964 resultados para poly(p-phenylene sulfide)


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Pós-graduação em Engenharia Mecânica - FEG

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The controlled synthesis of poly(neopentyl p-styrene sulfonate) (PNSS) using RAFT polymerisation has been studied. Selected experimental conditions led to the production of PNSS with variable molecular weights and low dispersities (D{stroke}≤1.50). The controlled synthesis of poly(neopentyl p-styrene sulfonate) (PNSS) using reversible addition-fragmentation chain transfer polymerisation has been studied under a wide range of experimental conditions. PNSS can be used as an organic-soluble, thermally labile precursor for industrially valuable poly(p-styrene sulfonate), widely employed in technologies such as ionic exchange membranes and organic electronics. The suitability of two different chain transfer agents, three solvents, three different monomer concentrations and two different temperatures for the polymerisation of neopentyl p-styrene sulfonate is discussed in terms of the kinetics of the process and characteristics of the final polymer. Production of PNSS with systematically variable molecular weights and low dispersities (D{stroke} ≤1.50 in all cases) has been achieved using 2-azidoethyl 2-(dodecylthiocarbonothioylthio)-2-methylpropionate in anisole at 75°C, with an initial monomer concentration of 4.0molL-1. Finally, a poly(neopentyl p-styrene sulfonate)-b-polybutadiene-b-poly(neopentyl p-styrene sulfonate) (PNSS-b-PBD-b-PNSS) triblock copolymer has been synthesised via azide-alkyne click chemistry. Moreover, subsequent thermolysis of the PNSS moieties generated poly(p-styrene sulfonate) end blocks. This strategy allows the fabrication of amphiphilic copolymer films from single organic solvents without the need for post-deposition chemical treatment.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Photoluminescence (PL), electroluminescence (EL) and photoconductivity (PC) of poly[(2,5-dimethoxy-p-phenylene) vinylene] (DMPPV) of varying conjugation length were studied. Thin film devices of the DMPPV with different conjugation lengths, as the active medium, were prepared. The PL emission spectra revealed the radiative decay of the singlet excitons with peak values corresponding to energies below the absorption onset. The PL. emission spectra of the copolymer films also revealed vibronic features, which get well resolved upon cooling to 80K, The devices exhibit light emitting diode (LED) behavior; the I-V curves and EL spectra are compared in these DMPPV samples having different conjugation lengths. The PC studies reveal subtle features, which can be attributed to the optically generated excitations in the system.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

1.热可交联聚酰亚胺/高性能热塑性树脂共混体系的研究聚苯硫醚[Poly(phenylene sulfide),PPS]是由刚性结构的苯环和柔性的硫醚连接起来,交替排列构成的线性高分子化合物,具有高的热稳定性、良好的耐化学药品性、优良的电绝缘性、耐老化性和阻燃性等综合性能优异的高性能树脂。聚醚矾〔Poly(ether sulfone),PES]是一种非结晶性的热塑性工程塑料一,具有优异的热稳定性、耐高温蠕变性及优异的物理机械性能。其高的玻璃化转变温度(Tg=225℃),使其可以在较高温度下作为结构材料使用。本论文研究了PPS/PES二元共混物的热性能和动态力学性能,并以热可控交联的低分子量多官能单体PMR-POI(聚醚酰亚胺)为界面增强剂,分别研究了POI与PPS、PES之间的接枝和/或交联反应,POI对PPS结晶行为的影响,POI对PES分子运动的影响和POI对PPS/PES共混体系的界面增强。主要结果如下:1.PPS/PES共混物相容性的特征在于选择性的部分相容,少量的非晶PPS分子可以扩散进入PES相区,相反的扩散过程则不会发生。2.PPS/PES共混物的热学性质和动态力学性能主要受连续相的控制。3.PPS相的性能主要受其结晶度的影响,因此能够改变其结晶度的因素均会改变PPS相的性质。4.光谱学和流变的证据表明,POI同PES,PPs共混过程中有接枝反应发生,分子链增长,分子量加大。这种接枝和/或交联反应的程度是热可控的。5.POI是PPS的增塑剂,成核剂和扩链剂,与POI共混使得PPS结晶速率增加,平衡熔点上升,表面折叠自由能降低。6;在PES/POI体系中Pol对PEs起到了增塑的作用,Tg降低,经高温热处理后Tg上升。因此,POI对PES性能的影响也是热可控的。7.PMR-POI能够在PPS/PES共混体系中有效地扩散并起到了降低分散相粒子的尺寸、增强界面的作用。它是该共混体系的有效界面增强剂。8."高温退火既能够提高扩散速率也能够提高反应速率;二者相互竞争。2.