697 resultados para Resíduo de cerâmica vermelha
Resumo:
The red ceramic industry is recognized as of major importance in Piauí State. The State capital, Teresina, is the greatest producer of this material ( production about 18 million peaces), which is used mainly for masonry sealing blocks. One of the most frequent problems in this kind of products is the efflorescence. This work has the main objective of studying the influence of gypsum addition on non-glazed tiles, by using the local industry production standards. The raw materials were characterized by FRX, DRX, TGA, DTA and AD. Extruded test specimens were made with the addition of 1, 3 and 5% of gypsum in the ceramic paste, burned at 850oC, 950oC and 1050oC and submitted to further technological tests and microestrutural analysis by the scanning electron microscope. In order to accelerate the aging of bodies of evidence, they were immersed in successive water baths and posterior drying. The reference ceramic paste showed tendency to efflorescence formation after drying and consolidated efflorescence after burning, but no affecting the technological results
Resumo:
This research presents an overview of the addition steelwork dust of ceramic shingles in order to contribute to the utilization use of such residue. The ceramic industry perspective in the Brazilian State of Piauí is quite promising. Unlike other productive sectors, the ceramic industry uses basically natural raw materials. Its final products are, in short, the result of transforming clay compounds. These raw materials are composed primarily of aluminum oxide, silicon, iron, sodium, magnesium, end calcium, among others. It was verified that steelwork dust is composed primarily of these same oxides, so that its incorporation in to structural ceramics is a very reasonable idea. Both clay and steelwork powder were characterized by AG, XRF, XRD, TGA and DTA. In addition, steelwork dust samples containing (0%, 5%, 10%, 15%, 20% and 25%) were extruded and burned at 800°C, 850°C, 900°C and 950°C. Then t echnological tests of linear shrinkage, water uptake, apparent porosity, apparent density and flexural strengthwere carried at. The results showed the possibility of using steelwork powder in ceramic shingles until 15% significant improvement in physical and mechanical properties. This behavior shows the possibility of burning at temperatures lower than 850ºC, thus promoting a product final cost reduction
Resumo:
Rio Grande do Norte State stands out as one great producer of structural clay of the brazilian northeastern. The Valley Assu ceramic tiles production stands out obtained from ilitics ball clays that abound in the region under study. Ceramics formulation and the design of experiments with mixture approach, has been applied for researchers, come as an important aid to decrease the number of experiments necessary to the optimization. In this context, the objective of this work is to evaluate the effects of the formulation, temperature and heating rate in the physical-mechanical properties of the red ceramic body used for roofing tile fabrication of the Valley Assu, using design of mixture experiments. Four clays samples used in two ceramics industry of the region were use as raw material and characterized by X-ray diffraction, chemical composition, differential thermal analysis (DTA), thermogravimetric analysis (TGA), particle size distribution analysis and plasticity techniques. Afterwards, they were defined initial molded bodies and made specimens were then prepared by uniaxial pressing at 25 MPa before firing at 850, 950 and 1050 ºC in a laboratory furnace, with heating rate in the proportions of 5, 10 e 15 ºC/min. The following tecnologicals properties were evaluated: linear firing shrinkage, water absorption and flexural strength. Results show that the temperature 1050 ºC and heating rate of 5 ºC/min was the best condition, therefore presented significance in all physical-mechanical properties. The model was accepted as valid based of the production of three new formulations with fractions mass diferents of the initial molded bodies and heated with temperature at 1050 ºC and heating rate of 5 ºC/min. Considering the formulation, temperature and heating rate as variables of the equations, another model was suggested, where from the aplication of design of experiments with mixtures was possible to get a best formulation, whose experimental error is the minor in relation to the too much formulations
Resumo:
