929 resultados para Phase formation


Relevância:

60.00% 60.00%

Publicador:

Resumo:

The thin films of Cu2ZnSnS4 (CZTS) were grown by co-sputtering further the structural, optical and electrical properties were analyzed and confirmed the CZTS phase formation. The photo response of CZTS in near IR photodectection has been demonstrated. The detector response was measured employing both the IR lamp and IR laser illuminations. The calculated growth and decay constants were 130 m sec and 700 m sec followed by the slower components upon lamp illumination. The external quantum efficiency of 15%, responsivity of 13 AW(-1) makes CZTS a suitable candidate for the IR photodectection.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Zinc Oxide (ZnO) and indium doped ZnO (IZO) thin films with different indium compositions were grown on p-type boron doped Si substrates by pulsed laser deposition (PLD). The effect of indium concentration on the structural, optical and electrical properties of the film was studied. XRD, XPS and Raman studies confirm the single phase formation and successful doping of In in to ZnO. We observed various photoluminescence emissions, ranging from UV to visible, with the incorporation of In into ZnO. Room temperature Current-Voltage (I-V) characteristics showed good p-n junction properties for n-type-undoped and In doped ZnO with p-type substrates. The turn on voltage was observed to be decreasing with increase in In composition.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Magneto-electric composites comprising Na0.5Bi0.5TiO3 (NBT) and MnFe2O4 (MFO) were fabricated using their fine powders obtained via sol-gel method. X-ray diffraction and scanning electron microscopy results confirmed the single-phase formation of NBT and MFO and the composite nature when these were mixed and sintered at appropriate temperatures. The dielectric constant (epsilon(r)) and dielectric loss (D) decreased with increase in frequency (40-110 MHz). Room temperature magnetization measurements established these composites to be soft magnetic. Further, the nature of these composites were established to be magneto-electric at 300 K. The highest ME response of 0.19 % was observed in 30NBT-70MFO composite. The ME coefficient (alpha) was 240 mV/cm Oe for the same composition. The present study demonstrated the effectiveness of NBT/MFO as a lead-free multiferroic composite and provides an alternative for environment-friendly ME device applications.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The Y3Fe5O12 (YIG) nanopowders were synthesised at different pH using co-precipitation method. The effect of pH on the phase formation of YIG is characterised using XRD, TEM, FTIR and TG/DTA. From the Scherer formula, the particle sizes of the powders were found to be 13, 19 and 28 nm for pH=10, 11 and 12 respectively. It is found that as the pH of the solution increase the particle size is also increases. It is also clear from the TG/DTA curves that as the pH is increasing the weight losses were found to be small. The nanopowders were sintered at 600, 700, 800 and 900 degrees C for 5 h using conventional sintering method. The phase formation is completed at 800 degrees C/5 h which is correlated with TG/DTA. The average grain size of the samples is found to be similar to 161 nm. The high values of M-s=23 emu g(-1) and H-c=22 Oe were recorded for the sample sintered at 900 degrees C.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The composites of xSrFe(12)O(19)-(1-x) BaTiO3 where x=0, 0.1, 0.3, 0.5, 0.7, 0.9 and 1were prepared by Sol gel method and consequently densified at 1100 degrees C/90 min using microwave sintering method. The phase formation and diphase microstructure of the composite samples was examined by X-ray diffraction and field emission electron microscope (FESEM), respectively. The effects of constituent phase variation on the ferroelecrric, dielectric and magnetic properties were examined. It was observed that with a decrease of x, the Curie temperature shifted towards low temperature side. