Since the end of the last millennium, the focused ion beam scanning electron microscopy (FIB-SEM) has progressively found use in biological research. This instrument is a scanning electron microscope (SEM) with an attached gallium ion column and the 2 beams, electrons and ions (FIB) are focused on one coincident point. The main application is the acquisition of three-dimensional data, FIB-SEM tomography. With the ion beam, some nanometres of the surface are removed and the remaining block-face is imaged with the electron beam in a repetitive manner. The instrument can also be used to cut open biological structures to get access to internal structures or to prepare thin lamella for imaging by (cryo-) transmission electron microscopy. Here, we will present an overview of the development of FIB-SEM and discuss a few points about sample preparation and imaging.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The influence of premetallization surface preparation on the structural, chemical, and electrical properties of Au-nGaN interfaces has been investigated by x-ray photoemission spectroscopy (XPS), current-voltage measurement (I-V) and cross-section transmission electron microscopy (TEM). XPS analysis showed that the three GaN substrate treatments investigated i.e., ex situ hydrofluoric acid etch, in situ anneal in ultrahigh-vacuum (UHV), and in situ Ga reflux cleaning in UHV result in surfaces increasingly free of oxygen contamination. XPS and TEM characterization of Au-nGaN formed after the three premetallization surface treatments show that HF etching and UHV annealing produce abrupt, well-defined interfaces. Conversely, GaN substrate cleaning in a Ga flux results in Au/GaN intermixing. I-V characterization of Au¿nGaN contacts yields a Schottky barrier height of 1.25 eV with a very low-ideality factor and very good contact uniformity for the premetallization UHV anneal, while the Ga reflux cleaning results in a much lower barrier (0.85 eV), with poor ideality and uniformity. I-V and XPS results suggest a high density of acceptor states at the surface, which is further enhanced by UHV annealing. These results are discussed in the context of current models of Schottky barrier formation.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Red blood cell (RBC) membrane fluctuations provide important insights into cell states. We present a spatial analysis of red blood cell membrane fluctuations by using digital holographic microscopy (DHM). This interferometric and dye-free technique, possessing nanometric axial and microsecond temporal sensitivities enables to measure cell membrane fluctuations (CMF) on the whole cell surface. DHM acquisition is combined with a model which allows extracting the membrane fluctuation amplitude, while taking into account cell membrane topology. Uneven distribution of CMF amplitudes over the RBC surface is observed, showing maximal values in a ring corresponding to the highest points on the RBC torus as well as in some scattered areas in the inner region of the RBC. CMF amplitudes of 35.9+/-8.9 nm and 4.7+/-0.5 nm (averaged over the cell surface) were determined for normal and ethanol-fixed RBCs, respectively.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The determination of line crossing sequences between rollerball pens and laser printers presents difficulties that may not be overcome using traditional techniques. This research aimed to study the potential of digital microscopy and 3-D laser profilometry to determine line crossing sequences between a toner and an aqueous ink line. Different paper types, rollerball pens, and writing pressure were tested. Correct opinions of the sequence were given for all case scenarios, using both techniques. When the toner was printed before the ink, a light reflection was observed in all crossing specimens, while this was never observed in the other sequence types. The 3-D laser profilometry, more time-consuming, presented the main advantage of providing quantitative results. The findings confirm the potential of the 3-D laser profilometry and demonstrate the efficiency of digital microscopy as a new technique for determining the sequence of line crossings involving rollerball pen ink and toner. With the mass marketing of laser printers and the popularity of rollerball pens, the determination of line crossing sequences between such instruments is encountered by forensic document examiners. This type of crossing presents difficulties with optical microscopic line crossing techniques involving ballpoint pens or gel pens and toner (1-4). Indeed, the rollerball's aqueous ink penetrates through the toner and is absorbed by the fibers of the paper, leaving the examiner with the impression that the toner is above the ink even when it is not (5). Novotny and Westwood (3) investigated the possibility of determining aqueous ink and toner crossing sequences by microscopic observation of the intersection before and after toner removal. A major disadvantage of their study resides in destruction of the sample by scraping off the toner line to see what was underneath. The aim of this research was to investigate the ways to overcome these difficulties through digital microscopy and three-dimensional (3-D) laser profilometry. The former was used as a technique for the determination of sequences between gel pen and toner printing strokes, but provided less conclusive results than that of an optical stereomicroscope (4). 