Photocatalytic degradation of estriol (E3) in an aqueous medium was investigated in the presence of TiO2 microcrystallized glass plates. To begin with, transparent glasses associated with the composition 0.4BaO-0.4TiO(2)-B2O3 (BTBO) were fabricated by the conventional melt-quench technique and subsequently subjected to controlled heat treatment at an appropriate temperature to grow anatase TiO2 microcrystals in the glass matrix. The fabricated samples were subjected to differential scanning calorimetry. X-ray diffraction and scanning electron microscopy to obtain thermal, structural and microstructural details. The photocatalytic activity of glass samples for estriol degradation was monitored by fluorescence spectroscopy. The limit of detection for estriol using fluorescence spectroscopy was analyzed. The results showed that microcrystallized TiO2 glass composites have more photocatalytic activity than as quenched glass. The degradation rate coefficient of microcrystallized TiO2 glass composite (334.54 min(-1) m(-2)) was found to be ten times larger than that of the as-quenched BTBO glasses (37.74 min(-1) m(-2)) implying that the anatase phase of TiO2 in BTBO glasses was responsible for high photocatalytic activity of estriol degradation. (c) 2014 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Microfluidic/optofluidic microscopy is a versatile modality for imaging and analyzing properties of cells/particles while they are in flow. In this paper, we demonstrate the integration of fused silica microfluidics fabricated using femtosecond laser machining into optofluidic imaging systems. By using glass for the sample stage of our microscope, we have exploited its superior optical quality for imaging and bio-compatibility. By integrating these glass microfluidic devices into a custom-built bright field microscope, we have been able to image red blood cells in flow with high-throughputs and good fidelity. In addition, we also demonstrate imaging as well as detection of fluorescent beads with these microfluidic devices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It is frequently assumed that in the limit of vanishing cooling rate, the glass transition phenomenon becomes a thermodynamic transition at a temperature T-K. However, with any finite cooling rate, the system falls out of equilibrium at temperatures near T-g(> T-K), implying that the very existence of the putative thermodynamic phase transition at T-K can be questioned. Recent studies of systems with randomly pinned particles have hinted that the thermodynamic glass transition may be observed for liquids with randomly pinned particles. This expectation is based on the results of approximate calculations that suggest that the thermodynamic glass transition temperature increases with increasing concentration of pinned particles and it may be possible to equilibrate the system at temperatures near the increased transition temperature. We test the validity of this prediction through extensive molecular dynamics simulations of two model glass-forming liquids in the presence of random pinning. We find that extrapolated thermodynamic transition temperature T-K does not show any sign of increasing with increasing pinning concentration. The main effect of pinning is found to be a rapid decrease in the kinetic fragility of the system with increasing pin concentration. Implications of these observations for current theories of the glass transition are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

One of the desired properties for any new biomaterial composition is its long-term stability in a suitable animal model and such property cannot be appropriately assessed by performing short-term implantation studies. While hydroxyapatite (HA) or bioglass coated metallic biomaterials are being investigated for in vivo biocompatibility properties, such study is not extensively being pursued for bulk glass ceramics. In view of their inherent brittle nature, the implant stability as well as impact of long-term release of metallic ions on bone regeneration have been a major concern. In this perspective, the present article reports the results of the in vivo implantation experiments carried out using 100% strontium (Sr)-substituted glass ceramics with the nominal composition of 4.5 SiO2-3Al(2)O(3)-1.5P(2)O(5)-3SrO-2SrF(2) for 26 weeks in cylindrical bone defects in rabbit model. The combination of histological and micro-computed tomography analysis provided a qualitative and quantitative understanding of the bone regeneration around the glass ceramic implants in comparison to the highly bioactive HA bioglass implants (control). The sequential polychrome labeling of bone during in vivo osseointegration using three fluorochromes followed by fluorescence microscopy observation confirmed homogeneous bone formation around the test implants. The results of the present study unequivocally confirm the long-term implant stability as well as osteoconductive property of 100% Sr-substituted glass ceramics, which is comparable to that of a known bioactive implant, that is, HA-based bioglass. (c) 2014 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 103B: 1168-1179, 2015.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Glass formation has been examined in the system 15PbO.xPbCl(2).(85-x)PbBr2 (where 0 <= x <= 25)where the PbO concentration is kept constant while PbCl2 and PbBr2 concentrations are varied. The glasses have been examined using thermal and spectroscopic techniques. T-8, Delta C-p, refractive index, optical basicity have been found to remain unaffected by the composition which is a curious feature of these glasses. It is found that there is a wide infrared window available for use in the investigated glasses. The IR window extends from 1000 to 1500 cm(-1) and in glasses where PbCl2 is less than 20 mol%, the window extends up to 2260 cm(-1). X-ray photoelectron spectra (XPS) revealed that the 4f(5/2) and 4f(7/2) peaks due to f-level transitions have a constant difference in energies, but with energy and FWHM values that varying sensitively and systematically with composition. The observations are discussed and suitable explanations are provided.