979 resultados para SUPERSATURATED SOLID SOLUTIONS


Relevância:

90.00% 90.00%

Publicador:

Resumo:

The tensile deformation behavior of a range of supersaturated Mg-Al solid solutions and an as-cast magnesium alloy AM60 has been studied. The Mg-Al alloys were tested at room temperature while the alloy AM60 was tested in the temperature range 293-573 K. The differences in the deformation behavior of the alloys is discussed in terms of hardening and softening processes. In order to identify which processes were active, the stress dependence of the strain-hardening coefficient was assessed using Lukac and Balik's model of hardening and softening. The analysis indicates that hardening involves solid solution hardening and interaction with forest dislocations and non-dislocation obstacles such as second phase particles. Cross slip is not a significant recovery process in the temperature range 293-423 K. At temperatures between 473 and 523 K the analysis suggests that softening is controlled by cross slip and climb of dislocations. At temperatures above 523 K softening seems to be controlled by dynamic recrystallisation. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Arsenogorceixite BaAl3AsO3(OH)(AsO4,PO4)(OH,F)6 belongs to the crandallite mineral subgroup of the alunite supergroup. Arsenogorceixite forms a continuous series of solid solutions with related minerals including gorceixite, goyazite, arsenogoyazite, plumbogummite and philipsbornite. Two minerals from (a) Germany and (b) from Ashburton Downs, Australia were analysed by Raman spectroscopy. The spectra show some commonality but the intensities of the peaks vary. Sharp intense Raman bands for the German sample, are observed at 972 and 814 cm−1 attributed to the ν1 PO43− and AsO43− symmetric stretching modes. Raman bands at 1014, 1057, 1148 and 1160 cm−1 are attributed to the ν1 PO2 symmetric stretching mode and ν3 PO43− antisymmetric stretching vibrations. Raman bands at 764 and 776 cm−1 and 758 and 756 cm−1 are assigned to the ν3 AsO43− antisymmetric stretching vibrations. For the Australian mineral, the ν1 PO43− band is found at 973 cm−1. The intensity of the arsenate bands observed at 814, 838 and 870 cm−1 is greatly enhanced. Two low intensity Raman bands at 1307 and 1332 cm−1 are assigned to hydroxyl deformation modes. The intense Raman band at 441 cm−1 with a shoulder at 462 cm−1 is assigned to the ν2 PO43− bending mode. Raman bands at 318 and 340 cm−1 are attributed to the (AsO4)3−ν2 bending. The broad band centred at 3301 cm−1 is assigned to water stretching vibrations and the sharper peak at 3473 cm−1 is assigned to the OH stretching vibrations. The observation of strong water stretching vibrations brings into question the actual formula of arsenogorceixite. It is proposed the formula is better written as BaAl3AsO3(OH)(AsO4,PO4)(OH,F)6·xH2O. The observation of both phosphate and arsenate bands provides a clear example of solid solution formation.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Complexes of the type \[M(phen)3](PF6)2 (M = Ni(II), Fe(II), Ru(II) and phen = 1,10-phenanthroline) were found to co-crystallize to form molecular alloys (solid solutions of molecules) with general formula \[MAxMB1–x(phen)3](PF6)2·0.5H2O in which the relative concentrations of the metal complexes in the crystals closely match those in the crystallizing solution. Consequently, the composition of the co-crystals can be accurately predicted and controlled by modulating the relative concentrations of the metal complexes in the crystallizing solution. Although they are chemically and structurally similar, complexes of the type \[M(bipy)3](PF6)2 (M = Ni(II), Fe(II), Ru(II) and bipy = 2,2′-bipyridine) display markedly different behavior upon co-crystallization. In this case, the resulting co-crystals of general formula \[MAxMB1–x(bipy)3](PF6)2 have relative concentrations of the constituent complexes that are markedly different from the relative concentrations of the complexes initially present in the crystallizing solution. For example, when the nickel and iron complexes are co-crystallized from a solution containing a 50:50 ratio of each, the result is the formation of some crystals with a higher proportion of iron and others with a higher proportion of nickel. The relative concentrations of the metal complexes in the crystals can vary from those in the crystallizing solutions by as much as 15%. This result was observed for a range of combinations of metal complexes (Ni/Fe, Ni/Ru, and Fe/Ru) and a range of starting concentrations in the crystallizing solutions (90:10 through to 10:90 in 10% increments). To explain this remarkable result, we introduce the concept of “supramolecular selection”, which is a process driven by molecular recognition that leads to the partially selective aggregation of like molecules during crystallization.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