3-D laser profilometry, which allows one to observe and measure the topography of a surface, has been the subject of a number of recent studies in this area. Berx and De Kinder (6) and Schirripa Spagnolo (7,8) have tested the application of laser profilometry to determine the sequence of intersections of several lines. The results obtained in these studies overcome disadvantages of other methods applied in this area, such as scanning electron microscope or the atomic force microscope. The main advantages of 3-D laser profilometry include the ease of implementation of the technique and its nondestructive nature, which does not require sample preparation (8-10). Moreover, the technique is reproducible and presents a high degree of freedom in the vertical axes (up to 1000 μm). However, when the paper surface presents a given roughness, if the pen impressions alter the paper with a depth similar to the roughness of medium, the results are not always conclusive (8). It becomes difficult in this case to distinguish which characteristics can be imputed to the pen impressions or the quality of the paper surface. This important limitation is assessed by testing different types of paper of variable quality (of different grammage and finishing) and the writing pressure. The authors will therefore assess the limits of 3-D laser profilometry technique and determine whether the method can overcome such constraints. Second, the authors will investigate the use of digital microscopy because it presents a number of advantages: it is efficient, user-friendly, and provides an objective evaluation and interpretation.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A method for the quantitative analysis of the hydrophobicity of the mycelial mat of filamentous fungi based on contact angle measurements is presented. It was tested for a range of fungi belonging to the classes of basidiomycetes, ascomycetes and deuteromycetes. The measured contact angles of the mycelial mats ranged between hydrophilic (<30 degrees) for the deuteromycetes Fusarium oxysporum Fo47 GUS1 and Trichoderma harzianum P1[pZEGA1] and hydrophobic (>60 degrees) for the ascomycete Cladosporium sp. DSE48.1b and the basidiomycetes Paxillus involutus WSL 37.7, Hebeloma crustiliniforme WSL 6.2, Suillus bovinus WSL 48.1 and Laccaria bicolor WSL 73.1. For some fungi, variations in the hydrophobicity of the mycelium depending on the growth medium, the physiological state and the exposure to water were distinguished.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Drug-nanoparticle conjugates: The anticancer drug camptothecin (CPT) was covalently linked at the surface of ultrasmall superparamagnetic iron oxide nanoparticles (USPIOs) via a linker, allowing drug release by cellular esterases. Nanoparticles were hierarchically built to achieve magnetically-enhanced drug delivery to human cancer cells and antiproliferative activity.The linking of therapeutic drugs to ultrasmall superparamagnetic iron oxide nanoparticles (USPIOs) allowing intracellular release of the active drug via cell-specific mechanisms would achieve tumor-selective magnetically-enhanced drug delivery. To validate this concept, we covalently attached the anticancer drug camptothecin (CPT) to biocompatible USPIOs (iron oxide core, 9-10 nm; hydrodynamic diameter, 52 nm) coated with polyvinylalcohol/polyvinylamine (PVA/aminoPVA). A bifunctional, end-differentiated dicarboxylic acid linker allowed the attachment of CPT to the aminoPVA as a biologically labile ester substrate for cellular esterases at one end, and as an amide at the other end. These CPT-USPIO conjugates exhibited antiproliferative activity in vitro against human melanoma cells. The intracellular localization of CPT-USPIOs was confirmed by transmission electron microscopy (iron oxide core), suggesting localization in lipid vesicles, and by fluorescence microscopy (CPT). An external static magnetic field applied during exposure increased melanoma cell uptake of the CPT-USPIOs.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Intracellular mature vaccinia virus, also called intracellular naked virus, and its core envelope have been observed in their native, unfixed, unstained, hydrated states by cryoelectron microscopy of vitrified samples. The virion appears as a smooth rounded rectangle of ca. 350 by 270 nm. The core seems homogeneous and is surrounded by a 30-nm-thick surface domain delimited by membranes. We show that surface tubules and most likely also the characteristic dumbbell-shaped core with the lateral bodies which are generally observed in negatively stained or conventionally embedded samples are preparation artifacts.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Over the last two decades, Atomic Force Microscopy (AFM) has emerged as the tool of choice to image living organisms in a near-physiological environment. Whereas fluorescence microscopy techniques allow labeling and tracking of components inside cells and the observation of dynamic processes, AFM is mainly a surface technique that can be operated on a wide range of substrates including biological samples. AFM enables extraction of topographical, mechanical and chemical information from these samples.