965 resultados para Tensile Properties


Relevância:

70.00% 70.00%

Publicador:

Resumo:

Virtually all fibers exhibit some dimensional and structural irregularities. These include the conventional textile fibers, the high-performance brittle fibers and even the newly developed nano-fibers. In recent years, we have systematically examined the effect of fiber dimensional irregularities on the mechanical behavior of the irregular fibers. This paper extends our research to include the combined effect of dimensional and structural irregularities, using the finite element method (FEM). The dimensional irregularities are represented by sine waves with a 30 % magnitude of diameter variation while the structural irregularities are represented by longitudinal and horizontal cavities distributed within the fiber structure. The results indicate that fiber geometrical or dimensional variations have a marked influence on the tensile properties of the fiber. It affects not only the values of the breaking load and extension, but also the shape of the load-extension curves. The fiber structural irregularities simulated in this study appear to have little effect on the shape of the load-extension curves.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

In this study, we have electrospun poly(vinyl alcohol)(PVA) nanofibres and PVA composite nanofibres containing multi-wall carbon nanotubes (MWNTs) (4.5 wt%), and examined the effect of the carbon nanotubes and the PVA morphology change induced by post-spinning treatments on the tensile properties, surface hydrophilicity and thermal stability of the nanofibres. Through differential scanning calorimetry (DSC) and wide-angle x-ray diffraction (WAXD) characterizations, we have observed that the presence of the carbon nanotubes nucleated crystallization of PVA in the MWNTs/PVA composite nanofibres, and hence considerably improved the fibre tensile strength. Also, the presence of carbon nanotubes in PVA reduced the fibre diameter and the surface hydrophilicity of the nanofibre mat. The MWNTs/PVA composite nanofibres and the neat PVA nanofibres responded differently to post-spinning treatments, such as soaking in methanol and crosslinking with glutaric dialdehyde, with the purpose of increasing PVA crystallinity and establishing a crosslinked PVA network, respectively. The presence of carbon nanotubes reduced the PVA crystallization rate during the methanol treatment, but prevented the decrease of crystallinity induced by the crosslinking reaction. In comparison with the crosslinking reaction, the methanol treatment resulted in better improvement in the fibre tensile strength and less reduction in the tensile strain. In addition, the presence of carbon nanotubes reduced the onset decomposition temperature of the composite nanofibres, but stabilized the thermal degradation for the post-spinning treated nanofibres. The MWNTs/PVA composite nanofibres treated by both methanol and crosslinking reaction gave the largest improvement in the fibre tensile strength, water contact angle and thermal stability.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

This study reports the latest research into alpaca and wool fibres. In particular, those properties that have received little attention in research literature have been examined. They include single fibre abrasion and bending fatigue, single fibre tensile properties, as well as resistance to compression behaviour. These properties are important because they affect the softness and pilling propensity of these fibres and the resultant fabrics. Clean wool and alpaca fibres were used in this study. Fibre abrasion/bending fatigue measurements were carried out using a Textechno FIBRESTRESS instrument. The resistance to compression (RtC) tests were carried out according to Australian Standard AS3535-1988. The results indicate that wool and alpaca fibres behave quite differently, even though both fibre types are of animal origin. Wool fibre resistance to compression decreases as fibre diameter increases while the opposite appears to occur for alpaca fibres. For both wool and alpaca the number of abrasion/bending cycles at fibre break increases with an increase in fibre diameter, it takes longer to break the alpaca fibres. Reasons for these differences have been postulated based on differences in fibre surface and structure between alpaca and wool.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Aluminum particles (Al) were added to polypropylene (PP) in the presence of poly ethylene glycol (PEG) and polypropylene-graft-maleic anhydride to produce composites. The composites were then melt-spun into a mono filament and tested for tensile properties, diameter evenness and morphology. Melt rheological properties of Al/PP composites were studied in linear viscoelastic response regions. It was observed that level of dispersion of aluminum particles within a polypropylene composite fiber could be improved by incorporating polyethylene glycol. The improvement of dispersion led to an improvement in the fibers mechanical properties through a reduction of the coefficient of variation of fiber diameter.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