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The combustion of oxidizer zinc nitrate and fuel oxalic acid results in quasi-fibrous zinc oxide. The processing parameters including oxidizer to fuel ratio, time and temperature were optimized for the resultant crystal structure and morphology. Pure hexagonal phase formation does not depend on the fuel ratio, but a stoichiometric ratio of oxidizer to fuel at 450 degrees C and 30 min results in highly crystalline ZnO with 3 mu m length and 0.5 mu m width. This quasi-fiber originates from partial fusion of near spherical, similar to 60 nm particles during the rapid rate of reaction in the combustion process. Transmission electron microscopic analysis confirms the anisotropic primary particle orientation and pore distribution within the developed quasi-fibrous particles. The degradation of methyl orange was assessed by degrading the dye in the presence of the synthesized ZnO (2.95 eV) under both UV and visible light. Quasi-fibrous zinc oxide exhibits effective photocatalytic efficiency under visible light irradiation.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We report here the investigations on the size dependent variation of magnetic properties of nickel ferrite nanoparticles. Nickel ferrite nanoparticles of different sizes (14 to 22 nm) were prepared by the sol-gel route at different annealing temperatures. They are characterized by TGA-DTA, XRD, SEM, TEM and Raman spectroscopy techniques for the confirmation of the temperature of phase formation, thermal stability, crystallinity, morphology and structural status of the nickel ferrite nanoparticles. The magnetization studies revealed that the saturation magnetization (M-s), retentivity (M-r) increase, while coercivity (H-c) and anisotropy (K-eff) decrease as the particle size increases. The observed value of M-s is found to be relatively higher for a particle size of 22 nm. In addition, we have estimated the magnetic domain size using magnetic data and correlated to the average particle size. The calculated magnetic domain size is closely matching with the particle size estimated from XRD. Impedance spectroscopy was employed to study the samples in an equivalent circuit to understand their transport phenomena. It shows that nickel ferrite nanoparticles exhibit a non-Debye behavior with increasing particle size due to the influence of increasing disorders, surface effects, grain size and grain boundaries, etc. (C) 2015 Author(s). All article content, except where otherwise noted, is licensed under a Creative Commons Attribution 3.0 Unported License.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Nanocrystalline Ba0.85Ca0.15Zr0.1Ti0.9O3 (BCZT) powder was synthesized via the complex oxalate precursor route at a relatively low temperature (800 degrees C/5 h). The phase formation temperature of BCZT at nanoscale was confirmed by thermogravimetric (TG), differential thermal analysis (DTA) followed by X-ray powder diffraction (XRD) studies. Fourier transform infrared (FTIR) spectroscopy was carried out to confirm the complete decomposition of oxalate precursor into BCZT phase. The XRD and profile fitting revealed the coexistence of cubic and tetragonal phases and was corroborated by Raman study. Transmission electron microscopy (TEM) carried out on 800 degrees C and 1000 degrees C/5 h heat treated BCZT powder revealed the crystallite size to be in the range of 20-50 nm and 40-200 nm respectively. The optical band gap for BCZT nanocrystalline powder was obtained using Kubelka Munk function and was found to be around 3.12 +/- 0.02 eV and 3.03 +/- 0.02 eV respectively for 800 degrees C (20-50 nm) and 1000 degrees C/5 h (40-200 nm) heat treated samples. The piezoelectric properties were studied for two different crystallite sizes (30 and 70 nm) using a piezoresponse force microscope (PFM). The d(33) coefficients obtained for 30 nm and 70 nm sized crystallites were 4 pm V-1 and 47 pm V-1 respectively. These were superior to that of BaTiO3 nanocrystal (approximate to 50 nm) and promising from a technological/industrial applications viewpoint.