611 resultados para EU3


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Y2O3:Eu3+ nanocrystals were prepared by combustion synthesis. The particle size estimated by X-ray powder diffraction (XRD) was about 10 nm. A blue-shift of the charge-transfer (CT) band in excitation spectra was observed in Y2O3:Eu3+ nanocrystals compared with bulk Y2O3:Eu3+. The electronic structure Of Y2O3 is calculated by density functional method and exchange and correlation have been treated by the generalized gradient approximation (GGA) within the scheme due to Perdew-Burke-Ernzerhof (PBE). The calculated results show that the energy centroid of 5d orbital in nanocrystal has increasing trend compared with that in the bulk material. The bond length and bond covalency are calculated by chemical bond theory. The bond lengths of Y2O3:Eu3+ nanocrystal are shorter than those of the bulk counterpart and the bond covalency of Y2O3:Eu3+ nanocrystal also has an increasing trend. By combining centroid shift and crystal-field splitting, the blue-shift of the CT band is interpreted.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dielectric definition of average energy gap E-g of the chemical bond has been calculated quantitatively in Eu3+-doped 30 lanthanide compounds based on the dielectric theory of chemical bond for complex structure crystals. The relationship between the experimental charge transfer (CT) energy of Eu3+ and the corresponding average energy gap E-g has been studied. The results show that the CT energy increases linearly with increasing of the average energy gap E-g. The linear model is obtained. It allows us to predict the CT position of Eu3+-doped lanthanide compounds with knowledge of the crystal structure and index of refraction. Applied to the Ca4GdO(BO3)(3):Eu and Li2Lu5O4(BO3)(3):Eu crystals, the predicted results of CT energies are in good agreement with the experimental values, and it can be concluded that the lowest CT energy in Li2Lu5O4(BO3)(3):Eu originates from the site of Lu1.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The deposition and coating of GdVO4: Eu3+ nanoparticles on spherical silica was carried out using a simple sol - gel method at low temperature. The GdVO4: Eu3+-coated silica composites obtained were characterized by differential thermal analysis (DTA), thermogravimetric (TG) analysis, x-ray diffraction (XRD), Fourier-transform IR spectroscopy (FT-IR), transmission electron microscopy (TEM), x-ray photoelectron spectroscopy (XPS), photoluminescence spectra, and kinetic decay. It is found that the similar to 5 nm GdVO4: Eu3+ nanoparticles coating the silica spheres are crystal in the as-prepared samples and the crystallinity increases with increasing annealing temperature. The composites obtained are spherical in shape with an average size of 100 nm. The GdVO4: Eu3+ nanoparticles are linked with silica cores by a chemical bond. The photoluminescence spectra of the obtained GdVO4: Eu3+-coated silica composites are similar to those of the bulk GdVO4: Eu3+ phosphors. The strongest peak is near 617 nm, which indicates that Eu3+ is located in the low symmetry site with non-inversion centre.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spherical and submicrometer-sized hollow Gd2O3:Eu3+ phosphors were prepared by homogeneous precipitation and hydrothermal method by varying the concentrations of reactants and changing the synthesis conditions. In the precipitation step, the spherical nucleus was formed and grew to large particles. In the hydrothermal step, the large particles crystallized to solid or hollow spheres. At last, Gd2O3:Eu3+ phosphors were obtained by annealing at the temperature more than 600 degrees C. The deduced mechanics of forming the solid and hollow spheres was proposed. And the obtained spherical Gd2O3:Eu3+ phosphors had better red luminescence properties. The relative luminescence intensity and the lifetime increased with increasing annealing temperatures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The nanocrystalline Gd2O3:Eu3+ powders with cubic phase were prepared by a combustion method in the presence of urea and glycol. The effects of the annealing temperature on the crystallization and luminescence properties were studied. The results of XRD show pure phase can be obtained, the average crystallite size could be calculated as 7, 8, 45, and 23 run for the precursor and samples annealed at 600, 700 and 800 degrees C, respectively, which coincided with the results from TEM images. The emission intensity, host absorption and charge transfer band intensity increased with increasing the temperature. The slightly broad emission peak at 610 nm for smaller particles can be observed. The ratio of host absorption to O-2-Eu3+ charge transfer band of smaller nanoparticles is much stronger compared with that for larger nanoparticles, furthermore, the luminescence lifetimes of nanoparticles increased with increasing particles size. The effects of doping concentration of Eu3+ on luminescence lifetimes and intensities were also discussed. The samples exhibited a higher quenching concentration of Eu3+, and luminescence lifetimes of nanoparticles are related to annealing temperature of samples and the doping concentration of Eu3+ ions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A reduction phenomenon of Eu3+ -> Eu2+ was observed for the first time when Eu3+ ions were doped into an AlO4-tetrahedron-containing compound BaAl2O4 in an oxidizing atmosphere of air by high-temperature solid-state reaction. X-ray powder diffraction patterns and photoluminescent spectra are used to confirm the compound structure and detect the simultaneous existence of both divalent and trivalent europium ions, respectively. The abnormal Eu3+ -> Eu2+ reduction is explained by a charge compensation model. Spectroscopic properties of BaAl2O4:Eu are discussed and Eu2+ emission spectrum shows consistence with the results reported by Katsumata et a]. [J. Cryst. Growth 198/199 (1999) 869.] and Lin et al. [Mater. Chem. Phys. 70 (2001) 156.].