The world market of Kaolin has been growing as new investments for better quality of materials have been applied. This market produces amounts of dross that are put in the environment in a wrong way, causing damages to it. Trying to reduce these damages, researches have been done in an attempt to use kaolin dross in ceramic. The disposal of kaolin dross in the environment by the industries of the states of Rio Grande do Norte and Paraiba have great impact in society. Usually this dross is disposed clandestinely in places like roads, river banks and lands of small cities. The present work shows the characteristics of the kaolin produced by the mining company in Junco do Seridó, Paraiba state, western Seridó, 300 km from Natal, in the border of both states. After that, researches were done to study its physical and the chemistry characteristics, trying to see if it can be used in white ceramic. The samples got were bolted in fabric of 325# . The technological characteristics tried to use it as a product in white ceramic. For that, it was made a haracterization of the subject matter through enlargement analyses, ATG and ATD, elaborating three formulations that were burned in four different temperatures, 1175, 1200, 1250 and 1300 degrees centigrade up to 30 minutes. After the burning, the subjects were submitted to water absorbing tests, linear retreating, apparent porosity, apparent specific mass, resistance to flexibility and MEV. For one of the mixtures it was obtained demanded properties for a semi porous material
Resumo:
Companies involved in kaolin mining and treatment represent an important area of industrial development in Brazil, significantly contribution to the worldwide production of such mineral. As a result, large volumes of kaolin residue are constantly generated and abandoned in the environment, negatively contributing to its preservation. In this scenario, the objective of the present study was to characterize the residue generated from kaolin mining as well as to assess its potential use as raw material for the production of ceramic tiles. Ceramic mixtures were prepared from raw materials characterized by X-ray fluorescence, X-ray diffraction, particle size analysis and thermal analysis. Three compositions were prepared using kaolin residue contents of 10%, 20% and 30%. Samples were uniaxially pressed, fired at 1200ºC and characterized aiming at establishing their mineralogical composition, water absorption, apparent porosity, specific mass, linear retraction and modulus of rupture. The results showed that the residue basically consisted of kaolinite and successfully replaced raw kaolin in the preparation of ceramic title formulations without significantly affecting the properties of the fired material
Resumo:
Companies involved in emerald mining and treatment represent an important area of industrial development in Brazil, with significative contribution to the worldwide production of such mineral. As a result, large volumes of emerald waste are constantly generated and abandoned in the environment, negatively contributing to its preservation. By the other side the interest of the use of mining waste as additive in ceramic products has been growing from researchers in recent years. The ceramic industry is constantly seeking to the marked amplification for the sector and perfecting the quality of the products and to increase the variety of applications. The technology of obtaining of ceramic tiles that uses mining residues assists market niches little explored. In this scenario, the objective of the present study was to characterize the residue generated from emerald mining as well as to assess its potential use as raw material for the production of ceramic tiles. Ceramic mixtures were prepared from raw materials characterized by X-ray fluorescence, X-ray diffraction, particle size analysis and thermal analysis. Five compositions were prepared using emerald residue contents of 0%, 10%, 20%, 30% and 40%. Samples were uniaxially pressed, fired at 1000, 1100 and 1200ºC and characterized aiming at establishing their mineralogical composition, water absorption, apparent porosity, specific mass, linear retraction and modulus of rupture. The results shows that the emerald residue, basically consisted of 73% of (SiO2 + Al2O3) and 17,77% of (MgO + Na2O+ K2O) (that facilitates sintering), can be added to the ceramic tile materials with no detrimental effect on the properties of the sintered products
Resumo:
One of the waste generated during the drilling of oil wells are gravel which are impregnated of drilling fluid. This residue consists of highly toxic chemicals, including toxic metals. This study suggests an alternative process to the treatment of this waste, by incorporating it the form of raw material in the ceramic matrix , and by solidification and stabilize the metals present, Aluminum (Al), Iron (Fe), Manganese (Mn) and Zinc (Zn). The raw materials were characterized by the techniques of X ray fluorescence (FRX), X ray diffraction (DRX), laser granulometry (GL), thermogravimetry (TG) and differential thermal analysis (ADT). To evaluate the percentage of gravel effect the environmental and technological properties were obtained from formulations containing 0, 10 and 20 % by weight of gravel in the ceramic matrix. After sintering at temperatures 1080, 1120 and 1160 °C, the samples were tested for water absorption, the linear shrinkage firing, voltage of rupture and solubility. The results obtained showed that the stabilization by solidification, is a viable alternative to safe disposal of waste drilling. Ceramics products can be used in the manufacture of solid bricks
Resumo:
