Lead (Pb) and cadmium (Cd) are known reproductive toxicants, which accumulate in granulosa cells of the ovary. Female Charles foster rats were treated with sodium acetate (control), lead acetate and cadmium acetate either alone or in combination at a dose 0.05 mg/kg body weight intra-peritoneally for 15 days daily. Animals were killed at proestrous stage and granulosa cells were isolated from the ovaries. Binding of I-125-luteinizing hormone (I-125-LH), I-125-follicle stimulating hormone (I-125-FSH) and 17 beta-hydroxysteroid dehydrogenase activity were measured. As these receptors are localized on the surface of the cell membrane, we also estimated the membrane parameters of these cells. Our results demonstrated that both lead and cadmium caused a significant reduction in gonadotropin binding, which altered steroidogenic enzyme activity of granulosa cells. These changes exhibited a positive correlation with membrane changes of the granulosa cells.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The alloy, Ti-6Al-4V is an alpha + beta Ti alloy that has large prior beta grain size (similar to 2 mm) in the as cast state. Minor addition of B (about 0.1 wt.%) to it refines the grain size significantly as well as produces in-situ TiB needles. The role played by these microstructural modifications on high temperature deformation processing maps of B-modified Ti64 alloys is examined in this paper.Power dissipation efficiency and instability maps have been generated within the temperature range of 750-1000 degrees C and strain rate range of 10(-3)-10(+1) s(-1). Various deformation mechanisms, which operate in different temperature-strain rate regimes, were identified with the aid of the maps and complementary microstructural analysis of the deformed specimens. Results indicate four distinct deformation domains within the range of experimental conditions examined, with the combination of 900-1000 degrees C and 10(-3)-10(-2) s(-1) being the optimum for hot working. In that zone, dynamic globularization of alpha laths is the principle deformation mechanism. The marked reduction in the prior beta grain size, achieved with the addition of B, does not appear to alter this domain markedly. The other domains, with negative values of instability parameter, show undesirable microstructural features such as extensive kinking/bending of alpha laths and breaking of beta laths for Ti64-0.0B as well as generation of voids and cracks in the matrix and TiB needles in the B-modified alloys. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An electron-beam melting and centrifugal splat-quenching technique for the production of microflakes of Ti-6A1-4V (wt%) alloy quenched at an average cooling rate of about 105 K sec–1 is described. The effect of substrate angle on the shape, size, microstructure and average cooling rate of the flakes of major sieve fractions is discussed. Morphologies of particles of minor sieve fractions are dealt with briefly.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The reaction of cadmium sulfate in the presence of polyazaheterocyclic organic molecules gave rise to a variety of new cadmium sulfate phases in water containing solvothermal reaction. The compounds have two- (I) and three-dimensionally (II-VI) extended structures. All the compounds have structures built up by the connectivity involving the cadmium octahedra and the sulfate tetrahedra in which the heterocyclic organic molecules act as the ligand. The linkages between the Cd2+ and (SO4)2- ions form one- (II), two- (I, III, and IV), and three- (V and VI) dimensionally extended cadmium sulfate phases. The connectivity between Cd2+ ion and the heterocyclic ligand also gives rise to one- and two-dimensional structures. The inter-connectivity between the two units gives rise to the observed structures. The presence of Cd-O-Cd chains and Cd-O-Cd layers in some of the structures is noteworthy. The adsorption/desorption studies suggest that the cadmium sulfate phases adsorb/desorb anionic dyes selectively in the presence of water/ethanol, respectively. The photocatalytic degradation studies on cationic dyes under UV-irradiation indicate modest activity. The cyanosilylation of imines using the present compounds as heterogeneous catalyst indicate good catalytic behavior. The various properties exhibited by the cadmium sulfate phases suggest that these compounds are versatile. All the compounds were characterized by powder X-ray diffraction, thermogravimetric analysis, infrared (IR) and UV-visible studies.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The regular associated solution model for binary systems has been modified by incorporating the size of the complex as an explicit variable. The thermodynamic properties of the liquid alloy and the interactions between theA ?B type of complex and the unassociated atoms in anA-B binary have been evaluated as a function of relative size of the complex using the activity coefficients at infinite dilution and activity data at one other composition in the binary. The computational procedure adopted for determining the concentration of clusters and interaction energies in the associated liquid is similar to that proposed by Lele and Rao. The analysis has been applied to the thermodynamic mixing functions of liquid Al-Ca alloys believed to contain Al2Ca associates. It is found that the size of the cluster significantly affects the interaction energies between the complex and the unassociated atoms, while the equilibrium constant and enthalpy change for the association reaction exhibit only minor variation, when the equations are fitted to experimental data. The interaction energy between unassociated free atoms remains virtually unaltered as the size of the complex is varied between extreme values. Accurate data on free energy, enthalpy, and volume of mixing at the same temperature on alloy systems with compound forming tendency would permit a rigorous test of the proposed model.