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the last two decades, the third-dimension has become a focus of attention in electron microscopy to better understand the interactions within subcellular compartments. Initially, transmission electron tomography (TEM tomography) was introduced to image the cell volume in semi-thin sections (∼500nm). With the introduction of the focused ion beam scanning electron microscope, a new tool, FIB-SEM tomography, became available to image much larger volumes. During TEM tomography and FIB-SEM tomography, the resin section is exposed to a high electron/ion dose such that the stability of the resin embedded biological sample becomes an important issue. The shrinkage of a resin section in each dimension, especially in depth, is a well-known phenomenon. To ensure the dimensional integrity of the final volume of the cell, it is important to assess the properties of the different resins and determine the formulation which has the best stability in the electron/ion beam. Here, eight different resin formulations were examined. The effects of radiation damage were evaluated after different times of TEM irradiation. To get additional information on mass-loss and the physical properties of the resins (stiffness and adhesion), the topography of the irradiated areas was analysed with atomic force microscopy (AFM). Further, the behaviour of the resins was analysed after ion milling of the surface of the sample with different ion currents. In conclusion, two resin formulations, Hard Plus and the mixture of Durcupan/Epon, emerged that were considerably less affected and reasonably stable in the electron/ion beam and thus suitable for the 3-D investigation of biological samples.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Résumé L'eau est souvent considérée comme une substance ordinaire puisque elle est très commune dans la nature. En fait elle est la plus remarquable de toutes les substances. Sans l'eau la vie sur la terre n'existerait pas. L'eau représente le composant majeur de la cellule vivante, formant typiquement 70 à 95% de la masse cellulaire et elle fournit un environnement à d'innombrables organismes puisque elle couvre 75% de la surface de terre. L'eau est une molécule simple faite de deux atomes d'hydrogène et un atome d'oxygène. Sa petite taille semble en contradiction avec la subtilité de ses propriétés physiques et chimiques. Parmi celles-là, le fait que, au point triple, l'eau liquide est plus dense que la glace est particulièrement remarquable. Malgré son importance particulière dans les sciences de la vie, l'eau est systématiquement éliminée des spécimens biologiques examinés par la microscopie électronique. La raison en est que le haut vide du microscope électronique exige que le spécimen biologique soit solide. Pendant 50 ans la science de la microscopie électronique a adressé ce problème résultant en ce moment en des nombreuses techniques de préparation dont l'usage est courrant. Typiquement ces techniques consistent à fixer l'échantillon (chimiquement ou par congélation), remplacer son contenu d'eau par un plastique doux qui est transformé à un bloc rigide par polymérisation. Le bloc du spécimen est coupé en sections minces (d’environ 50 nm) avec un ultramicrotome à température ambiante. En général, ces techniques introduisent plusieurs artefacts, principalement dû à l'enlèvement d'eau. Afin d'éviter ces artefacts, le spécimen peut être congelé, coupé et observé à basse température. Cependant, l'eau liquide cristallise lors de la congélation, résultant en une importante détérioration. Idéalement, l'eau liquide est solidifiée dans un état vitreux. La vitrification consiste à refroidir l'eau si rapidement que les cristaux de glace n'ont pas de temps de se former. Une percée a eu lieu quand la vitrification d'eau pure a été découverte expérimentalement. Cette découverte a ouvert la voie à la cryo-microscopie des suspensions biologiques en film mince vitrifié. Nous avons travaillé pour étendre la technique aux spécimens épais. Pour ce faire les échantillons biologiques doivent être vitrifiés, cryo-coupées en sections vitreuse et observées dans une cryo-microscope électronique. Cette technique, appelée la cryo- microscopie électronique des sections vitrifiées (CEMOVIS), est maintenant considérée comme étant la meilleure façon de conserver l'ultrastructure de tissus et cellules biologiques dans un état très proche de l'état natif. Récemment, cette technique est devenue une méthode pratique fournissant des résultats excellents. Elle a cependant, des limitations importantes, la plus importante d'entre elles est certainement dû aux artefacts de la coupe. Ces artefacts sont la conséquence de la nature du matériel vitreux et le fait que les sections vitreuses ne peuvent pas flotter sur un liquide comme c'est le cas pour les sections en plastique coupées à température ambiante. Le but de ce travail a été d'améliorer notre compréhension du processus de la coupe et des artefacts de la coupe. Nous avons ainsi trouvé des conditions optimales pour minimiser ou empêcher ces artefacts. Un modèle amélioré du processus de coupe et une redéfinitions des artefacts de coupe sont proposés. Les résultats obtenus sous ces conditions sont présentés et comparés aux résultats obtenus avec les méthodes conventionnelles. Abstract Water is