The disposal of sewage sludge is a growing problem face up to management of sanitary sevices. Otherwise, because its making process characteristic, the Ceramic Industry can tolerate the presence of this wastes as raw material. This study has as object to confirm the use of the sewage sluge in the Ceramic Industry like a sustentable alternative for its disposal. Futhermore, this study quests to evaluate the maximum proportion for incorporation of sludge wich result in technically and enviromentally suitable bricks. For found this proportion, the research consisted of (1) making of bricks in full scale, adde up 0%, 5%,10%, 15%, 20%, 25%,30%, 35% e 40% sludge, with size 220x105x45 mm, hand-molded by rammer and baked by industrial kiln; and (2) tecnical and enviromental evaluation of this bricks, according to Brazilian norms. The raw material uses were two distinct clays come from Goianinha/RN and sewage comes from a septic system tank and pumped into tank vehicle, of Natal/RN. The technical evaluation allowed to conclude the addiotion of the sludge brings about signifcant lost of mass and the water absorption grew up according to increase of sludge: every sludge-amended clay bricks absorved more water than control group. Thus, the compressive strength was signicantly decreased because the increase of sludge: bricks with 5% sludge added lost 45% of strength achieved at control group; the bricks made with 10 and 20% lost almost 70% of bigger strength. With up to 25% sludge added to the bricks, the streght decreased over 90%. Concerning heavy metal leaching, the two maximum proportion wich have tecnical approval, it means bricks sludge added with 15 and 20%, can say there is no risk of enviromental contamination using those bricks. This way, in this work context, it can to conclude the maximum proportion atends the technical and enviromental criterion is 20%
Resumo:
A utilização de novas técnicas de aproveitamento de resíduos tem-se tornado cada vez mais importante na construção civil, principalmente quando se trata da utilização de resíduos de outros segmentos industriais e da redução de consumo de matérias-primas naturais. O objetivo deste estudo foi avaliar a utilização da lama vermelha, resíduo proveniente da produção de alumina metalúrgica, na produção de blocos cerâmicos vazados estruturais. A produção dos blocos foi realizada em uma indústria cerâmica, a partir de uma mistura de 60% de lama vermelha (LV) e de 40% de argila. Após a produção dos blocos, realizaram-se ensaios de acordo com as normas técnicas, tais como absorção de água e compressão axial simples. A partir da análise dos resultados, observou-se que os blocos estruturais produzidos a partir da mistura de LV e argila atenderam aos parâmetros normativos quanto ao índice de absorção de água e de resistência à compressão, e que as resistências médias e características desses blocos foram superiores às dos blocos cerâmicos de referência.
Resumo:
O resíduo do refino da bauxita, comumente conhecido como lama vermelha, tem mostrado ser capaz de ligar metais traços tais como o cobre, cádmio, zinco, cromo, níquel e chumbo sob condições apropriadas. A neutralização da lama vermelha é necessária porque essa lama é tipicamente cáustica, com pH em torno de 13. Muitas pesquisas têm sido desenvolvidas envolvendo a utilização da lama vermelha, porque contem uma série de elementos valiosos. Assim a utilização da lama vermelha como material de construção e como adsorvente é atrativa porque ela é utilizada em grande quantidade. Nada pode ser feito sem descartar componentes valiosos como titânio, zircônio e principalmente ferro. A síntese de hidrotalcita conectada com a reciclagem de soluções alcalinas representa uma maneira efetiva de uso dessa solução considerando a forte demanda por proteção ambiental no mundo. Os compostos tipo hidrotalcita, precipitados durante a neutralização da lama, também removem oxi-ânions de metais de transição através da combinação de intercalações e adsorção de espécies aniônicas na sua superfície externa. Os hidróxidos duplos lamelares (HDL) vêm sendo investigados à muitos anos como materiais hospedeiros para uma variedade de reações de intercalação de anions. A estrutura lamelar dos HDLs pode ser usada para controlar a adição ou remoção de uma variedade de espécies químicas, tanto orgânicas quanto inorgânicas. Isto é alcançado através de sua habilidade de adaptar a separação das lamelas de hidróxidos, e da reatividade da região interlamelar. O material resultante adsorve anions quando colocado em soluções e reverte a estrutura da hidrotalcita. Avanços significativos têm sido alcançados recentemente na caracterização desses materiais, incluindo estudos estruturais sobre o mecanismo de intercalação. O objetivo desse trabalho foi a síntese e caracterização de HDLs a partir da lama vermelha, e testar esses materiais como adsorventes de metais pesados.