This paper describes tensile properties of a peak-aged Mg-4Y·3RE alloy at room temperature to 823 K with 10-5 - 10-1 s-1. The Mg alloy exhibited high strength (> 250 MPa) at room temperature to 473 K. However. the strength rapidly decreased at 573 K. It is suggested that a large decrease in strength at 573 K is attributed to grain boundary sliding. Also, elongation increased rapidly at 723 - 823 K. This is likely to arise from the relatively high strain rate sensitivity of about 0.3 due to the glide-controlled dislocation creep.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Silk fibroin films are promising materials for a range of biomedical applications. To understand the effects of casting solvents on film properties, we used water (W), formic acid (FA), and trifluoroacetic acid (TFA) as solvents. We characterized molecular weight, secondary structure, mechanical properties, and degradation behavior of cast films. Significant degradation of fibroin was observed for TFA-based film compared to W and TA-based films when analyzed by SDS-PAGE. Fibroin degradation resulted in a significant reduction in tensile strength and modulus of TFA-based films. Compared to water, TFA-based films demonstrated lower water solubility (19.6% vs. 62.5% in 12 h) despite having only a marginal increase in their ß-sheet content (26.9% vs. 23.7%). On the other hand, FA-based films with 34.3% ß-sheet were virtually water insoluble. Following solubility treatment, ß-sheet content in FA-based films increased to 50.9%. On exposure to protease XIV, water-annealed FA-based films lost 74% mass in 22 days compared to only 30% mass loss by ethanol annealed FA films. This study demonstrated that a small variation in the ß-sheet percentage and random coil conformations resulted in a significant change in the rates of enzymatic degradation without alteration to their tensile properties. The film surface roughness changed with the extent of enzymatic hydrolysis.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