often considered to be an ordinary substance since it is transparent, odourless, tasteless and it is very common in nature. As a matter of fact it can be argued that it is the most remarkable of all substances. Without water life on Earth would not exist. Water is the major component of cells, typically forming 70 to 95% of cellular mass and it provides an environment for innumerable organisms to live in, since it covers 75% of Earth surface. Water is a simple molecule made of two hydrogen atoms and one oxygen atom, H2O. The small size of the molecule stands in contrast with its unique physical and chemical properties. Among those the fact that, at the triple point, liquid water is denser than ice is especially remarkable. Despite its special importance in life science, water is systematically removed from biological specimens investigated by electron microscopy. This is because the high vacuum of the electron microscope requires that the biological specimen is observed in dry conditions. For 50 years the science of electron microscopy has addressed this problem resulting in numerous preparation techniques, presently in routine use. Typically these techniques consist in fixing the sample (chemically or by freezing), replacing its water by plastic which is transformed into rigid block by polymerisation. The block is then cut into thin sections (c. 50 nm) with an ultra-microtome at room temperature. Usually, these techniques introduce several artefacts, most of them due to water removal. In order to avoid these artefacts, the specimen can be frozen, cut and observed at low temperature. However, liquid water crystallizes into ice upon freezing, thus causing severe damage. Ideally, liquid water is solidified into a vitreous state. Vitrification consists in solidifying water so rapidly that ice crystals have no time to form. A breakthrough took place when vitrification of pure water was discovered. Since this discovery, the thin film vitrification method is used with success for the observation of biological suspensions of. small particles. Our work was to extend the method to bulk biological samples that have to be vitrified, cryosectioned into vitreous sections and observed in cryo-electron microscope. This technique is called cryo-electron microscopy of vitreous sections (CEMOVIS). It is now believed to be the best way to preserve the ultrastructure of biological tissues and cells very close to the native state for electron microscopic observation. Since recently, CEMOVIS has become a practical method achieving excellent results. It has, however, some sever limitations, the most important of them certainly being due to cutting artefacts. They are the consequence of the nature of vitreous material and the fact that vitreous sections cannot be floated on a liquid as is the case for plastic sections cut at room temperature. The aim of the present work has been to improve our understanding of the cutting process and of cutting artefacts, thus finding optimal conditions to minimise or prevent these artefacts. An improved model of the cutting process and redefinitions of cutting artefacts are proposed. Results obtained with CEMOVIS under these conditions are presented and compared with results obtained with conventional methods.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

L?objectif de ce travail de thèse est l?étude des changements conformationels des biomacromolecules à l?échelle d?une molécule unique. Pour cela on a utilisé la Microscopie à Force Atomique (AFM) appliqué à l?étude des protéines et des acides nucléiques déposés sur une surface. Dans ce type de microscopie, une pointe très fine attachée à l?extrémité d?un levier est balayée au dessus d?une surface. L?interaction de la pointe avec la surface de l?échantillon induit la déflection du levier et ce phénomène permet de reconstruire la topographie de l?échantillon. Très importante dans cette technique est la possibilité de travailler en liquide. Cela permet de étudier les biomolécules en conditions quasi-physiologiques sans qu?elles perdent leur activité. On a étudié GroEL, la chaperonin de E.coli, qui est un homo oligomère avec une structure à double anneau qui joue un rôle très important dans le repliement des protéines dénaturées et celles qui viennent d?être synthétisées. En particulier on a focalisé notre attention sur la stabilité mécanique et sur les changements conformationels qui ont lieu pendant l?activité de GroEL. Une analyse détaillée des changements dans la stabilité mécanique et des effets produits par la liaison et l?hydrolyse de l?ATP est présentée dans ce travail. On a montré que le point le plus faible dans la structure de GroEL est l?interface entre les deux anneaux et que l?étape critique dans l?affaiblissement de la structure est l?hydrolyse de l?ATP. En ce qui concerne le changement conformationel, le passage d?une surface hydrophobe à hydrophile, induit par l?hydrolyse de l?ATP, a été montré. Ensuite on a étudié le changement dans la conformation et dans la topologie de l?ADN résultant de l?interaction avec des molécules spécifiques et en réponse à l?exposition des cellules de E.coli à des conditions de stress. Le niveau de surenroulement est un paramètre très sensible, de façon variée, à tous ces facteurs. Les cellules qui ont crus à de températures plus élevées que leur température optimale ont la tendance à diminuer le nombre de surenroulements négatif pour augmenter la stabilité thermique de leur plasmides. L?interaction avec des agents intercalant induit une transition d?un surenroulement négatif à un surenroulement positif d?une façon dépendante de la température. Finalement, l?effet de l?interaction de l?ADN avec des surfaces différentes a été étudié et une application pratique sur les noeuds d?ADN est présentée.