141 resultados para butadiene
Resumo:
This paper deals with the effect of silica fume and styrene-butadiene latex (SBR) on the microstructure of the interfacial transition zone (ITZ) between Portland cement paste and aggregates (basalt). Scanning electron microscope (SEM) equipped with energy dispersive X-ray analysis system (EDX) was used to determine the ITZ thickness. In the plain concrete a marked ITZ around the aggregate particles (55 mu m) was observed, while in concretes with silica fume or latex SBR the ITZ was less pronounced (35-40 mu m). However, better results were observed in concretes with silica fume and latex SBR (20-25 mu m). (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
Oligonucleotides have unique molecular recognition properties, being involved in biological mechanisms such as cell-surface receptor recognition or gene silencing. For their use in human therapy for drug or gene delivery, the cell membrane remains a barrier, but this can be obviated by grafting a hydrophobic tail to the oligonucleotide. Here we demonstrate that two oligonucleotides, one consisting of 12 guanosine units (G(12)), and the other one consisting of five adenosine and seven guanosine (A(5)G(7)) units, when functionalized with poly(butadiene), namely PB-G(12) and PB-A(5)G(7), can be inserted into Langmuir monolayers of dipalmitoyl phosphatidyl choline (DPPC), which served as a cell membrane model. PB-G(12) and PB-A(5)G(7) were found to affect the DPPC monolayer even at high surface pressures. The effects from PB-G(12) were consistently stronger, particularly in reducing the elasticity of the DPPC monolayers, which may have important biological implications. Multilayers of DPPC and nucleotide-based copolymers could be adsorbed onto solid supports, in the form of Y-type LB films, in which the molecular-level interaction led to lower energies in the vibrational spectra of the nucleotide-based copolymers. This successful deposition of solid films opens the way for devices to be produced which exploit the molecular recognition properties of the nucleotides. (C) 2010 Elsevier Inc. All rights reserved.
Resumo:
In industrial polymer and synthetic rubber production facilities, workers are exposed to 1,3-butadiene. This compound is converted in vivo to 1,2,3,4-diepoxybutane (DEB) and has been linked to increased incidences of cancer in these individuals. Carcinogenesis has been attributed to formation of DEB induced DNA interstrand cross-links. Previous studies have demonstrated that DEB cross-links deoxyguanosine residues within 5'-GNC sequences in synthetic DNA, in restriction fragments, and in defined sequence nucleosomes. The current study utilized the polymerase chain reaction (PCR) to examine DEB damage frequencies within nuclear genes, found within "open" regions of chromatin, as compared to regions of unexpressed sequence that reside in tightly packed, "closed" chromatin, to more closely model DEB reactivity in vivo. These initial studies have been performed in chicken liver homogenates. Preliminarily, we have found a dose-dependent DEB lesion-forming response within "open" chromatin. DEB appears to have little-to-no effect upon regions of "closed" chromatin.
