age, gender, asthma and Body Mass Index (BMI). Results: Male asthmatic children under the age of 8 at normal body rate had the highest risk quotient among the subgroups. The general potential average dose of PM2.5 was 1.95 mu g/kg.day (95% CI: 1.62 - 2.27) during the dry scenario and 0.32 mu g/kg. day (95% CI: 0.29 - 0.34) in the rainy scenario. During the dry season, children and adolescents showed a toxicological risk to PM2.5 of 2.07 mu g/kg. day (95% CI: 1.85 - 2.30). Conclusions: Children and adolescents living in the Subequatorial Brazilian Amazon region were exposed to high levels of PM2.5 resulting in toxicological risk for this multi-pollutant. The toxicological risk quotients of children in this region were comparable or higher to children living in metropolitan regions with PM2.5 air pollution above the recommended limits to human health.
Resumo:
This work reports the development of GDE for electrogeneration of H2O2 and their application in the degradation process of Reactive Blue 19 dye. GDE produced by carbon black with 20% polytetrafluoroethylene generated up to 500 mg L-1 of H2O2 through the electrolysis of acidic medium at -0.8 V vs Ag/AgCl. Reactive Blue 19 dye was degraded most efficiently with H2O2 electrogenerated in the presence of Fe(II) ions, leading to removal of 95% of the original color and 39% of TOC at -0.8 V vs Ag/AgCl.
Resumo:
In questo studio verranno descritte formulazioni di materiali innovativi, completamente biodegradabili e compostabili, a base di acido polilattico e biochar. Queste formulazioni sono state ideate per applicazioni nel settore degli imballaggi alimentari, in particolare da utilizzare nella produzione di vaschette ortofrutticole nere termoformate come alternativa alle tradizionali vaschette a base di PP e PET. È stato scelto di testare il biochar poiché rappresenta un composto ecocompatibile esattamente come la matrice polimerica utilizzata, alternativo al carbon black di origine fossile utilizzato in queste applicazioni come colorante. Varie formulazioni di PLA contenenti biochar e plasticizzanti sono state preparate con un miscelatore Brabender e trasformate in fogli tramite una pressa a doppio piatto riscaldante. Da questi film sono stati poi realizzati provini per prove di trazione e strappo. Sono state sviluppate inoltre reazioni di funzionalizzazione sul biochar allo scopo di migliorare la sua la compatibilità con la matrice polimerica rendendo la miscela più omogenea.