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Ceramic materials the alumina base are large industrial applications. They are required for these products, specific characteristics obtained by following strict criteria during the manufacturing process. However, after life, not always these products are reused by a suitable waste management process. In ceramist context, advance research aimed at the reuse of waste aimed at obtaining ceramics and composite materials, with marked reduction of conventional raw materials. Aiming to generate scientific, technological and environmental contribution, this work studied to obtain a composite of alumina ceramic (Al2O3) and sodium beta alumina (NaAl11O17 ), and as starting materials the residue of the ceramic insulator of spark plugs, as a source alumina (Al2O3) powder and unusable sodium bicarbonate (NaHCO3) of fire extinguishers, as a source of sodium oxide (Na2O). The final ceramic product was obtained from a conventional mixture of sodium aluminum oxide in appropriate molar proportions. Sample spark plugs were obtained, discarded by lifetime, specific to a manufacturer, which, after passing through mechanical stress (grinding, magnetic purification, washing, drying and grinding the high energy), which resulted in residue powder with ceramic content of 84.34 % alumina (Al2O3), found by FRX chemical analysis, the phases present and identified by DRX. The dry chemical fire extinguisher, baking soda-based (NaHCO3) with expired, was obtained through direct collection of the waste generated during maintenance. Subjected to heat treatment at 120 °C , the NaHCO3 powder was decomposed in sodium oxide ( Na2O), which, subjected to chemical analysis (FRX) and mineralogical (DRX) revealed a content of 86.62 % sodium oxide (Na2O) . In the following steps the experimental procedure, chemical formulations were made on a molar basis of the starting material (1:9, 1:10 and 1:11 de Na2O/ Al2O3) inclusion of additives, milling parameters, sieve analysis, dilatometry, conformation of specimens, sintering in firing steps at 800 °C , 1000 °C and 1.200 °C with varying stays 30 , 60 and 120 minutes in each of the levels. The characterization of the final product was made by the following physical tests: water absorption, porosity, linear shrinkage, mineralogical analysis by DRX and microstructural analysis by MEV. A higher formation of sodium beta alumina (NaAl11O17), in sintered specimens in levels of 1.200 °C and 120 minutes, despite the prevailing coexistence of alpha phase alumina (Al2O3). From the results obtained opens up prospects for the reuse of waste studied in this work, the potter context and in other technological areas.
Resumo:
Ceramic materials the alumina base are large industrial applications. They are required for these products, specific characteristics obtained by following strict criteria during the manufacturing process. However, after life, not always these products are reused by a suitable waste management process. In ceramist context, advance research aimed at the reuse of waste aimed at obtaining ceramics and composite materials, with marked reduction of conventional raw materials. Aiming to generate scientific, technological and environmental contribution, this work studied to obtain a composite of alumina ceramic (Al2O3) and sodium beta alumina (NaAl11O17 ), and as starting materials the residue of the ceramic insulator of spark plugs, as a source alumina (Al2O3) powder and unusable sodium bicarbonate (NaHCO3) of fire extinguishers, as a source of sodium oxide (Na2O). The final ceramic product was obtained from a conventional mixture of sodium aluminum oxide in appropriate molar proportions. Sample spark plugs were obtained, discarded by lifetime, specific to a manufacturer, which, after passing through mechanical stress (grinding, magnetic purification, washing, drying and grinding the high energy), which resulted in residue powder with ceramic content of 84.34 % alumina (Al2O3), found by FRX chemical analysis, the phases present and identified by DRX. The dry chemical fire extinguisher, baking soda-based (NaHCO3) with expired, was obtained through direct collection of the waste generated during maintenance. Subjected to heat treatment at 120 °C , the NaHCO3 powder was decomposed in sodium oxide ( Na2O), which, subjected to chemical analysis (FRX) and mineralogical (DRX) revealed a content of 86.62 % sodium oxide (Na2O) . In the following steps the experimental procedure, chemical formulations were made on a molar basis of the starting material (1:9, 1:10 and 1:11 de Na2O/ Al2O3) inclusion of additives, milling parameters, sieve analysis, dilatometry, conformation of specimens, sintering in firing steps at 800 °C , 1000 °C and 1.200 °C with varying stays 30 , 60 and 120 minutes in each of the levels. The characterization of the final product was made by the following physical tests: water absorption, porosity, linear shrinkage, mineralogical analysis by DRX and microstructural analysis by MEV. A higher formation of sodium beta alumina (NaAl11O17), in sintered specimens in levels of 1.200 °C and 120 minutes, despite the prevailing coexistence of alpha phase alumina (Al2O3). From the results obtained opens up prospects for the reuse of waste studied in this work, the potter context and in other technological areas.