In wool dyeing and finishing processes, fabric is often treated under conditions of different pHs and is subjected to a variety of physical and chemical environments. This work investigates fabric tensile properties at three different fabric pHs. Wool fabric extensibility under a 5 N/cm load was observed to be greatest at the wool isoelectric point of pH 4.8 and lower at both pH 2.1 and pH 7.2. The impact of pH on fabric extensibility was found to be similar to the variation in fabric hygral expansion previously observed. Fabric stress–strain curves at different pHs showed that for a given fabric extension level, the work required to stretch a fabric was less at pH 2.1 than at pH 4.8. These results suggest that the strength of wool fabric is at maximum when the pH of the fibres is close to the wool isoelectric point and that for consistency, the pH of fabric should be adjusted before standard strength tests are carried out.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The protein structures of wool, treated in fabric form with ultrasonics for different time durations, were analysed by X-ray diffraction (XRD) and Fourier transform infrared (FTIR), in comparison with the wool without ultrasonic treatment. Fabric water absorption and tensile properties were measured in addition to the fibre micro-structure analysis. It is shown that while the ultrasonic treatment had little effect on the fibre crystallinity, some chemical structures in the protein were altered to some extent during the process. Disruption of fibre internal waxy lipids upon ultrasonic treatment provided the fibres with increased water absorption. Protein chains in the macro fibrils were shown to be rearranged to a more regular and less flexible structure, as a result of the ultrasonic treatment. Fabric tensile tests showed an increased tenacity and a reduced extensibility to the ultrasonically treated fabric. Prolonged ultrasonic treatment, however, significantly reduced both fabric tenacity and extensibility.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Wool fabrics, ultrasonically treated for different time durations, were analysed by Fourier transform infrared (FTIR), differential scanning calorimeter (DSC), and thermo-gravimetric analysis (TGA), in comparison with the wool without ultrasonic treatment. Fabric tensile and thermal properties were measured in addition to the fibre micro structure analysis. Wool protein chains in the macro fibrils were shown to be rearranged to a more regular and less flexible structure, as a result of the ultrasonically treated fabric. Prolonged ultrasonic treatment, however, significantly reduced both fabric tenacity and extensibility. Wool treated with ultrasonics was found to have less mass loss and a higher thermal degradation temperature than that of without ultrasonic treatment and prolonged treated. DSC analysis showed that while ultrasonic treatment has little effect on the fibre crystallinity, an appropriate treatment can provide wool with increased water absorption.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Based on the thermo-mechanical controlled process, the effects of Si on microstructural evolution, tensile properties, impact toughness, and stretch-flangeability of ferrite and bainite dual-phase (FBDP) steels were systematically investigated. The addition of Si from 0 to 0.95% promoted the formation of fine and equiaxed ferrite grains, and high Si (0.95%) also resulted in the formation of blocky martensite islands and retained austenite. Yield and tensile strengths, and uniform and total elongations all increased with increasing Si content. Therefore, the tensile strength and ductility balance was improved by Si addition due to the increasing strain-hardening rate. The fractured morphologies after hole-expansion showed that the excellent stretch-flangeability of FBDP steels was associated with the micro-cracks propagating through in ferrite phase as well as the elongated ferrite grains along the direction perpendicular to the crack. 0.95% Si steel had a similar high combination of tensile strength and impact toughness to 0.55% Si steel, and especially 0.95% Si steel exhibited an excellent combination of tensile strength and stretch-flangeability.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Advanced high-strength steels (AHSS) are a class of steel used primarily in sheet form for automotive structures. The microstructures of the types of steel in this classification were initially multiphase, with ferrite as the dominant phase; however, grades introduced more recently have been fully martensitic or based on austenite. This chapter initially introduces the requirements of an automotive body structure, then the different classes of AHSS that have been used in the automotive industry and their typical characteristic tensile properties. The specific properties that are required for steel used in automotive body structures are subsequently described, including formability and crash behaviour. Finally, some of the current and future trends in the development of new steel grades are discussed.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Titanium alloys are widely used in various engineering design application due to its superior material properties. The traditional manufacturing of titanium products is always difficult, time consuming, high material wastage and manufacturing costs. Selective laser melting (SLM), an additive manufacturing technology has widely gained attention due to its capability to produce near net shape components with less production time. In this technical paper,microstructure,chemical composition,tensile properties and hardness are studied for the wrought and additive manufactured SLM cylindrical bar. Microstructure,mechanical properties and hardness were studied in both the longitudinal and transverse directions of the bar to study the effect of orientation. It was found that additive manufactured bar have higher yield strength, ultimate tensile strength and hardness than the wrought bar. For both conventional and SLM test samples, the yield strength, ultimate tensile strength and hardness was found to be high in the transverse direction. The difference in the properties can be attributed to the difference in microstructure as a result of processing conditions. The tensile fracture area was quantified by careful examination of the fracture surfaces in the scanning electron microscope.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The influences of hygrothermal conditioning on mechanical properties of a fiber/metal laminate (FML) have been investigated by tensile and compression tests. The environmental action, such as high moisture concentration, high temperatures, corrosive fluids or ultraviolet radiation (UV), can affect the performance of advanced composites during service. In the present work, the results show that for the glass fiber/epoxy composites tensile and compression values decrease after hygrothermal conditioning. However, no changes on mechanical properties (tensile and compression strength) are observed for the Glare laminate, regardless the hygrothermal conditioning. (C) 2006 Elsevier Ltd. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The effect of UV-C irradiation of the TPS and PCL biocomposites with sisal bleached fibers was investigated. The biocomposite was UV-C irradiated at room temperature under air atmosphere. The structural and morphological changes produced when the films were exposed to UV irradiation for 142 h, were monitored using Scanning Electron Microscopy (SEM), Mechanical Tensile Tests, Differential Scanning Calorimetry (DSC), X-ray diffraction, Thermogravimetric analysis (TGA), and Fourier transform infra-red analysis (FTIR). Addition of 5-10% fibers in composites exhibited improved mechanical and thermal properties attributed to more efficient dispersibility of fiber in the matrix and good compatibility between fibers and the matrix polymer, however, after irradiated, the tensile properties decreased due to chain scission. The samples of irradiated PCL and IFS showed crystallinity increase, whereas the blend and composites showed a decrease in crystallinity. The DSC and X-ray diffraction studies suggested interaction between polymers in the blend via carboxyl groups in thermoplastic starch-PCL and hydroxyl groups in fibers. (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The influence of hygrothermal conditioning on mechanical properties of Carall laminates have been investigated by tensile and compression tests. The environmental factors can limit the applications of composites by deteriorating the mechanical properties during service. The importance of temperature at the time of conditioning plays an important role in environmental degradation of such composite materials. In this work, the results show that for carbon fiber/epoxy composites tensile and compression values decrease after hygrothermal conditioning. However, the changes on mechanical properties of Carall are negligible, regardless the hygrothermal conditioning.