To study the phase relations in the Bi-2212 and Yb2O3 system, Bi2Sr2Ca1-xYbxCu 2Oy thick films are prepared by partial melt processing via an intermediate reaction between Bi-2212 and Yb2O3. When Bi-2212 and Yb2O3 are partially melted and then slowly cooled, solid solutions of Bi2Sr2Ca 1-xYbxCu2Oy, form by reactions between liquid and solid phases which contain Yb. Following these reactions, Ca is partially replaced in Bi-2212 matrix and participates in the formation of secondary phases, such as Bi-free, (Ca, Sr)Ox and CaO. Variation of the Bi-2212-Yb2O3 ratios and processing parameters changes the balance between the phases and leads to different Yb:Ca ratios in the Bi-2212 matrix of processed thick films. When the partial melting process is optimized for each sample to minimize the growth of secondary phases, x = 0.42-0.46 for the samples prepared at pO2 = 0.01 atm, x = 0.24-0.29 for the samples prepared at pO2 = 0.21 atm, x = 0.18-0.23 for the samples prepared at pO2 = 0.99 atm are obtained regardless to the starting compositions. It is found that superconducting properties of Bi 2Sr2Ca1-xYbxCu2O y thick films strongly depend on the processing conditions, because the conditions result in different Yb content in the Bi-2212 matrix and the volume fraction of the secondary phases. The highest Tc(0) of 77, 90 and 91 K were obtained for the samples processed at 0.01, 0.21 and 0.99 atm of O2, respectively.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Mobile video, as an emerging market and a promising research field, has attracted much attention from both industry and researchers. Considering the quality of user-experience as the crux of mobile video services, this chapter aims to provide a guide to user-centered studies of mobile video quality. This will benefit future research in better understanding user needs and experiences, designing effective research, and providing solid solutions to improve the quality of mobile video. This chapter is organized in three main parts: (1) a review of recent user studies from the perspectives of research focuses, user study methods, and data analysis methods; (2) an example of conducting a user study of mobile video research, together with the discussion on a series of relative issues, such as participants, materials and devices, study procedure, and analysis results, and; (3) a conclusion with an open discussion about challenges and opportunities in mobile video related research, and associated potential future improvements.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The precipitation processes in dilute nitrogen alloys of titanium have been examined in detail by conventional transmission electron microscopy (CTEM) and high-resolution electron microscopy (HREM). The alloy Ti-2 at. pct N on quenching from its high-temperature beta phase field has been found to undergo early stages of decomposition. The supersaturated solid solution (alpha''-hcp) on decomposition gives rise to an intimately mixed, irresolvable product microstructure. The associated strong tweed contrast presents difficulties in understanding the characteristic features of the process. Therefore, HREM has been carried out with a view to getting a clear picture of the decomposition process. Studies on the quenched samples of the alloy suggest the formation of solute-rich zones of a few atom layers thick, randomly distributed throughout the matrix. On aging, these zones grow to a size beyond which the precipitate/matrix interfaces appear to become incoherent and the alpha' (tetragonal) product phase is seen distinctly. The structural details, the crystallography of the precipitation process, and the sequence of precipitation reaction in the system are illustrated.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The photocatalytic ability of cubic Bi1.5ZnNb1.5O7 (BZN) pyrochlore for the decolorization of an acid orange 7 (AO7) azo dye in aqueous solution under ultraviolet (UV) irradiation has been investigated for the first time. BZN catalyst powders prepared using low temperature sol-gel and higher temperature solid-state methods have been evaluated and their reaction rates have been compared.The experimental band gap energy has been estimated from the optical absorption edge and has been used as reference for theoretical calculations. The electronic band structure of BZN has been investigated using first-principles density functional theory (DFT) calculations for random, completely and partially ordered solid solutions of Zn cations in both the A and B sites of the pyrochlore structure.The nature of the orbitals in the valence band (VB) and the conduction band (CB) has been identified and the theoretical band gap energy has been discussed in terms of the DFT model approximations.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