Resumo:
O setor de construção civil enfrenta sérios problemas quanto à disposição de resíduos, uma vez que gera grandes quantidades ao longo do processo de execução das obras ou devido ao desmonte de construções já existentes. A disposição inadequada desses resíduos pode provocar sérios danos ambientais, tais como degradação do solo e recursos hídricos. Uma opção interessante pode ser seu uso agrícola, entretanto existem poucos estudos sobre o tema. Assim, o presente estudo visou caracterizar resíduos da construção civil e avaliar seu efeito sobre alguns atributos do solo. Para tal, foram realizadas análises de pH, teor de macro e micronutrientes e de elementos potencialmente tóxicos. Os resultados indicaram que os resíduos não poderiam ser utilizados como fonte de nutrientes e que também não apresentavam limitações quanto à presença de elementos potencialmente tóxicos. Os altos valores de pH encontrados indicaram potencial dos resíduos em alcalinizar do solo, o que foi confirmado no ensaio em vasos. Também se constatou que os resíduos provocaram aumento da CTC. Assim, concluiu-se que é viável utilizar esses resíduos da construção civil em solos agrícolas, embora mais avaliações ainda devam ser realizadas.
Resumo:
O presente trabalho divulga os resultados dos estudos levados a efeito nas matérias-primas argilosas que se integram tipologicamente na argila comum, ocorrentes na designada Plataforma do Mondego, Centro de Portugal, na região entre Miranda do Corvo, a SW, e Tábua, a NE. Para tal realizou-se a cartografia superficial dos sedimentos continentais do Cretácico e do Terciário, aí preservados, estabeleceram-se as colunas sedimentares, a nível regional e a nível local, nas áreas de maior potencial reconhecido e, caracterizaram-se as matérias-primas argilosas amostradas, em termos de composição, textura e aptidão cerâmica, objectivando a definição das zonas das jazidas com maior interesse industrial. A informação obtida e compilada, relativa ao caulino e ao feldspato é também apresentada, com vista a uma percepção da potencialidade destas matériasprimas cerâmicas ocorrentes na área. O estudo de caracterização dos materiais argilosos investigados teve como base 53 amostras obtidas em seis regiões da Plataforma do Mondego aqui definidas por motivo de organização do trabalho, segundo os critérios geográfico e geotectónico. As formações de Côja e de Campelo, do Terciário, constituem as unidades onde ocorrem litótipos produtivos, em termos de matéria-prima para a Cerâmica de Barro Vermelho ou Cerâmica de Construção. Relativamente às características texturais e composicionais, em síntese, apresentam-se os factos relevantes seguintes: A matéria-prima argilosa existente na área estudada materializa, granulometricamente, na maioria das amostras, silte, caindo os níveis amostrados com maior percentagem de argila, no domínio do silte argiloso. O défice em fracção argila implica limitações quanto à possibilidade de diversificação de produtos cerâmicos fabricados com estas matérias-primas tal-qual. Os diferentes métodos analíticos utilizados na caracterização mineralógica dos materiais amostrados confirmaram uma composição em termos dos minerais argilosos, consistindo de ilite/mica (em geral, o mais abundante), caulinite e esmectite, interestratificados e clorite. Os minerais não argilosos são quartzo (predominante), feldspato (sobretudo potássico) e hematite, com uma representação baixa. A mineralogia da fracção inferior a 2μm das amostras, não difere das amostras totais, salvo no teor mais elevado dos minerais argilosos e acentuada redução dos minerais não argilosos. Os resultados da análise química por fluorescência de raios X das amostras integrais correlacionam-se com as características mineralógicas observadas através das técnicas analíticas utilizadas. No respeitante às propriedades e comportamento cerâmico verifica-se: Os parâmetros relacionados com a plasticidade indicam que parte das pastas elaboradas com estes materiais argilosos têm uma trabalhabilidade aceitável, mas existem problemas de conformação e acentuada retracção num número significativo de amostras, devido à elevada plasticidade da maioria das amostras. A extrusão é satisfatória a óptima. A RMF e a retracção em seco assumem valores, respectivamente, moderados a baixos e moderados, embora seja necessário ter em conta o procedimento de extrusão dos provetes, sem dispositivo de vácuo. Todas as amostras foram sujeitas a cozedura a 900ºC, e um conjunto seleccionado foi cozido a 1000ºC e a 1100ºC. As fases mineralógicas ocorrentes após cozeduras a 900ºC e 1100ºC foram identificadas num conjunto de amostras, tendo-se evidenciado a coerência dessas fases, com a mineralogia das amostras em