Resumo:
Low cost seals are made of NBR, Nitrile Butadiene Rubber, a family of unsaturated copolymers that is higher resistant to oils the more content of nitrile have in its composition, although lower its flexibility. In Petroleum Engineering, NBR seal wear can cause fluid leakage and environmental damages, promoting an increasing demand for academic knowledge about polymeric materials candidate to seals submitted to sliding contacts to metal surfaces. This investigation aimed to evaluate tribological responses of a commercial NBR, hardness 73 ± 5 Sh A, polytetrafluoroethylene (PTFE), hardness 60 ± 4 HRE and PTFE with graphite, 68 ± 6 HRE. The testings were performed on a sliding tribometer conceived to explore the tribological performance of stationary polymer plane coupons submitted to rotational cylinder contact surface of steel AISI 52100, 20 ± 1 HRC Hardness, under dry and lubricated (oil SAE 15W40) conditions. After screening testings, the normal load, relative velocity and sliding distance were 3.15 N, 0.8 m/s and 3.2 km, respectively. The temperatures were collected over distances of 3.0±0.5 mm and 750±50 mm far from the contact to evaluate the heating in this referential zone due to contact sliding friction by two thermocouples K type. The polymers were characterized through Thermogravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA). The wear mechanisms of the polymer surfaces were analyzed by Scanning Electron Microscopy (SEM) and EDS (Energy-Dispersive X-ray Spectroscopy). NBR referred to the higher values of heating, suggesting higher sliding friction. PTFE and PTFE with graphite showed lower heating, attributed to the delamination mechanism
Resumo:
In order to cooperate in minimizing the problems of the current and growing volume of waste, this work aim at the production of panels made from industrial waste -thermoplastic (polypropylene; polyethylene and acrylonitrile butadiene styrene) reinforced with agro-industrial waste - peach palm waste (shells and sheaths). The properties of the panels like density, thickness swelling, water absorption and moisture content were evaluated using the ASTM D1037; EN 317; and ANSI A208.1 standards regarding particle boards. Good results were obtained with formulations of 100% plastic waste; 70% waste plastics and 30% peach palm waste; and 60% waste plastics and 40% peach palm waste.
Resumo:
Reusing scrap tires has become a worldwide challenge, especially due to the great difficulty in finding ecologically and economically feasible ways to dispose of them. This has led to the creation of specific programs and legislation for reusing scrap tires. Research has shown that a certain percentage of scrap tire rubber can be added to asphalt compositions, and this has become a worldwide practice. This paper describes the properties of four asphalt compositions modified with scrap tire rubber (STR) prepared in the laboratory. These properties are then compared with those of asphalt modified with styrene butadiene styrene (SBS), a synthetic polymer and one of the most common modifiers, to verify the feasibility of using scrap tire rubber as a substitute for SBS. The scope of this study does not include an analysis of how STR affects end-of-life asphalt. The main findings indicate that STR is a potential substitute of SBS in paving material, and although it does not meet some of the standard specifications when compared with SBS, these issues can be overcome by proper care during storage and transportation. The substitution of SBS by STR also showed the potential for about 10% in expenditure savings. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
In order to cooperate in minimizing the problems of the current and growing volume of waste, this work aims at the production of panels made from industrial waste -thermoplastic (Polypropylene - PP; Polyethylene - PE and Acrylonitrile Butadiene Styrene - ABS) reinforced with agro-industrial waste - pupunha palm waste (shells and sheaths). The properties of the panels were evaluated: density, thickness swelling, water absorption and moisture content. It was used the ASTM D1037; EN 317; and ANSI A208.1 standards regarding particle boards. The best results in physical tests were treatments 1 (100% waste plastic), 6 (60% plastic waste and 40% waste of pupunha) and 7 (70% waste plastic and 30% waste of pupunha). The best results in the mechanical tests were treatments 3 (30% de residuos plasticos e 70% de residuos da pupunha), 4 (40% de residuos plasticos c 60% de residuos da pupunha) and 5 (50% de residuos plasticos e 50% de residuos da pupunha). For mechanical tests it was concluded that the results of modulus of rupture and of modulus of elasticity the best treatments were those with more fibers. In the tensile tests perpendicular to the surface, it is clear that using more waste plastics leads to the best results. It was concluded that the waste can be used as raw material for the production of alternative materials mainly in civil construction and furniture industries, and it can be employed in urban or rural environment, given the concept of eco-efficient products.