<br/><br/>The aim of the present thesis work is to study the conformational changes of biomacromolecules at the single molecule level. To that end, Atomic Force Microcopy (AFM) imaging was performed on proteins and nucleic acids adsorbed onto a surface. In this microcopy technique a very sharp tip attached at the end of a soft cantilever is scanned over a surface, the interaction of the tip with the sample?s surface will induce the deflection of the cantilever and thus it will make possible to reconstruct the topography. A very important feature of AFM is the possibility to operate in liquid, it means with the sample immersed in a buffer solution. This allows one to study biomolecules in quasi-physiological conditions without loosing their activity. We have studied GroEL, the chaperonin of E.coli, which is a double-ring homooligomer which pays a very important role in the refolding of unfolded and newly synthetized polypeptides. In particular we focus our attention on its mechanical stability and on the conformational change that it undergoes during its activity cycle. A detailed analysis of the change in mechanical stability and how it is affected by the binding and hydrolysis of nucleotides is presented. It has been shown that the weak point of the chaperonin complex is the interface between the two rings and that the critical step to weaken the structure is the hydrolysis of ATP. Concerning the conformational change we have directly measured, with a nanometer scale resolution, the switching from a hydrophobic surface to a hydrophilic one taking place inside its cavity induced by the ATP hydrolysis. We have further studied the change in the DNA conformation and topology as a consequence of the interaction with specific DNA-binding molecules and the exposition of the E.coli cells to stress conditions. The level of supercoiling has been shown to be a very sensitive parameter, even if at different extents, to all these factors. Cells grown at temperatures higher than their optimum one tend to decrease the number of the negative superhelical turns in their plasmids in order to increase their thermal stability. The interaction with intercalating molecules induced a transition from positive to negative supercoiling in a temperature dependent way. The effect of the interaction of the DNA with different surfaces has been investigated and a practical application to DNA complex knots is reported.<br/><br/>Observer les objets biologiques en le touchant Schématiquement le Microscope a Force Atomique (AFM) consiste en une pointe très fine fixée a l?extrémité d?un levier Lors de l?imagerie, la pointe de l?AFM gratte la surface de l?échantillon, la topographie de celui-ci induit des déflections du levier qui sont enregistrées au moyen d?un rayon laser réfléchi par le levier. Ces donnés sont ensuit utilisés par un ordinateur pour reconstituer en 3D la surface de l?échantillon. La résolution de l?instrument est fonction entre autre de la dureté, de la rugosité de l?échantillon et de la forme de la pointe. Selon l?échantillon et la pointe utilisée la résolution de l?AFM peut aller de 0.1 A (sur des cristaux) a quelque dizaine de nanomètres (sur des cellules). Cet instrument est particulierment intéressant en biologie en raison de sa capacité à imager des échantillons immergés dans un liquide, c?est à dire dans des conditions quasiphysiologiques. Dans le cadre de ce travail nous avons étudié les changements conformationels de molécules biologiques soumises à des stimulations externes. Nous avons essentielment concentré notre attention sur des complexes protéiques nommé Chaperons Moléculaires et sur des molécules d?ADN circulaire (plasmides). Les Chaperons sont impliqués entre autre dans la résistance des organismes vivants aux stress thermiques et osmotiques. Leur activité consiste essentielment à aider les autres protéines à être bien pliés dans leur conformation finale et, en conséquence, à eviter que ils soient dénaturées et que ils puissent s?agréger. L?ADN, quant à lui est la molécule qui conserve, dans sa séquence, l?information génétique de tous les organismes vivants. Ce travail a spécifiquement concerné l?étude des changements conformationels des chaperonins suit a leur activation par l?ATP. Ces travaux ont montrés a l?échelle de molécule unique la capacité de ces protéines de changer leur surface de hydrophobique a hydrophilique. Nous avons également utilisé l?AFM pour étudier le changement du nombre des surenroulements des molécules d?ADN circulaire lors d?une exposition à un changement de température et de force ionique. Ces travaux ont permis de montrer comment la cellule regle le nombre de surenroulements dans ces molécules pour répondre et contrôler l?expression génétique même dans de conditions extrêmes. Pour les deux molécules en général, c?était très important d?avoir la possibilité de observer leur transitions d?une conformation a l?autre directement a l?