seco. Após cozedura a 900ºC, os valores de RMF das amostras satisfazem geralmente os valores mínimos, exigidos para o fabrico de tijolo, abobadilha e, com alguma frequência, de telha, como já se verificava com os valores daquela propriedade em seco. Os valores de retracção seco-cozido são em geral, modestos. A capacidade de absorção de água é maioritariamente elevada. A formação de vidro, sobretudo, condiciona o comportamento destas propriedades por cozedura dos provetes a 1000ºC e a 1100ºC. A coloração predominante em cru das matérias-primas argilosas amostradas é amarelo acastanhado a castanho avermelhado. Após cozedura a 900ºC, há um acentuado escurecimento e incremento no grau de vermelho. As cozeduras a 1000ºC e 1100ºC promovem escurecimento gradual, com ligeira influência na cor. O comportamento dos provetes após as cozeduras cerâmicas revelou-se homogéneo a cada uma das respectivas temperaturas, não se registando também defeitos significativos, nem eflorescências. A análise das amostras em termos composicionais e tecnológicos permitiu destacar as principais características e aspectos distintivos das matériasprimas, nas diferentes regiões definidas objectivando as diferentes potencialidades cerâmicas. Nesta abordagem comparativa foram consideradas só as amostras dos campos silte e silte arenoso, por serem aquelas com maior interesse para a Cerâmica de Construção. Nas colunas sedimentares das regiões de Tábua e Santa Quitéria constata-se a ocorrência de dois ritmos de sedimentação, que embora assumam características específicas em cada região, têm aspectos composicionais e tecnológicos em comum, traduzindo melhor aptidão cerâmica os ritmos inferiores. A conjugação da cartografia realizada com os estudos laboratoriais permite concluir que as regiões de Tábua e de Santa Quitéria serão as que têm maior potencial por explorar, em matéria-prima para Cerâmica de Construção, apesar da primeira já ser intensamente explorada. Na região de Tábua, as amostras têm como fases mineralógicas principais ilite e quartzo na mesma proporção média (35%) e caulinite (média=19%) que regista enriquecimento significativo na fracção argila (média=38%). As argilas desta região registam a cor em cru mais vermelha e pH mais ácido observados. O ritmo de sedimentação inferior, com esmectite e interestratificados e ligeiramente menos quartzoso, apresenta melhores propriedades cerâmicas. A composição mineralógica média das amostras da região de Santa Quitéria é próxima daquela da região de Tábua, mas menos caulinítica, em especial na sequência inferior, na qual o teor médio de caulinite na fracção argila (7%) é o mais baixo observado. Na região de Côja – Arganil, a actividade extractiva é significativa na bacia de Côja. Aqui, a exploração de novas áreas potenciais é condicionada pela cobertura conglomerática e por estruturas tectónicas e não tectónicas relacionadas com comportamento plástico. Na restante área desta região, os recursos argilosos são penalizados por material areno-conglomerático. As amostras desta região distinguem-se das restantes a nível textural pela maior fracção areia e mineralogicamente pela presença de clorite, teor reduzido de caulinite e elevado de feldspato. As potencialidades em barro vermelho na região de Sanguinheda não serão significativas, pois a Formação de Côja é predominantemente arcósica e a Formação de Campelo pouco espessa e conglomerática. As argilas com melhor aptidão cerâmica foram amostradas na região de Miranda do Corvo – Lousã. Na composição, estas amostras são as que contêm maior fracção de argila, maior teor de ilite e caulinite e menor de argilas expansivas. Registam os melhores valores nas características tecnológicas, nomeadamente a RMF e absorção de água. A consistência dos grupos amostrais e ritmos definidos em termos composicionais e tecnológicos é corroborada pelas técnicas de análise estatística multivariada aplicadas, que os identificam. As condições de amostragem na região de Tábua, permitiram a elaboração de uma coluna tipológica, na qual, a partir de uma caracterização expedita de amostras é possível identificar a sua afinidade com os ritmos argilosos definidos e, consequentemente, a sua situação na coluna sedimentar regional e aptidão cerâmica. A cartografia dos recursos argilosos potenciais, elaborada à escala 1:25.000, constitui um dos objectivos principais deste trabalho e nela constam unidades litológicas, nas quais são diferenciadas unidades argilosas tendo também em consideração a tipologia e guias mineralógicos resultantes da caracterização das amostras. As características composicionais destas unidades denotam diferente aptidão cerâmica e, portanto, permitem salientar as zonas com maior interesse económico.