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Thin films of Cu2SnS3 (CTS) were deposited by the facile solution processed sol-gel route followed by a low-temperature annealing. The Cu-Sn-thiourea complex formation was analysed using Fourier Transform Infrared spectrophotometer (FTIR). The various phase transformations and the deposition temperature range for the initial precursor solution was determined using Thermogravimetric analysis (TGA) and Differential Scanning Calorimetry (DSC). X-Ray Diffraction (XRD) studies revealed the tetragonal phase formation of the CTS annealed films. Raman spectroscopy studies further confirmed the tetragonal phase formation and the absence of any deterioratory secondary phases. The morphological investigations and compositional analysis of the films were determined using Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) respectively. Atomic Force Microscopy (AFM) was used to estimate the surface roughness of 1.3 nm. The absorption coefficient was found to be 10(4) cm(-1) and bandgap 1.3 eV which qualifies CTS to be a potential candidate for photovoltaic applications. The refractive index, extinction coefficient and relative permittivity of the film were measured by Spectroscopic ellipsometry. Hall effect measurements, indicated the p type nature of the films with a hole concentration of 2 x 10(18) cm(-3), electrical conductivity of 9 S/cm and a hole mobility of 29 cm(2)/V. The properties of CTS as deduced from the current study, present CTS as a potential absorber layer material for thin film solar cells. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Multiferroic Pb(Fe2/3W1/3)O-3 ceramics were synthesized via a modified two-stage Columbite method. Single phase formation was confirmed from the analysis of x-ray and neutron diffraction patterns recorded at room temperature. Structural analysis of the diffraction data reveals cubic phase (space group Pm-3m) for the title compound. Magnetic structure of the title compound at room temperature exhibits G-type antiferromagnetic structure. The Mossbauer spectroscopy and Electron Paramagnetic Resonance (EPR) studies were carried out at 300 K. The isomer shift and quadrupole splitting of the Mossbauer spectra confirms the trivalent state of iron (Fe3+). The Mossbauer spectra also suggest that the iron and tungsten are randomly distributed at the octahedral, B site. EPR spectra show a single broad line associated with Fe3+ ions. Both spectra clearly exhibit weak ferromagnetic behaviour of Pb(Fe2/3W1/3)O-3 ceramic at 300 K. Considering neutron diffraction, Mossbauer and EPR results together, it may be stated here that Pb(Fe2/3W1/3)O-3 exhibits antiferromagnetic behavior along with weak ferromagnetism at room temperature.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Lead magnesium niobate-lead titanate (PMN-PT) is an intriguing candidate for applications in many electronic devices such as multi-layer capacitors, electro-mechanical transducers etc. because of its high dielectric constant, low dielectric loss and high strain near the Curie temperature. As an extension of our previous work on Ta-doped PMNT-PT aimed at optimizing the performance and reducing the cost, this paper focuses on the effect of Pb volatilization on the dielectric properties of 0.77Pb(Mg1/3(Nb0.9Ta0.1)2/3)O3-0.23PbTiO3. The dielectric constant and loss of the samples are measured at different frequencies and different temperatures. The phase purity of this compound is determined by X-ray diffraction pattern. It is found that the volatilization during sintering does influence the phase formation and dielectric properties. The best condition is sintering with 0.5 g extra PbO around a 4 g PMNT-PT sample.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Cooperative director fluctuations in lipid bilayers have been postulated for many years. ^2H-NMR T_1^(-1), T_(1P)^(-1) , and T_2^(-1); measurements have been used identify these motions and to determine the origin of increased slow bilayer motion upon addition of unlike lipids or proteins to a pure lipid bilayer.