There have been major advances in the past couple of years in the rational synthesis of inorganic solids: synthesis of mercury-based superconducting cuprates showing transition temperatures up to 150 K; ZrP2-xVxO7 solid solutions showing zero or negative thermal expansion; copper oxides possessing ladder structures such as La1-xSrxCuO2.5; synthesis of mesoporous oxide materials having adjustable pore size in the range 15-100 Angstrom; and synthesis of a molecular ferromagnet showing a critical temperature of 18.6 K. Despite great advances in probing the structures of solids and measurement of their physical properties, the design and synthesis of inorganic solids possessing desired structures and properties remain a challenge today. With the availability of a variety of mild chemistry-based approaches, kinetic control of synthetic pathways is becoming increasingly possible, which, it is hoped, will eventually make rational design of inorganic solids a reality.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Sr2FeMoO6 oxides exhibit a half-metallic ferromagnetic (HM-FM) ground state and peculiar magnetic and magnetotransport properties, which are interesting for applications in the emerging field of spintronics and attractive for fundamental research in the field of heavily correlated electron systems. Sr2FeWO6 is an insulator with an antiferromagnetic (I-AFM) ground state. The solid solutions Sr2FeMoxW1-xO6 also have peculiar properties-W doping enhances chemical order which allows stabilization of the HM-FM state; as the W content exceeds a certain value a metal to insulator transition (MIT) occurs. The role of W in determining the physical properties of Sr2FeMoxW1-xO6 systems has been a matter of intense investigation. This work deals with the problem of the structural and electronic changes related to the MIT from a local perspective by means of x-ray absorption spectroscopy (XAS). This technique allows one to probe in detail the local structure and electronic modifications around selected absorber ions (W, Mo, Fe and Sr in our case). The results of XAS analysis in the whole composition range (0 <= x <= 1), in the near edge (XANES) and extended (EXAFS) regions, demonstrate an abrupt change of the local structure around the Fe and Mo sites at the critical composition, x(c). This change represents the microstructural counterpart associated with the MIT. Conversely, the local structure and electronic configuration of W ions remain unaltered in the whole composition range, suggesting indirect participation of W in the MIT.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The intensity of the EPR signal with g = 5.985 arising from a ferric ion â oxygen vacancy defect pair (Fe3+ â VO) in PbTiO3, varies with the extent of PbO nonstoichiometry at constant Fe3+ content due to an increased oxygen vacancy concentration. In PZT solid solutions, the signal intensity decreases with an increase in Zr. A lower intensity is also noticed for Fe3+ â VO signals in PbZrO3. This behaviour is explained on the basis of PbO nonstoichiometry arising from independent Pb- and O-vacancies as well as the randomly distributed crystallographic shear (CS) plane defects. The contribution to PbO nonstoichiometry from CS planes is larger in high zirconium compositions of PZT.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Attempts to prepare BaSnO3 by the hydrothermal method starting from SnO2·xH2O gel and Ba (OH)2 solution in teflonlined autoclaves at 150–260°C invariably lead to the formation of a hydrated phase, BaSn(OH)6·3H2O. On heating in air or on releasing the pressure Image at ≈260°C, BaSN (OH)6·3H2O converts to BaSnO3 fine powder which involves the formation of an intermediate oxyhydroxide, BaSnO(OH)4. TEM studies show that particle size of the resulting BaSnO3 ranges from 0.2–0.6 μm. Solid solutions of Ba(Ti, Sn) O3 were prepared from (TiO2+SnO2)·xH2O mixed gel and Ba(OH)2 solutions. Single-phase perovskite Ba(Ti, Sn)O3 was obtained up to 35 atom % Sn. Above this composition, the hydrothermal products are mixtures of BaTiO3 (cubic) and BaSn(OH)6·3H2O which on heating at ≈260°C give rise to BaTiO3+BaSnO3. Annealing at 1000°C results in monophasic Ba(Ti, Sn)O3, in the complete range of Sn/Ti. Formation of the hydrated phase is attributed to the amphoteric nature of SnO2·xH2O gel which stabilises Sn(OH)62− anions under higher H2O-pressures and elevated temperatures. The sintering characteristics and dielectric properties of ceramics prepared from these fine powders are presented.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The tie lines delineating ion-exchange equilibria between MCr2O4-MAl2O4 spinel solid solution, where M is either Mn or Co, and Cr2O3-Al2O3 solid solution with the corundum structure were determined at 1373 K by electron microprobe and E0AX point count analysis of the oxide phases equilibrated with metallic Co and Au-5% Mn. The component activities in the spinel solid solutions are derived from the tie lines and the thernodynamic data for Cr2O3-Al2O3 soiid solutions available hi the literature. The Gibbs free energies of mixing calculated from the experimental data are discussed in relation to the values derived from the cation distribution a.odel based on the site preference energies and assuming random mixing on both tetrahedral and octahedral sites. Positive deviations from ideality observed in this study suggest a miscibility gap for both series of spinel solid solutions at low temperatures in the absence of oxidation.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Rare-earth trioxocobaltates(lll), Ln[CoO,], with Ln = Pr, Nd, Tb, Dy. and Yb exhibit low-spin to high-spin transitions of cobalt characterised by a maximum in the Ax-l against temperature plots where Ax is the cobalt contribution to the magnetic susceptibility. The susceptibility behaviour is distinct from that of La[CoO,] which shows a plateau in the x-I-T curve accompanied by a structural transition. The temperature at which the AX- I-T curve shows a maximum increases with the decrease in the size of the rare-earth ion. The susceptibility behavior of solid solutions of La,,Nd,CoO, has been investigated to see how the behaviour characteristic of Nd[CoO,] changes to that of La[CoO,].