échelle d?une seul molécule et, surtout, avec une résolution largement au dessous des la longueur d?onde de la lumière visible que représente le limite pour l?imagerie optique.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this article, we explore the possibility of modifying the silicon nanocrystal areal density in SiOx single layers, while keeping constant their size. For this purpose, a set of SiOx monolayers with controlled thickness between two thick SiO2 layers has been fabricated, for four different compositions (x=1, 1.25, 1.5, or 1.75). The structural properties of the SiO x single layers have been analyzed by transmission electron microscopy (TEM) in planar view geometry. Energy-filtered TEM images revealed an almost constant Si-cluster size and a slight increase in the cluster areal density as the silicon content increases in the layers, while high resolution TEM images show that the size of the Si crystalline precipitates largely decreases as the SiO x stoichiometry approaches that of SiO2. The crystalline fraction was evaluated by combining the results from both techniques, finding a crystallinity reduction from 75% to 40%, for x = 1 and 1.75, respectively. Complementary photoluminescence measurements corroborate the precipitation of Si-nanocrystals with excellent emission properties for layers with the largest amount of excess silicon. The integrated emission from the nanoaggregates perfectly scales with their crystalline state, with no detectable emission for crystalline fractions below 40%. The combination of the structural and luminescence observations suggests that small Si precipitates are submitted to a higher compressive local stress applied by the SiO2 matrix that could inhibit the phase separation and, in turn, promotes the creation of nonradiative paths.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Spectroscopic ellipsometry and high resolution transmission electron microscopy have been used to characterize microcrystalline silicon films. We obtain an excellent agreement between the multilayer model used in the analysis of the optical data and the microscopy measurements. Moreover, thanks to the high resolution achieved in the microscopy measurements and to the improved optical models, two new features of the layer-by-layer deposition of microcrystalline silicon have been detected: i) the microcrystalline films present large crystals extending from the a-Si:H substrate to the film surface, despite the sequential process in the layer-by-layer deposition; and ii) a porous layer exists between the amorphous silicon substrate and the microcrystalline silicon film.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Glasses with low silica content are very susceptible to suffer pronounced degradation when exposed to room atmosphere during short times. In this work the results of the degradation of the surface of a metasilicate glass with composition 2Na2O.1CaO.3SiO2 are presented. Optical and scanning electron microscopy observations, X-ray diffraction, infrared and Raman microprobe spectroscopic measurements of the modified surface of this glass show strong evidences that it is formed essentially by a crystalline carbonate layer.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This thesis presents experimental studies of rare earth (RE) metal induced structures on Si(100) surfaces. Two divalent RE metal adsorbates, Eu and Yb, are investigated on nominally flat Si(100) and on vicinal, stepped Si(100) substrates. Several experimental methods have been applied, including scanning tunneling microscopy/spectroscopy (STM/STS), low energy electron diffraction (LEED), synchrotron radiation photoelectron spectroscopy (SR-PES), Auger electron spectroscopy (AES), thermal desorption spectroscopy (TDS), and work function change measurements (Δφ). Two stages can be distinguished in the initial growth of the RE/Si interface: the formation of a two-dimensional (2D) adsorbed layer at submonolayer coverage and the growth of a three-dimensional (3D) silicide phase at higher coverage. The 2D phase is studied for both adsorbates in order to discover whether they produce common reconstructions or reconstructions common to the other RE metals. For studies of the 3D phase Yb is chosen due to its ability to crystallize in a hexagonal AlB2 type lattice, which is the structure of RE silicide nanowires, therefore allowing for the possibility of the growth of one-dimensional (1D) wires. It is found that despite their similar electronic configuration, Eu and Yb do not form similar 2D reconstructions on Si(100). Instead, a wealth of 2D structures is observed and atomic models are proposed for the 2×3-type reconstructions. In addition, adsorbate induced modifications on surface morphology and orientational symmetry are observed. The formation of the Yb silicide phase follows the Stranski-Krastanov growth mode. Nanowires with the hexagonal lattice are observed on the flat Si(100) substrate, and moreover, an unexpectedly large variety of growth directions are revealed. On the vicinal substrate the growth of the silicide phase as 3D islands and wires depends drastically on the growth conditions. The conditions under which wires with high aspect ratio and single orientation parallel to the step edges can be formed are demonstrated.