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LEDSrCaSiO4:Eu3+.XRD,Pmnb;SrCaSiO4:Eu3+<12()Eu3+.,397nm,LED,612592586nm;SrCaSiO4:Eu3+Eu3+10(),(Re)1.2nm.,3ms

Relevância:

20.00% 20.00%

Publicador:

Resumo:

BaF2 nanocrystals doped with 5.0 mol% Eu3+ has been successfully synthesized via a facile, quick and efficient ultrasonic solution route employing the reactions between Ba(NO3)(2), Eu(NO3)(3) and KBF4 under ambient conditions. The product was characterized via X-ray powder diffraction (XRD), scanning electron micrographs (SEM), transmission electron microscopy (TEM), high-resolution transmission electron micrographs (HRTEM), selected area electron diffraction (SAED) and photoluminescence (PL) spectra. The ultrasonic irradiation has a strong effect on the morphology of the BaF2:Eu3+ particles. The caddice-sphere-like particles with an average diameter of 250 nm could be obtained with ultrasonic irradiation, whereas only olive-like particles were produced without ultrasonic irradiation. The results of XRD indicate that the obtained BaF2:Eu3+ nanospheres crystallized well with a cubic structure. The PL spectrum shows that the BaF2:Eu3+ nanospheres has the characteristic emission of Eu3+ D-5(0)-F-7(J) (J = 1-4) transitions, with the magnetic dipole D-5(0)-F-7(1) allowed transition (590 nm) being the most prominent emission line.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It is reported for the first time that the slow electrochemical kinetics process for the electro-oxidation of ethanol can be promoted by changing the electrochemical environment. The electro-oxidation of ethanol at a Pt electrode in the presence of Eu3+ cations was studied and an enhancement effect was exhibited. Cyclic voltammetry experiment results showed that the peak current density for the electro-oxidation of ethanol was increased in the presence of EU3+ in the ethanol solution. A preliminary discussion of the mechanism of the enhancement effect is given. This is based on a CO stripping experiment, which shows that either the onset potential or the peak potential of CO oxidation is shifted negatively after adding Eu3+ to the solution.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Gd2O3: EU3+ phosphors were prepared by urea homogeneous precipitation with different surfactant and sol-gel method. XRD patterns show that all the obtained samples are in cubic Gd2O3, and the results of FTIR and fluorescent spectra conformed that OP is a good surfactant for preparing the Gd2O3: Eu3+ phosphors. The SEM photographs show that the particles prepared by urea homogeneous precipitation method are all spherical and well-dispersed, and grain morphology can be controlled by different surfactant. XRD and SEM indicate that the particle sizes prepared by sol-gel method are in the range of 5 similar to 30 nm, and the grain sizes increase with increasing of heated temperatures. Luminescence spectra indication that the main emission peaks of all samples are at 610 nm, the intensities are different from samples prepared with different surfactant and the luminescence intensities increase with increasing of annealed temperatures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The monodisperse array and nanowires Of Y2O3:Eu3+ phosphor were synthesized using anodic aluminum oxide (AAO) template by sol-gel method. Scanning electron microscope (SEM) images indicated that Y2O3:Eu3+ nanowires are parallelly arranged, all of which are in uniform diameter of about 50 nm. The high-magnification SEM image showed that each nanowire is composed of a lot of agglutinating particles. The patterns of selected-area electron diffraction confirmed that Y2O3:EU3+ nanowires mainly consist of polycrystalline materials. Excitation and emission spectra Of Y2O3:E U3+/AAO composite films were measured. The characteristic red emission peak of EU3+ ion attributed to D-5(0)-->F-7(2) transition in Y2O3:EU3+/AAO nanowires broadened its halfwidth.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Vaterite-type YBO3:Eu3+ crystals with interesting flower and hedgehog fungus-like structures composed of nanosheets were obtained by controlled crystallization of Y2O3 and Eu2O3 in H3BO3 solutions under acidic hydrothermal (HT) conditions. Nanosheets of uniform thicknesses were formed by preferential crystal growth along the (100) crystallographic plane and specific three-dimensional structures were further developed through a homocentric growth mechanism. Optical emission measurements showed that the HT-grown nanosheet crystals exhibited a higher ratio of the emitted red-to-orange light ratio than crystals grown from solid-state reactions. The photoluminescence intensity and emission lifetimes were also studied as a function of the Eu3+ dopant concentration and the HT synthesis temperature. The effect of some additives: a chelating ligand, a surfactant and a polymer, on the YBO3:Eu3+ crystals morphology was also investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using CaCO3, metal oxides (all dissolved by nitric acid) and tetraethoxysilane Si(OC2H5)(4) (TEOS) as the main starting materials, Ca2R8(SiO4)(6)O-2:A (R = Y, La, Gd; A = EU3+, Tb3+) phosphor films have been dip-coated on quartz glass substrates through the sol-gel process. X-ray diffraction (XRD), atomic force microscope (AFM), scanning electron microscope (SEM) and photoluminescence (PL) spectra as well as lifetimes were used to characterize the resulting films. The results of XRD indicated that the 1000 degreesC annealed films are isomorphous and crystallize with the silicate oxyapatite structure. AFM and SEM studies revealed that the phosphor films consisted of homogeneous particles ranging from 30 to 90 nm, with an average thickness of 1.30 mum. The Eu3+ and Tb3+ show similar spectral properties independent of R 3, in the films due to their isomorphous crystal structures. However, both the emission intensity and lifetimes of Eu3+ and Tb3+ in Ca2R8(SiO4)(6)O-2 (R = Y, La, Gd) films decrease in the sequence of R = Gd > R = Y > R = La, which have been explained in accordance with the crystal structures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

