Nanostructured Pb0.90Ba0.10Zr0.40Ti0.60O3 dense ceramics presenting an average grain size of 62 +/- 5 nm was prepared by the polymeric precursor method and using the spark plasma sintering technique. The dielectric permittivity curves versus temperature exhibit broad anomaly, indicative of a diffuse phase transition. This result can be explained by the spread of Curie temperatures which are expected to depend on the degree of tetragonality related to the grain size distribution. A pronounced decrease in the maximum of the dielectric permittivity value is attributed to the existence of a large amount of grain boundaries which are non-ferroelectric regions.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Zirconium tin titanate (ZST) is often used as a dielectric resonator for the fabrication of microwave devices. Pure compositions do not sinter easily by solid state sintering; therefore, sintering ZST requires sintering aids capable of creating defects that could improve diffusion processes and/or promote liquid phase sintering. The mechanisms by which the additives influence the microstructure and, consequently, the ZSTs dielectric properties are not very clear. The effects of ZnO, Bi2O3, and La2O3, on the stoichiometry and dielectric properties of ZST sintered at different temperatures were investigated in this study.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ba0.77Ca0.23TiO3 ceramics were produced in this work starting from nanopowders synthesized via a polymeric precursor method. By adjusting the pH values of the precursor solutions above 7, it was possible to prepare powders weakly aggregated and with a smaller particle size, both facts which traduced into an enhanced nanopowders' sintering process at comparatively lower temperatures. Irrespective of the initial pH value, highly-dense and second phase-free ceramics were obtained following optimal sintering parameters (temperature and time) extracted from dilatometric and density measurements. By considering these and other sintering conditions, moreover, polycrystalline materials with an average grain size varying from 0.35 to 8 mm were produced, the grain growth process involving liquid phase-assisted sintering for heat treatments achieved at 1320 °C. The study of grain size effects on the ferroelectric properties of these materials was conducted, the results being discussed in the light of previous debates, including grain size-dependent degree of tetragonal distortion in such materials, as verified in this work.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Recently, a new ternary phase was discovered in the Ti-Si-B system, located near the Ti6Si2B composition. The present study concerns the preparation of titanium alloys that contain such phase mixed with α-titanium and other intermetallic phases. High-purity powders were initially processed in a planetary ball-mill under argon atmosphere with Ti-18Si-6B and Ti-7.5Si-22.5B at. (%) initial compositions. Variation of parameters such as rotary speed, time, and ball diameters were adopted. The as-milled powders were pressureless sintered and hot pressed. Both the as-milled and sintered materials were characterized by X-ray diffraction, scanning electron microscopy and energy-dispersive spectrometry. Sintered samples have presented equilibrium structures formed mainly by the α-Ti+Ti6Si2B+Ti5Si3+TiB phases. Silicon and boron peaks disappear throughout the milling processes, as observed in the powder diffraction data. Furthermore, an iron contamination of up to 10 at. (%) is measured by X-ray spectroscopy analysis on some regions of the sintered samples. Density, hardness and tribological results for these two compositions are also presented here.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

[EN]The continuous evolution of materials and technologies of Additive Manufacturing (AM) has led to a competitive production process even for functional parts. The capabilities of these technologies for manufacturing complex geometries allow the definition of new designs that cannot be obtained with any other manufacturing processes. An application where this capability can be exploited is the lightening of parts using internal structures. This allows to obtain more efficient parts and, at the same time, reduce the costs of material and manufacturing time. A new lightweight optimization method to optimize the design of these structures and minimize weight while keeping the minimal mechanical properties is presented in this paper.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The sintering behaviour and the microstructural evolution of W6+, Nb5+ and Ti4+iron-substituted BiFeO3 ceramics have been analyzed. The obtained results show that W6+ and Nb5+ ions interact with the secondary phases usually present in these materials, thus altering the solid state formation of the BiFeO3 phase. In contrast, Ti4+ ions incorporate into the perovskite structure, leading to an exceptionally low proportion of secondary phases. In addition to this, BiFe0.95Ti0.05O3 materials present a dense microstructure with submicronic and nanostructured grains, clearly smaller than those in the undoped materials.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El wolframio (W) y sus aleaciones se consideran los mejores candidatos para la construcción del divertor en la nueva generación de reactores de fusión nuclear. Este componente va a recibir las cargas térmicas más elevadas durante el funcionamiento del reactor ya que estará en contacto directo con el plasma. En los últimos años, después de un profundo análisis y siguiendo una estrategia de reducción de costes, la Organización de ITER tomó la decisión de construir el divertor integramente de wolframio desde el principio. Por ello, el wolframio no sólo actuará como material en contacto con el plasma (PFM), sino que también tendría aplicaciones estructurales. El wolframio, debido a sus excelentes propiedades termo-físicas, cumple todos los requerimientos para ser utilizado como PFM, sin embargo, su inherente fragilidad pone en peligro su uso estructural. Por tanto, uno de los principales objetivos de esta tesis es encontrar una aleación