马来酸配封端溉碳酸丙撑酯的研究二氧化碳与环氧丙烷交替共聚物(polypropylene careonate,PPC)是由二氧化碳活化并与环氧丙烷共聚而成的一类可完全生物降解的新型高分子材料,具有巨大的潜在应用价值。本论文讨论了马来酸配封端的聚碳酸丙撑酯(MA-PPC)和未封端的PPC的粘弹性、流变行为以及热降解和热分解行为,并得出如下结论:1.马来酸配封端抑制了PPC解拉链式的热分解和无规链断裂热降解,PPC的热稳定性和力学性能得到提高。2.PPC和MA-PPC在玻璃化转变温度有相似的自由体积分数,PPC的Tg比MA-PPC稍低。虽然PPC和MA-PPC玻璃化转变表观活化能E。和平均松弛时间T随温度升高单调降低,但PPC的分子运动对温度更敏感,而MA-PPC较稳定。马来酸配封端改变了PPC分子运动的特征及松弛行为,许多实验证据证明,这是由于封端后的PPC大分子链间的相互作用增强及分子链缠结密度增加。3.MA-PPC在70℃左右会发生脱水,实现大分子偶联反应并得到变温红外光谱、分子量成倍增加及线膨胀数据的有力支持。4.用零剪切粘度几。的方法测得PPC及MA-PPC加工过程中的热降解温度,它们分别为150℃和175℃,在此温度以上,η0降低速率的增加归因于大分子的主链断裂以及解拉链反应。5.测得了PPC的临界缠结分子量,它几乎是MA-PPC相应值(6613)的3倍。这表明马来酸配封端不仅改善了PPC的熔体弹性,而且也大大增强了PPC的缠结密度以及分子链间的相互作用。6.在本实验条件下在氮气和空气的气氛中,MA-PPC同PPC的热降解和热分解行为几乎一致,即在PPc的加土过程可以忽略氧气对其的影响。7.虽然MA-PPC的玻璃化温度在40℃左右,但在40℃-120℃的温度区间内,MA-PPC达不到粘流状态。8.没有剪切力时在120℃-150℃,30分钟内,MA-PPC几乎没有降解,在静态条件下,低于170℃时,MA-PPC的解拉链式降解是十分轻微的,当温度超过170℃,PPC降解相当严重。9.在热机械力存在的情况下,发生无规断链的机会增加,无规断链又会加速解拉链降解,因此实际加工中的加工窗口比静态下窄,MIA-PPC的加工窗口应为130℃-160℃。10.MA-PPC的热分解过程是一步完成的,热分解温度随升温速率的加快而提高,并计算出热分解的表观活化能为623.3KJ/mol。

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Nonisothermal and isothermal crystallization kinetics of an aromatic thermoplastic polyimide derived from 3,3',4,4'-oxydiphthalic dianhydride and 4,4'-oxydianiline have been investigated by means of differential scanning calorimetry (DSC) and wide-angle X-ray diffraction. The results for nonisothermal crystallization study showed that a weak melting peak appeared during the first heating process, whereas no crystallization peak appeared in the DSC curve during the subsequent cooling process. On the other hand, the study for the isothermal crystallization in the temperature range of 260-330 degrees C showed that a new exothermic peak appeared at lower temperature for the samples crystallized for 100 min at 300 degrees C.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Three series of poly(phenylene vinylene) (PPV) derivatives containing hole-transporting triphenylamine derivatives [N-(4-octoxylphenyl)diphenylamine, N,N'-di(4-octyloxylphenyl)-N,N'-diphenyl-1,4-phenylenediamine, and N,N'-di(4-octoxylphenyl)-N,N'-diphenylbenzidine] (donor) and electron-transporting oxadiazole unit (2,5-diphenyl-1,3,4-oxadiazole) (acceptor) in the main chain were synthesized by improved Wittig copolymerization. The resulting donor-acceptor (D-A) polymers are readily soluble in common organic solvents, such as chloroform, dichloroethane, THF, and toluene.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Four novel thermally stable poly(aryl ether)s, e.g., P3F, P5F, P2A3F, and P2A5K containing ter- or pentafluorene units in the side chains for efficient blue light emission have been designed and synthesized. All the polymers show the optical properties identical to the corresponding monomers and are amorphous with higher glass transition temperature (T-g) than their monomeric Counterparts. The polymer light-emitting diodes (PLEDs) were fabricated with the device structure of ITO/(PEDOT:PSS)/polymer/Ca/Al. The incorporation of diphenylamine group to oligofluorene terminals significantly reduces the hole-injection energy barrier in PLEDs. The devices based on P2A3F and P2A5F show the luminous efficiencies of 1.2 and 2.0 cd/A at a brightness of 300 cd/m(2) with the Commission Internationale de L'Eclairage (CIE) coordinates of (0.15, 0.13) and (0.19, 0.20), respectively. All these indicate that the high-performance light-emitting polymers can be synthesized with the traditional condensation polymerization through careful design of polymer structures.