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structural changes occurring during warm working of Cd-1.5 pct Zn alloy and their effect on the subsequent mechanical properties are studied. It is observed that changes in grain size and preferred orientation are important to a large extent in controlling the mechanical strength. The Hall-Petch slope,R decreases in the warm worked material while the friction stress, σo increases. The lowerR values are attributed to the development of a (101l) texture and the higher σo values are interpreted on the basis of changes in the basal texture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A minor addition of B to the Ti-6Al-4V alloy, by similar to 0.1 wt pct, reduces its as-cast prior beta grain size by an order of magnitude, whereas higher B content leads to the presence of in situ formed TiB needles in significant amounts. An experimental investigation into the role played by these microstructural modifications on the high-temperature deformation behavior of Ti-6Al-4V-xB alloys, with x varying between 0 wt pct and 0.55 wt pct, was conducted. Uniaxial compression tests were performed in the temperature range of 1023 K to 1273 K (750 degrees C to 1000 degrees C) and in the strain rate range of 10(-3) to 10(+1) s(-1). True stress-true strain responses of all alloys exhibit flow softening at lower strain rates and oscillations at higher strain rates. The flow softening is aided by the occurrence of dynamic recrystallization through lath globularization in high temperature (1173 K to 1273 K 900 degrees C to 1000 degrees C]) and a lower strain rate (10(-2) to 10(-3) s(-1)) regime. The grain size refinement with the B addition to Ti64, despite being marked, had no significant effect on this. Oscillations in the flow curve at a higher strain rate (10(0) to 10(+1) s(-1)), however, are associated with microstructural instabilities such as bending of laths, breaking of lath boundaries, generation of cavities, and breakage of TiB needles. The presence of TiB needles affected the instability regime. Microstructural evidence suggests that the matrix cavitation is aided by the easy fracture of TiB needles.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of magnesium addition and subsequent heat treatment on mild wear of a cast hypoeutectic aluminium-silicon alloy when slid against EN 24 steel is studied. Morphology and chemistry of worn surface and subsurface are studied with a view to identify wear mechanism. Stability of an iron-aluminium mixed surface layer was found to be the key factor controlling wear resistance.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A hypomonotectic alloy of Al-4.5wt%Cd has been manufactured by melt spinning and the resulting microstructure examined by transmission electron microscopy. As-melt spun hypomonotectic Al-4.5wt%Cd consists of a homogeneous distribution of faceted 5 to 120 nm diameter cadmium particles embedded in a matrix of aluminium, formed during the monotectic solidification reaction. The cadmium particles exhibit an orientation relationship with the aluminium matrix of {111}Al//{0001}Cd and lang110rangAlAl//lang11¯20> Cd, with four cadmium particle variants depending upon which of the four {111}Al planes is parallel to {0001}Cd. The cadmium particles exibit a distorted cuboctahedral shape, bounded by six curved {100}Al//{20¯23}Cd facets, six curved {111}Al/{40¯43}Cd facets and two flat {111}Al//{0001}Cd facets. The as-melt spun cadmium particle shape is metastable and the cadmium particles equilibrate during heat treatment below the cadmium melting point, becoming elongated to increase the surface area and decrease the separation of the {111}Al//{0001}Cd facets. The equilibrium cadmium particle shape and, therefore, the anisotropy of solid aluminium-solid cadmium and solid aluminium -liquid cadmium surface energies have been monitored by in situ heating in the transmission electron microscope over the temperature range between room temperature and 420 °C. The anisotropy of solid aluminium-solid cadmium surface energy is constant between room temperature and the cadmium melting point, with the {100}Al//{20¯23}Cd surface energy on average 40% greater than the {111}Al//{0001}Cd surface energy, and 10% greater than the {111}Al//{40¯43Cd surface energy. When the cadmium particles melt at temperatures above 321 °C, the {100}Al//{20¯23}Cd facets disappear and the {111}Al//{40¯43}Cd and {111}A1//{0001}Cd surface energies become equal. The {111}Al facets do not disappear when the cadmium particles melt, and the anisotropy of solid aluminium-liquid cadmium surface energy decreases gradually with increasing temperature above the cadmium melting point. The kinetics of cadmium solidification have been examined by heating and cooling experiments in a differential scanning calorimeter over a range of heating and cooling rates. Cadmium particle solidification is nucleated catalytically by the surrounding aluminium matrix on the {111}Al faceted surfaces, with an undercooling of 56 K and a contact angle of 42 °. The nucleation kinetics of cadmium particle solidification are in good agreement with the hemispherical cap model of heterogeneous nucleation.