The contribution of cooperative director fluctuations to NMR relaxation in lipid bilayers has been expressed mathematically using the approach of Doane et al.^1 and Pace and Chan.^2 The T_2^(-1)’s of pure dimyristoyllecithin (DML) bilayers deuterated at the 2, 9 and 10, and all positions on both lipid hydrocarbon chains have been measured. Several characteristics of these measurements indicate the presence of cooperative director fluctuations. First of all, T_2^(-1) exhibits a linear dependence on S2/CD. Secondly, T_2^(-1) varies across the ^2H-NMR powder pattern as sin^2 (2, β), where , β is the angle between the average bilayer director and the external magnetic field. Furthermore, these fluctuations are restricted near the lecithin head group suggesting that the head group does not participate in these motions but, rather, anchors the hydrocarbon chains in the bilayer.

T_2^(-1)has been measured for selectively deuterated liquid crystalline DML hilayers to which a host of other lipids and proteins have been added. The T_2^(-1) of the DML bilayer is found to increase drastically when chlorophyll a (chl a) and Gramicidin A' (GA') are added to the bilayer. Both these molecules interfere with the lecithin head group spacing in the bilayer. Molecules such as myristic acid, distearoyllecithin (DSL), phytol, and cholesterol, whose hydrocarbon regions are quite different from DML but which have small,neutral polar head groups, leave cooperative fluctuations in the DML bilayer unchanged.

The effect of chl a on cooperative fluctuations in the DML bilayer has been examined in detail using ^2H-NMR T_1^(-1), T_(1P)^(-1) , and T_2^(-1); measurements. Cooperative fluctuations have been modelled using the continuum theory of the nematic state of liquid crystals. Chl a is found to decrease both the correlation length and the elastic constants in the DML bilayer.

A mismatch between the hydrophobic length of a lipid bilayer and that of an added protein has also been found to change the cooperative properties of the lecithin bilayer. Hydrophobic mismatch has been studied in a series GA' / lecithin bilayers. The dependence of 2H-NMR order parameters and relaxation rates on GA' concentration has been measured in selectively deuterated DML, dipalmitoyllecithin (DPL), and DSL systems. Order parameters, cooperative lengths, and elastic constants of the DML bilayer are most disrupted by GA', while the DSL bilayer is the least perturbed by GA'. Thus, it is concluded that the hydrophobic length of GA' best matches that of the DSL bilayer. Preliminary Raman spectroscopy and Differential Scanning Calorimetry experiments of GA' /lecithin systems support this conclusion. Accommodation of hydrophobic mismatch is used to rationalize the absence of H_(II) phase formation in GA' /DML systems and the observation of H_(II) phase in GA' /DPL and GA' /DSL systems.

1. J. W. Doane and D. L. Johnson, Chem. Phy3. Lett., 6, 291-295 (1970). 2. R. J. Pace and S. I. Chan, J. Chem. Phy3., 16, 4217-4227 (1982).

Relevância:

60.00% 60.00%

Publicador:

Resumo:

O aço inoxidável hiperduplex possui alta resistência a corrosão por pite em ambientes contendo cloretos, quando comparado a outros aços inoxidáveis comercialmente conhecidos. Possui boas propriedades mecânicas, com limite de escoamento superior a 700MPa e limite de resistência a tração em torno de 1000MPa. Essas propriedades o tornam muito atrativos para aplicações em ambientes contendo cloretos, e por isso tem tido destaque na indústria de óleo e gás, refinarias, plataformas offshore, etc. A liga hiperduplex é composta por uma estrutura bifásica, contendo proporções aproximadamente iguais de ferrita e austenita. Esse material possui boa soldabilidade, mas por ser termodinamicamente metaestável, em altas temperaturas pode ocorrer a precipitação de fases intermetálicas não desejáveis, o que resulta em perda de propriedades mecânicas e diminuição da resistência a corrosão. A fase sigma tem sido fortemente estudada, pois é comum sua precipitação nos aços inoxidáveis da família duplex durante o procedimento de soldagem se este não for muito bem controlado. A fase sigma precipita preferencialmente na fase ferrítica, devido a maior concentração de Cr e Mo, que são os elementos formadores da fase. A resistência a corrosão é reduzida e as propriedades mecânicas do material são alteradas o tornando frágil devido a presença da fase sigma. É formada entre 600C e 1000C e possui uma estrutura tetragonal complexa. O objetivo do trabalho foi identificar a possível presença da fase sigma na junta soldada do aço inoxidável hiperduplex SAF 2707 HD (UNS S32707) pelo processo TIG autógeno manual através da difração de raios-x. Nessa pesquisa, foram analisadas uma junta soldada do material pelo processo TIG autógeno manual com arco pulsado. Complementando o estudo foram analisadas seis amostras do aço inoxidável superduplex, sendo que cinco amostras sofreram tratamento térmico para a proposital formação da fase sigma. O refinamento do resultado da difração das amostras foi feito utilizando o método de Rietveld no software Topas Academic versão 4.1. O resultado da amostra soldada de hiperduplex apresentou as fases austenita, ferrita e alguns prováveis óxidos. Os resultados das amostras de superduplex tratadas termicamente apresentaram a fase sigma, conforme esperado na pesquisa, e as fases austenita e ferrita.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Os manguezais são ecossistemas estuarinos, representando a transição entre os ambientes continentais e marinhos, e tendo sua formação relacionada com as flutuações do nível do mar no Quaternário. No Manguezal de Guaratiba, diversos estudos sobre as variações do nível do mar, mais precisamente no Holoceno, têm sido realizados, sob os enfoques sedimentológicos, geoquímicos, palinológicos e micropaleontológicos. Entre os estudos micropaleontológicos, destacam-se os que utilizam os foraminíferos bentônicos, micro-organismos amplamente utilizados como indicadores paleoecológicos e paleoambientais do Holoceno. No presente trabalho, foi coletado, através de um amostrador do tipo trado russo, um testemunho (T1) no Manguezal de Guaratiba, no qual foram realizadas análises de parâmetros como granulometria, teores de matéria orgânica (MO), carbonato, carbono orgânico total (COT) e enxofre (S) (abióticos) e da fauna de foraminíferos bentônicos (bióticos). Foram utilizadas também índices ecológicos e análises de agrupamento, através das quais foi possível estabelecer quatro associações faunísticas (I,II,III e IV), assim como os fatores ambientais que mais influenciaram a distribuição da fauna. A correlação com assembleias de foraminíferos de outros testemunhos que possuem datação por Carbono 14 (C14), assim como outros trabalhos que versam sobre a evolução da Baía de Sepetiba, permitiu o estabelecimento de três ciclos de emersão-submersão para a área da planície de maré estudada: 1)Fase transgressiva: nível de concentração de conchas em depósitos lagunares formados por sedimentos finos, sem foraminíferos; provavelmente posterior a uma regressão; 2) Fase transgressiva: formação de uma baía, com presença exclusiva de espécies de foraminíferos calcários (Associação III) com maiores valores de riqueza e queda nos valores de COT; ocorrida há cerca de 3.800 anos A.P 3) Fase transgressiva: período de submersão, presença de espécies de foraminíferos tipicamente estuarinos (Associação IV), com duração entre 3.500 anos A.P. e 2.700 anos A.P.; 4)Fase transgressiva: caracterizada pela alternância entre a formação de baías rasas e lagunas marinhas (maiores índices de riqueza nas associações faunísticas), menores valores de MO e COT e aumento na proporção de sedimentos finos; evento iniciado há cerca de 2.700 anos A.P.; e 5)Fase regressiva: fauna de foraminíferos aglutinantes, resistente às condições de salinidade e acidez características de ambientes confinados como os manguezais, além do incremento nos teores de areia, evidenciando a fase final de confinamento da Baía de Sepetiba pela Restinga da Marambaia; evento iniciado por volta de 2.400 anos A.P., estendendo-se até o presente. Os resultados obtidos mostram a importância da correlação lateral entre testemunhos na interpretação paleoambiental da Baía de Sepetiba, além da identificação de estágios de transgressão e regressão que se aproximam da curva de variação do nível do mar proposta por SUGUIO et al.(1985) para o litoral do Estado do Rio de Janeiro

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The structural and magnetic properties of Sm ion-implanted GaN with different Sm concentrations are investigated. XRD results do not show any peaks associated with second phase formation. Magnetic investigations performed by superconducting quantum interference device reveal ferromagnetic behavior with an ordering temperature above room temperature in all the implanted samples, while the effective magnetic moment per Sm obtained from saturation magnetization gives a much higher value than the atomic moment of Sm. These results could be explained by the phenomenological model proposed by Dhar et al. [Phys. Rev. Lett. 94(2005) 037205, Phys. Rev. B 72(2005) 245203] in terms of a long-range spin polarization of the GaN matrix by the Sm atoms.