994 resultados para Rubber Treatment
Resumo:
A super-tough polycarbonate (PC) blend was obtained by using epoxidized ethylene propylene diene (eEPDM) rubber as modifier. The notched Izod impact strength of PC/eEPDM (96/4) blend shows a great improvement, with a value about 25 times of that of pure PC. Finely and homogeneously dispersed rubber particles (0.2-0.8 mu m) in the PC matrix indicated good adhesion between the eEPDM rubber phase and the PC matrix. (C) 1997 Elsevier Science Ltd.
Resumo:
Measurement of iron and manganese is very important in evaluating the quality of natural waters. We have constructed an automated Fe(II), total dissolved iron(TDI), Mn(II), and total dissolved manganese(TDM) analysis system for the quality control of underground drinking water by reverse flow injection analysis and chemiluminescence detection(rFIA-CL), The method is based on the measurement of the metal-catalyzed light emission from luminol oxidation by potassium periodate. The typical signal is a narrow peak, in which the height is proportional to light emitted and hence to the concentration of metal ions. The detection limits were 3 x 10(-6) mu g ml(-1) for Fe(II) and the linear range extents up to 1.0 x 10(-4) and 5 x 10(-6) mu g ml(-1) for Mn(II) cover a linear range to 1.0 x 10(-4) mu g ml(-1). This method was used for automated in-situ monitoring of total dissolved iron and total dissolved in underground water during water treatment. (C) 1997 Elsevier Science B.V.
Resumo:
In this paper, epoxidation of ethylene propylene diene rubber by in situ generated performic acid is discussed. The samples have been characterized by infra-red and H-1-nuclear magnetic resonance analyses. Quantitative analysis of the reaction products is made possible by using the methyl deformation band at 1377 cm(-1) as internal standard. The conversion of double bonds increases rapidly within the first 1 h, then gradually, over 2 h, has only a slight increase. The maximum conversion ratio of double bonds is about 70%. The relative content of epoxy groups has a top value at about 7 h. The side reactions are also discussed. (C) 1997 Elsevier Science Ltd.
Resumo:
Using the wide-angle X-ray diffraction method, the variation of crystallographic parameters of poly(aryl ether ether ketone ketone) (PEEKK) has been studied in different heat treatment temperatures. All the reflections and their intensities as well as their Miller indices are presented in detail according to an orthorhombic system. The investigation indicates that the unit cell parameters a, b, c and the unit cell volume V systematically decrease with increasing heat treatment temperature. This variation is interpreted by the change of conformation of polymer molecular chains during thermal treatment. The results calculated from the formula of degree of crystallinity (W-c,W-x) for PEEKK, which was derived based on X-ray scattering intensity theory and the graphic multipeak resolution method, are compatible with the density measurement (W-c,W-d) and calorimetry (W-c,W-h) values. (C) 1997 Elesevier Science Ltd.