X-2-y(2)SiO(5):A (A = Eu3+, Tb3+, Ce3+) phosphor films and their patterning were fabricated by a sol-gel process combined with a soft lithography. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), atomic force microscopy (AFM), scanning electron microscopy (SEM) optical microscopy and photoluminescence (PL) were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 900 degreesC with X-1-Y2SiO5, which transformed completely to X-2-Y2SiO5 at 1250 degreesC. Patterned thin films with different band widths (5 pin spaced by 5 pm and 16 pm spaced by 24 pm) were obtained by a soft lithography technique (micromoulding in capillaries, MIMIC). The SEM and AFM study revealed that the nonpattemed phosphor films were uniform and crack free, and the films mainly consisted of closely packed grains with an average size of 350 run. The doped rare earth ions (A) showed their characteristic emissions in X-2-Y2SiO5 phosphor films, i.e., D-5(0)-F-7(J) (J = 0, 1, 2,3,4) for Eu3+, D-5(3), (4)-F-7(J) (J = 6, 5, 4, 3) for Tb3+ and 5d (D-2)-4f (F-2(2/5),(2/7)) for Ce3+, respectively. The optimum doping concentrations for EU3+, Tb3+ were determined to be 13 and 8 mol% of Y3+ in X-2-Y2SiO5 films, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Gd2Ti2O7: Eu3+ thin film phosphors were fabricated by a sol-gel process. X-ray diffraction (XRD), atomic force microscopy (AFM) and photoluminescence (PL) spectra as well as lifetimes were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 800 degreesC and the crystallinity increased with the elevation of annealing temperatures. Uniform and crack free phosphor films were obtained, which mainly consisted of grains with an average size of 70 nm. The doped Eu3+ showed orange-red emission in crystalline Gd2Ti2O7 phosphor films due to an energy transfer from Gd2Ti2O7 host to them. Both the lifetimes and PL intensity of the Eu3+ increased with increasing the annealing temperature from 800 to 1000 degreesC, and the optimum concentrations for Eu3+ were determined to be 9 at.%. of Gd3+ in Gd2Ti2O7 film host.