de wolframio con menor fragilidad. Durante éste trabajo, se realizó la caracterización microstructural y mecánica de diferentes materiales basados en wolframio. Sin embargo, ésta tarea es un reto debido a la pequeña cantidad de material suministrado, su reducido tamaño de grano y fragilidad. Por ello, para una correcta medida de todas las propiedades físicas y mecánicas se utilizaron diversas técnicas experimentales. Algunas de ellas se emplean habitualmente como la nanoindentación o los ensayos de flexión en tres puntos (TPB). Sin embargo, otras fueron especificamente desarrolladas e implementadas durante el desarrollo de esta tesis como es el caso de la medida real de la tenacidad de fractura en los materiales masivos, o de las medidas in situ de la tenacidad de fractura en las láminas delgadas de wolframio. Diversas composiciones de aleaciones de wolframio masivas (W-1% Y2O3, W-2% V-0.5% Y2O3, W-4% V-0.5% Y2O3, W-2% Ti-1% La2O3 y W-4% Ti-1% La2O3) se han estudiado y comparado con un wolframio puro producido en las mismas condiciones. Estas aleaciones, producidas por ruta pulvimetalúrgica de aleado mecánico (MA) y compactación isostática en caliente (HIP), fueron microstructural y mecánicamente caracterizadas desde 77 hasta 1473 K en aire y en alto vacío. Entre otras propiedades físicas y mecánicas se midieron la dureza, el módulo elástico, la resistencia a flexión y la tenacidad de fractura para todas las aleaciones. Finalmente se analizaron las superficies de fractura después de los ensayos de TPB para relacionar los micromecanismos de fallo con el comportamiento macroscópico a rotura. Los resultados obtenidos mostraron un comportamiento mecánico frágil en casi todo el intervalo de temperaturas y para casi todas las aleaciones sin mejoría de la temperatura de transición dúctil-frágil (DBTT). Con el fin de encontrar un material base wolframio con una DBTT más baja se realizó también un estudio, aún preliminar, de láminas delgadas de wolframio puro y wolframio dopado con 0.005wt.% potasio (K). Éstas láminas fueron fabricadas industrialmente mediante sinterizado y laminación en caliente y en frío y se sometieron posteriormente a un tratamiento térmico de recocido desde 1073 hasta 2673 K. Se ha analizado la evolución de su microestructura y las propiedades mecánicas al aumentar la temperatura de recocido. Los resultados mostraron la estabilización de los granos de wolframio con el incremento de la temperatura de recocido en las láminas delgadas de wolframio dopado con potasio. Sin embargo, es necesario realizar estudios adicionales para entender mejor la microstructura y algunas propiedades mecánicas de estos materiales, como la tenacidad de fractura. Tungsten (W) and tungsten-based alloys are considered to be the best candidate materials for fabricating the divertor in the next-generation nuclear fusion reactors. This component will experience the highest thermal loads during the operation of a reactor since it directly faces the plasma. In recent years, after thorough analysis that followed a strategy of cost reduction, the ITER Organization decided to built a full-tunsgten divertor before the first nuclear campaigns. Therefore, tungsten will be used not only as a plasma-facing material (PFM) but also in structural applications. Tungsten, due to its the excellent thermo-physical properties fulfils the requirements of a PFM, however, its use in structural applications is compromised due to its inherent brittleness. One of the objectives of this phD thesis is therefore, to find a material with improved brittleness behaviour. The microstructural and mechanical characterisation of different tunsgten-based materials was performed. However, this is a challenging task because of the reduced laboratory-scale size of the specimens provided, their _ne microstructure and their brittleness. Consequently, many techniques are required to ensure an accurate measurement of all the mechanical and physical properties. Some of the applied methods have been widely used such as nanoindentation or three-point bending (TPB) tests. However, other methods were specifically developed and implemented during this work such as the measurement of the real fracture toughness of bulk-tunsgten alloys or the in situ fracture toughness measurements of very thin tungsten foils. Bulk-tunsgten materials with different compositions (W-1% Y2O3, W-2% V- 0.5% Y2O3, W-4% V-0.5% Y2O3, W-2% Ti-1% La2O3 and W-4% Ti-1% La2O3) were studied and compared with pure tungsten processed under the same conditions. These alloys, produced by a powder metallurgical route of mechanical alloying (MA) and hot isostatic pressing (HIP), were microstructural and mechanically characterised from 77 to 1473 K in air and under high vacuum conditions. Hardness, elastic modulus, flexural strength and fracture toughness for all of the alloys were measured in addition to other physical and mechanical properties. Finally, the fracture surfaces after the TPB tests were analysed to correlate the micromechanisms of failure with the macroscopic behaviour. The results reveal brittle mechanical behaviour in almost the entire temperature range for the alloys and micromechanisms of failure with no improvement in the ductile-brittle transition temperature (DBTT). To continue the search of a tungsten material with lowered DBTT, a preliminary study of pure tunsgten and 0.005 wt.% potassium (K)-doped tungsten foils was also performed. These foils were industrially produced by sintering and hot and cold rolling. After that, they were annealed from 1073 to 2673 K to analyse the evolution of the microstructural and mechanical properties with increasing annealing temperature. The results revealed the stabilisation of the tungsten grains with increasing annealing temperature in the potassium-doped tungsten foil. However, additional studies need to be performed to gain a better understanding of the microstructure and mechanical properties of these materials such as fracture toughness.