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of novel nitrogen- and sulfur-containing conjugated polymers with well-defined conjugation length have been synthesized via an acid-induced self-polycondensation of functional monomers with methylsulfinyl groups. Synthesized polymers exhibit good solubility in common solvents, such as CHCl3, THF, DMF, DMSO, and NMP. With increased numbers of aminophenyl groups, these polymers have shown similar electrical properties to polyaniline (PAn), and these are demonstrated by UV-vis spectroscopy and cyclic voltammetry (CV) measurements on the polymers. The conductivity of preliminarily protonic-doped poly[phenylene sulfide-alt-tetrakis(aniline)] (PPSTEA) is up to 10(-1) S cm(-1).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tensile properties of poly (P-hydroxybutyrate)/poly (ethylene oxide) (PHB/PEO) blends were reported in this paper. It was found that the blends of PHB with different molecular-weight PEO exhibited different mechanical properties. The mechanical properties of the blends of PHB and PEO3 (M-w=0.3x10(6)) were very poor. However, the blends of PHB and PEO5 (M-w=5x10(6)) showed compatible in mechanical properties. Excellent synergism was observed not only in tensile stress and tensile elongation but also in modulus. Moreover, the ductility of the blends could be improved further under proper heat-treatment.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The effect of PMR-polyimide(POI) as the interfacial agent on the interface characteristics, morphology features and crystallization of poly (ether sulfone) /poly (phenylene sulfide) (PES/PPS) and poly(ether ether ketone)/poly (ether sulfone) (PEEK/PES) partly miscible blends were investigated by means of the scanning electron microscopy, WAXD and XPS surface analysis. It is found that the interfacial adhesion was enhanced remarkably, the size of the dispersed phase particles was reduced significantly and the miscibility was improved by the addition of POI. During melt blending cross-link and/or grafting reaction of POI with PES, PEEK and PPS homopolymers was detected, however the reaction activity of POI with PPS was much higher than that of PES and PEEK. It was also found that POI was an effective nucleation agent of the crystallization of PPS.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Nonisothermal crystallization and melting behavior of poly(P-hydroxybutyrate) (PHB)-poly(vinyl acetate) (PVAc) blends from the melt were investigated by differential scanning calorimetry using various cooling rates. The results show that crystallization of PHB from the melt in the PHB-PVAc blends depends greatly upon cooling rates and blend compositions. For a given composition, the crystallization process begins at higher temperatures when slower scanning rates are used. At a given cooling rate, the presence of PVAc reduces the overall PHB crystallization rate. The Avrami analysis modified by Jeziorny and a new method were used to describe the nonisothermal crystallization process of PHB-PVAc blends very well. The double-melting phenomenon is found to be caused by crystallization during heating in DSC. (C) 1999 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Poly(vinyl acetate-co-vinyl alcohol) copolymers (P(VAc-co-VA)) were synthesized by hydrolysis-alcoholysis of PVAc. The miscibility, crystallization, and morphology of poly(P-hydroxybutyrate) (PHB) and P(VAc-co-VA) blends were studied by differential scanning calorimetry, optical microscopy (OM), and SAXS. It is found that the P(VAc-co-VA)s with vinyl alcohol content of 9, 15, and 22 mol % will form a miscible phase with the amorphous part of PHB in the solution-cast samples. The melting-quenched samples of PHB/P(VAc-co-VA) blends with different vinyl alcohol content show different phase behavior. PHB and