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Fine powders of submicron-sized crystallites of BaTiO3 were prepared at 85–130°C by the hydrothermal method, starting from TiO2.ξH2O gel and Ba(OH)2 solution. The products obtained below 110°C incorporated considerable amounts of H2O and OH− in the lattice. As-prepared BaTiO3 is cubic and converts to the tetragonal phase after heat treatment at 1200°C, accompanied by the loss of residual OH− ions. Hydrothermal reaction of SnO2.ξH2O gel with Ba(OH)2 at 150–260°C gives rise to the hydrated phase, BaSn(OH)6.3H2O, due to the amphoteric nature of SnO2.ξH2O which stabilises Sn(OH)62− anions in basic media. On heating in air or releasing the pressure in situ at 260°C, BaSn(OH)6.3H2O converts to BaSnO3 through an intermediate, BaSnO(OH)4. Solid solutions of Ba(Ti,Sn)O3 are directly formed from (TiO2 + SnO2)..ξH2O gel up to 35 mol% SnO2. At higher Sn contents, the hydrothermal products are mixtures of BaSn(OH)6.3H2O and BaTiO3, which on annealing at 1000°C result in monophasic Ba(Ti,Sn)O3. The sintering characteristics and the dielectric properties of the ceramics prepared out of these fine powders are presented. The dielectric properties of fine-grained Ba(Ti,Sn)O3 ceramics are explained on the basis of the prevailing diffuse phase transition behaviour.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The aim of this research is to study the boundary zone of home and work and the tensions people experience while reconciling home and work? How are the requirements of the family, the home and the work taken care of in everyday life? What kind of difficulties does the individual experience when reconciling home activities and job requirements together? What kind of activity policies have families created to ease the everyday life? What kind of goals and requirements do families feel behind the difficulties in adjusting home and work? What kind of changes would make the adjusting of home and work easier? The changing family life, everyday home activities and the changing Finnish working life are studied to describe the adjusting of home and work. In addition the boundary zone of home and work and its tensions are studied. 337 research persons who find reconciling home and work challenging were elected from different sectors of the working life. Research persons were gathered from the public, private and third sectors. The research material was gathered with a semi-structured qualitative questionnaire published in internet. Contents analysis was the analysis method of the research material. The tensions of adjusting home and work are various. Several activity systems meet on the boundary zone of home and work causing boundary zones to expand and tensions to increase and expand like a network. In the everyday life of an individual the boundary zone fades out and home and work overlap. Tensions can be examined as internal conflicts of the individual through the activity system of everyday life. Individuals balance between individualism and familism, feeling bad, suffering from lack of time and struggling with childcare organizing problems and inflexible employers. The solutions to reconciling home and work difficulties are situational. Often is the help of family and friends required without any solid solutions. The conflict of the goals, requirements and the reality is behind the problems as well as the tightening terms of the working life and its growing expectations. Change requests are proposed on the levels of individual, home, work and the society. Reconciling home and work is not only a challenge between the employee and the employer. It s a problem that needs multilateral solutions and changes on the levels of individual, home, work and society. The challenge remaining is to find out if it would be successful to take the everyday life as starting point to negotiate the reconciling of home and work and how the possible family, social and work political solutions appear in everyday life.