973 resultados para Bulk Metallic-Glass
Resumo:
Anelastic and viscoplastic characteristics of Cu50Zr50 and Cu65Zr35 binary bulk metallic glasses at room temperature were examined through nanoindentation creep experiments. Results show that both the deformations are relatively more pronounced in Cu50Zr50 than in Cu65Zr35, and their amount increases with the loading rate. The results are analyzed in terms of the influences of structural defects and loading rate on the room temperature indentation creep.
Resumo:
The effect of hydrogen (H) charging on the shear yield strength (tau(max)) and shear transformation zone volume (Omega) of Ni-Nb-Zr metallic glass ribbons, with varying Zr content, were studied through the first pop-in loads during nanoindentation. Weight gain measurements after H charging and desorption studies were utilized to identify how the total H absorbed during charging is partitioned into mobile and immobile (or trapped) parts. These, in turn, indicate the significant role of H mobility in the amorphous structure on the yielding behavior. In high-Zr alloys, tau(max) increases significantly whereas Omega decreases. In low-Zr alloys, a slight decrease in tau(max) and increase in Omega were noted. These experimental observations are rationalized in terms of the mobility of the absorbed H in the amorphous structure and the possible role of it in the shear transformation zone dynamics during deformation of the metallic glass. (C) 2014 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The nanoindentation technique was employed to examine the strain rate sensitivity, m, and its dependence on the structural state of a Zr-based bulk metallic glass (BMG). The free volume content in the BMG was varied by examining samples in the as-cast (AC), shot-peened (SP), and structurally relaxed (SR) states. Hardness values measured at different loading rates and over a temperature range of 300-423 K as well as the strain-rate jump tests conducted in the quasi-static regime at room temperature, show that m is always negative. All the load-displacement (P-h) curves in this temperature regime exhibit serrated load-displacement responses, indicating that the shear band mediated inhomogeneous plastic flow governs deformation. Such localization of flow and associated softening is the raison d'etre for the negative m. Significant levels of pile-up around the indents were also noted. The order in the average values of hardness, pile-up heights, and the displacement bursts on the P-h curves was always such that SR > AC > SP, which is also the order of increasing free volume content. These observations were utilized to discuss the reasons for the negative strain rate sensitivity, and its dependence on the structural state of metallic glasses. It is suggested that the positive values of m reported in the literature for them are possibly experimental artefacts that arise due to large pile ups around the indents which lead to erroneous estimation in hardness values. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
The mode I fracture toughness, K-Ic, of ductile bulk metallic glasses (BMGs) exhibits a high degree of specimen-to-specimen variability. By conducting fracture experiments in modes I and II, we demonstrate that the observed high variability in mode I, vis-a-vis mode II, is a result of highly variable propensity for the conversion of shear bands into cracks in mode I whereas in mode II, crack growth direction is fixed. Thus, the measured variability in K-Ic is intrinsic to the nature of BMGs. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The room temperature creep behaviors of Ce-based bulk metallic glasses were examined by the use of nanoindentation. The creep rate and creep rate sensitivity of Ce-based BMGs were derived from indentation creep curves. The low creep rate sensitivity of Ce-based BMGs indicates that the room temperature creep is dominated by localized shear flow. The experimental creep curves can be described by a generalized Kelvin model. Furthermore, the creep retardation spectrum is calculated for the Ce-based metallic glasses. The results showed that creep retardation spectrum consists of two relatively separated peaks with the well defined characteristic relaxation times.
Resumo:
(Zr65Al10Ni10Cu15)(100-x) Nb-x glass forming alloys with Nb contents ranging from 0 to 15 at.% were prepared by water-cooled copper mould cast. The alloys with different Nb contents exhibited different microstructures and mechanical properties. Unlike the monolithic Zr65Al10Ni10Cu15 bulk metallic glass, only a few primary bee beta-Ti phase dendrites were found to distribute in the glassy matrix of the alloys with x = 5. For alloys with x = 10, more beta-phase dendrites forms, together with quasicrystalline particles densely distributed in the matrix of the alloys. For alloys with x = 15, the microstructure of the alloy is dominated by a high density of fully developed P-phase dendrites and the volume fraction of quasicrystalline particles significantly decreases. Room temperature compression tests showed that the alloys with x = 5 failed at 1793 MPa and exhibited an obvious plastic strain of 3.05%, while the other samples all failed in a brittle manner. The ultimate fracture strengths are 1793, 1975 and 1572 MPa for the alloys with x = 0, 10 and 15 at.% Nb, respectively.