P(VAc-co-VA9) with low vinyl alcohol content (9% mel) will form a miscible blend in the melt state. PHB and P(VAc-co-VA15) with 15 mol % vinyl alcohol will not form miscible blends while PHB/P(VAc-co-VA15) blend with 20/80 composition will form a partially miscible blend in the melt state. PHB and P(VAc-co-VA22) with 22 mol % vinyl alcohol are not miscible in the whole composition range. The single glass transition temperature of the blends within the whole composition range suggests that PHB and P(VAc-co-VA9) are totally miscible in the melt. The crystallization kinetics was studied from the whole crystallization and spherulite growth for the miscible blends. The equilibrium melting point of PHB in the PHB/P(VAc-co-VA9) blends, which was obtained from DSC results using the Hoffman-Weeks equation, decreases with the increase in P(VAc-co-VA9) content. The negative value of the interaction parameter determined from the equilibrium melting point depression supports the miscibility between the components. The kinetics of spherulitic crystallization of PHB in the blends was analyzed according to nucleation theory in the temperature range studied in this work. The best fit of the data to the kinetic theory is obtained by employing WLF parameters and the equilibrium melting points obtained by DSC. The addition of P(VAc-co-VA) did not affect the crystalline structure of PHB, as shown by the WAXD results. The long periods of blends obtained from SAXS increase with the increase in P(VAc-co-VA) content. It indicates that the amorphous P(VAc-co-VA) was rejected to interlamellar phase corporating with the amorphous part of PHB.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bright blue electroluminescent devices have been fabricated using poly (N-vinylcarbazole) (PVK) doped with perylene as the emissive layer, poly(p-phenylenevinylene) (PPV) as the hole-transporting layer, 2-(4-biphenylyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole (PBD), tris(8-hydroxyquinoline)aluminum (Alq(3)) as the electron-transporting layer, and Al as the cathode. A luminance of 700 cd/m(2) and a luminescent efficiency of 0.8% are achieved at a drive voltage of 36 V. In the experiment, it is found that the introduction of electron-transporting layer PBD has a great effect on the emissive color of the electroluminescent devices prepared by PVK doped with perylene. Yellow-green emission is observed from the device structure of glass substrate/indium-tin-oxide/PVK:perylene/Al. The possible emissive mechanisms are given. The effect of the transporting layer on the electroluminescence is also discussed. (C) 1997 Elsevier Science S.A.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

2,2'-Bis(3,4-dicarboxyphenoxy)-1,1'-binaphthyl dianhydride was used as a new monomer with various aromatic diamines to obtain polyimides by the usual two-step method. The bis(ether anhydride) was prepared by a nucleophilic substitution of I,1'-bi-2-naphthol with N-phenyl-4-chlorophthalimide, N-methyl-4-nitrophthalimide or 4-nitrophthalonitrile in aprotic polar solvent, and subsequent hydrolysis of the resulting bis(ether imide)s or bis(ether dinitrile), and then dehydration of the corresponding tetracarboxylic acid to afford the dianhydride. Most of the obtained polyimides were soluble in chloroform, pyridine, DMF, etc. The polyimide prepared from p-phenylene diamine was partial crystalline, whereas the others showed amorphous patterns in a WAXD study. These polymers have glass transition temperatures between 255-294 degrees C and 5% weight loss temperatures in the range of 502-541 degrees C in nitrogen and 473-537 degrees C in air. (C) 1997 Elsevier Science Ltd.