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This work reports the synthesis of nanoTiC–graphite composites using mesophase pitch containing titanium as TiC or TiO2 nanoparticles. NanoTiC–graphite composites have been prepared using Ti-doped self-sintering mesophase powders as starting materials without using any binders or a metal carbide-carbon mixing stage. The effect of manufacture variables on the graphite compacts properties was studied. Graphites were characterised using XRD and Raman spectroscopy, SEM and TEM, as well as by their mechanical, electrical and thermal properties. The presence of TiC promotes graphitisation producing materials with larger crystal sizes. The kind of titanium source and mesophase content of the starting pitch affects to the final properties. Mesophase pitch with higher amount of mesophase content produces graphites with higher degree of graphitisation. The incorporation of TiC nanoparticles to the graphites composites improved thermal conductivity more than four times, and mechanical properties are not significantly modified by the presence of TiC.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The Rh diamine complex [Rh(COD)NH2(CH2)2NH(CH2)3Si(OCH3)3] BF4 was heterogenized by covalent bonding on two carbon xerogels and on carbon nanofibers, with the objective of preparing hydrogenation hybrid catalysts. Gas adsorption, SEM, TEM, DTP, ICP-OES and XPS were used for characterization. The results indicate that the active molecule is mainly located in supermicropores and produces microporosity blockage. The hybrid catalysts are more active than the homogeneous complex, but the Rh complex is partially reduced upon reaction. This modification is related to the nature of the support, which also shows effects in the stabilization against sintering of the Rh particles formed. The support porosity is a key factor in the selectivity differences between the catalysts.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Analytical transmission electron microscopy indicates that liquid film migration occurs during sintering of an Al-Cu-Mg alloy, that intragranular liquid pools develop from migrating films and that iron segregates to these pools. It is suggested that a high localised iron concentration retards the liquid film migration rate by reducing the coherency strain in the retreating grain, causing a region of the film to detach from the boundary, thus forming an intragranular pool in the advancing grain. Alloys with low iron levels develop few intragranular pools and have high sintered densities. (C) 2003 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper describes the sintering of an 18Ni(350) maraging steel with additions of boron, with the aim of producing high hardness rapid tooling. Reaction of the boron with the alloying elements in the maraging steel resulted in the formation of a Mo- and Ti-rich borides. The former melted at similar to1220degreesC, providing a liquid phase for enhanced sintering. Although densification could occur regardless of the boron content, especially at high temperature, 0.4% B was required to produce a near full density component. The formation of the various borides depleted the matrix of critical age hardening elements. However, by altering the starting powder composition to compensate for this, hardness close to the wrought alloy has been achieved. This hardness was comparable to a common die casting tool steel. Examples of dies produced using selective laser sintering (SLS) are also shown. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The role of the resin type on the sintering of maraging steel with boron additions has been investigated. Two different resins were added to the steel mixture and their subsequent debinding was evaluated and sintering responses compared with that of a resin-free alloy. The two resins used, nylon and a mixture of phenolic resin and synthetic wax, possessed different debinding behaviour, with the latter causing significant carbon contamination of the parts. This caused the formation of a Ti-Mo carbide, depleting the matrix of these elements. Consequently, the microstructure consisted of the equilibrium Fe-Fe2B eutectic, as well as a Mo-rich boride. The liquid phase also appeared to contain significant amounts of carbon, which lowered the temperature at which the liquid formed, resulting in high density occurring at a much lower temperature. When nylon was used as the binder, a similar sintering response to the resin-free alloy was observed. (C) 2002 Published by Elsevier Science B.V.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The effect of the addition of elemental Mg, Sri and Pb on the sintering of impressed prealloyed 2124 and 6061 powder has been investigated. Despite being sintered at a temperature that resulted in similar to20 vol.% liquid phase, high density was possible only upon the addition of similar to1% elemental Mg as well as trace amounts of Sri or Pb. Additions of Mg facilitated oxide disruption, while Sri and Pb segregated to the liquid phase, where they reduced the liquid's surface tension, thus improving sintering. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Doped ceria (CeO2) compounds are fluorite-type oxides that show oxide ionic conductivity higher than yttria-stabilized zirconia in oxidizing atmosphere. As a consequence of this, considerable interest has been shown in application of these materials for low (500 degrees-650 degrees C) temperature operation of solid oxide fuel cells (SOFCs). To improve the conductivity in dysprosium (Dy) doped CeO2, nano-size round shape particles were prepared using a coprecipitation method. The dense sintered bodies with small grain sizes (< 300 nm) were fabricated using a combined process of spark plasma sintering (SPS) and conventional sintering (CS). Dy-doped CeO2 sintered body with large grains (1.1 mu m) had large micro-domains. The conductivity in the sintered body was low (-3.2 S/cm at 500 degrees C). On the other hand, the conductivity in the specimens obtained by the combined process was considerably improved. The micro-domain size in the grain was minimized using the present process. It is concluded that the enhancement of conductivity in dense specimens produced by the combined process (SPS+CS) is attributable to the microstructural changes within the grains.