The nucleotide sequence encoding the C terminus of the nucleocapsid protein of measles virus (MV) is the most variable in the genome. The sequence of this region is reported for 21 new MV strains and for virus RNA obtained from cases of subacute panencephalitis (SSPE) tissue. The nucleotide sequence of a total of 65 MV strains has been analysed using the CLUSTAL program to determine the relationships between the strains. An unrooted tree shows that eight different genotypes can be discerned amongst the sequences analysed so far. The data show that the C-terminal coding sequence of the nucleocapsid gene, although highly variable between strains, is stable in a given strain and does not appear to diverge in tissue culture. It therefore provides a good 'signature' sequence for specific genotypes. The sequence of this region can be used to discriminate new imported viruses from old 'endemic' strains of MV in a geographical area. The different genotypes are not geographically restricted although some appear to be the mainly 'endemic' types in large areas of the world. In global terms there appears to be at least four co-circulating genotypes of MV. The low level of divergence in the Edmonston lineage group isolated before 1970 indicates that some isolates are probably laboratory contaminants. This applies to some SSPE isolates such as the Halle, Mantooth and Horta-Barbosa strains as well as some wild-type isolates from that period.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Compared to other cereals, rice has particular strong As accumulation. Therefore, it is very important to understand As uptake and translocation among different genotypes. A field study in Chenzhou city, Hunan province of China, was employed to evaluate the effect of arsenic-contaminated soil on uptake and distribution in 34 genotypes of rice (including unpolished rice, husk, shoot, and root). The soil As concentrations ranged from 52.49 to 83.86 mg kg-1, with mean As concentration 64.44 mg kg-1. The mean As concentrations in rice plant tissues were different among the 34 rice genotypes. The highest As concentrations were accumulated in rice root (196.27-385.98 mg kg-1 dry weight), while the lowest was in unpolished rice (0.31-0.52 mg kg-1 dry weight). The distribution of As in rice tissue and paddy soil are as follows root » soil > shoot > husk > unpolished rice. The ranges of concentrations of inorganic As in all of unpolished rice were from 0.26 to 0.52 mg kg-1 dry weight. In particular, the percentage of inorganic As in the total As was more than 67 %, indicating that the inorganic As was the predominant species in unpolished rice. The daily dietary intakes of inorganic As in unpolished rice ranged from 0.10 to 0.21 mg for an adult, and from 0.075 to 0.15 mg for a child. Comparison with tolerable daily intakes established by FAO/WHO, inorganic As in most of unpolished rice samples exceeded the recommended intake values. The 34 genotypes of rice were classified into four clusters using a criteria value of rescaled distance between 5 and 10. Among the 34 genotypes, the genotypes II you 416 (II416) with the lowest enrichment of As and the lowest daily dietary intakes of inorganic As could be selected as the main cultivar in As-contaminated field.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Laser welding is an important process for fabricating complex components involving NiTi shape memory
alloy. As welding is a thermal process, the amount of heat input and the rate of cooling have significant
impact on the microstructure and hence the resultant characteristics of NiTi. In this study, the effect of
laser welding and post-weld-annealing from 573 K to 1173 K on the thermal phase transformation behaviors,
tensile deformation and micro-hardness characteristics of the laser-welded NiTi thin foils were investigated.
It was found that the as-welded sample exhibited inferior super-elasticity compared to the base
material, and the super-elasticity could be partially restored by annealing at 573 K. On the other hand,
annealing of the weldment above the recrystallization temperature would lower the super-elasticity.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this study, two L27 Taguchi experiments were carried out to study the effect of fibre laser welding parameters and their interactions upon the weld bead aspect ratio of nickel–titanium thin foil. The optimum parameters to produce full penetrated weld with the largest aspect ratio and desirable microstructure were successfully obtained by the Taguchi experimental design. The corrosion property of the optimized NiTi weld in Hank’s solution at 37.5 °C was studied and compared with the as-received NiTi. To improve the corrosion properties of the weld, the effect of post-weld-heat-treatments ranging from 573 to 1173 K was investigated. The corrosion properties, surface morphology, microstructure and Ti/Ni ratio of the heat-treated NiTi weld were analysed. It was found that a post-weld heat treatment at 573 K for 1 h provided the best pitting corrosion resistance at the weld zone.