Resumo:
Nylon6 is an attractive polymer for engineering applications because it has reactive functionality through amine and carboxyl end groups that are capable of reacting. For this reason, it has been used a lot in polymeric blends. Blends of nylon6/ABS (acrylonitrile-butadiene-styrene) were produced using glycidyl methacrylate-methyl methacrylate (GMA-MMA) copolymers as compatibilizer. The binary blends were immiscible and exhibited poor mechanical properties that stemmed from the unfavorable interactions among their molecular segments. This produced an unstable coarse phase morphology and weak interfaces between the phases in the solid state. The presence of the copolymer in the blends clearly led to a more efficient dispersion of the ABS phase and consequently optimized Izod impact properties. However, the compatibilized blend showed poor toughness at room temperature and failed in a brittle manner at subambient temperatures. © 2005 Springer Science + Business Media, Inc.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
The properties of the hot melt adhesive pressure sensitive (HMPSA) using an elastomer as a base polymer a copolymer of styrene and butadiene (SBS) and variation of tackifiers resins such as hydrocarbon resins and hydrogenated hydrocarbon were investigated. The formulations were prepared by mixing process within shear. The adhesives prepared were evaluated in test Brookfield viscosity and softening point Ring and Ball to compare the formulations and the influence of variations in raw materials. Infrared analyzes were performed to detect the reactions between the inputs and investigate the chemical interactions of the same properties of the adhesive. In thermal analysis, the assay was performed thermogravimetry (TG) and diferencial exploratory calorimetry (DSC). Were investigated the parameters of the tensile test on each of the formulations. Finally, were analysed comparatively the basic formulations of adhesives with their respective raw materials
Resumo:
Living anionic polymerization of 4-vinylbenzocylobutene was performed in benzene at room temperature using sec-butyllithium as the initiator. Results of the kinetic studies indicated the termination- and transfer-free nature of the polymerization. Homopolymers with predictable molecular weights and narrow molecular weight distributions were produced, excluding the interference of the cyclobutene rings during initiation and propagation. Thermogravimetric analysis of poly(4-vinylbenzocyclobutene) in air showed a small weight gain at ~200 °C, a rapid decomposition at ~455 °C, and a gradual decomposition at ~566 °C. This behavior was attributed to the formation of radicals from the pendent benzocyclobutene functionality through o-quinodimethane intermediates and simultaneous decomposition/cross-linking reactions at high temperature. The living nature of the polymerization was also examined via sequential copolymerization with butadiene to form diblock copolymers.
Resumo:
Gas-phase reactions of model carbosulfonium ions (CH3-S+?=?CH2; CH3CH2-S+?=?CH2 and Ph-S+?=?CH2) and an O-analogue carboxonium ion (CH3-O+?=?CH2) with acyclic (isoprene, 1,3-butadiene, methyl vinyl ketone) and cyclic (1,3-cyclohexadiene, thiophene, furan) conjugated dienes were systematically investigated by pentaquadrupole mass spectrometry. As corroborated by B3LYP/6-311?G(d,p) calculations, the carbosulfonium ions first react at large extents with the dienes forming adducts via simple addition. The nascent adducts, depending on their stability and internal energy, react further via two competitive channels: (1) in reactions with acyclic dienes via cyclization that yields formally [4?+?2+] cycloadducts, or (2) in reactions with the cyclic dienes via dissociation by HSR loss that yields methylenation (net CH+ transfer) products. In great contrast to its S-analogues, CH3-O+?=?CH2 (as well as C2H5-O+?=?CH2 and Ph-O+?=?CH2 in reactions with isoprene) forms little or no adduct and proton transfer is the dominant reaction channel. Isomerization to more acidic protonated aldehydes in the course of reaction seems to be the most plausible cause of the contrasting reactivity of carboxonium ions. The CH2?=?CH-O+?=?CH2 ion forms an abundant [4?+?2+] cycloadduct with isoprene, but similar to the behavior of such alpha,beta-unsaturated carboxonium ions in solution, seems to occur across the C?=?C bond. Copyright (c) 2012 John Wiley & Sons, Ltd.
