998 resultados para Gold alloy
Resumo:
A novel method for fabrication of horseradish peroxidase (HRP) biosensor has been developed by self-assembling gold nanoparticles on thiol-functionalized poly(styrene-co-acrylic acid) (St-co-AA) nanospheres. At first, a cleaned gold electrode was immersed in thiol-functionalized poly(St-co-AA) nanosphere latex prepared by emulsifier-free emulsion polymerization of St with AA and function with dithioglycol to assemble the nanospheres, then gold nanoparticles were chemisorbed onto the thiol groups. Finally, horseradish peroxi- dase was immobilized on the surface of the gold nanoparticles. The sensor displayed an excellent electrocatalytical response to reduction of H2O2 without the aid of an electron mediator. The sensor was highly sensitive to hydrogen peroxide with a detection limit of 4.0 mumol l(-1), and the linear range was from 10.0 mumol l(-1) to 7.0 mmol l(-1). The biosensor retained more than 97.8% of its original activity after 60 days of use. Moreover, the Studied biosensor exhibited good current repeatability and good fabrication reproducibility.
Resumo:
A simple, green method was developed for the synthesis of gold and silver nanoparticles by using polysaccharides as reducing/stabilizing agents. The obtained positively charged chitosan-stabilized gold nanoparticles and negatively charged heparin-stabilized silver nanoparticles were characterized with UV-vis spectroscopy and transmission electron microscopy. The results illustrated the formation of gold and silver nanoparticles inside the nanoscopic polysaccharide templates. Moreover, the morphology and size distribution of prepared gold and silver nanoparticles varied with the concentration of both the polysaccharides and the precursor metal salts.
Resumo:
Gold nanoparticles were prepared by reducing gold salt with a polysaccharide, chitosan, in the absence/ presence of tripolyphosphate (TPP). Here, chitosan acted as a reducing/stabilizing agent. The obtained gold nanoparticles were characterized with UV-vis spectroscopy and transmission electron microscopy. The results indicated that the shape and size distribution of gold nanoparticles changed with the molecular weight and concentration of chitosan. More interestingly, the gelation of chitosan upon contacting with polyanion (TPP) can also affect the shape and size distribution of gold nanoparticles. By adding TPP to chitosan solution before the reduction of gold salt, gold nanoparticles have a bimodal size distribution, and at the same time, polygonal gold particles were obtained in addition to spherical gold nanoparticles.
Resumo:
The RENi3 (RE = La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Y) series compounds have been prepared by arc melting constituent elements under Ar atmosphere. X-ray diffraction (XRD) analysis reveals that the as-prepared alloys have different lattice parameters and cell volumes, depending on different rare earth (RE) element. The electrochemical characteristics, including the electrochemical capacity, P-C isotherms, high rate chargeability (HRC) and high-rate dischargeability (HRD), of these alloys have been studied through the charge-discharge recycle testing at different temperatures, charge currents and discharge currents. The results show that YNi3 has the largest cell volume, smallest density, and moreover, it shows more satisfactory electrochemical characteristics than other alloys, including discharge capacity, HRC, HRD and low temperature dischargeablity.
Resumo:
In this Letter, P-cyclodextrin (P-CD) was employed as stabilizer in the synthesis of gold nanoparticles. Gold nanoparticles were synthesized by the reduction of HAuCl4 by NaBH4 in the presence of P-CD. Varying the ratio of P-Cl) to HAuCl4, isolated gold nanoparticles could be assembled into nanowires. The nanoparticles and nanowires were characterized by transmission electron microscopy, UV/visible spectroscopy, infrared spectroscopy and X-ray photoelectron spectroscopy. The decreased relative intensity of skeletal and ring vibration in FT-IR spectra and the negative shift of the Au4f(7/2) binding energy in XPS spectra confirmed that beta-CD was chemisorped on An nanoparticles via hydroxyl group.
Resumo:
One-dimensional gold/polyaniline (Au/PANI-CSA) coaxial nanocables with an average diameter of 5060 nm and lengths of more than 1 mu m were successfully synthesized by reacting aniline monomer with chlorauric acid (HAuCl4) through a self-assembly process in the presence Of D-camphor-10-sulfonic acid (CSA), which acts as both a dopant and surfactant. It was found that the formation probability and the size of the Au/PANI-CSA nanocables depends on the molar ratio of aniline to HAuCl4 and the concentration of CSA, respectively. A synergistic growth mechanism was proposed to interpret the formation of the Au/PANI-CSA nanocables. The directly measured conductivity of a single gold/polyaniline nanocable was found to be high (approximate to 77.2S cm(-1)). Hollow PANI-CSA nanotubes, with an average diameter of 50-60 nm, were also obtained successfully by dissolving the Au nanowire core of the Au/PANI-CSA nanocables.
Resumo:
A useful method for the synthesis of various gold nanostructures is presented. The results demonstrated that flowerlike nanoparticle arrays, nanowire networks, nanosheets, and nanoflowers were obtained on the solid substrate under different experimental conditions. In addition, surface-enhanced Raman scattering (SERS) spectra of 4-aminothiophenol (4-ATP) on the as-prepared gold nanostructures of various shapes were measured, and their shape-dependent properties were evaluated. The intensity of the SERS signal was the smallest for the gold nanosheets, and the flowerlike nanoparticle arrays gave the strongest SERS signals.