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present study discusses the photosensitivity of GeS2 chalcogenide glass in response to irradiation with femtosecond pulses at 1047 nm. Bulk GeS2 glasses are prepared by conventional melt quenching technique and the amorphous nature of the glass is confirmed using X-ray diffraction. Ultrafast laser inscription technique is used to fabricate the straight channel waveguides in the glass. Single scan and multi scan waveguides are inscribed in GeS2 glasses of length 0.65 cm using a master oscillator power amplifier Yb doped fiber laser (IMRA mu jewel D400) with different pulse energy and translation speed. Diameters of the inscribed waveguides are measured and its dependence on the inscription parameters such as translation speed and pulse energy is studied. Butt coupling method is used to characterize the loss measurement of the inscribed optical waveguides. The mode field image of the waveguides is captured using CCD camera and compared with the mode field image of a standard SMF-28 fibers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dependence of shear yield strain, the activation energy and volume of shear transformation zone on the glass transition temperature was investigated through the analysis of statistical distributions of the first pop-in events during spherical indentation of four different thin film metallic glasses. Only the Cu-Zr metallic glass exhibits a bimodal distribution of the first pop-in loads, whereas W-Ru-B, Zr-Cu-Ni-Al and La-Co-Al metallic glasses show an unimodal distribution. Results show that shear yield strain and activation energy of shear transformation zone decrease whereas the volume of shear transformation zone increases with increasing homologous temperature, indicating that it is the activation energy rather than the volume of shear transformation zone that controls shear yield strain. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(vinyl butyral) - MMT clay nanocomposites were synthesized in situ with three different degrees of acetalization and with varying clay content for each vinyl butyral polymer ratio. The clay nano-platelet galleries were expanded, as determined by X-ray diffraction and TEM analysis. The glass transition temperature of the polymer nanocomposites were found to be similar to 56 degrees C and similar to 52 degrees C for the neat polymer and the 4% clay loaded samples, respectively. The 4 wt% clay loaded film showed higher strength and low strain to failure. The dynamic mechanical analysis also confirmed the improved stability of the matrix. The matrix with 0.5 butyral to alcohol ratio for 4 wt% clay exhibited good water vapor transmission compared to all other compositions. The encapsulated devices with 2.5 and 4 wt% clay loaded films increases the device life time and the efficiencies of these films were 50% higher than their encapsulated pristine polymer films. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Recent experiments have shown that nano-sized metallic glass (MG) specimens subjected to tensile loading exhibit increased ductility and work hardening. Failure occurs by necking as opposed to shear banding which is seen in bulk samples. Also, the necking is generally observed at shallow notches present on the specimen surface. In this work, continuum finite element analysis of tensile loading of nano-sized notched MG specimens is conducted using a thermodynamically consistent non-local plasticity model to clearly understand the deformation behavior from a mechanics perspective. It is found that plastic zone size in front of the notch attains a saturation level at the stage when a dominant shear band forms extending across the specimen. This size scales with an intrinsic material length associated with the interaction stress between flow defects. A transition in deformation behavior from quasi-brittle to ductile becomes possible when this critical plastic zone size is larger than the uncracked ligament length. These observations corroborate with atomistic simulations and experimental results. (C) 2015 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The central problem in the study of glass-forming liquids and other glassy systems is the understanding of the complex structural relaxation and rapid growth of relaxation times seen on approaching the glass transition. A central conceptual question is whether one can identify one or more growing length scale(s) associated with this behavior. Given the diversity of molecular glass-formers and a vast body of experimental, computational and theoretical work addressing glassy behavior, a number of ideas and observations pertaining to growing length scales have been presented over the past few decades, but there is as yet no consensus view on this question. In this review, we will summarize the salient results and the state of our understanding of length scales associated with dynamical slow down. After a review of slow dynamics and the glass transition, pertinent theories of the glass transition will be summarized and a survey of ideas relating to length scales in glassy systems will be presented. A number of studies have focused on the emergence of preferred packing arrangements and discussed their role in glassy dynamics. More recently, a central object of attention has been the study of spatially correlated, heterogeneous dynamics and the associated length scale, studied in computer simulations and theoretical analysis such as inhomogeneous mode coupling theory. A number of static length scales have been proposed and studied recently, such as the mosaic length scale discussed in the random first-order transition theory and the related point-to-set correlation length. We will discuss these, elaborating on key results, along with a critical appraisal of the state of the art. Finally we will discuss length scales in driven soft matter, granular fluids and amorphous solids, and give a brief description of length scales in aging systems. Possible relations of these length scales with those in glass-forming liquids will be discussed.