Resumo:
Plastic deformation behaviors of Zr65Al10Ni10CU15 and Zr52.5Al10Ni10Cu15Be12.5 bulk metallic glasses (BMGs) are studied by using the depth-sensing nanoindentation, microindentation and uniaxial compression. The Be-containing BMG exhibits a significantly improved overall plastic strain compared with the Be-free alloy during compressive tests. Both BMGs show a loading-rate-dependent serrated flow during nanoindentation measurements, but the Be-containing alloy exhibits a much lower critical loading rate for the disappearance of the serration than the Be-free BMG. The shear band patterns developed during plastic deformation are investigated by microindentation technique, wherein much higher shear band density is found in the Be-containing alloy than in the Be-free alloy, indicating an easier nucleation of shear bands in the former BMG. The difference in the plastic deformation behavior of the two BMGs can be explained by a free volume model.
Resumo:
A novel multicomponent thick metallic glass coating has been synthesised by laser cladding. The maximum coating thickness was I mm. The clad cooling rate restrained the epitaxial growth of dendrites in the metallic glass coating. The metallic glass had high glass forming ability with a wide supercooled liquid region ranging from 59 to 70 K. The metallic glass coating also revealed high hardness and good corrosion resistance.
Resumo:
Plastic deformation behaviour of Zr52.5Al10Ni10Cu15Be12.5 and Mg65Cu25Gd10 bulk metallic glasses (BMGs) is studied by using the depth-sensing nanoindentation and microindentation. The subsurface plastic deformation zone of the BMGs is investigated using the bonded interface technique. Both the BMGs exhibit the serrated flow depending on the loading rate in the loading process of indentation. Slow indentation rates promote more conspicuous serrations, and rapid indentations suppress the serrated flow. Mg-based BMG shows a much higher critical loading rate for the disappearance of the serration than that in Zr-based BMG. The significant difference in the shear band pattern in the subsurface plastic deformation zone is responsible for the different deformation behaviour between the two BMGs. Increase of the loading rate can lead to the increase of the density of shear bands. However, there is no distinct change in the character of shear bands at the loading rate of as high as 1000 nm/s.
Resumo:
We investigate the plastic deformation and constitutive behaviour of bulk metallic glasses (BMGs). A dimensionless Deborah number De(ID) = t(r)/t(i) is proposed to characterize the rate effect in BMGs, where t(r) is the structural relaxing characteristic time of BMGs under shear load, t(i) is the macroscopic imposed characteristic time of applied stress or the characteristic time of macroscopic deformation. The results demonstrate that the modified free volume model can characterize the strain rate effect in BMGs effectively.
Resumo:
The deformation behavior and the effect of the loading rate on the plastic deformation features in (numbers indicate at.%) Ce60Al15Cu10Ni15, Ce65Al10Cu10Ni10Nb5, Ce68Al10Cu20Nb2, and Ce70Al10Cu20 bulk metallic glasses (BMGs) were investigated through nanoindentation. The load-displacement (P-h) curves of Ce65Al10Cu10Ni10Nb5, Ce68Al10Cu2, and Ce70Al10Cu20 BMGs exhibited a continuous plastic deformation at all studied loading rate. Whereas, the P-h curves of Ce60Al15Cu10Ni15 BMG showed a quite unique feature, i.e. homogeneous plastic deformation at low loading rates, and a distinct serrated flow at high strain rates. Moreover, a creep deformation during the load holding segment was observed for the four Ce-based BMGs at room temperature. The mechanism for the appearance of the "anomalous" plastic deformation behavior in the Ce-based BMGs was discussed. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The microstructure of Nd_{60}Al_{10}Ni_{10}Cu_{20-x}Fex (x = 0, 5, 7, 10, 15, 20) alloys can change from homogeneous phase to a composite structure consisting of amorphous phase plus clusters or nanocrystals by adjusting the Fe content. The effect of microstructure on the plastic deformation behavior in this alloy system is studied by using nanoindentation. The alloys with homogeneous amorphous structure exhibit pronounced flow serrations during the loading process of nanoindentation. The addition of Fe changes the plastic deformation behavior remarkablely. No flow serration is observed in the alloys with high Fe content for the indentation depth of 500 nm. The mechanism for the change of plastic serrated flow behavior is discussed.
Resumo:
A systematic survey of the available data such as elastic constants, density, molar mass, and glass transition temperature of 45 metallic glasses is conducted. It is found that a critical strain controlling the onset of plastic deformation is material-independent. However, the correlation between elastic constants of solid glass and vitrification characteristics of its liquid does not follow a simple linear relation, and a characteristic volume, viz. molar volume, maybe relating to the characteristic size of a shear transformation zone (STZ), should be involved.
Resumo:
131 p.