Resumo:
Bearing pads are used in precast concrete connections to avoid concentrated stresses in the contact area between the precast elements. In the present research, the bearing pads are Portland cement mortar with styrene-butadiene latex (SB), lightweight aggregate (expanded vermiculite-term) and short fibers (polypropylene, glass and PVA), in order to obtain a material with low modulus of elasticity and high tenacity, compared with normal Portland cement mortar. The objective of this paper is to analyze the influence of surface roughness on the pads and test other types of polypropylene fibers. Tests were carried out to characterize the composite and test on bearing pads. Characterization tests show compressive strength of 41MPa and modulus of elasticity of 12.8GPa. The bearing pads tests present 30% reduction of stiffness in relation to a reference mortar. The bearing pads with roughness on both sides present a reduction up to 30% in stiffness and an increase in accumulated deformation of more than 120%, regarding bearing pads with both sides smooth.
Resumo:
Nanopartikel durch Strukturfixierung mizellarer Assoziate aus amphiphilen, endgruppenfunktionalisierten Diblockcopolymeren Zwei unterschiedliche Diblockcopolymersysteme mit Molmassen unterhalb von Mw = 10 000 g/mol wurden über anionische Polymerisation synthetisiert. Ein hetero-telecheles a,w-Poly(dimethylsiloxan)-b-Poly(ethylenoxid) (PDMS-PEO) Diblockcopolymer wurde mit einer Methacrylatendgruppe am PDMS und entweder einer Benzyl-, Hydroxy- oder Carboxylatendgruppe am PEO funktionalisiert. Ein Poly(butadien)-b-Poly(ethylenoxid) (PB-PEO) Diblockcopolymer wurde am PEO ebenfalls entweder mit einer Benzyl-, Hydroxy- oder Carboxylatendgruppe funktionalisiert. In selektiven Lösungsmitteln wie Wasser oder Methanol bilden beide Diblockcopolymersysteme supramolekulare Strukturen mit sphärischer, zylindrischer oder toroider Geometrie aus, die mit statischer und dynamischer Lichtstreuung in Lösung und mit Rasterkraftmikroskopie (AFM) und Transmissionselektronenmikroskopie (TEM) auf der Oberfläche untersucht wurden. Durch Zusatz eines Vernetzers und Initiators wurden die selbstassoziierenden Mizellen des PDMS-PEO Diblockcopolymers permanent durch radikalische Polymerisation mit UV-Licht fixiert. Mizellen des PB-PEO Diblockcopolymers wurden über Bestrahlung mit gamma-Strahlen permanent fixiert. Die Untersuchung der resultierenden Nanopartikel beider Diblockcopolymersysteme mit AFM und TEM zeigte, daß diese sogar in nicht selektiven Lösungsmitteln wie Tetrahydrofuran formstabil bleiben.
Resumo:
Lo scopo di questo lavoro è stato quello di studiare dettagliatamente la reattività dell’N-benzilossicarbonil-1-aza-butadiene, utilizzando diversi dienofili in reazioni di Diels-Alder catalitiche enantioselettive promosse da organocatalizzatori bifunzionali in grado di dare interazioni deboli come legami a idrogeno. Questo 1-azadiene infatti può dare in linea di principio sia prodotti derivanti da reazioni di Diels-Alder a domanda elettronica diretta in cui funge da diene, sia reazioni a domanda elettronica inversa in cui il doppio legame terminale dell’1-azadiene, maggiormente reattivo in quanto meno ingombrato, funge da olefina elettronricca (reazione di Povarov). Per effettuare questo studio sono stati provati vari dienofili tra cui olefine elettron povere bi- e monosostituite che portavano alla degradazione del diene; derivati della malimmide e del pirazolo che davano cilcloaddotti derivanti dalla classica cicloaddizione [4+2] Diels-Alder con ottime conversioni in modo altamente diastereoselettivo, ma bassi eccessi enantiomerici ed infine si sono provate diverse immine che portavano al cicloaddotto della reazione di Povarov con ottimi risultati in termini di conversione e buoni eccessi enantiomerici. Quest’ultima applicazione che permette la sintesi di interessanti prodotti variamente funzionalizzabili, sarà oggetto di studio in futuro per ottimizzare le condizioni della reazione.